TWI254672B - Forming method of cubic patterns on textile ribbon surface and forming mechanism therefore - Google Patents

Forming method of cubic patterns on textile ribbon surface and forming mechanism therefore Download PDF

Info

Publication number
TWI254672B
TWI254672B TW94113225A TW94113225A TWI254672B TW I254672 B TWI254672 B TW I254672B TW 94113225 A TW94113225 A TW 94113225A TW 94113225 A TW94113225 A TW 94113225A TW I254672 B TWI254672 B TW I254672B
Authority
TW
Taiwan
Prior art keywords
webbing
sequin
substrate
dimensional
pattern
Prior art date
Application number
TW94113225A
Other languages
Chinese (zh)
Other versions
TW200637727A (en
Inventor
Tsung-Wen Shiu
Original Assignee
He Mei Aquatint Garment Co Ltd
Jia Luen Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by He Mei Aquatint Garment Co Ltd, Jia Luen Co Ltd filed Critical He Mei Aquatint Garment Co Ltd
Priority to TW94113225A priority Critical patent/TWI254672B/en
Application granted granted Critical
Publication of TWI254672B publication Critical patent/TWI254672B/en
Publication of TW200637727A publication Critical patent/TW200637727A/en

Abstract

The invention is a forming method of cubic patterns on textile ribbon surface and forming mechanism thereof, the forming method includes: providing a textile ribbon and a glitter material, wherein the bottom of the glitter material is an adhesive surface that makes the glitter material located upon; then employing push and punch means to drop the predetermined blocks on material and to be pressed and bound on the corresponding sites of the textile ribbon surface, meanwhile, the pressed glitter on the ribbon surface can achieve binding and fastening status with textile ribbon via the adhesive surface (or in coordination with heating)at the bottom that can form cubic and glittering patterns on textile ribbon surface, hence, in aspects of the forming mechanism, it discloses realistic mechanism styles to finish the existing formation method; the invention can fulfill more achievements about easy manufacture, increased efficiency, cost reduction, cubic and gradation beauty, and protective membrane for patterns than the previous trans-printing method.

Description

1254672 ' 九、發明說明: 【發明所屬之技術領域】 本發明係涉及一種織帶,特別是指織帶表面之立體亮面圖案的創新成 型方法以及成型機構者。 【先前技術】 按,織帶於日常生活中,被廣泛使用於一些飾品吊帶、置物包 背帶上;有鑑於傳統織帶表面單調欠缺豐富、活潑風格之缺弊, • 遂有業者陸續開發出表面具有花紋圖案的創新織帶產品;現有織 帶表面上的花紋圖案構造型態,概分為編織形成方式及轉印成型 方式,其中,若要達到亮面效果,則編織方式難以達成,目前多 採用轉印方式製成,該所述轉印方式,必須將亮面圖紋之色料先 印製於一基材之不沾黏性表面上形成預定之圖案花紋,接著再藉 由加熱加壓手段將該基材上之亮面圖紋轉印到織帶表面上;惟, 此種習知結構型態於實際使用經驗中發現仍存在下述之問題點·· ^ 1、就生產效率及製造成本而言:由於轉印方式必須先將圖案花 紋印製於一基材上,再從該基材上將圖案花紋轉印到織帶上, 如此,不僅使得製造流程延長而降低效率、提高成本,其原本印製 圖案花紋的基材也將於轉印之後全數報廢,造成資源上的浪 費。 2、就裝飾性而言··由於該藉由轉印形成之亮面圖紋層於織帶表 面上僅為薄狀色料所形成之亮面型態,欠缺立體層次之美感 1254672 s 3、就結構性而言:該藉由緣E 丄 得P ^/成之壳面圖紋層表面並無法直 接形成保護膜,如此,〗生士)方古 化成5亥冗面圖紋層容易被磨損而淡化 失去壳度、不夠持久耐用之問題點。 是以’針對上述所言’如何研發出—種更符合產業利用性、 更具理想實用性的織帶亮面圖案成型方法及成㈣構,實有待業 界再加以思索突破者。</ RTI> </ RTI> <RTIgt; </ RTI> <RTIgt; </ RTI> <RTIgt; </ RTI> <RTIgt; </ RTI> <RTIgt; </ RTI> <RTIgt; </ RTI> <RTIgt; [Prior Art] According to the weaving belt, it is widely used in some slings and storage bag straps in daily life. In view of the lack of monotonous and lively style of traditional webbing, the company has developed a surface with patterns. The innovative webbing product of the pattern; the pattern pattern of the pattern on the surface of the existing webbing is divided into the weaving forming method and the transfer forming method. In order to achieve the glossy surface effect, the weaving method is difficult to achieve, and the transfer method is currently used. In the transfer method, the color of the glossy pattern must be printed on the non-stick surface of a substrate to form a predetermined pattern, and then the substrate is heated and pressurized. The glossy pattern on the material is transferred onto the surface of the webbing; however, this kind of conventional structural pattern has found that the following problems still exist in the actual use experience. 1. In terms of production efficiency and manufacturing cost: Since the transfer method must first print the pattern on a substrate, and then transfer the pattern from the substrate to the webbing, thus not only prolonging the manufacturing process but also reducing the manufacturing process. Efficiency and cost, after its original design patterns printed substrate transfer will also be fully scrapped, resulting in waste of resources. 2. In terms of decorativeness, the bright surface pattern formed by the transfer of the glossy surface layer on the surface of the webbing is only a thin surface, and the aesthetics of the three-dimensional layer are lacking 1254672 s. Structurally speaking, the surface of the shell surface layer of P ^ / formed by the edge E can not directly form a protective film, so that the layer of the surface of the surface of the surface is easily worn out. Lighten the problem of losing shell and not being durable enough. It is based on how the above-mentioned words have been developed to develop a method for forming a webbing glossy pattern that is more in line with industrial applicability and more desirable and practical, and it is a matter of fact that the industry has to think about breakthroughs.

【發明内容】 即,本發明之主要目的,係在提供—種織帶表面立體Μ成型方法, 其較佳實施例係包括:提供-織帶和―亮片基材,其中該亮片基材底部為 黏性面;以使亮片基材置於織帶上方呈不壓合之對應狀態 ;復施以一沖斷 手段將亮片基材上的就雜區塊沖落壓合於織帶表社姆應處,此同 時,被壓合於織帶表面上的亮片並得藉由其底部黏性面(或配合加熱)與 織帶達成結合蚊狀態;藉由前述健合於織帶表社的以,得形成實 心形狀的立體亮面圖案。該成型方法的另—較佳實施例,則是採用了兩次 的沖麼手段’其中施以第-次沖斷手段時得將亮片基材上的預定形狀之中 空區塊先沖^施以第二次沖斷手段時則是將亮片基材上的狀形狀之外 框區塊沖落壓合於織帶表面上;藉此得形射空形狀的立體亮面圖案。 本發明之另一主要目的,係在提供 種織帶表面立體圖案成型機構, 1254672 =檢構,,=基材-亮片缺料檢知 定亮片圖案之中空部位.以及&quot;Γ ’―弟一党心型機構,藉以沖斷形成預 之位移及停止時機;一钟^=私1丨 曰 於成’纖V放料機構,藉以架置織帶·一筮—古μ &amp; 構,藉以將亮片基材上預心精卞置、、《一党片造型機 土何上頂叹之邊形狀區塊加以 ,以及,一亮片伺服拉料機構,藉以控制亮片基材 1 ; 一第二亮片造型禎 成品伺服拉料機構,葬^丨^7 一。一〜丨^里壓合黏貼於織帶上; 藉以收置完成結合亮片之=及二止時機;一成品收料機構, 基材之廢料者。 ^成…一冗片廢料收集機構,藉以收置亮片 置有一亮片滿 其中,该受片飼服拉料機構與織帶放料機構之間更可設 料檢知機構。 其中,該第-、第二亮片造型機構中更包括有加熱裝置 間更可再設置有_二次 其中,該成品飼服拉料機構與成品收料機構之 加溫壓合機構者。 承上 不兔明主要可較習知轉印方 簡便、效率提高'具立體層次美感以=織帶亮面圖案達到製造更 茶具有保護膜等實用效益。 【實施方式】 為使貴審查委員對本發明之目的 解與認識,茲請配合【圖式簡單說明】詳】坡及功效能夠有更進一步之暸 請配合參閱第1、2圖所示,係太ϋ后· 法暨其成型機之較佳實施例,首先,該成:明織帶表面立體圖案成型方 a、 提供具預定長寬及厚度之一織帶、型方法之較佳實施例係包括: 其中,該亮片基材(3 〇);部Y)和&amp;亮片基材(3 〇 ),且 b、 使亮片基材(3〇)置於織帶(^生,(31); c、 如第2圖之(a)所示,施以一&quot;上方王不壓合之對應狀態; 〇)上的預定形狀之中空區塊亮7沖斷手段,將亮片基材(3 d、 如第2圖之(b)所示,施以;J2)先沖落; 弟一二入沖斷手段,將亮片基材(3 7 1254672 Ο)上的預疋形狀之外框區塊亮片(3 q+ 表面上相對應處,此同時,碰合於織帶2 =5於織f (2 0) 3 )並得藉由其底部祕面(3 i )、iH)表面上的亮片(3 固定狀態(如第3_示)。川賴^2〇)表面達成結合 e、藉由前述被壓合於織帶(2〇)表面上 空形狀的立體亮面圖案者。 # (33),付以形成中 承上述成型方法,其中,如第2圖之 所沖落之中空區塊亮片(3 2)亦可為沖壓貼合於===沖斷手段 狀態,以使第二次沖斷手段所沖壓(2 Q)表面上之 狀亮面圖案者。 ^成兼,、貝心及中空特色之規則排列 又其中’如第4圖之(a)所+ ^ /r/- 空亮面圖案,此如第Υ、適5製成不規則形狀的中 亮片(3 3 b)者。 所不’係形成不規則中空狀之外框區塊 基材一熱手段,藉一 其成ΐ機之 =實二 =所示’本發明所揭-種織帶表*立趙圖案 一亮片基材放料機構(0 1 ) 亮片基材底部為黏性面⑴)(參第!0圖:示:及3 0 ) ’其中該 ,後一 機構(Q 2),係設置於亮片基材放料機構(0 1)之 二1造Γ機構(〇 3 )’係設置於亮片缺料檢知機構(〇 2 )之 流粒後置/ ’猎財_成預定&amp; Μ之中空部位;以及 ) 士㈣晋1^飼月民拉’料機構(0 4 ) ’係設置於第一亮片造型機構(〇 3 )之 流輕後置處’精以控制亮片基材(3⑴之位移及停止的時機= 8 1254672 崎置亮機構(◦5),係設置於亮片伺服拉料機構(⑷之 一織帶放料機構(0 6 ),設置於亮片滿料檢 置處,^藉以架置織帶(2 0 )之用;以及 再㈧5 )之4後 -第二亮片造型機構(Q 7 ),設置於織帶放料機構⑺ 於i帶ί二Γ片基材(3 0)依預設之邊形設定加以沖斷並壓^黏貼 細ΐίΓ服拉料機構(G 8),係設置於第二亮片造型機構(〇 了)之 欠加f壓合機構(Q 9 ) ’係設置於成品伺服拉料機構(0 8 )之 以對織帶(2 〇 )上結合之亮片進行再次之熱壓合動作, 強化、、、σ a之穩固性者;以及 後置^成^收料機構(1 〇 )’係設置於二次加溫壓合機構(0 9 )之流程 处L係糟以收置完成結合亮片動作的織帶(2 〇)成品;以及 處,传集Γ構⑴)’設置於第二亮片造型機構之流程後置 〜你精以收置焭片基材(3 0)之廢料者。 其中,該第二亮片造型機構(0 7)中更包括有加熱裝置,藉以軟化 儿片基材(3 Q )之黏性面(3 1 ),已利於貼合於織帶(2 〇 )之表面上。 u又^、中,如第6圖所不,係本發明所揭一種織帶表面立體圖案其成 ^機^另一較佳實施例,其與前述實施例之不同點在於其僅設置有單一組 二片機構(Q 7b)之型態,該亮片造型機構(〇 了b)係設置於織 f放料,構(◦6)之流程後置處’係藉以將亮片基材(3 Q)依預設之 邊幵疋加以冲斷並壓合黏貼於織帶上,此實施例由於先前作業中並不包 括冲壓形成中空區塊亮片的流程,因此所得成品將僅為實心熊樣之亮面圖 案型態者。 ' 【本發明之優點】 1254672 1、 本發明所揭成型方法及機構係直接由亮片基材上藉由沖斷手段將亮 面圖案壓合於織帶上’因此可較習知轉印方式更加直接而有效率,達 到製造更簡易、成本可大幅降低之較佳產業利用性。 2、 本發明所揭成型方法及機構所得的織帶成品將具有習知轉印方式所 不具備的的立體層次美感’亦即,可藉由結合於織帶表面上的亮片來 達到此一極佳之立體層次美感。 φ 3、 -般亮片基材表面會複合有一透明保護膜,而本發明所揭成型方法及 機構將亮片基材結合於織帶上後,該所述透縣麵仍可完整㈣於 亮片表面’藉此確可_知轉印方式所得亮__磨損淡化之 缺弊’達到亮祕果可更加敎_之進步性者。 則文係針對本發明之較佳實施例為本發明之 明;惟,熟悉此項技術之人士當可在不脫離本發明之行具體之說 更與修改’而變更與修改,皆應 1、原則下進行變SUMMARY OF THE INVENTION That is, the main object of the present invention is to provide a method for forming a surface of a webbing, and a preferred embodiment thereof comprises: providing a webbing and a sequin substrate, wherein the bottom of the sequin substrate is viscous. The surface of the sequin substrate is placed in a corresponding state without being pressed under the webbing; the re-application is performed by a punching means to press the miscellaneous block on the sequin substrate to the webbing table, and at the same time The sequins pressed onto the surface of the webbing are combined with the webbing by the adhesive side of the bottom (or with heating); the solid shape is formed by the above-mentioned bonding to the webbing club. Face pattern. Another preferred embodiment of the molding method is to use a two-time punching method, in which the hollow block of a predetermined shape on the sequin substrate is first applied by applying the first-stage punching means. In the second punching method, the outer frame portion on the sequin substrate is crushed and pressed onto the surface of the webbing; thereby forming a stereoscopic bright surface pattern of the hollow shape. Another main object of the present invention is to provide a three-dimensional pattern forming mechanism for a kind of webbing surface, 1254672=Detection, ==substrate-seam blank lacking material to detect the hollow portion of the sequin pattern. And &quot;Γ'- The heart-shaped mechanism can be used to break the pre-displacement and stop the opportunity; one clock ^= private 1丨曰 in the 'fibre V-discharge mechanism, by which the webbing, the 筮--μμ- ancient μ &amp; The material is pre-set, and the "one-party film molding machine is placed on the side of the shape of the sigh, and a sequin servo pulling mechanism to control the sequin substrate 1; a second sequin shape 祯 finished product Servo pulling mechanism, burial ^ 丨 ^ 7 one. A ~ 丨 ^ 里 压 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴 贴^ into a redundant waste collection mechanism, in order to collect the sequins with a sequins full, the receiving device feeding mechanism and the webbing discharge mechanism between the more information detection mechanism. Wherein, the first and second sequin molding mechanisms further comprise a heating device, wherein the heating device is further provided with a heating press mechanism of the finished feeding device and the finished material receiving mechanism. It is simpler and more efficient to change the size of the rabbit. It has a three-dimensional beauty and a soft-skinned pattern to achieve a practical effect such as a protective film. [Embodiment] In order for your review committee to understand and understand the purpose of the present invention, please cooperate with [Simple Description]. The slope and function can be further improved. Please refer to Figures 1 and 2 for details. The preferred embodiment of the method and the molding machine thereof, firstly, the method for forming a surface of a three-dimensional pattern of a surface of a woven fabric, a method for providing a webbing having a predetermined length and width and a thickness, and a preferred embodiment of the method includes: , the sequin substrate (3 〇); the part Y) and the &amp; sequin substrate (3 〇), and b, the sequin substrate (3 〇) is placed on the webbing (^, (31); c, as in the first 2 (a) shows the corresponding state of the upper king without pressing the upper part; 中空) the hollow block of the predetermined shape on the bright 7 punching means, the sequin substrate (3 d, such as the second Figure (b), applied; J2) first flush; brother one or two into the thrust means, the sequined substrate (3 7 1254672 Ο) on the pre-cut shape outside the box block sequins (3 q + surface Corresponding to the upper part, at the same time, it touches the webbing 2 = 5 on the weave f (2 0) 3 ) and has the sequins on the surface of the bottom secret surface (3 i ), iH) (3 fixed state ( The first 3_ shown). ^ 2〇 Lai Chuan) to reach the surface bound e, is pressed by the webbing (2〇) Glossy three-dimensional space by the pattern shape of the upper surface. # (33), in order to form the above-mentioned forming method, wherein the hollow block sequins (32) which are washed off as shown in Fig. 2 may also be stamped and attached to the ===punching means state, so that The second punching means stamps (2 Q) the surface of the bright surface pattern. ^成成,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,,, Sequins (3 3 b). Does not form an irregular hollow outer frame material, a thermal means, by means of a smashing machine = real two = shown in the present invention - the woven tape table * Li Zhao pattern a sequin substrate Dispensing mechanism (0 1 ) The bottom of the sequin substrate is a viscous surface (1)) (Refer to Fig. 0: shows: and 3 0 ) 'Where the latter mechanism (Q 2) is placed on the sequin substrate The mechanism (0 1) bis 1 Γ Γ 〇 〇 〇 设置 设置 设置 设置 设置 设置 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮 亮士(四)晋1^食月民拉's material mechanism (0 4 ) ' is set in the first light piece modeling mechanism (〇3) in the light rear position 'fine to control the timing of the sequin substrate (3 (1) displacement and stop = 8 1254672 Kawasaki Brightening Mechanism (◦5), set in the sequin servo pulling mechanism ((4) one of the webbing discharge mechanism (0 6 ), set at the sequin full material inspection, ^ by means of the mounting webbing (2 0 ); and then (8) 5) after 4 - the second sequin molding mechanism (Q 7 ), set in the webbing feeding mechanism (7) in the i belt Γ two 基材 substrate (3 0) according to the preset edge setting Flush Broken and pressed ^ adhesively attached ΐ Γ 拉 拉 拉 拉 G G G G G G G G 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二 第二8) The re-compression of the sequins combined on the webbing (2 〇), the reinforcement of the reinforcement, and the stability of σ a; and the rear placement of the receiving mechanism (1 〇) The process of the secondary heating and pressing mechanism (0 9 ) is to collect the finished webbing (2 〇) which is combined with the sequining action; and the collecting and constructing structure (1)) is disposed in the second sequining mechanism. After the process, you will be able to collect the scrap of the enamel substrate (30). Wherein, the second sequin molding mechanism (0 7) further comprises a heating device for softening the adhesive surface (3 1 ) of the tablet substrate (3 Q ), which is favorable for conforming to the surface of the webbing (2 〇) on. u, ^, 中, as shown in Fig. 6, is a preferred embodiment of the three-dimensional pattern of the surface of the webbing disclosed in the present invention, which differs from the previous embodiment in that it is only provided with a single group. The type of the two-piece mechanism (Q 7b), the sequin-shaped mechanism (〇b) is set in the weaving f-laying, and the structure (◦6) is placed behind the process to make the sequin substrate (3 Q) The preset edge is punched and pressed and adhered to the webbing. This embodiment does not include the process of forming a hollow block sequin by stamping in the previous work, so the finished product will be only a solid bear-like glossy pattern. State. [Advantages of the Invention] 1254672 1. The molding method and mechanism disclosed in the present invention directly presses the glossy pattern onto the webbing by means of a punching means on the sequin substrate, so that the transfer method can be more direct than the conventional transfer method. And efficient, to achieve better industrial utilization with easier manufacturing and significantly lower costs. 2. The finished webbing obtained by the molding method and mechanism of the present invention will have a three-dimensional aesthetic that is not possessed by the conventional transfer method', that is, it can be achieved by the sequins bonded to the surface of the webbing. Three-dimensional beauty. Φ 3, the surface of the general sequin substrate will be compounded with a transparent protective film, and the forming method and mechanism of the present invention, after the sequin substrate is bonded to the webbing, the through-counter surface can still be completed (four) on the surface of the sequin This can be _ know the transfer method to get the light __ wear and tear of the shortcomings to achieve the bright secrets can be more 敎 _ progressive. The preferred embodiments of the present invention are intended to be illustrative of the present invention; however, those skilled in the art can change and modify the present invention without departing from the scope of the invention. Change under

疇中。 后之申晴專利範圍所界定範 10 1254672 [圖式簡單說明】 第1圖:係本發明之成财法之步驟示意圖- ,係說明該亮月基材底部 為黏性面。 ,2,:係本發明之成型方法較佳實_圖。 f回·係本發明之亮片結合於織帶表面上之剖視圖。 f圖·係本發明之成型方法另一較佳實施例圖。 ,5圖·係本發明之成型機之較佳實施例圖。 第6圖·係本發明之成型機之另一較佳實施例圖。 &gt;【主要元件符號說明】 亮片基材放料機構一一(〇工) 第一亮片造型機構一一(〇 3) 亮片滿料檢知機構—一(〇 5) 第二亮片造型機構——(〇7) 成品伺服拉料機構—一(〇 8) 成品收料機構 々it 纖 V _ 亮片基材—〜 集Η (10) (20) (30) 冗片缺料檢知機構一一(Q 2 ) 亮片伺服拉料機構—一(0 4) 織帶放料機構一一—〜(0 6) 亮片造型機構一———(07b =次加溫壓合機構一一(09) 亮片廢料收集機構——α工) 黏性面一—In the domain. The scope of the patent scope of the later Shenqing patent is 101254672 [Simple description of the drawing] Fig. 1 is a schematic diagram of the steps of the financial method of the present invention, which indicates that the bottom of the bright moon substrate is a viscous surface. 2, the molding method of the present invention is better. f Back is a cross-sectional view of the sequin of the present invention bonded to the surface of the webbing. Fig. 1 is a view showing another preferred embodiment of the molding method of the present invention. Fig. 5 is a view showing a preferred embodiment of the molding machine of the present invention. Fig. 6 is a view showing another preferred embodiment of the molding machine of the present invention. &gt;[Main component symbol description] Sequin substrate discharge mechanism one by one (completed) First sequin molding mechanism one by one (〇3) Sequin full material detection mechanism—one (〇5) Second sequin molding mechanism—— (〇7) Finished Servo Pulling Mechanism—One (〇8) Finished Material Receiving Mechanism 々it Fiber V _ Sequined Substrate—~ Collection 10 (10) (20) (30) Redundant material detection mechanism one by one ( Q 2) Sequin servo pull mechanism—one (0 4) webbing discharge mechanism one-to-one (0 6) sequin molding mechanism one———(07b = sub-heating press mechanism one by one (09) sequin waste collection Institution - α工) Viscous surface one -

一-(32)(32b) 1J 〜( 3 3 )( 3 3 b)One-(32)(32b) 1J ~( 3 3 )( 3 3 b)

Claims (1)

1254672 h、申請專利範圍: 丨丨、年丨月 包括 種織帶表面立體亮面圖案成型方法, 且其中,該亮片基 a、提供具預定長寬及厚度之一織帶和一亮片基材, 材底部為黏性面; t使免片基材置於織帶上方呈不麼合之對應狀態; 部黏性面與織帶達成二:‘表面上的卿藉由其底 d、述被壓合於織帶表面上的亮片,得形成實心形狀的立體亮面 、依=請專利範圍第所述之織帶表面立體圖案成型方法,盆中實 S冲斷手段時’更可_施以—加熱手段,藉以軟化亮片基材之黏 一種織帶表面立體亮面圖案成型方法,包括: 该免片基 、提供具預定長寬及厚度之一織帶和一亮片基材,且其中 材底部為黏性面; b、使亮片基材置於織帶上方呈不壓合之對應狀態; c =以一第一次沖斷手段,將亮片基材上的預定形狀之中空區塊先沖 、%以一第二次沖斷手段,將亮片基材上的預定形狀之外框區塊沖落 壓合於織帶表面上相對應處,此同時,被壓合於織帶表面上的亮片 並得藉由其底部黏性面與織帶達成結合固定狀態。 藉由如述被壓合於織帶表面上的焭片,得形成中空形狀的立體亮面 圖案者。 4、依據申請專利範圍第3項所述之織帶表面立體亮面圖案成型方法,其 中該第一次沖斷手段所沖落之中空區塊亮片亦可為沖壓於織帶表面上 12 1254672 二次沖斷手段所沖壓於織帶表面之外框區塊亮片係與 之呈錯位配置者。 、範圍第3項所述之織帶表面立體亮面圖案成型方法’其 、:手,冲落之中空區塊亮片亦可沖落成廢料者。 二二4關第3項所述之織帶表面立體亮關誠型方法,其 斷手㈣’更可同時施以—加熱手段,藉以軟化亮片基材 之黏性面。 7、 一種織帶表面立體亮面圖案成型機,包括: 一受片基材放料機構,係藉以架置亮片基材;以及 -1缺料檢知機構,設置於亮片基材放料機構之絲後置處,藉以 檢知亮片基材之有無狀態;以及 、第一壳片造型機構,設置於亮片缺料檢知機構之流程後置處,藉以 沖斷形成預定亮片圖案之中空部位;以及 一売^伺服拉料機構,設置於第一亮片造型機構之流程後置處,藉以 控制亮片基材之位移及停止時機;以及 織π放料機構,設置於亮片伺服拉料機構之流程後置處,係藉以架 置織帶;以及 =第二亮片造型機構,設置於織帶放料機構之流程後置處,係藉以將 冗片基材依預設邊形設定加以沖斷並壓合黏貼於織帶上;以及 一成品伺服拉料機構,設置於第二亮片造型機構之流程後置處,藉以 控制織帶之位移及停止時機;以及 一成品收料機構,設置於成品伺服拉料機構之流程後置處,係藉以收 置元成結合党片的織帶成品;以及 一免片廢料收集機構,設置於第二亮片造型機構之流程後置處,係藉 以收置亮片基材之廢料者。 8、 依據申請專利範圍第7項所述之織帶表面立體亮面圖案成型機,其中 該亮片伺服拉料機構與織帶放料機構之間更可設置有一亮片滿料檢知 機構者。 13 J254672 9依據申w專她圍第7項所述之織帶表面立體亮關誠型機,其中 該第二亮片造型機構中更包括有加熱裝置。 1 0、依射«利範圍第7項所述之織帶表面立體亮面圖誠型機,其 中該成品伺服拉料機構與成品收料機構之間更可再設置有—二次加溫 壓合機構者。 •種織帶表面立體亮面_成型機,包括: 11 -亮片基材放料機構,係藉以架置亮片基材;以及 二機構’設置於亮片基材放料機構之流程後置處,藉以 榀知焭片基材之有無狀態;以及 拉韻構,設置於亮片造顯構之流程後置處,藉以控制 焭片基材之位移及停止時機;以及 置t放=構,叹置於党片飼服拉料機構之流程後置處’係藉以架 二σ又置於織帶放料機構之流程後置處,係藉以將亮片 土,依預§又邊形設定加以沖斷並壓合黏貼於織帶上;以及 -成品伺服拉料機構,設置於第二 控制織帶之位移及停止時機;以&amp; 线構之4後级精U 置設置於成品伺服拉料機構之流程後置處,係藉以收 置凡成結合党片的織帶成品;以及 一亮片廢料收集機構,兮w_古u ^ 以收置亮片基材之廢料者。、一冗^型機構之流程後置處’係藉 12、依據申請專利_第11項所述之織帶表面立體亮面_成型機, 其中該亮⑽服拉料機構與織帶放料機構之間更可設置有―亮片滿料 檢知機構者。 13 、依據中4專利範圍第丨i顧述之織帶表面立體亮捕減型機, 14 1254672 其中該第二亮片造型機構中更包括有加熱裝置。 14、依據申請專利範圍第1 1項所述之織帶表面立體亮面圖案成型機, 其中該成品伺服拉料機構與成品收料機構之間更可再設置有一二次加 溫壓合機構者。 151254672 h, the scope of application for patents: 丨丨, 丨 丨 包括 包括 包括 包括 包括 包括 包括 包括 包括 包括 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种 种It is a viscous surface; t makes the uncoated substrate placed on the top of the webbing in a corresponding state; the viscous surface and the webbing reach the second: 'The surface is embossed on the surface of the webbing by its bottom d On the upper sequins, it is necessary to form a solid shape of the three-dimensional bright surface, according to the patent scope of the first three-dimensional pattern forming method of the webbing surface, when the basin is in the S-breaking means, it can be used to heat the sequins. A method for forming a three-dimensional glossy pattern on a surface of a substrate, comprising: the substrate free, providing a webbing having a predetermined length and width and thickness, and a sequin substrate, wherein the bottom of the material is a viscous surface; b. The substrate is placed in a corresponding state without pressing on the webbing; c = the hollow block of the predetermined shape on the sequin substrate is firstly punched by a first punching means, and the second is a second punching means. Sequin substrate The predetermined shape of the dashed outline block nip on the surface of the corresponding web at the same time, is pressed to the surface of sequins on the webbing and obtained by its bottom surface and the adhesive binding webbing reached a fixed state. By forming a cymbal sheet which is pressed against the surface of the webbing as described above, it is possible to form a hollow-shaped three-dimensional glossy pattern. 4. The method for forming a three-dimensional bright surface pattern of a webbing surface according to claim 3, wherein the hollow piece of the hollow piece which is washed by the first punching means can also be stamped on the surface of the webbing 12 1254672 secondary punching The breaking means is stamped on the surface of the webbing, and the sequins of the frame block are arranged in a misaligned configuration. The method for forming a three-dimensional glossy pattern on the surface of a webbing as described in the third item, wherein: the hand, the hollow piece of the hollow block can be washed off into a waste. The method of the three-dimensional bright-cut type of the surface of the webbing described in Item No. 2, No. 2, No. 4, wherein the broken hand (four)' can be simultaneously applied by heating means to soften the adhesive surface of the sequin substrate. 7. A three-dimensional bright surface pattern forming machine for a webbing surface, comprising: a receiving substrate substrate discharging mechanism for mounting a sequin substrate; and a -1 material missing detecting mechanism, which is disposed on the sequin substrate discharging mechanism a rear portion for detecting the presence or absence of the sequin substrate; and a first shell molding mechanism disposed at a rear portion of the process of the sequin missing material detecting mechanism to break the hollow portion forming the predetermined sequin pattern;売^The servo pulling mechanism is disposed at the rear of the flow of the first sequining mechanism to control the displacement and stop timing of the sequin substrate; and the weaving π discharging mechanism is disposed at the rear of the process of the sequin servo pulling mechanism , by means of the mounting of the webbing; and = the second sequining modeling mechanism, which is disposed at the rear of the process of the webbing discharge mechanism, whereby the redundant substrate is punched and pressed against the webbing according to the preset edge setting. And a finished servo pulling mechanism disposed at the rear of the second sequining mechanism to control the displacement and stop timing of the webbing; and a finished receiving mechanism The post-process of the servo-drawing mechanism is used to collect the finished product of the ribbon that is combined with the party piece; and a waste-free material collecting mechanism is disposed at the rear of the process of the second sequining mechanism to receive the sequin base. Material waste. 8. The webbing surface stereoscopic bright surface pattern forming machine according to claim 7, wherein the sequin servo pulling mechanism and the webbing discharging mechanism are further provided with a sequin full material detecting mechanism. 13 J254672 9 According to the application of the invention, the webbing surface stereoscopic machine of the seventh aspect, wherein the second sequin molding mechanism further comprises a heating device. 1 0, according to the scope of the scope of the seventh paragraph of the scope of the three-dimensional glossy surface of the machine, in which the finished servo-drawing mechanism and the finished material receiving mechanism can be further set with - secondary heating and pressing Institutional. • Three-dimensional glossy surface of the woven belt _ forming machine, including: 11 - sequin substrate discharge mechanism for mounting the sequin substrate; and two mechanisms 'located at the rear of the process of the sequin substrate discharge mechanism, whereby Knowing the presence or absence of the substrate of the enamel sheet; and pulling the rhyme structure, setting it at the back of the process of creating the slab, thereby controlling the displacement and stopping timing of the substrate of the cymbal; The process post-feeding mechanism of the feeding and pulling mechanism is based on the process of placing the two sigma and placing it in the process of the webbing discharge mechanism, so as to break the sequined soil and press it according to the pre-set and the edge shape. On the webbing; and - the finished servo pulling mechanism is set at the second control webbing displacement and stop timing; the rear stage of the &amp; line structure is set at the rear of the process of the finished servo pulling mechanism, thereby The finished product of the ribbon that combines the party pieces; and a sequin waste collection mechanism, 兮w_古u^ to collect the scrap of the sequin substrate. The process of a redundant type of mechanism is located at 12, according to the patent application _11, the three-dimensional glossy surface of the webbing_forming machine, wherein the bright (10) feeding mechanism and the webbing discharging mechanism It can also be set up with a "sequin full material detection mechanism". 13. According to the scope of the fourth patent, the third-dimensional brightening and reducing machine for the webbing surface, 14 1254672, wherein the second sequin molding mechanism further comprises a heating device. 14. The three-dimensional bright surface pattern forming machine of the webbing surface according to claim 1 of the patent application scope, wherein the finished product servo pulling mechanism and the finished product receiving mechanism can further be provided with a second heating and pressing mechanism. . 15
TW94113225A 2005-04-26 2005-04-26 Forming method of cubic patterns on textile ribbon surface and forming mechanism therefore TWI254672B (en)