TWI679134B - Three-dimensional transfer product and manufacturing method thereof - Google Patents

Three-dimensional transfer product and manufacturing method thereof Download PDF

Info

Publication number
TWI679134B
TWI679134B TW106122496A TW106122496A TWI679134B TW I679134 B TWI679134 B TW I679134B TW 106122496 A TW106122496 A TW 106122496A TW 106122496 A TW106122496 A TW 106122496A TW I679134 B TWI679134 B TW I679134B
Authority
TW
Taiwan
Prior art keywords
layer
pattern
sublayer
light
shielding
Prior art date
Application number
TW106122496A
Other languages
Chinese (zh)
Other versions
TW201906743A (en
Inventor
吳盧漢檉
Han-Cheng Wu-Lu
黃朝鍵
Chao-Chein Huang
Original Assignee
大勤化成股份有限公司
Daigin Chemical Co., Ltd.
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 大勤化成股份有限公司, Daigin Chemical Co., Ltd. filed Critical 大勤化成股份有限公司
Priority to TW106122496A priority Critical patent/TWI679134B/en
Priority to JP2018014498A priority patent/JP6461387B2/en
Publication of TW201906743A publication Critical patent/TW201906743A/en
Application granted granted Critical
Publication of TWI679134B publication Critical patent/TWI679134B/en

Abstract

一種轉印膜結構包含一彈性薄膜基材層、一模板層、一第一遮光層、一第二遮光層、一填充層、一暗反應層、一第一圖案層及一固定層。該模板層形成在該彈性薄膜基材層上,該第一遮光層形成在該彈性薄膜基材層上,該第二遮光層形成在該模板層上,該填充層形成在該第二遮光層上,該暗反應層形成在該填充層上,該第一圖案層形成在該第一遮光層上,該固定層位在該暗反應層與該第一圖案層上。本發明的轉印膜結構於一物件表面所形成的立體轉印圖案上不會殘留離型劑。 A transfer film structure includes an elastic film substrate layer, a template layer, a first light-shielding layer, a second light-shielding layer, a filling layer, a dark reaction layer, a first pattern layer, and a fixing layer. The template layer is formed on the elastic film substrate layer, the first light-shielding layer is formed on the elastic film substrate layer, the second light-shielding layer is formed on the template layer, and the filling layer is formed on the second light-shielding layer Above, the dark reaction layer is formed on the filling layer, the first pattern layer is formed on the first light-shielding layer, and the fixed layer is located on the dark reaction layer and the first pattern layer. The transfer film structure of the present invention does not leave a release agent on the three-dimensional transfer pattern formed on the surface of an object.

Description

立體轉印品及其製法 Three-dimensional transfer product and manufacturing method thereof

本發明是有關於一種轉印膜結構及其製法與轉印品及其製法,特別是指一種包含遮光層的轉印膜結構及其製法與立體轉印品及其製法。 The invention relates to a transfer film structure, a manufacturing method thereof and a transfer product and a manufacturing method thereof, and particularly to a transfer film structure including a light-shielding layer, a manufacturing method thereof, and a three-dimensional transfer product, and a manufacturing method thereof.

為了增加物品外觀的美感,現有已存在各種能貼覆於一物件表面且具有各式轉印圖案的轉印膜,例如可貼覆於如手機或筆記型電腦等電子產品外殼上的轉印膜。然而,大多數轉印膜上的圖案皆僅限於平面轉印圖案,非為能產生具有立體觸感的立體轉印圖案。 In order to increase the aesthetics of the appearance of articles, there are various transfer films that can be applied to the surface of an object and have various transfer patterns, such as transfer films that can be attached to the casing of electronic products such as mobile phones or notebook computers. . However, most of the patterns on the transfer film are limited to planar transfer patterns, and are not three-dimensional transfer patterns with three-dimensional touch.

目前市面上已出現能於物件上產生立體轉印圖案的轉印膜結構,此轉印膜結構的製法是先提供一離型劑層,並於該離型劑層上設置一軟性塗層,接著於該軟性塗層上相反於該離型劑層的一側設置一油墨層,再於該油墨層上相反於該軟性塗層的一側設置一黏著層,最後製得一轉印膜結構。前述的轉印膜結構在透過該黏著層固定在一物件表面並移除該離型劑層後,該物件表面上即會形成 立體轉印圖案。 At present, a transfer film structure capable of generating a three-dimensional transfer pattern on an object has appeared on the market. The method of manufacturing the transfer film structure is to first provide a release agent layer and set a soft coating on the release agent layer. Then, an ink layer is disposed on the soft coating layer on the side opposite to the release agent layer, and then an adhesive layer is disposed on the ink layer on the side opposite to the soft coating layer, and finally a transfer film structure is prepared. . After the aforementioned transfer film structure is fixed on the surface of an object through the adhesive layer and the release agent layer is removed, the surface of the object is formed. Three-dimensional transfer pattern.

然而,前述的轉印膜結構在移除該離型劑層後,常會於該立體轉印圖案上殘留離型劑,並無法將離型劑完全移除乾淨,影響到立體轉印圖案的美觀。因此,如何解決現有的轉印膜結構因離型劑所產生的缺點,成為目前致力研究的目標。 However, after the release film layer is removed from the aforementioned transfer film structure, a release agent is often left on the three-dimensional transfer pattern, and the release agent cannot be completely removed, which affects the appearance of the three-dimensional transfer pattern. . Therefore, how to solve the shortcomings of the existing transfer film structure caused by the release agent has become the goal of current research.

因此,本發明的第一目的,即在提供一種轉印膜結構。該轉印膜結構於一物件表面所形成的立體轉印圖案上不會殘留離型劑。 Therefore, a first object of the present invention is to provide a transfer film structure. The transfer film structure does not leave a release agent on the three-dimensional transfer pattern formed on the surface of an object.

於是,本發明轉印膜結構包含一彈性薄膜基材層、一模板層、一第一遮光層、一第二遮光層、一填充層、一暗反應層、一第一圖案層及一固定層。 Therefore, the transfer film structure of the present invention includes an elastic film substrate layer, a template layer, a first light shielding layer, a second light shielding layer, a filling layer, a dark reaction layer, a first pattern layer, and a fixing layer .

該模板層以第一圖樣形成在該彈性薄膜基材層上且由塗料形成。 The template layer is formed on the elastic film substrate layer in a first pattern and is formed of a paint.

該第一遮光層以互補於該第一圖樣的第二圖樣形成在該彈性薄膜基材層上且由紫外光吸收油墨形成,該第一遮光層與該模板層位在同一平面上。 The first light-shielding layer is formed on the elastic film substrate layer with a second pattern complementary to the first pattern and is formed of an ultraviolet light absorbing ink. The first light-shielding layer and the template layer are located on the same plane.

該第二遮光層以該第一圖樣形成在該模板層上且由紫外光吸收油墨形成。 The second light-shielding layer is formed on the template layer with the first pattern and is formed of an ultraviolet light absorbing ink.

該填充層以該第一圖樣形成在該第二遮光層上且由透明 油墨形成。 The filling layer is formed on the second light-shielding layer in the first pattern and is transparent. Ink formation.

該暗反應層以該第一圖樣形成在該填充層上。 The dark reaction layer is formed on the filling layer in the first pattern.

該第一圖案層以該第二圖樣形成在該第一遮光層上且由油溶性塗料形成,該第一圖案層與該第二遮光層、該填充層及該暗反應層接觸。 The first pattern layer is formed on the first light-shielding layer with the second pattern and is formed of an oil-soluble paint. The first pattern layer is in contact with the second light-shielding layer, the filling layer, and the dark reaction layer.

該固定層位在該暗反應層與該第一圖案層上。 The fixed layer is located on the dark reaction layer and the first pattern layer.

因此,本發明的第二目的,即在提供一種前述轉印膜結構的製法。 Therefore, a second object of the present invention is to provide a method for manufacturing the aforementioned transfer film structure.

於是,本發明轉印膜結構的製法包含下列步驟:(a)在一彈性薄膜基材層上以第一圖樣形成一由塗料形成的模板層;(b)在該彈性薄膜基材層上以互補於該第一圖樣的第二圖樣形成一由紫外光吸收油墨形成的第一遮光層,該第一遮光層與該模板層位在同一平面上;(c)在該模板層上以該第一圖樣形成一由紫外光吸收油墨形成的第二遮光層;(d)在該第一遮光層上以該第二圖樣形成一由油溶性塗料形成的第一圖案次層,該第一圖案次層與該第二遮光層位在同一平面上;(e)在該第二遮光層上以該第一圖樣形成一由透明油墨形成的填充層;(f)在該第一圖案次層上以該第二圖樣形成一由油溶性塗料形成的 第二圖案次層,該第二圖案次層與該填充層位在同一平面上;(g)在該填充層上以該第一圖樣形成一暗反應層;(h)在該第二圖案次層上以該第二圖樣形成一由油溶性塗料形成的第三圖案次層,該第三圖案次層與該暗反應層位在同一平面上,該第一圖案次層、該第二圖案次層與該第三圖案次層共同界定出一第一圖案層;及(i)形成一位在該暗反應層與該第三圖案次層上方的固定層,以得到該轉印膜結構。 Therefore, the method for manufacturing the transfer film structure of the present invention includes the following steps: (a) forming a template layer made of paint on a flexible film substrate layer with a first pattern; (b) forming a flexible film substrate layer on the elastic film substrate layer; The second pattern complementary to the first pattern forms a first light-shielding layer formed by the ultraviolet light absorbing ink, and the first light-shielding layer is on the same plane as the template layer; (c) the first layer is A pattern forms a second light-shielding layer made of ultraviolet light absorbing ink; (d) a first pattern sub-layer made of an oil-soluble paint is formed on the first light-shielding layer with the second pattern, and the first pattern is The layer is on the same plane as the second light-shielding layer; (e) forming a filling layer made of a transparent ink on the second light-shielding layer in the first pattern; (f) forming a filling layer on the first pattern sublayer. The second pattern forms an oil-soluble paint A second pattern sublayer, the second pattern sublayer being on the same plane as the filling layer; (g) forming a dark reaction layer on the filling layer with the first pattern; (h) in the second pattern sublayer A third pattern sub-layer formed of an oil-soluble paint is formed on the layer with the second pattern, the third pattern sub-layer is on the same plane as the dark reaction layer, and the first pattern sub-layer and the second pattern sub-layer The layer and the third pattern sub-layer together define a first pattern layer; and (i) forming a fixed layer above the dark reaction layer and the third pattern sub-layer to obtain the transfer film structure.

此外,本發明還有一第三目的,即在提供一種於其立體轉印圖案上不會殘留離型劑的立體轉印品。 In addition, a third object of the present invention is to provide a three-dimensional transfer product that does not leave a release agent on the three-dimensional transfer pattern.

於是,本發明立體轉印品包含一物件、一固定層、一暗反應層、一第三圖案次層、一填充層、一第二圖案次層及一第一圖案次層。 Therefore, the three-dimensional transfer product of the present invention includes an object, a fixed layer, a dark reaction layer, a third pattern sublayer, a filling layer, a second pattern sublayer, and a first pattern sublayer.

該固定層貼覆在該物件表面上。 The fixed layer is adhered on the surface of the object.

該暗反應層以第一圖樣位在該固定層上。 The dark reaction layer is positioned on the fixed layer in a first pattern.

該第三圖案次層以互補於該第一圖樣的第二圖樣位在該固定層上且由油溶性塗料形成,該第三圖案次層與該暗反應層位在同一平面上。 The third pattern sub-layer is located on the fixed layer with a second pattern complementary to the first pattern and is formed of an oil-soluble paint, and the third pattern sub-layer is on the same plane as the dark reaction layer.

該填充層以該第一圖樣覆蓋在該暗反應層上且由透明油墨形成。 The filling layer covers the dark reaction layer with the first pattern and is formed of transparent ink.

該第二圖案次層以該第二圖樣覆蓋在該第三圖案次層上且由油溶性塗料形成,該第二圖案次層與該填充層位在同一平面上。 The second pattern sub-layer is covered with the second pattern on the third pattern sub-layer and is formed of an oil-soluble paint, and the second pattern sub-layer is on the same plane as the filling layer.

該第一圖案次層以該第二圖樣覆蓋在該第二圖案次層上且由油溶性塗料形成,該第一圖案次層、該第二圖案次層與該第三圖案次層共同界定出一第一圖案層。 The first pattern sublayer is overlaid on the second pattern sublayer with the second pattern and is formed of an oil-soluble paint. The first pattern sublayer, the second pattern sublayer, and the third pattern sublayer are collectively defined. A first pattern layer.

而本發明的第四目的,即在提供一種前述立體轉印品的製法。 The fourth object of the present invention is to provide a method for manufacturing the three-dimensional transfer product.

於是,本發明立體轉印品的製法包含前述轉印膜結構的製法所有步驟及下列步驟:(j)使該轉印膜結構的固定層貼覆於一物件表面;(k)在該步驟(j)之後,以紫外光自該彈性薄膜基材層朝該固定層的方向照射;(l)在該步驟(k)之後,自該填充層與該第一圖案層移除該第一遮光層、該第二遮光層、該模板層與該彈性薄膜基材層;及(m)在該步驟(l)之後,以紫外光照射該第一圖案層、該填充層、該暗反應層與該固定層,以得到該立體轉印品。 Therefore, the method for manufacturing a three-dimensional transfer product of the present invention includes all the steps of the aforementioned method for manufacturing a transfer film structure and the following steps: (j) attaching a fixed layer of the transfer film structure to an object surface; j) afterwards, the ultraviolet light is irradiated from the elastic film substrate layer toward the fixed layer; (l) after the step (k), removing the first light-shielding layer from the filling layer and the first pattern layer The second light-shielding layer, the template layer and the elastic film substrate layer; and (m) after step (l), irradiating the first pattern layer, the filling layer, the dark reaction layer and the The layer is fixed to obtain the three-dimensional transfer product.

而本發明的第五目的,即在提供另一種前述立體轉印品的製法。 A fifth object of the present invention is to provide another method for manufacturing the three-dimensional transfer product.

於是,本發明立體轉印品的製法包含前述轉印膜結構的 製法(a)~(h)步驟及下列步驟:(h1)在該暗反應層與該第三圖案次層上形成一由油溶性塗料形成的第二圖案層;(i)形成一位在該第二圖案層上方的固定層,以得到該轉印膜結構;(j)使該轉印膜結構的固定層貼覆於一物件表面;(k)在該步驟(j)之後,以紫外光自該彈性薄膜基材層朝該固定層的方向照射;(l)在該步驟(k)之後,自該填充層與該第一圖案層移除該第一遮光層、該第二遮光層、該模板層與該彈性薄膜基材層;及(m)在該步驟(l)之後,以紫外光照射該第一圖案層、該第二圖案層、該填充層、該暗反應層與該固定層,以得到該立體轉印品。 Therefore, the method for producing a three-dimensional transfer product of the present invention includes the above-mentioned transfer film structure. Manufacturing method (a) ~ (h) steps and the following steps: (h1) forming a second pattern layer formed of an oil-soluble paint on the dark reaction layer and the third pattern sublayer; (i) forming a single bit on the A fixed layer above the second pattern layer to obtain the transfer film structure; (j) pasting the fixed layer of the transfer film structure on an object surface; (k) after step (j), using ultraviolet light Irradiate from the elastic film substrate layer toward the fixed layer; (l) after step (k), remove the first light-shielding layer, the second light-shielding layer, and the first layer from the filling layer and the first pattern layer; The template layer and the elastic film substrate layer; and (m) after the step (l), irradiating the first pattern layer, the second pattern layer, the filling layer, the dark reaction layer and the fixing with ultraviolet light Layer to obtain the three-dimensional transfer product.

本發明的功效在於:本發明的轉印膜結構是通過該第一遮光層與該第二遮光層的設置,使其在貼覆於一物件表面後,僅需照射紫外光即可使該第一遮光層、該第二遮光層、該模板層與該彈性薄膜基材層能從該填充層與該第一圖案層上被輕易移除,與現有的轉印膜結構是貼覆於一物件表面後再移除離型劑層的技術不同。因此,本發明的轉印膜結構於該物件表面所形成的立體轉印圖案上(即該填充層與該第一圖案層上)不會殘留離型劑。 The effect of the present invention is that the transfer film structure of the present invention is provided with the first light-shielding layer and the second light-shielding layer, so that after being adhered to the surface of an object, the first A light-shielding layer, the second light-shielding layer, the template layer, and the elastic film substrate layer can be easily removed from the filling layer and the first pattern layer, and the existing transfer film structure is attached to an object The technique of removing the release agent layer after the surface is different. Therefore, the transfer film structure of the present invention does not leave a release agent on the three-dimensional transfer pattern formed on the surface of the object (that is, on the filling layer and the first pattern layer).

以下將就本發明內容進行詳細說明: The following will describe the content of the present invention in detail:

[轉印膜結構][Transfer film structure]

較佳地,該彈性薄膜基材層的材料為聚乙烯醇、耐綸、聚甲基戊烯、聚對苯二甲酸乙二酯、聚對苯二甲酸丁二酯、聚乙烯吡咯啶酮、聚乙烯、聚丙烯或其組合。 Preferably, the material of the elastic film substrate layer is polyvinyl alcohol, nylon, polymethylpentene, polyethylene terephthalate, polybutylene terephthalate, polyvinylpyrrolidone, Polyethylene, polypropylene, or a combination thereof.

較佳地,該暗反應層的材料為陽離子型樹脂、硫醇樹脂或其組合。 Preferably, the material of the dark reaction layer is a cationic resin, a thiol resin, or a combination thereof.

較佳地,該模板層固著於該彈性薄膜基材層上。 Preferably, the template layer is fixed on the elastic film substrate layer.

較佳地,本發明的轉印膜結構還包含一位在該暗反應層、該第一圖案層與該固定層之間且由油溶性塗料形成的第二圖案層。 Preferably, the transfer film structure of the present invention further includes a second pattern layer formed between the dark reaction layer, the first pattern layer and the fixed layer and formed of an oil-soluble paint.

較佳地,本發明的轉印膜結構還包含一貼覆在該固定層上的離型膜。 Preferably, the transfer film structure of the present invention further includes a release film attached to the fixing layer.

[轉印膜結構的製法][Manufacturing method of transfer film structure]

較佳地,本發明的轉印膜結構的製法還包含一在該步驟(h)後的步驟(h1),該步驟(h1)是在該暗反應層與該第三圖案次層上形成一由油溶性塗料形成的第二圖案層,該步驟(i)是在該第二圖案層上形成該固定層。 Preferably, the method for manufacturing the transfer film structure of the present invention further includes a step (h1) after the step (h). The step (h1) is to form a layer on the dark reaction layer and the third pattern sublayer. In the second pattern layer formed of an oil-soluble paint, the step (i) is to form the fixed layer on the second pattern layer.

[立體轉印品][Three-dimensional transfer product]

較佳地,本發明的立體轉印品還包含一位在該暗反應層、該第一圖案層與該固定層之間且由油溶性塗料形成的第二圖案層。 Preferably, the three-dimensional transfer product of the present invention further includes a second pattern layer formed between the dark reaction layer, the first pattern layer and the fixing layer and formed of an oil-soluble paint.

100‧‧‧轉印膜結構 100‧‧‧ transfer film structure

1‧‧‧彈性薄膜基材層 1‧‧‧ elastic film substrate layer

20‧‧‧第一圖樣 20‧‧‧First Pattern

2‧‧‧模板層 2‧‧‧ template layer

30‧‧‧第二圖樣 30‧‧‧Second pattern

3‧‧‧第一遮光層 3‧‧‧first light-shielding layer

4‧‧‧第二遮光層 4‧‧‧second light-shielding layer

5‧‧‧填充層 5‧‧‧ Filler

6‧‧‧暗反應層 6‧‧‧ dark reaction layer

7‧‧‧第一圖案層 7‧‧‧ the first pattern layer

71‧‧‧第一圖案次層 71‧‧‧first pattern sublayer

72‧‧‧第二圖案次層 72‧‧‧Second pattern sublayer

73‧‧‧第三圖案次層 73‧‧‧ third pattern sublayer

8‧‧‧固定層 8‧‧‧ fixed layer

9‧‧‧第二圖案層 9‧‧‧ second pattern layer

40‧‧‧物件 40‧‧‧ objects

200‧‧‧立體轉印品 200‧‧‧ three-dimensional transfer

本發明的其他的特徵及功效,將於參照圖式的實施方式中清楚地呈現,其中:圖1是一剖面示意圖,說明實施例1的製法的步驟(a);圖2是一剖面示意圖,說明實施例1的製法的步驟(b);圖3是一剖面示意圖,說明實施例1的製法的步驟(c);圖4是一剖面示意圖,說明實施例1的製法的步驟(d);圖5是一剖面示意圖,說明實施例1的製法的步驟(e);圖6是一剖面示意圖,說明實施例1的製法的步驟(f);圖7是一剖面示意圖,說明實施例1的製法的步驟(g);圖8是一剖面示意圖,說明實施例1的製法的步驟(h);圖9是一剖面示意圖,說明實施例1的製法的步驟(i)及由實施例1得到的轉印膜結構;圖10是一剖面示意圖,說明由實施例2得到的轉印膜結構;圖11是一剖面示意圖,說明由實施例1的製法得到的轉印膜結構通過其固定層貼覆於一物件的表面;圖12是一剖面示意圖,說明應用例1的製法的步驟(m)及由應用例1得到的立體轉印品;圖13是一剖面示意圖,說明由實施例2的製法得到的轉印膜 結構通過其固定層貼覆於一物件的表面;及圖14是一剖面示意圖,說明應用例2的製法的步驟(m)及由應用例2得到的立體轉印品。 Other features and effects of the present invention will be clearly presented in the embodiment with reference to the drawings, in which: FIG. 1 is a schematic cross-sectional view illustrating the step (a) of the manufacturing method of Example 1; FIG. 2 is a schematic cross-sectional view, Step (b) of the manufacturing method of Example 1 is illustrated; FIG. 3 is a schematic cross-sectional view illustrating step (c) of the manufacturing method of Example 1; FIG. 4 is a schematic cross-sectional view illustrating step (d) of the manufacturing method of Example 1; 5 is a schematic cross-sectional view illustrating step (e) of the manufacturing method of Embodiment 1; FIG. 6 is a schematic cross-sectional view illustrating steps (f) of the manufacturing method of Embodiment 1; FIG. 7 is a schematic cross-sectional view illustrating the manufacturing method of Embodiment 1 Step (g) of the manufacturing method; FIG. 8 is a schematic cross-sectional view illustrating the step (h) of the manufacturing method of Example 1; FIG. 9 is a schematic cross-sectional view illustrating the step (i) of the manufacturing method of Example 1 and obtained from Example 1. FIG. 10 is a schematic cross-sectional view illustrating the structure of the transfer film obtained in Example 2. FIG. 11 is a schematic cross-sectional view illustrating the structure of the transfer film obtained by the manufacturing method of Example 1 through its fixed layer. Covering the surface of an object; Figure 12 is a schematic cross-sectional view illustrating the application Step (m) of Preparation method 1 and the Example 1 obtained by the application perspective transfer article; FIG. 13 is a schematic cross-sectional, illustration of a transfer film obtained by the procedure of Example 2 The structure is attached to the surface of an object through its fixed layer; and FIG. 14 is a schematic cross-sectional view illustrating step (m) of the manufacturing method of the application example 2 and the three-dimensional transfer product obtained from the application example 2.

在本發明被詳細描述前,應當注意在以下的說明內容中,類似的元件是以相同的編號來表示。 Before the present invention is described in detail, it should be noted that in the following description, similar elements are represented by the same numbers.

<實施例1><Example 1>

製備轉印膜結構(包含一個圖案層)Preparation of transfer film structure (including a pattern layer)

本實施例1的轉印膜結構的製法包含下列步驟: The method for manufacturing the transfer film structure in this embodiment 1 includes the following steps:

步驟(a):參閱圖1,在一彈性薄膜基材層1上以第一圖樣20形成一由HA-Clear塗料(廠商為大勤化成股份有限公司)形成的模板層2,其中,該彈性薄膜基材層1是由一聚乙烯醇次層及兩個分別位於該聚乙烯醇次層相反兩側的耐綸次層經共同擠壓所形成。 Step (a): Referring to FIG. 1, a template layer 2 formed of HA-Clear coating (manufactured by Daqin Chemical Co., Ltd.) is formed on a flexible film substrate layer 1 with a first pattern 20. The film substrate layer 1 is formed by co-extrusion of a polyvinyl alcohol sublayer and two nylon sublayers respectively located on opposite sides of the polyvinyl alcohol sublayer.

步驟(b):參閱圖2,在該彈性薄膜基材層1上以互補於該第一圖樣20的第二圖樣30形成一由紫外光吸收油墨(UV-AB INK;廠商為大勤化成股份有限公司)形成的第一遮光層3,該第一遮光層3與該模板層2位在同一平面上。 Step (b): Referring to FIG. 2, a second pattern 30 complementary to the first pattern 20 is formed on the elastic film substrate layer 1 to form a UV-AB INK; the manufacturer is Daqin Chemical Co., Ltd. Co., Ltd.) formed a first light-shielding layer 3, the first light-shielding layer 3 and the template layer 2 are located on the same plane.

步驟(c):參閱圖3,在該模板層2上以該第一圖樣20形成一由紫外光吸收油墨(UV-AB INK)形成的第二遮光層4。 Step (c): Referring to FIG. 3, a second light-shielding layer 4 made of ultraviolet-absorbing ink (UV-AB INK) is formed on the template layer 2 with the first pattern 20.

步驟(d):參閱圖4,在該第一遮光層3上以該第二圖樣30形成一由油溶性塗料(HA-K、HA-C、HA-M或HA-Y;廠商為大勤化成股份有限公司)形成的第一圖案次層71,該第一圖案次層71與該第二遮光層4位在同一平面上。 Step (d): Referring to FIG. 4, an oil-soluble paint (HA-K, HA-C, HA-M, or HA-Y) is formed on the first light-shielding layer 3 with the second pattern 30; the manufacturer is Daqin Chemical Co., Ltd.) formed a first pattern sub-layer 71, the first pattern sub-layer 71 and the second light-shielding layer 4 are located on the same plane.

步驟(e):參閱圖5,在該第二遮光層4上以該第一圖樣20形成一由透明油墨(UV-H Clear;廠商為大勤化成股份有限公司)形成的填充層5。 Step (e): Referring to FIG. 5, a filling layer 5 formed of a transparent ink (UV-H Clear; the manufacturer is Daqin Chemical Co., Ltd.) is formed on the second light-shielding layer 4 with the first pattern 20.

步驟(f):參閱圖6,在該第一圖案次層71上以該第二圖樣30形成一由油溶性塗料(HA-K、HA-C、HA-M或HA-Y)形成的第二圖案次層72,該第二圖案次層72與該填充層5位在同一平面上。 Step (f): Referring to FIG. 6, a first pattern formed of an oil-soluble paint (HA-K, HA-C, HA-M, or HA-Y) is formed on the first pattern sub-layer 71 with the second pattern 30. The two pattern sublayers 72 are located on the same plane as the filling layer 5.

步驟(g):參閱圖7,在該填充層5上以該第一圖樣20形成一由油墨(UV-SH INK;廠商為大勤化成股份有限公司)形成的暗反應層6。 Step (g): Referring to FIG. 7, a dark reaction layer 6 formed of ink (UV-SH INK; manufacturer: Daqin Chemical Co., Ltd.) is formed on the filling layer 5 with the first pattern 20.

步驟(h):參閱圖8,在該第二圖案次層72上以該第二圖樣30形成一由油溶性塗料(HA-K、HA-C、HA-M或HA-Y)形成的第三圖案次層73,該第三圖案次層73與該暗反應層6位在同一平面上,該第一圖案次層71、該第二圖案次層72與該第三圖案次層73共同界定出一第一圖案層7。 Step (h): Referring to FIG. 8, a second pattern 30 is formed on the second pattern sublayer 72 to form a first layer formed of an oil-soluble paint (HA-K, HA-C, HA-M, or HA-Y). Three pattern sublayers 73, the third pattern sublayer 73 and the dark reaction layer 6 are located on the same plane, the first pattern sublayer 71, the second pattern sublayer 72 and the third pattern sublayer 73 are jointly defined A first pattern layer 7 is obtained.

步驟(i):參閱圖9,在該暗反應層6與該第三圖案次層73 上方形成一由HAB背膠形成的固定層8,以得到該轉印膜結構100。 Step (i): Referring to FIG. 9, a fixing layer 8 made of HAB adhesive is formed on the dark reaction layer 6 and the third pattern sub-layer 73 to obtain the transfer film structure 100.

需說明的是,該填充層5與該第二圖案次層72的形成順序無特別限制,在本實施例的方法中,可以先形成該第二圖案次層72[步驟(f)]後,再形成該填充層5[步驟(e)]。此外,該暗反應層6與該第三圖案次層73的形成順序同樣也無特別限制,在本實施例的方法中,可以先形成該第三圖案次層73[步驟(h)]後,再形成該暗反應層6[步驟(g)]。 It should be noted that the formation order of the filling layer 5 and the second pattern sub-layer 72 is not particularly limited. In the method of this embodiment, the second pattern sub-layer 72 may be formed first [step (f)], This filling layer 5 is formed again [step (e)]. In addition, the formation order of the dark reaction layer 6 and the third pattern sub-layer 73 is also not particularly limited. In the method of this embodiment, the third pattern sub-layer 73 may be formed first [step (h)], This dark reaction layer 6 was further formed [step (g)].

實施例1得到的轉印膜結構Structure of the transfer film obtained in Example 1

參閱圖9,實施例1得到的轉印膜結構100包含一彈性薄膜基材層1、一模板層2、一第一遮光層3、一第二遮光層4、一填充層5、一暗反應層6、一第一圖案層7及一固定層8。 Referring to FIG. 9, the transfer film structure 100 obtained in Example 1 includes an elastic film substrate layer 1, a template layer 2, a first light-shielding layer 3, a second light-shielding layer 4, a filling layer 5, and a dark reaction. Layer 6, a first pattern layer 7, and a fixed layer 8.

該模板層2以第一圖樣20形成並固著在該彈性薄膜基材層1上且由HA-Clear塗料形成。 The template layer 2 is formed with a first pattern 20 and is fixed on the elastic film substrate layer 1 and is formed of a HA-Clear coating.

該第一遮光層3以互補於該第一圖樣20的第二圖樣30形成在該彈性薄膜基材層1上且由紫外光吸收油墨(UV-AB INK)形成,該第一遮光層3與該模板層2位在同一平面上。 The first light-shielding layer 3 is formed on the elastic film substrate layer 1 with a second pattern 30 complementary to the first pattern 20 and is formed of ultraviolet-absorbing ink (UV-AB INK). The first light-shielding layer 3 and The template layer is located on the same plane.

該第二遮光層4以該第一圖樣20形成在該模板層2上且由紫外光吸收油墨(UV-AB INK)形成。 The second light-shielding layer 4 is formed on the template layer 2 with the first pattern 20 and is formed of a UV-AB INK.

該填充層5以該第一圖樣20形成在該第二遮光層4上且由透明油墨(UV-H Clear)形成。 The filling layer 5 is formed on the second light-shielding layer 4 with the first pattern 20 and is formed of a transparent ink (UV-H Clear).

該暗反應層6由油墨(UV-SH INK)形成且以該第一圖樣20形成在該填充層5上。 The dark reaction layer 6 is formed of ink (UV-SH INK) and is formed on the filling layer 5 in the first pattern 20.

該第一圖案層7以該第二圖樣30形成在該第一遮光層3上且由油溶性塗料(HA-K、HA-C、HA-M或HA-Y)形成。該第一圖案層7包括一第一圖案次層71、一第二圖案次層72及一第三圖案次層73,且該第一圖案層7與該第二遮光層4、該填充層5及該暗反應層6接觸,並與該彈性薄膜基材層1相間隔。 The first pattern layer 7 is formed on the first light-shielding layer 3 with the second pattern 30 and is formed of an oil-soluble paint (HA-K, HA-C, HA-M, or HA-Y). The first pattern layer 7 includes a first pattern sub-layer 71, a second pattern sub-layer 72, and a third pattern sub-layer 73, and the first pattern layer 7 and the second light-shielding layer 4 and the filling layer 5 It is in contact with the dark reaction layer 6 and is spaced from the elastic film substrate layer 1.

該固定層8位在該暗反應層6與該第一圖案層7上且由HAB背膠形成。 The fixing layer 8 is located on the dark reaction layer 6 and the first pattern layer 7 and is formed of HAB adhesive.

需特別說明的是,本實施例的轉印膜結構100還可以依使用者需求包含一位在該暗反應層6、該第一圖案層7與該固定層8之間且呈現金屬質感的蒸鍍層(圖未示)。此外,本實施例的轉印膜結構100也可以依使用者需求包含一貼覆在該固定層8上的離型膜(圖未示),且當欲使用本實施例的轉印膜結構100於物件上產生立體轉印圖案時,需先將該離型膜從該固定層8上移除。 It should be particularly noted that the transfer film structure 100 of this embodiment may further include a metal-based steam layer between the dark reaction layer 6, the first pattern layer 7, and the fixed layer 8 according to user requirements. Plating (not shown). In addition, the transfer film structure 100 of this embodiment may also include a release film (not shown) attached to the fixing layer 8 according to user needs, and when the transfer film structure 100 of this embodiment is to be used When generating a three-dimensional transfer pattern on an object, the release film needs to be removed from the fixing layer 8 first.

<實施例2><Example 2>

製備轉印膜結構(包含兩個圖案層)Preparation of transfer film structure (including two pattern layers)

參閱圖10,本實施例2的轉印膜結構100的製法與實施例1相似,其差別在於,本實施例的製法在該步驟(h)之後,還包含一在該第三圖案次層73與該暗反應層6上形成一第二圖案層9的步驟 (h1),該第二圖案層9是由油溶性塗料(HA-K、HA-C、HA-M或HA-Y)形成,且該步驟(i)是在該第二圖案層9上形成該固定層8。 Referring to FIG. 10, the manufacturing method of the transfer film structure 100 of this embodiment 2 is similar to that of embodiment 1, except that the manufacturing method of this embodiment further includes a third pattern sublayer 73 after the step (h). Forming a second pattern layer 9 on the dark reaction layer 6 (h1), the second pattern layer 9 is formed of an oil-soluble paint (HA-K, HA-C, HA-M, or HA-Y), and the step (i) is formed on the second pattern layer 9 The fixed layer 8.

實施例2得到的轉印膜結構Structure of the transfer film obtained in Example 2

參閱圖10,實施例2得到的轉印膜結構100與實施例1得到的轉印膜結構類似,其差別在於,實施例2的轉印膜結構100還包含一位在該暗反應層6、該第一圖案層7與該固定層8之間的第二圖案層9,且該第二圖案層9與該彈性薄膜基材層1相間隔。 Referring to FIG. 10, the transfer film structure 100 obtained in Example 2 is similar to the transfer film structure obtained in Example 1. The difference is that the transfer film structure 100 of Example 2 further includes a bit in the dark reaction layer 6, The second pattern layer 9 between the first pattern layer 7 and the fixed layer 8 is spaced from the elastic film substrate layer 1.

需特別說明的是,參閱圖9與圖10,不論是實施例1或實施例2,該轉印膜結構100的第一遮光層3接觸該第一圖案層7的一面可設計為具有光滑結構的表面(例如亮面)或具有粗糙結構的表面(例如霧面),或者也可以同時具有光滑結構及粗糙結構的表面,當該第一遮光層3接觸該第一圖案層7的一面為具有粗糙結構的表面時,該第一圖案層7接觸該第一遮光層3的一面也會成為具有粗糙結構的表面。 It should be particularly noted that, referring to FIG. 9 and FIG. 10, whether in Embodiment 1 or Embodiment 2, the side of the first light-shielding layer 3 of the transfer film structure 100 that contacts the first pattern layer 7 may be designed to have a smooth structure. Surface (such as a bright surface) or a surface with a rough structure (such as a matte surface), or a surface with a smooth structure and a rough structure at the same time, when the side of the first light-shielding layer 3 contacting the first pattern layer 7 has When the surface of the rough structure is rough, the side of the first pattern layer 7 that contacts the first light-shielding layer 3 also becomes a surface with a rough structure.

<應用例1><Application Example 1>

製備立體轉印品(由實施例1得到的轉印膜結構製得)Preparation of a three-dimensional transfer product (made from the transfer film structure obtained in Example 1)

本應用例1的立體轉印品的製法除了包含前述實施例1的轉印膜結構的製法所有步驟外,還包含及下列步驟: The manufacturing method of the three-dimensional transfer product of this application example 1 includes all the steps of the manufacturing method of the transfer film structure of the foregoing embodiment 1, and includes the following steps:

步驟(j):參閱圖11,使該轉印膜結構100的固定層8貼覆於一物件40表面。 Step (j): Referring to FIG. 11, the fixing layer 8 of the transfer film structure 100 is attached to the surface of an object 40.

步驟(k):在該步驟(j)之後,以紫外光自該彈性薄膜基材層1朝該固定層8的方向照射,使該第一遮光層3與該第二遮光層4能從該填充層5與該第一圖案層7上剝離。 Step (k): After step (j), ultraviolet light is irradiated from the elastic film substrate layer 1 toward the fixing layer 8 so that the first light-shielding layer 3 and the second light-shielding layer 4 can pass from the The filling layer 5 is separated from the first pattern layer 7.

步驟(l):在該步驟(k)之後,自該填充層5與該第一圖案層7移除該第一遮光層3、該第二遮光層4、該模板層2與該彈性薄膜基材層1。 Step (l): After step (k), remove the first light-shielding layer 3, the second light-shielding layer 4, the template layer 2 and the elastic film base from the filling layer 5 and the first pattern layer 7.材 层 1 Material layer 1.

步驟(m):參閱圖12,在該步驟(l)之後,以紫外光照射該第一圖案層7、該填充層5、該暗反應層6與該固定層8,使該第一圖案層7、該填充層5、該暗反應層6與該固定層8固化後,得到該具有立體轉印圖案的立體轉印品200。 Step (m): Referring to FIG. 12, after the step (1), the first pattern layer 7, the filling layer 5, the dark reaction layer 6 and the fixing layer 8 are irradiated with ultraviolet light to make the first pattern layer 7. After the filling layer 5, the dark reaction layer 6, and the fixing layer 8 are cured, the three-dimensional transfer product 200 having a three-dimensional transfer pattern is obtained.

需特別說明的是,該暗反應層6在紫外光被移除後仍會持續進行固化,用以接著該填充層5、該第一圖案層7與該固定層8。 It should be particularly noted that the dark reaction layer 6 continues to be cured after the ultraviolet light is removed, and is used to follow the filling layer 5, the first pattern layer 7 and the fixing layer 8.

應用例1得到的立體轉印品Three-dimensional transfer product obtained in application example 1

參閱圖12,應用例1得到的立體轉印品200包含一物件40、一固定層8、一暗反應層6、一填充層5、一第三圖案次層73、一第二圖案次層72及一第一圖案次層71。 Referring to FIG. 12, the three-dimensional transfer product 200 obtained in the application example 1 includes an object 40, a fixed layer 8, a dark reaction layer 6, a filling layer 5, a third pattern sublayer 73, and a second pattern sublayer 72. And a first pattern sublayer 71.

該固定層8由HAB背膠形成且貼覆在該物件40表面上。 The fixing layer 8 is formed of HAB adhesive and is attached on the surface of the object 40.

該暗反應層6由油墨(UV-SH INK)形成且以第一圖樣20位在該固定層8上。 The dark reaction layer 6 is formed of ink (UV-SH INK) and is positioned on the fixed layer 8 in a first pattern 20.

該第三圖案次層73以互補於該第一圖樣20的第二圖樣 30位在該固定層8上且由油溶性塗料(HA-K、HA-C、HA-M或HA-Y)形成,該第三圖案次層73與該暗反應層6位在同一平面上。 The third pattern sub-layer 73 is a second pattern complementary to the first pattern 20 30 positions on the fixed layer 8 and formed of oil-soluble paint (HA-K, HA-C, HA-M or HA-Y), the third pattern sub-layer 73 and the dark reaction layer 6 are on the same plane .

該填充層5以該第一圖樣20覆蓋在該暗反應層6上且由透明油墨(UV-H Clear)形成。 The filling layer 5 covers the dark reaction layer 6 with the first pattern 20 and is formed of a transparent ink (UV-H Clear).

該第二圖案次層72以該第二圖樣30覆蓋在該第三圖案次層73上且由油溶性塗料(HA-K、HA-C、HA-M或HA-Y)形成,該第二圖案次層72與該填充層5位在同一平面上。 The second pattern sub-layer 72 covers the third pattern sub-layer 73 with the second pattern 30 and is formed of an oil-soluble paint (HA-K, HA-C, HA-M or HA-Y). The pattern sublayer 72 is located on the same plane as the filling layer 5.

該第一圖案次層71以該第二圖樣30覆蓋在該第二圖案次層72上且由油溶性塗料(HA-K、HA-C、HA-M或HA-Y)形成,該第一圖案次層71、該第二圖案次層72與該第三圖案次層73共同界定出一第一圖案層7。通過該第一圖案次層71的設置而使該物件40表面上形成具有立體觸感的立體轉印圖案。 The first pattern sub-layer 71 covers the second pattern sub-layer 72 with the second pattern 30 and is formed of an oil-soluble paint (HA-K, HA-C, HA-M or HA-Y). The pattern sub-layer 71, the second pattern sub-layer 72 and the third pattern sub-layer 73 jointly define a first pattern layer 7. A three-dimensional transfer pattern with a three-dimensional touch is formed on the surface of the object 40 by the first pattern sub-layer 71 being disposed.

<應用例2><Application Example 2>

製備立體轉印品(由實施例2得到的轉印膜結構製得)Preparation of a three-dimensional transfer product (made from the transfer film structure obtained in Example 2)

本應用例2的立體轉印品的製法除了包含前述實施例2的轉印膜結構的製法所有步驟外,還包含及下列步驟: The manufacturing method of the three-dimensional transfer product of this application example 2 includes all the steps of the manufacturing method of the transfer film structure of the foregoing embodiment 2 and includes the following steps:

步驟(j):參閱圖13,使該轉印膜結構100的固定層8貼覆於一物件40表面。 Step (j): Referring to FIG. 13, the fixing layer 8 of the transfer film structure 100 is attached to the surface of an object 40.

步驟(k):在該步驟(j)之後,以紫外光自該彈性薄膜基材層1朝該固定層8的方向照射,使該第一遮光層3與該第二遮光層 4能從該填充層5與該第一圖案層7上剝離。 Step (k): After step (j), ultraviolet light is irradiated from the elastic film substrate layer 1 toward the fixing layer 8 so that the first light-shielding layer 3 and the second light-shielding layer 4 can pass from the The filling layer 5 is separated from the first pattern layer 7.

步驟(l):在該步驟(k)之後,自該填充層5與該第一圖案層7移除該第一遮光層3、該第二遮光層4、該模板層2與該彈性薄膜基材層1。 Step (l): After step (k), remove the first light-shielding layer 3, the second light-shielding layer 4, the template layer 2 and the elastic film base from the filling layer 5 and the first pattern layer 7.材 层 1 Material layer 1.

步驟(m):參閱圖14,在該步驟(l)之後,以紫外光照射該第一圖案層7、該第二圖案層9、該填充層5、該暗反應層6與該固定層8,使該第一圖案層7、該第二圖案層9、該填充層5、該暗反應層6與該固定層8固化後,得到該立體轉印品200。 Step (m): Referring to FIG. 14, after the step (l), the first pattern layer 7, the second pattern layer 9, the filling layer 5, the dark reaction layer 6 and the fixing layer 8 are irradiated with ultraviolet light. After curing the first pattern layer 7, the second pattern layer 9, the filling layer 5, the dark reaction layer 6 and the fixing layer 8, the three-dimensional transfer product 200 is obtained.

需特別說明的是,該暗反應層6在紫外光被移除後仍會持續進行固化,用以接著該填充層5、該第一圖案層7與該第二圖案層9。 It should be particularly noted that the dark reaction layer 6 continues to be cured after the ultraviolet light is removed, and is used to follow the filling layer 5, the first pattern layer 7 and the second pattern layer 9.

應用例2得到的立體轉印品Three-dimensional transfer product obtained in application example 2

參閱圖14,應用例2得到的立體轉印品200與應用例1得到的立體轉印品相似,其差別在於,應用例2得到的立體轉印品200還包含一位在該暗反應層6、該第一圖案層7與該固定層8之間且由油溶性塗料(HA-K、HA-C、HA-M或HA-Y)形成的第二圖案層9。該第二圖案層9使該物件40表面所形成的立體轉印圖案除了能呈現該第一圖案層7的花紋外,還能呈現另一種有別於該第一圖案層9的花紋。 Referring to FIG. 14, the three-dimensional transfer product 200 obtained in Application Example 2 is similar to the three-dimensional transfer product obtained in Application Example 1. The difference is that the three-dimensional transfer product 200 obtained in Application Example 2 further includes one bit in the dark reaction layer 6. A second pattern layer 9 formed between the first pattern layer 7 and the fixed layer 8 and formed of an oil-soluble paint (HA-K, HA-C, HA-M, or HA-Y). The second pattern layer 9 enables the three-dimensional transfer pattern formed on the surface of the object 40 to present the pattern of the first pattern layer 7 as well as another pattern different from the first pattern layer 9.

綜上所述,本發明的轉印膜結構100是通過該第一遮光 層3與該第二遮光層4的設置,使其在貼覆於一物件40表面後,僅需照射紫外光即可使該第一遮光層3、該第二遮光層4、該模板層2與該彈性薄膜基材層1能從該填充層5與該第一圖案層7上被輕易移除。因此,本發明的轉印膜結構100於該物件40表面所形成的立體轉印圖案上(即該填充層5與該第一圖案層7上)不會殘留離型劑,故確實能達成本發明的目的。 In summary, the transfer film structure 100 of the present invention is The layer 3 and the second light-shielding layer 4 are arranged so that after being affixed to the surface of an object 40, the first light-shielding layer 3, the second light-shielding layer 4, and the template layer 2 need only be irradiated with ultraviolet light. The elastic film substrate layer 1 can be easily removed from the filling layer 5 and the first pattern layer 7. Therefore, the transfer film structure 100 of the present invention does not leave a release agent on the three-dimensional transfer pattern formed on the surface of the object 40 (that is, on the filling layer 5 and the first pattern layer 7), so the cost can be achieved. The purpose of the invention.

惟以上所述者,僅為本發明的實施例而已,當不能以此限定本發明實施的範圍,凡是依本發明申請專利範圍及專利說明書內容所作的簡單的等效變化與修飾,皆仍屬本發明專利涵蓋的範圍內。 However, the above are only examples of the present invention. When the scope of implementation of the present invention cannot be limited by this, any simple equivalent changes and modifications made according to the scope of the patent application and the contents of the patent specification of the present invention are still Within the scope of the invention patent.

Claims (6)

一種立體轉印品,包含:一物件;一貼覆在該物件表面上的固定層;一以第一圖樣位在該固定層上的暗反應層;一以互補於該第一圖樣的第二圖樣位在該固定層上且由油溶性塗料形成的第三圖案次層,該第三圖案次層與該暗反應層位在同一平面上;一以該第一圖樣覆蓋在該暗反應層上且由透明油墨形成的填充層;一以該第二圖樣覆蓋在該第三圖案次層上且由油溶性塗料形成的第二圖案次層,該第二圖案次層與該填充層位在同一平面上;及一以該第二圖樣覆蓋在該第二圖案次層上且由油溶性塗料形成的第一圖案次層,該第一圖案次層、該第二圖案次層與該第三圖案次層共同界定出一第一圖案層。A three-dimensional transfer product includes: an object; a fixed layer attached to the surface of the object; a dark reaction layer positioned on the fixed layer in a first pattern; and a second complementary to the first pattern A third pattern sub-layer formed on the fixed layer and formed of an oil-soluble paint, the third pattern sub-layer being on the same plane as the dark reaction layer; one covering the dark reaction layer with the first pattern And a filling layer formed of transparent ink; a second pattern sublayer covered with the second pattern on the third pattern sublayer and formed of an oil-soluble paint, the second pattern sublayer being at the same level as the filling layer On a plane; and a first pattern sublayer covered with the second pattern on the second pattern sublayer and formed of an oil-soluble paint, the first pattern sublayer, the second pattern sublayer, and the third pattern The sub-layers together define a first pattern layer. 如請求項1所述的立體轉印品,還包含一位在該暗反應層、該第一圖案層與該固定層之間且由油溶性塗料形成的第二圖案層。The three-dimensional transfer product according to claim 1, further comprising a second pattern layer formed between the dark reaction layer, the first pattern layer, and the fixing layer and formed of an oil-soluble paint. 一種立體轉印品的製法,包含下列步驟:(a)在一彈性薄膜基材層上以第一圖樣形成一由塗料形成的模板層;(b)在該彈性薄膜基材層上以互補於該第一圖樣的第二圖樣形成一由紫外光吸收油墨形成的第一遮光層,該第一遮光層與該模板層位在同一平面上;(c)在該模板層上以該第一圖樣形成一由紫外光吸收油墨形成的第二遮光層;(d)在該第一遮光層上以該第二圖樣形成一由油溶性塗料形成的第一圖案次層,該第一圖案次層與該第二遮光層位在同一平面上;(e)在該第二遮光層上以該第一圖樣形成一由透明油墨形成的填充層;(f)在該第一圖案次層上以該第二圖樣形成一由油溶性塗料形成的第二圖案次層,該第二圖案次層與該填充層位在同一平面上;(g)在該填充層上以該第一圖樣形成一暗反應層;(h)在該第二圖案次層上以該第二圖樣形成一由油溶性塗料形成的第三圖案次層,該第三圖案次層與該暗反應層位在同一平面上,該第一圖案次層、該第二圖案次層與該第三圖案次層共同界定出一第一圖案層;(i)形成一位在該暗反應層與該第三圖案次層上方的固定層,以得到一轉印膜結構;(j)使該轉印膜結構的固定層貼覆於一物件表面;(k)在該步驟(j)之後,以紫外光自該彈性薄膜基材層朝該固定層的方向照射;(l)在該步驟(k)之後,自該填充層與該第一圖案層移除該第一遮光層、該第二遮光層、該模板層與該彈性薄膜基材層;及(m)在該步驟(l)之後,以紫外光照射該第一圖案層、該填充層、該暗反應層與該固定層,以得到該立體轉印品。A method for manufacturing a three-dimensional transfer product includes the following steps: (a) forming a template layer made of paint on a flexible film substrate layer with a first pattern; (b) complementing the elastic film substrate layer with The second pattern of the first pattern forms a first light-shielding layer formed of an ultraviolet light absorbing ink, and the first light-shielding layer is on the same plane as the template layer; (c) the first pattern is used on the template layer Forming a second light-shielding layer made of ultraviolet light absorbing ink; (d) forming a first pattern sub-layer made of an oil-soluble paint on the first light-shielding layer in the second pattern, the first pattern sub-layer and The second light-shielding layer is on the same plane; (e) a filling layer formed of a transparent ink is formed on the second light-shielding layer in the first pattern; (f) the first pattern sub-layer is formed on the first pattern sublayer with the first The two patterns form a second pattern sublayer formed of an oil-soluble paint, and the second pattern sublayer is on the same plane as the filling layer; (g) forming a dark reaction layer on the filling layer with the first pattern; ; (H) forming a second pattern on the second pattern sublayer from an oil-soluble paint A third pattern sublayer, the third pattern sublayer and the dark reaction layer being on the same plane, the first pattern sublayer, the second pattern sublayer, and the third pattern sublayer jointly defining a first pattern (I) forming a fixed layer over the dark reaction layer and the third pattern sublayer to obtain a transfer film structure; (j) attaching the fixed layer of the transfer film structure to an object Surface; (k) after the step (j), irradiate ultraviolet light from the elastic film substrate layer toward the fixed layer; (l) after the step (k), from the filling layer and the first The pattern layer removes the first light-shielding layer, the second light-shielding layer, the template layer, and the elastic film substrate layer; and (m) after the step (1), irradiates the first pattern layer, the The filling layer, the dark reaction layer and the fixing layer to obtain the three-dimensional transfer product. 如請求項3所述的立體轉印品的製法,其中,該彈性薄膜基材層的材料為聚乙烯醇、耐綸、聚甲基戊烯、聚對苯二甲酸乙二酯、聚對苯二甲酸丁二酯、聚乙烯吡咯啶酮、聚乙烯、聚丙烯或其組合。The method for producing a three-dimensional transfer product according to claim 3, wherein the material of the elastic film substrate layer is polyvinyl alcohol, nylon, polymethylpentene, polyethylene terephthalate, polyparaphenylene Butyl diformate, polyvinyl pyrrolidone, polyethylene, polypropylene, or a combination thereof. 一種立體轉印品的製法,包含下列步驟:(a)在一彈性薄膜基材層上以第一圖樣形成一由塗料形成的模板層;(b)在該彈性薄膜基材層上以互補於該第一圖樣的第二圖樣形成一由紫外光吸收油墨形成的第一遮光層,該第一遮光層與該模板層位在同一平面上;(c)在該模板層上以該第一圖樣形成一由紫外光吸收油墨形成的第二遮光層;(d)在該第一遮光層上以該第二圖樣形成一由油溶性塗料形成的第一圖案次層,該第一圖案次層與該第二遮光層位在同一平面上;(e)在該第二遮光層上以該第一圖樣形成一由透明油墨形成的填充層;(f)在該第一圖案次層上以該第二圖樣形成一由油溶性塗料形成的第二圖案次層,該第二圖案次層與該填充層位在同一平面上;(g)在該填充層上以該第一圖樣形成一暗反應層;(h)在該第二圖案次層上以該第二圖樣形成一由油溶性塗料形成的第三圖案次層,該第三圖案次層與該暗反應層位在同一平面上,該第一圖案次層、該第二圖案次層與該第三圖案次層共同界定出一第一圖案層;(h1)在該暗反應層與該第三圖案次層上形成一由油溶性塗料形成的第二圖案層;(i)形成一位在該第二圖案層上的固定層,以得到一轉印膜結構;(j)使該轉印膜結構的固定層貼覆於一物件表面;(k)在該步驟(j)之後,以紫外光自該彈性薄膜基材層朝該固定層的方向照射;(l)在該步驟(k)之後,自該填充層與該第一圖案層移除該第一遮光層、該第二遮光層、該模板層與該彈性薄膜基材層;及(m)在該步驟(l)之後,以紫外光照射該第一圖案層、該第二圖案層、該填充層、該暗反應層與該固定層,以得到該立體轉印品。A method for manufacturing a three-dimensional transfer product includes the following steps: (a) forming a template layer made of paint on a flexible film substrate layer with a first pattern; (b) complementing the elastic film substrate layer with The second pattern of the first pattern forms a first light-shielding layer formed of an ultraviolet light absorbing ink, and the first light-shielding layer is on the same plane as the template layer; (c) the first pattern is used on the template layer Forming a second light-shielding layer made of ultraviolet light absorbing ink; (d) forming a first pattern sub-layer made of an oil-soluble paint on the first light-shielding layer in the second pattern, the first pattern sub-layer and The second light-shielding layer is on the same plane; (e) a filling layer formed of a transparent ink is formed on the second light-shielding layer in the first pattern; (f) the first pattern sub-layer is formed on the first pattern sublayer with the first The two patterns form a second pattern sublayer formed of an oil-soluble paint, and the second pattern sublayer is on the same plane as the filling layer; (g) forming a dark reaction layer on the filling layer with the first pattern; ; (H) forming a second pattern on the second pattern sublayer from an oil-soluble paint A third pattern sublayer, the third pattern sublayer and the dark reaction layer being on the same plane, the first pattern sublayer, the second pattern sublayer, and the third pattern sublayer jointly defining a first pattern (H1) forming a second pattern layer formed of an oil-soluble paint on the dark reaction layer and the third pattern sublayer; (i) forming a fixed layer on the second pattern layer to obtain A transfer film structure; (j) attaching the fixed layer of the transfer film structure to an object surface; (k) after step (j), using ultraviolet light from the elastic film substrate layer toward the fixed layer (1) after step (k), remove the first light-shielding layer, the second light-shielding layer, the template layer and the elastic film substrate layer from the filling layer and the first pattern layer; And (m) after step (1), the first pattern layer, the second pattern layer, the filling layer, the dark reaction layer and the fixing layer are irradiated with ultraviolet light to obtain the three-dimensional transfer product. 如請求項5所述的立體轉印品的製法,其中,該彈性薄膜基材層的材料為聚乙烯醇、耐綸、聚甲基戊烯、聚對苯二甲酸乙二酯、聚對苯二甲酸丁二酯、聚乙烯吡咯啶酮、聚乙烯、聚丙烯或其組合。The method for producing a three-dimensional transfer product according to claim 5, wherein the material of the elastic film substrate layer is polyvinyl alcohol, nylon, polymethylpentene, polyethylene terephthalate, polyparaphenylene Butyl diformate, polyvinyl pyrrolidone, polyethylene, polypropylene, or a combination thereof.
TW106122496A 2017-07-05 2017-07-05 Three-dimensional transfer product and manufacturing method thereof TWI679134B (en)