TWI765502B - A method for forming the groove of a golf club head - Google Patents

A method for forming the groove of a golf club head Download PDF

Info

Publication number
TWI765502B
TWI765502B TW109146683A TW109146683A TWI765502B TW I765502 B TWI765502 B TW I765502B TW 109146683 A TW109146683 A TW 109146683A TW 109146683 A TW109146683 A TW 109146683A TW I765502 B TWI765502 B TW I765502B
Authority
TW
Taiwan
Prior art keywords
groove
club head
forming
semi
mold
Prior art date
Application number
TW109146683A
Other languages
Chinese (zh)
Other versions
TW202224831A (en
Inventor
李柏宗
Original Assignee
復盛應用科技股份有限公司
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 復盛應用科技股份有限公司 filed Critical 復盛應用科技股份有限公司
Priority to TW109146683A priority Critical patent/TWI765502B/en
Priority to CN202111061820.8A priority patent/CN114682689B/en
Application granted granted Critical
Publication of TWI765502B publication Critical patent/TWI765502B/en
Publication of TW202224831A publication Critical patent/TW202224831A/en

Abstract

A method for forming the groove of a golf club head is used to solve the problem that in the conventional method of forming the groove of the head, the upper die does not correspond to the position of the groove of the head correctly, which leads to the problem that the head product is defective. This method includes: cold pressing a semi-finished club with a first forming pressure by a first die and a second die, the first die has a cavity, the back of the semi-finished club is positioned in the cavity, and the second die have a groove forming protrusion, and the groove forming protrusion is used to form a rough groove-shaped part on the face of the semi-finished club; and the first die is separated from the second die, Remove the semi-finished club form the first die; after the semi-finished club is positioned on the groove forming protrusion of the second die with the rough groove-shaped part, the semi-finished club is cold pressed with a second forming pressure.

Description

高爾夫桿頭線溝成形方法Golf club head groove forming method

本發明係關於一種桿頭線溝成形方法,尤其是一種冷壓以成形線溝的高爾夫桿頭線溝成形方法。The present invention relates to a method for forming a groove of a club head, in particular to a method for forming a groove of a golf club head by cold pressing to form the groove.

高爾夫球桿頭成形後須於桿面(face)成形線溝,形成線溝的方法有熱壓、洗削或冷壓等各種加工方法,以冷壓成形線溝時,係藉由一上下模具對高爾夫球桿頭進行壓合,該上模具係具有對應線溝形狀的凸出模穴,該上模具對該高爾夫球桿頭的桿面進行壓製,以成形出對應的線溝,一般以冷壓成形該線溝時,並未使該高爾夫球桿頭升溫,因此無法一次完整的壓製成形該線溝,須先以上模具對高爾夫球桿頭進第一次粗壓,以對該線溝進行大致成形後,再以上模具對高爾夫球桿頭進行第二次的精壓以形成預定的線溝。惟,在該上模具進行第二次的精壓的過程中,該高爾夫球桿頭會因機台震動或人為擺放不佳等因素而產生位移,即使該位移量非常微小,亦會造成上模具未正確對應於第一次粗壓的線溝位置,使上模具壓合後造成線溝的歪斜或變形,導致該桿頭形成瑕疵不良品,使該桿頭產品的良率無法提升。After the golf club head is formed, the grooves must be formed on the face. The methods of forming the grooves include various processing methods such as hot pressing, washing or cold pressing. When the grooves are formed by cold pressing, an upper and lower mold is used. For pressing the golf club head, the upper mold has a protruding die cavity corresponding to the shape of the line groove, and the upper mold presses the face of the golf club head to form the corresponding line groove. When the groove is pressed, the golf club head does not heat up, so it is impossible to press the groove completely at one time. After being roughly formed, the golf club head is coined a second time with the die to form a predetermined groove. However, during the second precision pressing of the upper mold, the golf club head will be displaced due to machine vibration or improper placement by humans. The mold does not correctly correspond to the line groove position of the first rough pressing, so that the line groove is skewed or deformed after the upper mold is pressed, resulting in the formation of defective products of the head, so that the yield rate of the head product cannot be improved.

有鑑於此,習知的桿頭線溝成形方法確實仍有加以改善之必要。In view of this, it is still necessary to improve the conventional method of forming the head line groove.

為解決上述問題,本發明的目的是提供一種高爾夫桿頭線溝成形方法,係可以提升模具壓製成形線溝準確度者。In order to solve the above problems, the purpose of the present invention is to provide a method for forming grooves of golf club heads, which can improve the accuracy of forming grooves by die pressing.

本發明全文所述方向性或其近似用語,例如「前」、「後」、「左」、「右」、「上(頂)」、「下(底)」、「內」、「外」、「側面」等,主要係參考附加圖式的方向,各方向性或其近似用語僅用以輔助說明及理解本發明的各實施例,非用以限制本發明。The directional or similar terms used throughout this disclosure, such as "front", "back", "left", "right", "top (top)", "bottom (bottom)", "inside", "outside" , "side surface", etc., mainly refer to the directions of the attached drawings, each directionality or its similar terms are only used to assist the description and understanding of the various embodiments of the present invention, and are not intended to limit the present invention.

本發明全文所記載的元件及構件使用「一」或「一個」之量詞,僅是為了方便使用且提供本發明範圍的通常意義;於本發明中應被解讀為包括一個或至少一個,且單一的概念也包括複數的情況,除非其明顯意指其他意思。The use of the quantifier "a" or "an" for the elements and components described throughout the present invention is only for convenience and provides a general meaning of the scope of the present invention; in the present invention, it should be construed as including one or at least one, and a single The concept of also includes the plural case unless it is obvious that it means otherwise.

本發明全文所述「結合」、「組合」或「組裝」等近似用語,主要包含連接後仍可不破壞構件地分離,或是連接後使構件不可分離等型態,係本領域中具有通常知識者可以依據欲相連之構件材質或組裝需求予以選擇者。Similar terms such as "combined", "combined" or "assembled" mentioned in the whole text of the present invention mainly include the components that can be separated without destroying the components after the connection, or the components can not be separated after being connected, which are common knowledge in the field. It can be selected according to the material of the components to be connected or the assembly requirements.

本發明的高爾夫桿頭線溝成形方法,包含:由一第一模具與一第二模具以一第一成形壓力對一桿頭半成品冷壓,該第一模具具有一模穴,該桿頭半成品的背部定位於該模穴,該第二模具具有一線溝成形凸部,以該線溝成形凸部於該桿頭半成品的桿面成形一粗溝形部;及使該第一模具與該第二模具分離,並從該第一模具取下該桿頭半成品;將該桿頭半成品以該粗溝形部定位於該第二模具的線溝成形凸部後,以一第二成形壓力對該桿頭半成品冷壓。The golf club head line groove forming method of the present invention comprises: cold pressing a semi-finished club head by a first mold and a second mold with a first forming pressure, the first mold having a cavity, and the semi-finished club head The back of the head is positioned in the cavity, the second mold has a line groove forming convex part, and a rough groove-shaped part is formed on the face of the semi-finished club head with the line groove forming convex part; and the first mold and the first mold are formed. The two molds are separated, and the semi-finished club head is removed from the first mold; after the semi-finished club head is positioned on the groove forming convex portion of the second mold with the rough groove-shaped portion, a second forming pressure is applied to the semi-finished club head. The semi-finished club head is cold pressed.

據此,本發明的高爾夫桿頭線溝成形方法,係藉由對該桿頭半成品冷壓形成該粗溝形部,並將該粗溝形部定位於具有相對應線溝成形凸部的模具上,以對該桿頭半成品進行二次冷壓,係可以確保該桿頭半成品穩固地定位,使該桿頭半成品不會因為模具震動,或人為擺放的疏失而產生位移,當對該桿頭半成品進行二次冷壓時,該桿面可以準確地成形該預定線溝,係可以達到提升產品良率的功效。Accordingly, in the method for forming a groove of a golf club head of the present invention, the rough groove-shaped portion is formed by cold pressing the semi-finished product of the club head, and the rough groove-shaped portion is positioned on a mold having a corresponding groove forming convex portion. , to perform secondary cold pressing on the semi-finished club head, which can ensure that the semi-finished club head is stably positioned, so that the semi-finished club head will not be displaced due to the vibration of the mold or the negligence of artificial placement. When the first semi-finished product is subjected to secondary cold pressing, the face can accurately form the predetermined groove, which can achieve the effect of improving product yield.

其中,該桿頭半成品由碳的重量百分比為0.18~0.48的碳鋼材料製成。如此,該桿頭半成品可以具有較佳的可塑性,係可以降低該模具與該桿頭半成品進行冷壓時所產生的損耗。Wherein, the semi-finished product of the club head is made of carbon steel material with a carbon weight percentage of 0.18-0.48. In this way, the semi-finished club head can have better plasticity, which can reduce the loss generated when the mold and the semi-finished club head are cold-pressed.

其中,以150~350噸的第一成形壓力對該桿頭半成品進行冷壓3~10秒,及以150~350噸的第二成形壓力,對該桿頭半成品進行冷壓3~10秒。如此,係具有對該桿面上的預定線溝進行成形的功效。The semi-finished club head is cold-pressed for 3-10 seconds at a first forming pressure of 150-350 tons, and the semi-finished club head is cold-pressed for 3-10 seconds at a second forming pressure of 150-350 tons. In this way, the system has the effect of forming the predetermined groove on the face.

其中,以175~225噸的第一成形壓力對該桿頭半成品進行冷壓3~10秒,及以230~290噸的第二成形壓力,對該桿頭半成品進行冷壓3~10秒。如此,係具有精確地對該桿面上的預定線溝進行成形的功效。The semi-finished club head is cold-pressed for 3-10 seconds at a first forming pressure of 175-225 tons, and the semi-finished club head is cold-pressed for 3-10 seconds at a second forming pressure of 230-290 tons. In this way, the system has the effect of accurately shaping the predetermined groove on the face.

其中,該粗溝形部具有複數個深度為0.2~0.5mm,寬度為0.5~0.9mm的溝。如此,係可以在該桿面上的預定線溝進行大致上成形的功效。The rough groove-shaped portion has a plurality of grooves having a depth of 0.2 to 0.5 mm and a width of 0.5 to 0.9 mm. In this way, the function of substantially forming the predetermined groove on the face can be performed.

其中,該第二成形壓力對該桿頭半成品冷壓,以使該粗溝形部成形為一預定線溝,該預定線溝相對於該粗溝形部的深度變化率≦17.5%。如此,係使該預定線溝可以精確成形的功效。Wherein, the second forming pressure cold-presses the semi-finished rod head, so that the thick groove portion is formed into a predetermined line groove, and the depth change rate of the predetermined line groove relative to the thick groove portion is ≦17.5%. In this way, the predetermined line groove can be precisely formed.

其中,該第二成形壓力大於該第一成形壓力。如此,該第二成形壓力可以更容易地將該粗溝形部成形為預定的深度,係具有提升該預定線溝成形良率的功效。Wherein, the second forming pressure is greater than the first forming pressure. In this way, the second forming pressure can more easily form the rough groove portion to a predetermined depth, which has the effect of improving the forming yield of the predetermined line groove.

其中,對形成該粗溝形部的桿面進行研磨或銑削後,將該粗溝形部定位於該線溝成形凸部。如此,該桿面可以維持平整,係具有提升該桿面美觀性的功效。Here, after grinding or milling the face on which the rough groove portion is formed, the rough groove portion is positioned on the groove forming convex portion. In this way, the club face can be kept flat, which has the effect of enhancing the aesthetics of the club face.

其中,該桿面的研磨或銑削量為0.03~0.15mm。如此,該桿面可以維持平整,係具有提升該桿面美觀性的功效。Wherein, the amount of grinding or milling of the face is 0.03 to 0.15 mm. In this way, the club face can be kept flat, which has the effect of enhancing the aesthetics of the club face.

其中,將該桿頭半成品以該粗溝形部定位於具有該線溝成形凸部的另一模具後,以一第二成形壓力對該桿頭半成品冷壓。如此,可以快速地定位該桿頭半成品,係具有提升生產效率的功效。The semi-finished club head is cold-pressed with a second forming pressure after positioning the semi-finished club head with the rough groove-shaped portion on another mold having the groove forming convex portion. In this way, the semi-finished club head can be quickly positioned, which has the effect of improving production efficiency.

其中,將該第一模具與該第二模具反置後,將該桿頭半成品以該粗溝形部定位於該第二模具,以一第二成形壓力對該桿頭半成品冷壓。如此,可以避免不同模具製造上的公差所造成該線溝成形凸部與該粗溝形部之間配對上的微小差異,係具有提升該預定線溝成形良率的功效。Wherein, after the first mold and the second mold are reversed, the semi-finished club head is positioned on the second mold with the rough groove portion, and the semi-finished club head is cold-pressed with a second forming pressure. In this way, it is possible to avoid the slight difference in matching between the line groove forming convex portion and the thick groove-shaped portion caused by the manufacturing tolerance of different molds, which has the effect of improving the predetermined line groove forming yield.

為讓本發明之上述及其他目的、特徵及優點能更明顯易懂,下文特舉本發明之較佳實施例,並配合所附圖式,作詳細說明如下:In order to make the above-mentioned and other objects, features and advantages of the present invention more obvious and easy to understand, the preferred embodiments of the present invention are exemplified below, and are described in detail as follows in conjunction with the accompanying drawings:

請參照第1、3圖所示,本發明高爾夫桿頭線溝成形方法,係包含以一第一成形壓力對一桿頭半成品H冷壓,以於該桿頭半成品H的桿面H1成形一粗溝形部H2,及將該粗溝形部H2定位於一模具後,以一第二成形壓力對該桿頭半成品H冷壓。Referring to Figures 1 and 3, the method for forming a groove for a golf club head according to the present invention includes cold pressing a semi-finished club head H with a first forming pressure to form a face H1 of the semi-finished club head H. The rough groove-shaped portion H2, and after the rough groove-shaped portion H2 is positioned in a mold, the semi-finished club head H is cold-pressed with a second forming pressure.

詳言之,係可以藉由一第一模具1與一第二模具2對該桿頭半成品H進行冷壓,該第一模具1具有一模穴11,該模穴11係可以具有對應該桿頭半成品H背部(back)的形狀,使該桿頭半成品H的背部可以定位於該第一模具1,及使該桿頭半成品H的桿面H1(face)朝向該第二模具2,該第二模具2具有一線溝成形凸部21,該線溝成形凸部21係具有並排的數個凸肋,該數個凸肋用以成形一預定線溝。在本實施例中,該桿頭半成品H可以採用碳的重量百分比為0.18~0.48的碳鋼材料所製成,如此,該桿頭半成品H可以具有較佳的可塑性,係可以降低模具與該桿頭半成品H冷壓時所產生的損耗。Specifically, the semi-finished rod head H can be cold-pressed by a first mold 1 and a second mold 2. The first mold 1 has a cavity 11, and the cavity 11 can have a corresponding rod. The back of the head semi-finished product H is shaped so that the back of the head semi-finished product H can be positioned on the first mold 1, and the face H1 (face) of the head semi-finished product H faces the second mold 2, and the first mold The two molds 2 have a line groove forming convex portion 21, and the line groove forming convex portion 21 has a plurality of convex ribs arranged side by side, and the plurality of convex ribs are used to form a predetermined line groove. In this embodiment, the semi-finished product H of the club head can be made of carbon steel with a carbon weight percentage of 0.18-0.48. In this way, the semi-finished product H of the club head can have better plasticity, which can reduce the mold and the rod. The loss caused by the cold pressing of the first semi-finished product H.

請參照第2、3圖所示,該第一模具1與該第二模具2係能夠對該桿頭半成品H進行第一次冷壓,該第一模具1可以作為一下模具,該第二模具2可以作為一上模具,以使該第二模具2朝該第一模具1進行冷壓,該第一模具1與該第二模具2可以以150~350噸(ton)的第一成形壓力,對該桿頭半成品H進行冷壓3~10秒後,較佳地,該第一模具1與該第二模具2可以以175~225噸(ton)的壓力對該桿頭半成品H進行第一次冷壓,如此,使該第一模具與該第二模具分離後,該桿頭半成品H的桿面H1可以形成該粗溝形部H2,該粗溝形部H2係與該第二模具2的線溝成形凸部21相對應。在本實施例中,該粗溝形部H2係具有複數個深度為0.2~0.5mm,寬度為0.5~0.9mm的溝,如此,可以對該桿面H1上的預定線溝進行大致上的成形。Referring to Figures 2 and 3, the first mold 1 and the second mold 2 can be used for the first cold pressing of the semi-finished rod head H. The first mold 1 can be used as a lower mold, and the second mold 2 can be used as an upper mold, so that the second mold 2 is cold-pressed toward the first mold 1, and the first mold 1 and the second mold 2 can be formed with a first forming pressure of 150-350 tons (ton), After cold-pressing the semi-finished club head H for 3-10 seconds, preferably, the first mold 1 and the second mold 2 can press the semi-finished club head H with a pressure of 175-225 tons (ton). The second cold pressing, so that after the first mold is separated from the second mold, the face H1 of the semi-finished head H can form the rough groove H2, and the rough groove H2 is connected with the second mold 2. The line groove forming convex portion 21 corresponds to. In this embodiment, the thick groove portion H2 has a plurality of grooves with a depth of 0.2 to 0.5 mm and a width of 0.5 to 0.9 mm, so that the predetermined line grooves on the face H1 can be roughly formed. .

請參照第4圖所示,值得注意的是,該線溝成形凸部21係對該桿面H1施予外力以進行第一次冷壓,因此,該粗溝形部H2成形後,該粗溝形部H2的溝槽開口處容易因為結構的改變而形成一塌陷部T,該塌陷部T即會造成相鄰二粗溝形部H2之間的該桿面H1不平整,較佳地,可以對形成該相鄰二粗溝形部H2的桿面H1進行研磨或銑削,即,對相鄰二粗溝形部H2之間的該桿面H1進行研磨或銑削。在本實施例中,該桿面H1的研磨或銑削量可以為0.03~0.15mm,如此,該桿面H1可以維持平整,具有提升該桿面H1美觀性的作用。Please refer to FIG. 4, it is worth noting that the groove forming convex portion 21 exerts an external force on the face H1 to perform the first cold pressing. Therefore, after the rough groove portion H2 is formed, the rough groove portion H2 is formed The groove opening of the groove portion H2 is likely to form a collapsed portion T due to structural changes, and the collapsed portion T will cause the club face H1 between the two adjacent rough grooved portions H2 to be uneven. Preferably, The face H1 forming the two adjacent rough groove portions H2 may be ground or milled, that is, the face H1 between the two adjacent rough groove portions H2 may be ground or milled. In this embodiment, the grinding or milling amount of the face H1 can be 0.03-0.15 mm, so that the face H1 can be kept flat, which has the effect of improving the aesthetics of the face H1.

請參照第5圖所示,將成形該粗溝形部H2的桿頭半成品H由該第一模具1取下後,再將該桿頭半成品H由該粗溝形部H2定位於該第二模具2的線溝成形凸部21,以對該桿頭半成品H進行第二次冷壓。該第二模具2可以為具有該線溝成形凸部21的另一模具,或者,將該第一模具1與該第二模具2反置,使該第二模具2可以作為一下模具,及使該第一模具1可以作為一上模具,再將該桿頭半成品H的粗溝形部H2結合於該第二模具2的線溝成形凸部21,使該半頭半成品H的背部朝向該第一模具1,以使該第一模具1朝該第二模具2進行冷壓。在本實施例中,該桿頭半成品H的粗溝形部H2可以定位於原第二模具2,係可以避免將該桿頭半成品H定位於另一第二模具2時,不同模具製造上的公差所造成另一第二模具2的線溝成形凸部21與該粗溝形部H2之間配對上的微小差異,以提升該預定線溝的成形良率。由於該粗溝形部H2具有與該模具(第二模具2)之該線溝成形凸部21相對應的形狀,因此,該線溝成形凸部21的數個凸肋結構,可以分別對位於該粗溝形部H2的數個溝,藉此,可以使該桿頭半成品H穩固地定位於該第二模具2的線溝成形凸部21而不會產生位移。Referring to FIG. 5 , after removing the semi-finished club head H forming the rough groove H2 from the first mold 1 , then positioning the semi-finished club H from the rough groove H2 on the second The groove of the mold 2 forms the convex portion 21 to perform the second cold pressing on the semi-finished product H of the head. The second mold 2 may be another mold having the groove forming protrusions 21, or the first mold 1 and the second mold 2 may be reversed, so that the second mold 2 can be used as a lower mold, and The first mold 1 can be used as an upper mold, and then the rough groove-shaped portion H2 of the semi-finished head H is combined with the groove forming convex portion 21 of the second mold 2, so that the back of the semi-finished head H faces the first A mould 1 for cold pressing the first mould 1 towards the second mould 2 . In the present embodiment, the rough groove-shaped portion H2 of the semi-finished club head H can be positioned on the original second mold 2, so as to avoid the possibility of locating the semi-finished club head H in another second mold 2, which may result in different mold manufacturing processes. A slight difference in matching between the line groove forming convex portion 21 of the other second mold 2 and the thick groove-shaped portion H2 caused by the tolerance can improve the forming yield of the predetermined line groove. Since the rough groove-shaped portion H2 has a shape corresponding to the wire groove forming convex portion 21 of the mold (second mold 2 ), the plurality of rib structures of the wire groove forming convex portion 21 can be respectively aligned with each other. The plurality of grooves of the rough groove-shaped portion H2, thereby, can make the semi-finished product H of the club head firmly positioned on the groove forming convex portion 21 of the second mold 2 without displacement.

該第一模具1與該第二模具2能夠以150~350噸(ton)的第二成形壓力,對該桿頭半成品H進行冷壓3~10秒,較佳地,該第一模具1與該第二模具2能夠以230~290噸(ton)的壓力對該桿頭半成品H進行第二次冷壓,如此,該粗溝形部H2可以被擠壓整形以成形為該預定線溝。在本實施例中,該桿面H1受到研磨或銑削而使該粗溝形部H2的深度改變,據此,該第一模具1與該第二模具2能夠以大於該第一成形壓力的第二成形壓力對該桿頭半成品H進行第二次冷壓,如此,該第二成形壓力可以更容易地將該粗溝形部H2成形為預定的深度,較佳地,該預定線溝的深度為0.2~0.5mm,寬度為0.5~0.9mm,使該預定線溝相對於該粗溝形部H2的深度變化率≦17.5%。The first mold 1 and the second mold 2 can cold-press the semi-finished club head H for 3 to 10 seconds at a second forming pressure of 150-350 tons. Preferably, the first mold 1 and the The second die 2 can perform a second cold pressing on the semi-finished club head H with a pressure of 230-290 tons, so that the rough groove-shaped portion H2 can be extruded and shaped to form the predetermined line groove. In this embodiment, the face H1 is ground or milled to change the depth of the rough groove portion H2. Accordingly, the first mold 1 and the second mold 2 can use a second mold greater than the first molding pressure. The second forming pressure performs the second cold pressing on the semi-finished rod head H, so that the second forming pressure can more easily form the rough groove-shaped portion H2 to a predetermined depth, preferably, the depth of the predetermined line groove The thickness is 0.2 to 0.5 mm, the width is 0.5 to 0.9 mm, and the depth change rate of the predetermined line groove with respect to the thick groove-shaped portion H2 is ≦17.5%.

綜上所述,本發明的高爾夫桿頭線溝成形方法,係藉由對該桿頭半成品冷壓形成該粗溝形部,並將該粗溝形部定位於具有相對應線溝成形凸部的模具上,以進行二次冷壓,係可以確保該桿頭半成品可以穩固地定位,使該桿頭半成品不會因為模具震動,或人為擺放的疏失而產生位移,及當對該桿頭半成品進行二次冷壓時,該桿面係可以準確地成形該預定線溝,係可以達到提升產品良率的功效。To sum up, the method for forming a groove of a golf club head of the present invention is to form the rough groove-shaped portion by cold pressing the semi-finished product of the golf club head, and position the thick groove-shaped portion on a groove having a corresponding groove forming convex portion. It can be used for secondary cold pressing on the mold, which can ensure that the semi-finished club head can be stably positioned, so that the semi-finished club head will not be displaced due to mold vibration or artificial placement. When the semi-finished product is subjected to secondary cold pressing, the face system can accurately form the predetermined groove, which can achieve the effect of improving the product yield.

雖然本發明已利用上述較佳實施例揭示,然其並非用以限定本發明,任何熟習此技藝者在不脫離本發明之精神和範圍之內,相對上述實施例進行各種更動與修改仍屬本發明所保護之技術範疇,因此本發明之保護範圍當視後附之申請專利範圍所界定者為準。Although the present invention has been disclosed by the above-mentioned preferred embodiments, it is not intended to limit the present invention. Any person skilled in the art can make various changes and modifications relative to the above-mentioned embodiments without departing from the spirit and scope of the present invention. Therefore, the scope of protection of the present invention should be determined by the scope of the patent application attached hereto.

1:第一模具 11:模穴 2:第二模具 21:線溝成形凸部 H:桿頭半成品 H1:桿面 H2:粗溝形部 T:塌陷部1: The first mold 11: Mold cavity 2: Second mold 21: Wire groove forming convex part H: Semi-finished club head H1: club face H2: Rough groove T: collapsed part

[第1圖]  本發明一較佳實施例的模具立體圖。 [第2圖]  本發明一較佳實施例的第一次冷壓示意圖。 [第3圖]  本發明一較佳實施例的粗溝形部成形示意圖。 [第4圖]  本發明一較佳實施例的粗溝形部局部放大圖。 [第5圖]  本發明一較佳實施例的第二次冷壓示意圖。 [Figure 1] A perspective view of a mold according to a preferred embodiment of the present invention. [Fig. 2] A schematic diagram of the first cold pressing of a preferred embodiment of the present invention. [FIG. 3] A schematic diagram of the forming of the rough groove-shaped portion in a preferred embodiment of the present invention. [FIG. 4] A partial enlarged view of the rough groove-shaped portion of a preferred embodiment of the present invention. [Fig. 5] A schematic diagram of the second cold pressing of a preferred embodiment of the present invention.

1:第一模具 1: The first mold

11:模穴 11: Mold cavity

2:第二模具 2: Second mold

21:線溝成形凸部 21: Wire groove forming convex part

H:桿頭半成品 H: Semi-finished club head

H1:桿面 H1: club face

Claims (11)

一種高爾夫桿頭線溝成形方法,包含: 由一第一模具與一第二模具以一第一成形壓力對一桿頭半成品冷壓,該第一模具具有一模穴,該桿頭半成品的背部定位於該模穴,該第二模具具有一線溝成形凸部,以該線溝成形凸部於該桿頭半成品的桿面成形一粗溝形部;及 使該第一模具與該第二模具分離,並從該第一模具取下該桿頭半成品; 將該桿頭半成品以該粗溝形部定位於該第二模具的線溝成形凸部後,以一第二成形壓力對該桿頭半成品冷壓。 A golf club head line groove forming method, comprising: A first mold and a second mold are cold-pressed to a semi-finished club head with a first forming pressure, the first mold has a mold cavity, the back of the semi-finished club head is positioned in the mold cavity, and the second mold has a line groove forming convex portion, and a rough groove-shaped portion is formed on the face of the semi-finished club head with the line groove forming convex portion; and separating the first mold from the second mold, and removing the semi-finished club head from the first mold; The semi-finished club head is cold-pressed with a second forming pressure after the rough groove-shaped portion is positioned on the groove-forming convex portion of the second mold. 如請求項1之高爾夫桿頭線溝成形方法,其中,該桿頭半成品由碳的重量百分比為0.18~0.48的碳鋼材料製成。As claimed in claim 1, the golf club head line groove forming method, wherein the semi-finished product of the club head is made of carbon steel material with a carbon weight percentage of 0.18-0.48. 如請求項1之高爾夫桿頭線溝成形方法,其中,以150~350噸的第一成形壓力對該桿頭半成品進行冷壓3~10秒,及以150~350噸的第二成形壓力,對該桿頭半成品進行冷壓3~10秒。The method for forming grooves of golf club heads according to claim 1, wherein the semi-finished club head is cold-pressed for 3 to 10 seconds at a first forming pressure of 150-350 tons, and the second forming pressure is 150-350 tons, This semi-finished club head is cold-pressed for 3 to 10 seconds. 如請求項3之高爾夫桿頭線溝成形方法,其中,以175~225噸的第一成形壓力對該桿頭半成品進行冷壓3~10秒,及以230~290噸的第二成形壓力,對該桿頭半成品進行冷壓3~10秒。The golf club head line groove forming method of claim 3, wherein the semi-finished club head is cold-pressed for 3-10 seconds with a first forming pressure of 175-225 tons, and the second forming pressure is 230-290 tons, This semi-finished club head is cold-pressed for 3 to 10 seconds. 如請求項1之高爾夫桿頭線溝成形方法,其中,該粗溝形部具有複數個深度為0.2~0.5mm,寬度為0.5~0.9mm的溝。The method for forming a golf club head line groove according to claim 1, wherein the thick groove-shaped portion has a plurality of grooves having a depth of 0.2 to 0.5 mm and a width of 0.5 to 0.9 mm. 如請求項1之高爾夫桿頭線溝成形方法,其中,該第二成形壓力對該桿頭半成品冷壓,以使該粗溝形部成形為一預定線溝,該預定線溝相對於該粗溝形部的深度變化率≦17.5%。The method for forming a line groove of a golf club head according to claim 1, wherein the second forming pressure is cold-pressed on the semi-finished club head, so that the thick groove-shaped portion is formed into a predetermined line groove, and the predetermined line groove is opposite to the rough line groove. The depth change rate of the groove portion is ≦17.5%. 如請求項1之高爾夫桿頭線溝成形方法,其中,該第二成形壓力大於該第一成形壓力。The method for forming a line groove of a golf club head according to claim 1, wherein the second forming pressure is greater than the first forming pressure. 如請求項1之高爾夫桿頭線溝成形方法,其中,對形成該粗溝形部的桿面進行研磨或銑削後,將該粗溝形部定位於該線溝成形凸部。The method for forming a groove of a golf club head according to claim 1, wherein after grinding or milling the face on which the rough groove portion is formed, the rough groove portion is positioned on the groove forming convex portion. 如請求項8之高爾夫桿頭線溝成形方法,其中,該桿面的研磨或銑削量為0.03~0.15mm。The method for forming a groove of a golf club head according to claim 8, wherein the grinding or milling amount of the face is 0.03-0.15 mm. 如請求項1之高爾夫桿頭線溝成形方法,其中,將該桿頭半成品以該粗溝形部定位於具有該線溝成形凸部的另一模具後,以一第二成形壓力對該桿頭半成品冷壓。The method for forming a groove for a golf club head according to claim 1, wherein after positioning the semi-finished club head with the rough groove-shaped portion on another mold having the groove forming convex portion, a second forming pressure is applied to the golf club. The first semi-finished product is cold pressed. 如請求項1之高爾夫桿頭線溝成形方法,其中,將該第一模具與該第二模具反置後,將該桿頭半成品以該粗溝形部定位於該第二模具,以一第二成形壓力對該桿頭半成品冷壓。The golf club head line groove forming method of claim 1, wherein after the first mold and the second mold are reversed, the semi-finished club head is positioned on the second mold with the rough groove-shaped portion, and a first The second forming pressure is cold pressing on the semi-finished product of the head.
TW109146683A 2020-12-29 2020-12-29 A method for forming the groove of a golf club head TWI765502B (en)