TWI332528B - - Google Patents
Download PDFInfo
- Publication number
- TWI332528B TWI332528B TW96112652A TW96112652A TWI332528B TW I332528 B TWI332528 B TW I332528B TW 96112652 A TW96112652 A TW 96112652A TW 96112652 A TW96112652 A TW 96112652A TW I332528 B TWI332528 B TW I332528B
- Authority
- TW
- Taiwan
- Prior art keywords
- furnace
- gas
- cooling
- heating
- steel
- Prior art date
Links
- 0 *CC1CCCC1 Chemical compound *CC1CCCC1 0.000 description 1
Landscapes
- Solid-Phase Diffusion Into Metallic Material Surfaces (AREA)
- Heat Treatment Of Articles (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
TW96112652A TW200840872A (en) | 2007-04-11 | 2007-04-11 | Method for increasing hardness of the surface of the stainless steel of Martensitic series |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
TW96112652A TW200840872A (en) | 2007-04-11 | 2007-04-11 | Method for increasing hardness of the surface of the stainless steel of Martensitic series |
Publications (2)
Publication Number | Publication Date |
---|---|
TW200840872A TW200840872A (en) | 2008-10-16 |
TWI332528B true TWI332528B (enrdf_load_html_response) | 2010-11-01 |
Family
ID=44821328
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
TW96112652A TW200840872A (en) | 2007-04-11 | 2007-04-11 | Method for increasing hardness of the surface of the stainless steel of Martensitic series |
Country Status (1)
Country | Link |
---|---|
TW (1) | TW200840872A (enrdf_load_html_response) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
TWI421375B (zh) * | 2011-01-28 | 2014-01-01 | Taiwan Powder Technologies Co Ltd | Methods for improving the mechanical properties of non - Austrian iron - based stainless steel surfaces |
TWI796861B (zh) * | 2021-12-03 | 2023-03-21 | 吳祥 | 可直接鑽鎖之不銹鋼螺絲成型方法 |
-
2007
- 2007-04-11 TW TW96112652A patent/TW200840872A/zh unknown
Also Published As
Publication number | Publication date |
---|---|
TW200840872A (en) | 2008-10-16 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
DE4033706C2 (enrdf_load_html_response) | ||
KR100707220B1 (ko) | 개량된 저온 표면 경화 공정 | |
CN100519779C (zh) | 滚动部件及其制造方法 | |
DE102006026883B3 (de) | Verfahren zum Härten von Edelstahl und Salzschmelze zur Durchführung des Verfahrens | |
US10604832B2 (en) | Enhanced activation of self-passivating metals | |
BR112012001238B1 (pt) | Método para carbonetar, nitretar ou nitrocarbonetar um artigo | |
TWI332528B (enrdf_load_html_response) | ||
US20210054866A1 (en) | Bimetallic screw with martensitically hardenable steel | |
JP2020519757A (ja) | マルテンサイト硬化性鋼およびその使用、特にねじの製造 | |
TWI582267B (zh) | 鋼件之表面處理劑及鋼件之表面處理方法 | |
CN101338358A (zh) | 提升马氏体不锈钢表面硬度的方法 | |
JP4551428B2 (ja) | マルテンサイト系ステンレス鋼の表面硬度を向上する方法 | |
US6328819B1 (en) | Method and use of an apparatus for the thermal treatment, in particular nitriding treatment, of metal workpieces | |
CN103774085A (zh) | 一种在低碳合金钢表面制备的高氮奥氏体层及制备方法 | |
JP2006028588A (ja) | 窒化処理方法 | |
CN117965855A (zh) | 一种用于高氮不锈钢的表面处理方法 | |
Bagul et al. | Effects on hardness by various heat treatments processes on HSS tool bit | |
JP5371376B2 (ja) | ステンレス鋼製の加工品の表面硬化方法及び該方法の実施のための溶融塩 | |
US1961520A (en) | Method of case hardening steel | |
CN106756263A (zh) | 一种空气净化预处理室用铝合金制备方法 | |
US10351944B2 (en) | Ferrous alloy | |
Stojanović et al. | Decarburization and Its Effects on the Properties of Plasma-Nitrided AISI 4140 Steel: A Review | |
Greßmann | Fe-C and Fe-N compound layers: Growth kinetics and microstructure | |
KR100902169B1 (ko) | 마르텐사이트계 스테인레스 표면경도 강화방법 | |
CN118308579A (zh) | 一种高耐蚀、抗疲劳的高氮马氏体不锈钢及其制备方法 |