TWI328682B - Method of inspecting film and inspection device using the same - Google Patents

Method of inspecting film and inspection device using the same Download PDF

Info

Publication number
TWI328682B
TWI328682B TW96109595A TW96109595A TWI328682B TW I328682 B TWI328682 B TW I328682B TW 96109595 A TW96109595 A TW 96109595A TW 96109595 A TW96109595 A TW 96109595A TW I328682 B TWI328682 B TW I328682B
Authority
TW
Taiwan
Prior art keywords
glue
characteristic line
midpoint
attached
predetermined
Prior art date
Application number
TW96109595A
Other languages
Chinese (zh)
Other versions
TW200839216A (en
Inventor
Yi Wang
Original Assignee
Au Optronics Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Au Optronics Corp filed Critical Au Optronics Corp
Priority to TW96109595A priority Critical patent/TWI328682B/en
Publication of TW200839216A publication Critical patent/TW200839216A/en
Application granted granted Critical
Publication of TWI328682B publication Critical patent/TWI328682B/en

Description

13286821328682

三達編號:TW3304PA ' 九、發明說明: 【發明所屬之技術領域】 本發明係有關於一種膠材之檢測方法及檢測裝置’且 特別是有關於一種膠材貼附準確性之檢測方法及檢測裝 ·置。 【先前技術】 近年來,平面化顯示裝置由於體積小、重量輕以及低 • 輻射等特點,愈來愈受到消費者的喜愛。此外,更由於製 程的進步,使得平面化顯示裝置在顯示品質大幅提昇的同 時,亦能夠不斷降低生產成本,使得平面化顯示裝置的價 格能夠趨於大眾化,進一步提昇了市場的佔有率。在市場 上銷售的各式各樣平面化顯示裝置中,又以液晶顯示裝置 最為普及,成為現代家庭或辦公室中不可或缺的電子產 品。 在一般薄膜電晶體液晶顯示器的製造過程中’常應用 • 一種將晶粒覆晶接合(Flip Chip Bonding)於軟性電路板 (Flexible Printed Circuit board,FPC board)基材上的技術, 也就是將驅動IC及其電子零件直接安放於薄膜上,用以 節省基板上所需之空間,一般稱之為軟膜上覆晶(ChipO Film,COF)技術。當欲將COF技術之軟膜接合於印刷電 路板(Printed Circuit Board,PCB )時,常常是利用異方 性導電膜(Anisotropic Conductive Film,ACF)將印刷電路 板與軟膜黏合,同時使印刷電路板上之多條導電線路(a 6 1328682 三雜號:TW3304PA 稱之為金手指)連接於軟膜上對應之導電線路。普遍之作 法係將異方性導毛膜貼附於印刷電路板之表面,並且於進 行其他製程步驟前,檢測異方性導電膜之貼附狀況。达达编号号: TW3304PA ' 九, invention description: [Technical field of invention] The present invention relates to a method and a detection device for a rubber material, and in particular to a method for detecting the adhesion accuracy of a glue material and detecting the same Install and set. [Prior Art] In recent years, flat panel display devices have become more and more popular among consumers due to their small size, light weight, and low radiation. In addition, due to the advancement of the process, the flat display device can continuously reduce the production cost while the display quality is greatly improved, so that the price of the flat display device can be popularized, and the market share is further improved. Among the various flat-panel display devices marketed on the market, liquid crystal display devices are most popular, becoming an indispensable electronic product in modern homes or offices. In the manufacturing process of a general thin film transistor liquid crystal display, it is often used. • A technique of Flip Chip Bonding on a flexible printed circuit board (FPC board) substrate, that is, driving The IC and its electronic components are placed directly on the film to save space on the substrate. This is commonly referred to as ChipO Film (COF) technology. When a soft film of COF technology is to be bonded to a printed circuit board (PCB), an anisotropic conductive film (ACF) is often used to bond the printed circuit board to the flexible film while making the printed circuit board. A plurality of conductive lines (a 6 1328682 three miscellaneous numbers: TW3304PA is called a gold finger) are connected to the corresponding conductive lines on the soft film. It is common practice to attach an anisotropic film to the surface of a printed circuit board and to detect the attachment of the anisotropic conductive film before performing other processing steps.

由於異方性導電膠膜一般而言係為半透明,因此導電 線路上有貼附導電臈處之灰度值會低於無貼附導電膜處 之灰度值。傳統之檢測方法,首先係於電路板上定義一檢 測區域,並且設定一門檻灰度值,此門檻灰度值係介於導 電線路上有無貼附導電膜之兩灰度值之間。接著利用電耦 中多個偵測點的灰度值,然後統計此些偵測點之灰度值。 此些偵測點之灰度值可分為第一部分及第二部分,第一部 分之灰度值係超過該門檻灰度值,第二部分之灰度值係低 於該門檻灰度值。當第一部分之灰度值所佔的比例超過二 定值蚪’則判斷異方性導電膜無貼附於印刷電路板上(灰 度值較高)4目反地,當第二部分之灰度值所佔的比例= 過一定值時,則判斷異方性導電膜有貼附於印刷電路 (灰度值較低)。 然每一導電線路由於製程因素或材料因素,其灰户值 不儘相同,因此當統計此些偵測點之灰度值時會受到 導電線路之不同灰度值影響。當此些導電線路之顏色2古 時,容易使得此些_點之灰度值偏高,而將有貼附 性導電膠之印刷電路板誤判為未貼附異方性導電膠。ς 些導電線路之顏色太暗時,容易使得此些偵測點二此 偏低,而將無貼附異方性導電膠之印刷電路板誤判 7 1328682Since the anisotropic conductive film is generally translucent, the gray value attached to the conductive trace on the conductive line is lower than the gray value at the non-attached conductive film. The conventional detection method first defines a detection area on the circuit board, and sets a threshold gray value which is between the two gray values of the conductive film on the conductive line. Then, the gray values of the plurality of detection points in the electrical coupling are utilized, and then the gray values of the detection points are counted. The gray values of the detection points can be divided into a first part and a second part. The gray value of the first part exceeds the gray value of the threshold, and the gray value of the second part is lower than the gray value of the threshold. When the proportion of the gray value of the first part exceeds the second value 蚪', it is judged that the anisotropic conductive film is not attached to the printed circuit board (higher gray value), and the second part is grayed out. The ratio of the degree value = When the value exceeds a certain value, it is judged that the anisotropic conductive film is attached to the printed circuit (the gray value is low). However, the ash value of each conductive line is not the same due to process factors or material factors. Therefore, when the gray values of these detection points are counted, they are affected by different gray values of the conductive lines. When the color of the conductive lines is 2, it is easy to make the gray value of the _ points higher, and the printed circuit board with the adhesive conductive paste is mistakenly judged as the unattached conductive adhesive.时 When the color of some conductive lines is too dark, it is easy to make these detection points lower, and the printed circuit board without the anisotropic conductive adhesive is misjudged 7 1328682

TW3304PA ^方性導電膠。如此〜來導致檢測錯誤, 之^ J"何提高檢測異方性導電膠貼附狀況 貝為目Θ逐待研究的重要課題之一。 【發明内容】 用在之檢測方法及檢測裝置,其係利 裳扁 之表面上定義一膠材預定貼附區域以及一 ::偵測區之方式’藉由偵測各條導電線路本二同i灰 附,爭可划齡寸之特徵線,不僅可判斷膠材是否貼 有可提高檢測^被貼附之寬度、偏移量或傾斜度。其係具 ,性以及增進檢測效率等優點。 根據本發明之—古 以檢測—騎_於n_材之檢測方法,用 多條導電線路。此些導附狀況,此表面上係具有 度值,此些導電唆Μ電線路有貼附膠材處對應-第-灰 檢測方法i先無貼附膠材處對應-第二灰度值。此 區域係具有—第一2表面上定義一預定膠材貼附區域,此 叩,此第―上疋義第债 -偵測區内之多個^ ^之第—邊緣。其次,镇測第 一及 已貼 第二灰度值來點的灰度值,藉以根據第 附的一第一特徵線 偵測區内是否存在代表膠材 根據本發明之另一 用以撿測-膠材貼附:提出一種膠材之檢測裝置, 置有多條導電線路。照二表面之貼附狀況,此表面上係設 夕材係貼附於此表面上,此些導電線 8 1328682TW3304PA ^ square conductive adhesive. Such a ~ to lead to detection errors, ^ J " how to improve the detection of the anisotropic conductive adhesive tape attached to the shell is one of the important topics to be studied. SUMMARY OF THE INVENTION The detection method and the detection device are used to define a predetermined attachment area of a rubber material on the surface of the Lishang flat and a method of detecting the area by detecting the respective conductive lines. i gray attached, can compete for the feature line of the age, not only can be judged whether the glue is attached to improve the width, offset or inclination of the detection ^ attached. Its accessories, sex and improved detection efficiency. According to the present invention, a plurality of conductive lines are used for the detection method of detecting-riding_n_material. In these lead-in conditions, the surface has a degree value, and the conductive electric circuit has a corresponding glue-attached material. The first-gray detection method i has no corresponding glue-attached material-second gray value. This area has a first predetermined surface on which a predetermined adhesive attachment area is defined, and this first, upper 疋 第 - - - - - - - - - - - Secondly, the first and the second gray value are pasted to the gray value, so that the presence or absence of the representative glue in the detection area according to the first feature line attached to the first one is used for speculation according to the present invention. - Adhesive attach: A detection device for the adhesive material is proposed, which is provided with a plurality of conductive lines. According to the attachment condition of the two surfaces, the surface of the surface is attached to the surface, and the conductive wires 8 1328682

三達編號:TW3304PA * 路有貼附膠材處係對應一第一灰度值,而無貼附膠材處係 對應一第二灰度值。此裝置包括一參數設置單元、一影像 擷取單元以及一中央處理單元。參數設置單元用以於此表 面上定義一預定膠材貼附區域,此區域具有第一邊緣。此 參數設置單元另用以於此表面上定義第一偵測區,此第一 • 偵測區係涵蓋第一邊緣的一部分。影像擷取單元用於偵測 第一偵測區内多個第一偵測點的灰度值。中央處理單元用 於根據第一灰度值及第二灰度值來判斷第一偵測區内是 • 否存在代表膠材已貼附的一第一特徵線。 為讓本發明之上述之内容能更明顯易懂,下文特舉較 佳之實施例,並配合所附圖式,作詳細說明如下: 【實施方式】 第一實施例 依照本發明第一實施例之膠材的檢測方法,係用以檢 測一膠材貼附於一表面之貼附狀況。請參照第1圖,其繪 示依照本發明第一實施例之膠材的檢測法的流程圖。此表 面上設置有多條導電線路,此些導電線路有貼附膠材之處 係對應一第一灰度值,此些導電線路無貼附膠材之處係對 應一第二灰度值。此檢測方法包括下述步驟。 首先,如步驟110所示,於此表面上定義一預定膠材 貼附區域,此預定膠材貼附區域具有一第一邊緣。 其次,於此表面上定義一第一偵測區,如步驟120所 示。此第一偵、測區係涵蓋第一邊緣的一部分。 9Sanda number: TW3304PA * The road has a glue attached to the first gray value, and the non-attached glue corresponds to a second gray value. The device includes a parameter setting unit, an image capturing unit, and a central processing unit. The parameter setting unit is configured to define a predetermined glue attachment area on the surface, the area having a first edge. The parameter setting unit is further configured to define a first detection area on the surface, and the first detection area covers a part of the first edge. The image capturing unit is configured to detect gray values of the plurality of first detecting points in the first detecting area. The central processing unit is configured to determine, according to the first gray value and the second gray value, whether the first detection area is in the first detection area or not. In order to make the above-mentioned contents of the present invention more comprehensible, the following detailed description of the preferred embodiments, together with the accompanying drawings, will be described in detail as follows: [Embodiment] The first embodiment is in accordance with the first embodiment of the present invention. The method for detecting the glue is used to detect the attachment of a glue to a surface. Referring to Fig. 1, there is shown a flow chart of a method for detecting a rubber material according to a first embodiment of the present invention. A plurality of conductive lines are disposed on the surface, and the conductive lines are attached with a first gray value corresponding to the adhesive material, and the conductive lines are not attached with the glue material corresponding to a second gray value. This detection method includes the following steps. First, as shown in step 110, a predetermined glue attachment area is defined on the surface, the predetermined glue attachment area having a first edge. Next, a first detection zone is defined on the surface, as shown in step 120. This first detection and measurement area covers a part of the first edge. 9

S達編號:TW3304PA 依照本實施例之檢測方法,接著進行步驟⑽, 區内多個第一偵測點的灰度值,藉以根據各條導 兒線路本身之第一灰度值及第二 ,存在代表獅占附的—第一特徵線斷第更丨 二當膠材貼附於表面時’藉由祕一憤測區内不二 第一债測點之灰度值,可找出膠材貼附之邊界,即為此^ —特徵線。也就是說’當第_特徵線存在_,即代表夥材 已貼附於表面上。相反地,若第一特徵線不存在,則 谬材未貼附於表面上。 、 上述依照本發明第-實施例之膠材的檢測方法,係於 表面上^義第―_區’並且利詩-導電線路本身有貼 附膠材處及無貼附膠材處不同的第一灰度值及第二灰产 值之交界,來取得第-特徵線。若無法取得此第一特^ 線,則代表騎未朗於表面上。錢點在於,由於依昭 本發明第-實施例之檢财法,制料—導電線路本身、 有貼附膠材處及無貼附膠材處不同的第一 灰=來判斷第一特徵線是否存在’可避免因:導電線: 之灰度值過〶或過低,或是*同導電線路間灰 異’導致檢測膠材貼附時誤判的狀況,坦4 測之正確性。 ^了谬材貼附檢 第二實施例 請同時參照第2〜5Β圖,第2圖洽;7 實施例之檢測方法中待檢測二二 !328682 %S number: TW3304PA According to the detection method of the embodiment, step (10), the gray value of the plurality of first detection points in the area, according to the first gray value of the respective line of the guide line and the second, There is a representative of the lion's possession—the first characteristic line breaks the second time. When the glue is attached to the surface, 'the gray value of the first debt measurement point in the secret area of the secret test can be found. The attached border is the ^-feature line. That is to say, 'When the _ characteristic line exists _, it means that the buddy has been attached to the surface. Conversely, if the first characteristic line is not present, the coffin is not attached to the surface. The method for detecting the rubber material according to the first embodiment of the present invention is based on the surface of the first __ zone and the Lishi-conductive circuit itself has a different adhesive attached to the material and no attached material. A boundary between a gray value and a second gray value is obtained to obtain a first feature line. If this first special line cannot be obtained, it means that the ride is not on the surface. The point of money lies in the fact that the first characteristic line is judged by the first method of the invention, in which the first ash of the material-conducting circuit itself, the attached adhesive material and the non-adhesive material are different. Whether there is 'can avoid the cause: the conductive line: the gray value is too low or too low, or * the same as the gray line between the conductive lines' leads to the detection of the misjudgment when the glue is attached, the accuracy of the test. ^Coffin Attachment Inspection Second Embodiment Please refer to the 2nd to 5th drawings at the same time, the second diagram is in contact; 7 The detection method of the embodiment is to be tested 22!328682%

Ξ達編號:TW3304PA 圖,第3圖繪示第2圖中第一及第二偵測區、預定朦材貼 附區域以及膠材之示意圖;第4至第5Β圖繪示依照本發 明第二貫施例之膠材的檢測方法的流程圖。膠材U係貼 • 附於表面12上’且表面12上設置有多條導電線路13,如 , 第2圖所示。此些導電線路13有貼附膠材11之處13a係 對應一第一灰度值,而此些導電線路13無貼附膠材11之 處13b係對應一第二灰度值。於本實施例中,此表面12 例如是為一印刷電路板(Printed Circuit Board,PCB)之表 鲁 面’而膠材11例如是一異方性導電膜(Anisotropic Conductive Film,ACF)。 依照本發明第二貫施例之膠材之檢測方法,係可僅由 單一特徵線檢測膠材貼附之傾斜狀況,首先如第4圖之步 驟210所示,於表面12上定義一預定膠材貼附區域14, 此預定膠材貼附區域14具有一第—邊緣14a。 接著,如步驟220所示’於表面12上定義一第一價 測區15 ’此第一偵測區15係涵蓋第一邊緣i4a的一部分。 然後’進行步驟230,偵測第一偵測區15内複數個第 一偵測點的灰度值,藉以根據各條導電線路13本身之第 一灰度值及第二灰度值來判斷第一偵測區15内是否存在 一第一特徵線L1。當膠材11貼附於表面12時,藉由偵測 第一偵測區15内不同第〆彳貞測點之灰度值,可找出膠村 11貼附之邊界’即為此第一特敬線L1。也就是說,當第 一特徵線L1存在時,即代表膠枒11已貼附於表面12上。 此外’若判斷第一特徵線L1不存在,本實施例之檢测方 11 1328682Ξ达号: TW3304PA, Figure 3 shows the first and second detection zones in Figure 2, the predetermined coffin attachment area and the schematic view of the glue; the fourth to fifth figures show the second according to the present invention. A flow chart of the method for detecting the glue of the embodiment. The glue U-tie is attached to the surface 12' and the surface 12 is provided with a plurality of conductive lines 13, as shown in Fig. 2. Where the conductive lines 13 have the adhesive material 11 attached thereto, 13a corresponds to a first gray value, and the conductive lines 13 do not have the attached material 11 at a position 13b corresponding to a second gray value. In this embodiment, the surface 12 is, for example, a surface of a printed circuit board (PCB), and the glue 11 is, for example, an anisotropic conductive film (ACF). According to the method for detecting the rubber material according to the second embodiment of the present invention, the inclination of the adhesive material can be detected by only a single characteristic line. First, as shown in step 210 of FIG. 4, a predetermined glue is defined on the surface 12. The material attachment area 14, the predetermined glue attachment area 14 has a first edge 14a. Next, as shown in step 220, a first coupon region 15' is defined on the surface 12. The first detection region 15 covers a portion of the first edge i4a. Then, in step 230, the gray value of the plurality of first detection points in the first detection area 15 is detected, thereby determining the first gray value and the second gray value according to the respective conductive lines 13 themselves. A first feature line L1 is present in a detection area 15. When the glue material 11 is attached to the surface 12, by detecting the gray value of different 〆彳贞 measurement points in the first detection area 15, the boundary of the glued village 11 can be found. Special line L1. That is, when the first feature line L1 is present, it means that the capsule 11 has been attached to the surface 12. In addition, if it is judged that the first characteristic line L1 does not exist, the detecting side of the embodiment 11 1328682

三達編號:TW3304PA " 法接著則發出一膠材未貼附信息,如步驟231所示。 若於上述步驟230中判斷第一特徵線L1存在時,此 檢測方法接著進行步驟232,取得一第一傾角θ 1,以判 斷膠材11貼附之傾斜狀況。此第一傾角0 1係為第一特 徵線L1及第一邊緣14a之夾角。其次,當第一傾角Θ1 未在一角度預設範圍内時,發出一膠材貼附角度異常信 息,如步驟233所示。 另外,依照本發明第二實施例之膠材之檢測方法,亦 ® 可利用第一特徵線及第二特徵線來檢測膠材貼附寬度、膠 材貼附偏移量及膠材貼附之傾斜狀況。如第5A圖所示, 首先進行步驟310,定義預定膠材貼附區域14。接著進行 步驟320,定義第一偵測區15。步驟310及步驟320之内 容與上述利用單一特徵線進行檢測之步驟210及步驟220 (繪示於第4圖)相同,此處不再贅述。 預定膠材貼附區域14另包括一第二邊緣14b,第二邊 緣14b與第一邊緣14a彼此相對,如第2圖所示。此檢測 • 方法更可包括步驟340,於表面12上定義一第二偵測區 16。此第二偵測區16係涵蓋第二邊緣14b的一部分,且 對應於第一偵測區15之處。 接著,此檢測方法進行步驟330,判斷第一偵測區15 内是否存在第一特徵線ί 1,若判斷第一特徵線L1不存 在,則執行步驟331,發出膠材未貼附信息。步驟330及 步驟331之内容亦相同於上述利用單一特徵線進行檢測之 步驟230及步驟231 (繪示於第4圖),不再重複敘述。 12 1328682The Sanda number: TW3304PA " method then sends a glue unattached information, as shown in step 231. If it is determined in the above step 230 that the first feature line L1 is present, the detecting method proceeds to step 232 to obtain a first tilt angle θ1 to determine the tilting state of the glue 11 attached. The first inclination angle 0 1 is an angle between the first feature line L1 and the first edge 14a. Secondly, when the first inclination angle Θ1 is not within an angle preset range, a glue attachment angle abnormality information is issued, as shown in step 233. In addition, according to the method for detecting the rubber material according to the second embodiment of the present invention, the first characteristic line and the second characteristic line can be used to detect the adhesive width of the adhesive material, the offset of the adhesive material, and the adhesive material attached thereto. Tilt condition. As shown in Fig. 5A, step 310 is first performed to define a predetermined glue attachment area 14. Next, step 320 is performed to define the first detection area 15. The steps of step 310 and step 320 are the same as steps 210 and 220 (shown in FIG. 4) for detecting by using a single feature line, and are not described herein again. The predetermined glue attachment area 14 further includes a second edge 14b which is opposite to the first edge 14a as shown in Fig. 2. The detection method may further include a step 340 of defining a second detection zone 16 on the surface 12. The second detection zone 16 covers a portion of the second edge 14b and corresponds to the first detection zone 15. Then, the detecting method proceeds to step 330 to determine whether the first feature line ί exists in the first detecting area 15. If it is determined that the first feature line L1 does not exist, step 331 is executed to issue the glue unattached information. The contents of the steps 330 and 331 are the same as those of the step 230 and the step 231 (shown in FIG. 4) for detecting using a single feature line, and the description will not be repeated. 12 1328682

三達編號:TW3304PA 然後,此檢測方法可更進一步包括步驟350,偵測第 二偵測區16内複數個第二偵測點的灰度值,藉以根據第 一灰度值及第二灰度值來判斷第二偵測區16内是否存在 代表膠材11已貼附的一第二特徵線L2。若判斷第一特徵 線L2不存在,則發出膠材未貼附信息,如步驟351所示。 請參考第5B圖,若於上述步驟350中判斷第二特徵 線L2存在,也就是第一特徵線L1及第二特徵線L2皆存 在時,此檢測方法接著進行步驟360,根據第一特徵線L1 之中點S1及第二特徵線L2之中點S2,取得膠材11貼附 之寬度,用以判斷膠材11貼附之寬度狀況。兩中點S1及 S2之距離係約略相等於膠材11貼附之寬度。接著,如步 驟361所示,當膠材11貼附之寬度未在一預設寬度範圍 内時,發出一膠材貼附寬度異常信息。 更進一步來說,第一邊緣14a對應於該第一偵測區15 内之部分具有一第一預定中點S1’,第二邊緣14b對應於 第二偵測區16内之部分具有一第二預定中點S2’。本實施 例之檢測方法亦可利用第一預定中點S1’、第二預定中點 S2’、第一特徵線L1之中點S1及第二特徵線L2之中點 S2,來判斷膠材11貼附之寬度狀況。第一預定中點S1’ 與第二預定中點S2’的距離為一第一寬度W1,第一特徵線 L1之中點S1與第二特徵線L2之中點S2的距離為一第二 寬度W2,此第二寬度W2係約略相等於膠材11貼附之寬 度。接著,如步驟362所示,當第一寬度W1與第二寬度 W2兩者之差值大於一寬度容許誤差值時,發出膠材貼附 13 1328682The third method is TW3304PA. The detection method may further include a step 350 of detecting a gray value of the plurality of second detection points in the second detection area 16 according to the first gray value and the second gray level. The value is used to determine whether there is a second characteristic line L2 in the second detection area 16 that the adhesive material 11 has attached. If it is judged that the first characteristic line L2 does not exist, the glue unattached information is issued, as shown in step 351. Referring to FIG. 5B, if it is determined in the above step 350 that the second feature line L2 exists, that is, both the first feature line L1 and the second feature line L2 are present, the detecting method proceeds to step 360, according to the first feature line. A point S2 between the midpoint S1 of the L1 and the second characteristic line L2 obtains the width of the adhesive material 11 attached to determine the width of the adhesive material 11 attached. The distance between the two midpoints S1 and S2 is approximately equal to the width to which the glue 11 is attached. Next, as shown in step 361, when the width of the adhesive 11 is not within a predetermined width, a glue attachment width abnormality information is issued. Further, the first edge 14a has a first predetermined midpoint S1' corresponding to the portion of the first detection region 15, and the second edge 14b has a second portion corresponding to the portion of the second detection region 16. The midpoint S2' is scheduled. The detecting method of this embodiment may also determine the glue 11 by using the first predetermined midpoint S1', the second predetermined midpoint S2', the point S1 of the first characteristic line L1, and the point S2 of the second characteristic line L2. The width of the attached. The distance between the first predetermined midpoint S1' and the second predetermined midpoint S2' is a first width W1, and the distance between the point S1 of the first characteristic line L1 and the point S2 of the second characteristic line L2 is a second width. W2, this second width W2 is approximately equal to the width to which the glue 11 is attached. Next, as shown in step 362, when the difference between the first width W1 and the second width W2 is greater than a width tolerance value, the adhesive material is attached 13 1328682

三達編號:TW3304PA ' 寬度異常信息。 其次,若於上述步驟350中判斷第二特徵線L2存在, 也就是第一特徵線L1及第二特徵線L2皆存在時,此檢測 方法亦可進行步驟370,根據第一預定中點S1’ 、第二預 定中點S2’ 、第一特徵線L1之中點S1及第二特徵線L2 -· 之中點S2,取得膠材11貼附之偏移量,用以判斷膠材11 貼附之偏移狀況。接著,如步驟371所示,當膠材11貼 附之偏移量超出一偏移容許誤差範圍時,發出一膠材貼附 • 偏移量異常信息。 更進一步來說,本實施例之檢測方法係利用一第一偏 移量及一第二偏移量來判斷膠材11貼附之偏移狀況。此 第一偏移量係為第一預定中點S1’與第一特徵線L1之中 點S1的距離,此第二偏移量係為第二預定中點S2’與第 二特徵線L2之中點S2的距離。接著,如步驟372所示, 當第一偏移量與第二偏移量兩者其中之一超出一偏移容 許誤差範圍時,發出膠材貼附偏移量異常信息。 ® 再者,若於上述步驟350中判斷第二特徵線L2存在, 也就是第一特徵線L1及第二特徵線L2皆存在時,此檢測 方法更可進行步驟380,取得第一傾角0 1以及一第二傾 角Θ2,藉以判斷膠材貼附之傾斜狀況,此第二傾角02 係為第二特徵線L2及第二邊緣14b之夾角。接著,如步 驟381所示,當第一傾角01及第二傾角02兩者至少其 中之一超出一角度容許誤差範圍時,發出膠材貼附角度異 常信息。 14 1328682Sanda number: TW3304PA 'Width exception information. Next, if it is determined in the above step 350 that the second feature line L2 exists, that is, both the first feature line L1 and the second feature line L2 are present, the detecting method may also perform step 370 according to the first predetermined midpoint S1' a second predetermined midpoint S2', a point S1 in the first characteristic line L1, and a point S2 in the second characteristic line L2 -·, and an offset amount of the glue 11 attached is obtained to determine the adhesion of the glue 11 The offset condition. Next, as shown in step 371, when the offset of the glue 11 is attached beyond an offset tolerance, a glue attachment/offset abnormality information is issued. Furthermore, the detecting method of this embodiment utilizes a first offset amount and a second offset amount to determine the offset condition of the glue 11 attached. The first offset is the distance between the first predetermined midpoint S1' and the point S1 of the first characteristic line L1, and the second offset is the second predetermined midpoint S2' and the second characteristic line L2. The distance from the midpoint S2. Next, as shown in step 372, when one of the first offset and the second offset exceeds an offset tolerance error range, the glue attachment offset abnormality information is issued. Further, if it is determined in the above step 350 that the second characteristic line L2 exists, that is, both the first characteristic line L1 and the second characteristic line L2 are present, the detecting method may further perform step 380 to obtain the first inclination angle 0 1 And a second inclination angle Θ2 for judging the inclination of the glue attached, the second inclination angle 02 being an angle between the second characteristic line L2 and the second edge 14b. Next, as shown in step 381, when at least one of the first inclination angle 01 and the second inclination angle 02 exceeds an angular tolerance range, the glue attachment angle abnormality information is issued. 14 1328682

三達編號:TW3304PA 另一方面,上述依照本發明較佳實施例之膠材的檢測 方法,係可應用於一檢測裝置中。請同時參照第6圖,其 繪示依照本發明較佳實施例之膠材的檢測裝置的方塊 圖。檢測裝置20包括一參數設置單元21、一影像擷取單 元22以及一中央處理單元23。參數設置單元21用以於表 面12上定義前述之預定膠材貼附區域14、第一偵測區15 及第二偵測區16。影像擷取單元22用於偵測第一偵測區 15内此些第一偵測點的灰度值,以及偵測第二偵測區16 内此些第二偵測點的灰度值。於本實施例中,此影像擷取 單元22可例如是一電搞合裝置(Charged-Coupled Device,CCD)。中央處理單元23用於根據第一灰度值及 第二灰度值來判斷第一偵測區15以及第二偵測區16内是 否存在代表膠材11已貼附的第一特徵線L1及第二特徵線 L2 ° 更進一步來說,當中央處理單元23判斷第一特徵線 L1及第二特徵線L2皆存在後,中央處理單元23係可進 一步判斷膠材11貼附的狀況。首先,中央處理單元23可 根據第一特徵線L1之中點S1及第二特徵線L2之中點 S2,取得膠材11之貼附寬度,藉以判斷膠材11貼附之寬 度狀況。第二,中央處理單元23可根據第一預定中點 S1,、第二預定由點S2,、第一特徵線L1之中點S1及 第二特徵線L2之中點S2,取得膠材11貼附之偏移量,藉 以判斷膠材11貼附之偏移狀況。其次,中央處理單元23 可根據第一傾角Θ1及第二傾角Θ2,判斷該膠材11貼附 15 1328682Sanda number: TW3304PA On the other hand, the above-described method for detecting a rubber material according to a preferred embodiment of the present invention can be applied to a detecting device. Please also refer to Fig. 6, which is a block diagram of a detecting device for a rubber material in accordance with a preferred embodiment of the present invention. The detecting device 20 includes a parameter setting unit 21, an image capturing unit 22, and a central processing unit 23. The parameter setting unit 21 is configured to define the predetermined predetermined glue attaching area 14, the first detecting area 15 and the second detecting area 16 on the surface 12. The image capturing unit 22 is configured to detect gray values of the first detecting points in the first detecting area 15 and detect gray values of the second detecting points in the second detecting area 16 . In this embodiment, the image capturing unit 22 can be, for example, a Charged-Coupled Device (CCD). The central processing unit 23 is configured to determine, according to the first gray value and the second gray value, whether the first feature line L1 and the first feature line L1 on which the representative glue 11 has been attached are present in the first detection area 15 and the second detection area 16 Second feature line L2 ° Further, when the central processing unit 23 determines that both the first feature line L1 and the second feature line L2 are present, the central processing unit 23 can further determine the condition in which the glue 11 is attached. First, the central processing unit 23 can obtain the attachment width of the glue 11 based on the point S2 of the first feature line L1 and the point S2 of the second feature line L2, thereby judging the width condition of the glue 11 attached. Second, the central processing unit 23 can obtain the glue 11 according to the first predetermined midpoint S1, the second predetermined point S2, the point S1 of the first characteristic line L1, and the point S2 of the second characteristic line L2. The offset is attached to judge the offset of the glue 11 attached. Next, the central processing unit 23 can determine that the glue 11 is attached according to the first inclination angle Θ1 and the second inclination angle Θ2. 15 1328682

三達編號:TW3304PA 之傾斜狀況。 另外,檢測裝置20更包括一警告單元24,當膠材11 貼附之寬度未在預設寬度範圍内,或者第一寬度W1與第 二寬度W2兩者之差值大於寬度容許誤差值時,此警告單 元24係發出膠材貼附寬度異常信息。其次,當膠材11貼 •附之偏移量超出偏移容許誤差範圍,或者第一偏移量與第 二偏移量兩者其中之一超出偏移容許誤差範圍時,警告單 元係發出膠材貼附偏移量異常信息。再者,當第一傾角Θ1 • 及第二傾角Θ2兩者至少其中之一超出角度容許誤差範圍 時,警告單元係發出膠材貼附角度異常信息。 上述依照本發明較佳實施例之膠材的檢測方法及檢 測裝置,係於表面上定義第一偵測區及第二偵測區,並且 利用每一導電線路本身有貼附膠材處及無貼附膠材處不 同的第一灰度值及第二灰度值之交界,來取得第一特徵線 及第二特徵線。如此一來,係可藉由第一特徵線之中點及 第二特徵線之中點,判斷膠材貼附之寬度狀況是否異常。 * 其次,更可藉由第一偏移量及第二偏移量來判斷膠材貼附 之偏移狀況是否異常。第一偏移量係為第一預定中點與第 一特徵線之中點的距離,第二偏移量係為第二預定中點與 第二特徵線之中點的距離。此外,此檢測方法及檢測裝置 亦可藉由第一傾角或是第-一傾角來判斷膠材貼附之傾斜 狀況是否異常。第一傾角係為第一特徵線與膠材預定貼附 區域之第一邊緣間的夾角,第二傾角係為第二特徵線與膠 材預定貼附區域之第二邊緣間的夾角。其係可避免因導電 1328682Sanda number: Tilt condition of TW3304PA. In addition, the detecting device 20 further includes a warning unit 24, when the width of the glue 11 attached is not within the preset width, or the difference between the first width W1 and the second width W2 is greater than the width tolerance value, This warning unit 24 issues a glue attachment width abnormality information. Secondly, when the offset of the glue 11 is out of the offset tolerance range, or one of the first offset and the second offset exceeds the offset tolerance range, the warning unit emits glue The material is attached with offset error information. Furthermore, when at least one of the first inclination angle Θ1 and the second inclination angle Θ2 exceeds the angle tolerance range, the warning unit issues the glue attachment angle abnormality information. The method for detecting and detecting the rubber material according to the preferred embodiment of the present invention defines a first detection area and a second detection area on the surface, and each of the conductive lines itself has a glue attached thereto and no The first feature line and the second feature line are obtained by attaching a boundary between the first gray value and the second gray value at different positions of the glue. In this way, whether the width of the glue attached is abnormal is determined by the midpoint of the first characteristic line and the middle of the second characteristic line. * Secondly, it can be judged whether the offset condition of the glue attached is abnormal by the first offset and the second offset. The first offset is the distance between the first predetermined midpoint and the midpoint of the first characteristic line, and the second offset is the distance between the second predetermined midpoint and the midpoint of the second characteristic line. In addition, the detecting method and the detecting device can also judge whether the tilting state of the glue attached is abnormal by the first inclination angle or the first inclination angle. The first angle of inclination is the angle between the first characteristic line and the first edge of the predetermined attachment area of the glue, and the second angle of inclination is the angle between the second characteristic line and the second edge of the predetermined attachment area of the glue. Its system can avoid conduction due to conduction 1328682

三達編號:TW3304PA 線路之灰度值過商或過低5或是不同導電線路間灰度值的 差異,導致檢測膠材貼附時誤判的狀況,增加了膠材貼附 檢測之正確性。此外,由於影像擷取單元僅需偵測第一偵 測區及第二偵測區内之多個第一偵測點及多個第二偵測 點,係可增進檢測膠材貼附之效率。再者,由於膠材貼附 ' 於表面之寬度、偏移量及傾斜角度均受到檢測,係可增進 膠材貼附之準確性,進一步提昇了產品品質。 综上所述,雖然本發明已以較佳之實施例揭露如上, • 然其並非用以限定本發明。本發明所屬技術領域中具有通 常知識者,在不脫離本發明之精神和範圍内,當可作各種 之更動與潤飾。因此,本發明之保護範圍當視後附之申請 專利範圍所界定者為準。Sanda number: TW3304PA line gray value is too low or too low 5 or the difference in gray value between different conductive lines, which leads to the detection of misjudgment when the glue is attached, which increases the correctness of the glue attachment test. In addition, since the image capturing unit only needs to detect a plurality of first detection points and a plurality of second detection points in the first detection area and the second detection area, the efficiency of detecting the adhesion of the glue material can be improved. . In addition, since the width, offset and inclination angle of the adhesive attached to the surface are detected, the accuracy of the adhesive attachment can be improved, and the product quality is further improved. In view of the foregoing, the invention has been described above in terms of preferred embodiments, which are not intended to limit the invention. It will be apparent to those skilled in the art that various changes and modifications can be made without departing from the spirit and scope of the invention. Therefore, the scope of the invention is defined by the scope of the appended claims.

17 132868217 1328682

三達編號:TW3304PA ' 【圖式簡單說明】 第1圖繪示依照本發明第一實施例之膠材的檢測方法 的流程圖; 第2圖繪示依照本發明第二實施例之檢測方法中待檢 測之膠材貼附於表面上之示意圖; • · 第3圖繪示第2圖中第一及第二偵測區、預定膠材貼 附區域以及膠材之示意圖; 第4至第5B圖繪示依照本發明第二實施例之膠材的 _ 檢測方法的流程圖,以及 第6圖繪示依照本發明較佳實施例之膠材的檢測裝置 的方塊圖。 【主要元件符號說明】 11 :膠材 12 ··表面 13 :導電線路 • 、-· 13 a .導電線路有貼附膠·材之處 13 b ·導電線路無貼附朦材之處 14 :預定膠材貼附區域 14a :第一邊緣 14b :第二邊緣 15 :此第一偵測區 16 :第二偵測區 20 :檢測裝置 18 1328682 三達編號:TW3304PA 21 : 參數設置單元 22 : 影像擷取單元 23 : 中央處理單元 24 : 警告單元 L1 : 第一特徵線 L2 : 第二特徵線 S1 : 第一特徵線之中點 sr :第一預定中點 • S2 :第二特徵線之中點 S2,:第二預定中點 W1 :第一寬度 W2 :第二寬度 0 1 :第一傾角 02 :第二傾角Sanda number: TW3304PA' [Simple description of the drawing] FIG. 1 is a flow chart showing a method for detecting a rubber material according to a first embodiment of the present invention; and FIG. 2 is a view showing a detecting method according to a second embodiment of the present invention. Schematic diagram of the glue to be tested attached to the surface; • Figure 3 shows the first and second detection zones in Figure 2, the predetermined glue attachment area and the schematic view of the glue; 4th to 5B The figure shows a flow chart of a method for detecting a glue material according to a second embodiment of the present invention, and Fig. 6 is a block diagram showing a device for detecting a glue material according to a preferred embodiment of the present invention. [Description of main components] 11: Adhesive material 12 ·· Surface 13 : Conductive line • , -· 13 a . Conductive line with adhesive and material 13 b · Conductive line without attached coffin 14 : Schedule Adhesive attachment area 14a: first edge 14b: second edge 15: this first detection area 16: second detection area 20: detection device 18 1328682 three-number: TW3304PA 21: parameter setting unit 22: image 撷The taking unit 23: central processing unit 24: warning unit L1: first characteristic line L2: second characteristic line S1: first point of the first characteristic line sr: first predetermined midpoint • S2: point S2 of the second characteristic line ,: second predetermined midpoint W1: first width W2: second width 0 1 : first inclination angle 02: second inclination angle

Claims (1)

1328682 三達編號:TW3304PA 十、申請專利範圍: 1. 一種膠材之檢測方法,用以檢測一膠材貼附於一表 面之貼附狀況,該表面上設置有複數條導電線路,該等導 電線路有貼附該膠材之處係對應一第一灰度值,該等導電 線路無貼附該膠材之處係對應一第二灰度值,該檢測方法 包括: (a)在該表面上定義一預定膠材貼附區域,該預定膠 材貼附區域具有一第一邊緣; 鲁 (b)在該表面上定義一第一偵測區,該第一偵測區係 涵蓋該第一邊緣的一部分;以及 (c)偵測該第一偵測區内複數個第一偵測點的灰度 值,藉以根據該第一灰度值及該第二灰度值來判斷該第一 偵測區内是否存在代表該膠材已貼附的一第一特徵線。 2. 如申請專利範圍第1項所述之檢測方法,其中當該 第一特徵線存在時,該檢測方法包括: (dl)取得一第一傾角,該第一傾角係為該第一特徵線 ^ 及該第一邊緣之夾角,藉以判斷該膠材貼附之傾斜狀況。 3. 如申請專利範圍第2項所述之檢測方法,另包括: (d2)當該第一傾角未在一角度預設範圍内時,發出一 膠材貼附角度異常信息。 4. 如申請專利範圍第1項产斤述之檢測方法,另包括: (e)當第一特徵線不存在時,發出一膠材未貼附信息。 5. 如申請專利範圍第1項所述之檢測方法,其中該預 定膠材貼附區域另包括一第二邊緣,該第二邊緣與該第一 20 1328682 三達編號:TW3304PA 邊緣彼此相對,該檢測方法另包括: (f) 在該表面上定義一第二偵測區,該第二偵測區係 涵蓋該第二邊緣的一部分,且該第二偵測區係對應於該第 一偵測區之處;以及 (g) 偵測該第二偵測區内複數個第二偵測點的灰度 值,藉以根據該第一灰度值及該第二灰度值來判斷該第二 偵測區内是否存在代表該膠材已貼附的一第二特徵線。 6. 如申請專利範圍第5項所述之檢測方法,其中當該 ® 第一特徵線及該第二特徵線皆存在時,該檢測方法另包 括: (hi)根據該第一特徵線之中點及該第二特徵線之中 點,取得該膠材貼附之寬度。 7. 如申請專利範圍第6項所述之檢測方法,另包括: (h2)當該膠材貼附之寬度未在一預設寬度範圍内 時,發出一膠材貼附寬度異常信息。 I 8.如申請專利範圍第6項所述之檢測方法,其中該第 一邊緣對應於該第一偵測區内之部分具有一第一預定中 點,該第二邊緣對應於該第二偵測區内之部分具有一第二 預定中點,該第一預定中點與該第二預定中點的距離係為 一第一寬度,該第一特徵線之中點與該第二特徵線之中點 的距離係為一第二寬度,該檢測方法另包括: (h3)當該第一寬度與該第二寬度兩者之差值大於一 寬度容許誤差值時,發出一膠材貼附寬度異常信息。 21 1328682 三達編號:TW3304PA * 9.如申請專利範圍第5項所述之檢測方法,其中該第 一邊緣具有一第一預定中點,該第二邊緣具有一第二預定 中點,且當該第一特徵線及該第二特徵線皆存在時,該檢 測方法另包括: (il)根據該第一預定中點、該第二預定中點、該第一 ' 特徵線之中點及該第二特徵線之中點,取得該膠材貼附之 偏移量。 10. 如申請專利範圍第9項所述之檢測方法,另包括: ® (i2)當該膠材貼附之偏移量超出一偏移容許誤差範 圍時,發出一膠材貼附偏移量異常信息。 11. 如申請專利範圍第9項所述之檢測方法,其中該 第一預定中點與該第一特徵線之中點的距離係為一第一 偏移量,該第二預定中點與該第二特徵線之中點的距離係 為一第二偏移量,該檢測方法另包含: (i3)當該第一偏移量與該第二偏移量兩者其中之一 超出一偏移容許誤差範圍時,發出一膠材貼附偏移量異常 馨信息。 12. 如申請專利範圍第5項所述之檢測方法,其中當 該第一特徵線及該第二特徵線皆存在時,該檢測方法另包 括: (jl)取得一第一傾角及一第二傾角,藉以判斷該膠材 貼附之傾斜狀況,該第一傾角係為該第一特徵線及該第一 邊緣之夾角,該第二傾角係為該第二特徵線及該第二邊緣 之夾角。 22 1328682 三達編號:TW3304PA 材係貼附於該表面上,其中該等導電線路有貼附該膠材之 處係對應一第一灰度值,該等導電線路無貼附該膠材之處 係對應一第二灰度值,該裝置包括: 一參數設置單元,用以於該表面上定義一預定膠材貼 附區域,該預定膠材貼附區域具有第一邊緣,該參數設置 單元另用以於該表面上定義一第一偵測區,該第一偵測區 係涵蓋該第一邊緣的一部分; 一影像擷取單元,用於偵測該第一偵測區内複數個第 一偵測點的灰度值;以及 一中央處理單元,用於根據該第一灰度值及該第二灰 度值來判斷該第一偵測區内是否存在代表該膠材已貼附 的一第一特徵線。 21. 如申請專利範圍第20項所述之檢測裝置,其中該 預定膠材貼附區域另包括第二邊緣,該第二邊緣與該第一 邊緣彼此相對; 該參數設置單元另用以於該表面上定義一第二偵測 區,該第二偵測區係涵蓋該第二邊緣的一部分; 該影像擷取單元另用於偵測該第二偵測區内複數個 第二偵測點的灰度值; 該中央處理單元另用於根據該第一灰度值及該第二 灰度值來判斷該第二偵測區内是否存在代表該膠材已貼 附的一第二特徵線。 22. 如申請專利範圍第21項所述之檢測裝置,其中當 該第一特徵線及該第二特徵線皆存在時,該中央處理單元 24 1328682 三達編號:TW3304PA 另用於根據該第一特徵線之中點及該第二特徵線之中 點,取得該膠材之貼附寬度,藉以判斷該膠材貼附之寬度 狀況。 23. 如申請專利範圍第22項所述之檢測裝置,另包 括: / 一警告單元,當該膠材貼附之寬度未在一預設寬度範 圍内時,該警告單元係發出一膠材貼附寬度異常信息。 24. 如申請專利範圍第22項所述之檢測裝置,其中該 ® 第一邊緣對應該第一偵測區内之部分具有一第一預定中 點,該第二邊緣對應該第二偵測區内之部分具有一第二預 定中點,該第一預定中點與該第二預定中點的距離係為一 第一寬度,該第一特徵線之中點與該第二特徵線之中點的 距離係為一第二寬度,該檢測裝置另包括: 一警告單元,當該第一寬度與該第二寬度兩者之差值 大於一寬度容許誤差值時,該警告單元係發出一膠材貼附 ^ 寬度異常信息。 25. 如申請專利範圍第21項所述之檢測裝置,其中當 該第一特徵線及該第二特徵線皆存在時,該中央處理單元 另用於根據該第一預定中點、該第二預定中點、該第一特 徵線之中點及該第二特徵線之中點,取得該膠材貼附之偏 移量,藉以判斷該膠材貼附之偏移狀況。 26. 如申請專利範圍第25項所述之檢測裝置,另包 括: 一警告單元,當該膠材貼附之偏移量超出一偏移容許 25 1328682 三達編號:TW3304PA 誤差範圍時,發出一膠材貼附偏移量異常信息。 27. 如申請專利範圍第25項所述之檢測裝置,其中該 第一預定中點與該第一特徵線之中點的距離係為一第一 偏移量,該第二預定中點與該第二特徵線之中點的距離係 為一第二偏移量,該檢測裝置另包括: 一警告單元,當該第一偏移量與該第二偏移量兩者其 中之一超出一偏移容許誤差範圍時,該警告單元係發出一 膠材貼附偏移量異常信息。 28. 如申請專利範圍第21項所述之檢測裝置,其中當 該第一特徵線及該第二特徵線皆存在時,該中央處理單元 另用於取得一第一傾角及一第二傾角,藉以判斷該膠材貼 附之傾斜狀況,該第一傾角係為該第一特徵線及該第一邊 緣之爽角’該第二傾角係為該第二特徵線及該第二邊緣之 夾角。 29. 如申請專利範圍第28項所述之檢測裝置,另包 括: 一警告單元,當該第一傾角及該第二傾角兩者至少其 中之一超出一角度容許誤差範圍時,該警告單元係發出一 膠材貼附角度異常信息。 30. 如申請專利範圍拿20項所述之檢測裝置,其中該 影像擷取單元係為一電子耦合裝置。 261328682 Sanda number: TW3304PA X. Patent application scope: 1. A method for detecting a glue material for detecting the attachment condition of a glue attached to a surface, the surface is provided with a plurality of conductive lines, the conductive Where the line has the glue attached thereto corresponds to a first gray value, and the conductive line is not attached to the glue corresponding to a second gray value, the detection method comprises: (a) on the surface Defining a predetermined glue attachment area, the predetermined glue attachment area having a first edge; and (b) defining a first detection area on the surface, the first detection area covering the first a portion of the edge; and (c) detecting a gray value of the plurality of first detection points in the first detection area, thereby determining the first detection according to the first gray value and the second gray value A first characteristic line representing the glue has been attached to the test area. 2. The detecting method according to claim 1, wherein when the first characteristic line exists, the detecting method comprises: (dl) obtaining a first inclination angle, wherein the first inclination angle is the first characteristic line ^ and the angle between the first edge, in order to judge the inclination of the glue attached. 3. The method of detecting according to item 2 of the patent application, further comprising: (d2) issuing a glue attachment angle abnormality information when the first inclination angle is not within a predetermined range of an angle. 4. For the test method of the first paragraph of the patent application scope, the method further includes: (e) When the first characteristic line does not exist, a glue unattached information is issued. 5. The method of claim 1, wherein the predetermined glue attachment area further comprises a second edge, the second edge and the first 20 1328682 three-numbered: TW3304PA edges are opposite each other, The detection method further includes: (f) defining a second detection area on the surface, the second detection area covers a portion of the second edge, and the second detection area corresponds to the first detection And (g) detecting a gray value of the plurality of second detection points in the second detection area, thereby determining the second detection according to the first gray value and the second gray value A second characteristic line representing the glue has been attached to the test area. 6. The detecting method according to claim 5, wherein when the first characteristic line and the second characteristic line are both present, the detecting method further comprises: (hi) according to the first characteristic line The point and the midpoint of the second characteristic line are obtained to obtain the width of the adhesive attached. 7. The method of detecting according to item 6 of the patent application, further comprising: (h2) when the width of the glue attached is not within a predetermined width range, an adhesive material width error information is issued. The detection method of claim 6, wherein the first edge corresponds to a portion of the first detection zone having a first predetermined midpoint, and the second edge corresponds to the second detection The portion of the measurement area has a second predetermined midpoint, and the distance between the first predetermined midpoint and the second predetermined midpoint is a first width, and the middle point of the first characteristic line and the second characteristic line The distance between the midpoints is a second width, and the detecting method further comprises: (h3) issuing a glue attachment width when a difference between the first width and the second width is greater than a width tolerance value Abnormal information. The method of claim 5, wherein the first edge has a first predetermined midpoint, the second edge has a second predetermined midpoint, and When the first feature line and the second feature line are both present, the detecting method further includes: (il) according to the first predetermined midpoint, the second predetermined midpoint, the first 'feature line midpoint, and the The midpoint of the second characteristic line obtains the offset of the glue attached. 10. The test method as described in claim 9 of the patent application, further comprising: ® (i2) issuing a glue attachment offset when the offset of the adhesive attached exceeds an offset tolerance Abnormal information. 11. The detection method of claim 9, wherein the distance between the first predetermined midpoint and the midpoint of the first characteristic line is a first offset, the second predetermined midpoint and the The distance between the points in the second characteristic line is a second offset, and the detecting method further comprises: (i3) when one of the first offset and the second offset exceeds an offset When the tolerance is within the range, a mislabeling information is attached to the adhesive. 12. The detecting method of claim 5, wherein when the first characteristic line and the second characteristic line are both present, the detecting method further comprises: (jl) obtaining a first tilt angle and a second The inclination angle is used to determine the inclination of the adhesive attached. The first inclination angle is an angle between the first characteristic line and the first edge, and the second inclination angle is an angle between the second characteristic line and the second edge. . 22 1328682 Sanda number: TW3304PA is attached to the surface, wherein the conductive lines have a first gray value corresponding to the glue, and the conductive lines are not attached to the glue. Corresponding to a second gray value, the device comprises: a parameter setting unit, configured to define a predetermined glue attachment area on the surface, the predetermined glue attachment area has a first edge, and the parameter setting unit further A first detection area is defined on the surface, the first detection area is a part of the first edge; an image capturing unit is configured to detect the plurality of first areas in the first detection area Detecting a gray value of the point; and a central processing unit, configured to determine, according to the first gray value and the second gray value, whether there is a one in the first detection area that represents that the glue has been attached The first characteristic line. 21. The detecting device of claim 20, wherein the predetermined glue attachment area further comprises a second edge, the second edge and the first edge being opposite to each other; the parameter setting unit is further configured to A second detection area is defined on the surface, and the second detection area is a part of the second edge. The image capturing unit is further configured to detect a plurality of second detection points in the second detection area. The central processing unit is further configured to determine, according to the first gray value and the second gray value, whether there is a second characteristic line in the second detection area that is attached to the glue. 22. The detecting device of claim 21, wherein when the first characteristic line and the second characteristic line are both present, the central processing unit 24 1328682 has a serial number: TW3304PA is further used according to the first The midpoint of the characteristic line and the middle point of the second characteristic line obtain the attachment width of the glue material, thereby judging the width condition of the glue attached. 23. The detecting device according to claim 22, further comprising: / a warning unit, when the width of the adhesive is not within a predetermined width, the warning unit issues a glue sticker Width exception information is attached. 24. The detecting device of claim 22, wherein the first edge corresponds to a portion of the first detection zone having a first predetermined midpoint, and the second edge corresponds to the second detection zone The inner portion has a second predetermined midpoint, and the distance between the first predetermined midpoint and the second predetermined midpoint is a first width, and the midpoint of the first characteristic line and the middle of the second characteristic line The detecting device further includes: a warning unit, when the difference between the first width and the second width is greater than a width tolerance value, the warning unit sends out a glue Attach the width exception information. 25. The detecting device of claim 21, wherein when the first characteristic line and the second characteristic line are both present, the central processing unit is further configured to use the first predetermined midpoint, the second The midpoint of the predetermined midpoint, the midpoint of the first characteristic line, and the midpoint of the second characteristic line are obtained by the offset of the adhesive attached to determine the offset of the adhesive attached. 26. The detecting device according to claim 25, further comprising: a warning unit, when the offset of the adhesive attached exceeds an offset tolerance of 25 1328682 three-number: TW3304PA error range, one is issued The offset information of the offset is attached to the glue. 27. The detecting device of claim 25, wherein the distance between the first predetermined midpoint and the midpoint of the first characteristic line is a first offset, the second predetermined midpoint and the The distance between the points in the second characteristic line is a second offset. The detecting device further includes: a warning unit, when one of the first offset and the second offset exceeds a bias When the tolerance range is shifted, the warning unit issues a glue attachment offset abnormality information. 28. The detecting device of claim 21, wherein the central processing unit is further configured to obtain a first tilt angle and a second tilt angle when both the first feature line and the second feature line are present. The first inclination angle is the first characteristic line and the refreshing angle of the first edge, and the second inclination angle is an angle between the second characteristic line and the second edge. 29. The detecting device of claim 28, further comprising: a warning unit, wherein the warning unit is when at least one of the first inclination angle and the second inclination angle exceeds an angular tolerance range Send a glue to attach an angle abnormality information. 30. The invention as claimed in claim 20, wherein the image capturing unit is an electronic coupling device. 26
TW96109595A 2007-03-20 2007-03-20 Method of inspecting film and inspection device using the same TWI328682B (en)