TW524921B - A processing method of wooden curtain slats and the products thereof - Google Patents

A processing method of wooden curtain slats and the products thereof Download PDF

Info

Publication number
TW524921B
TW524921B TW91114780A TW91114780A TW524921B TW 524921 B TW524921 B TW 524921B TW 91114780 A TW91114780 A TW 91114780A TW 91114780 A TW91114780 A TW 91114780A TW 524921 B TW524921 B TW 524921B
Authority
TW
Taiwan
Prior art keywords
wooden
water
primer
far
scope
Prior art date
Application number
TW91114780A
Other languages
Chinese (zh)
Inventor
Ming Nian
Original Assignee
Nien Made Entpr Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nien Made Entpr Co Ltd filed Critical Nien Made Entpr Co Ltd
Priority to TW91114780A priority Critical patent/TW524921B/en
Application granted granted Critical
Publication of TW524921B publication Critical patent/TW524921B/en

Abstract

Disclosed is a processing method of wooden curtain slats and the products thereof, consisting of: applying paint on wooden slats, which have been gone through processes of sterilizing, antisepsis and dehydration, to avoid possible damages from sunburn, humidity, and worm bite. The painting process mentioned above includes material supply, base painting, finish painting, and material removal as the painting work using by spraying hydraulic coating and radiating under ultra infrared rays to shorten drying time thereof.

Description

524921524921

五、發明說明( 5 15 經濟部智慧財產局員工消費合作社印製 20 工 本發明係與木質窗簾葉片有關 木質窗簾葉片之加工處理方法及其成品。^4一種 材製I用I葉t簾所使㈣錢葉片係以pc «或是銘 ^成#,上述材質於加工製作時容易造成環境 =為-種改以木質板片(如竹片)製作成窗簾葉片的加工製 程漸為業界所採用,藉以達到降低環境污染。 水等板片在製作過程中,於經過殺菌、防腐及脫 水伟序處理後,尚必須於板片表面進行上漆塗裝作業, 以避免木質板片結構因曰曬受潮或是蟲虫主等原因而損壞; 減然,職木質板片做成的窗簾葉片雖富質感,但,—般 木質板片在上漆塗裝過程(包括底漆作業及面漆作業)中,係又 以油性漆做為塗料而依序覆設於板片表面上,_,使用該 油性漆做為塗裝加工仍有以下缺失·· 、第-,油性漆具有刺鼻的味道,當塗裝作業者長期在 =有刺鼻味道的環境中作業時,對其自身的健康而言將 緩ί更造成不良影響。 第二’該油性漆成份中包含有可對環境造成污染的溶 劑在内,因此,每次的上漆塗裝作業皆將對環境造成破壞。 第三,由於該木質板片至少須經過多道的上漆塗裝加 以確保品質,因此,當木質板片在每一次的進料與上漆 處理後,仍需等待該油性漆乾燥之後始可繼續爾後的下料 (或往下-塗裝程序)作業,雖然,在製作過程中會以風扇等 方式對已上底漆(或面漆)的木質板片進行風乾處理,但,其 乾燥時間過長無法提昇加工效率。 • i §s I I— ^ -I d I I 1 I I s I ! I I f f ! t g I s 畐 I i |~1!^1^^^^|事項再填寫本頁) - -3- 本紙張尺度適用中國國家標準(CNS)A4規格(210 X 297公釐) 524921 A7 Β7 五、發明說明(V. Description of the invention (5 15 Printed by the Consumer Cooperatives of the Intellectual Property Bureau of the Ministry of Economic Affairs 20 The present invention relates to the processing method and finished products of wooden curtain blades related to wooden curtain blades. ^ 4 A material made of I leaf t curtains The money leaf is made of pc «or Ming ^ 成 #. The above materials are easy to cause the environment when processing. =-The process of changing curtain boards made of wooden boards (such as bamboo) into curtain leaves is gradually adopted by the industry. In order to reduce environmental pollution. In the production process of water and other plates after sterilization, antiseptic and dehydration treatment, you must still paint on the surface of the plate to avoid the wood plate structure due to sunlight Or the insects are damaged due to other reasons; In a word, although the curtain leaves made of professional wooden boards are rich in texture, but—general wooden boards are used in the painting and coating process (including primer and topcoat operations). The oil-based paint is used as a coating and is sequentially covered on the surface of the plate. _, Using this oil-based paint as a coating process still has the following missing ..., No.-, the oil-based paint has a pungent taste, when Painting operator It is expected that when working in an environment with a pungent smell, it will have a negative impact on its own health. Secondly, the oil paint composition contains solvents that can pollute the environment. Therefore, Each painting operation will cause damage to the environment. Third, because the wood panel must be painted at least multiple times to ensure the quality, when the wood panel is After the painting process, you still need to wait for the oily paint to dry before you can continue the subsequent blanking (or down-painting process) operation, although, during the production process, the primer (or surface) has been coated with a fan or other means. Lacquer) wood panels are air-dried, but their drying time is too long to improve processing efficiency. • i §s II— ^ -I d II 1 II s I! II ff! Tg I s 畐 I i | ~ 1 ! ^ 1 ^^^^ | Please fill in this page again for matters)--3- This paper size applies to China National Standard (CNS) A4 (210 X 297 mm) 524921 A7 Β7 V. Description of the invention (

5 15 !四,承續上述第三點,為達到確實的乾燥處理,常 見於母猶環的塗裝作業過程中,會以增加風乾機具 傳送輸程或是增闕收集風乾區等方式而做為加強乾燥,炊 此等方式不僅增加成本支出,更有耗佔空間之虞。… …有繁於此,本案發明人乃經詳思細索,並積多年 έ簾的製作及研究開發經驗,終而有本發明之產生。 即,本發明之主要目的在於提供一種木質窗簾葉片之 加工處理万法及其成品,其以水性漆做騎裝原料,可 少對環境的污染及降低危害作業者的健康。 彳 又,本發明之次要目的在於提供一種木質窗簾葉片之 加工處理万法及其成品,其以遠紅外線照射做為上漆之後 的乾燥處理,可縮短乾燥時間,提昇加工效率。 本發明之另-目的在於提供一種木質窗簾葉片之加工 處理方法及其成品,其成本降低且整個上漆塗裝設備 佔空間。5 15! IV. Continuing the third point mentioned above. In order to achieve a reliable drying process, it is often used in the coating process of the mother and the ring. It will be done by increasing the conveying distance of the air-drying equipment or increasing the air-drying area. In order to enhance drying, such methods not only increase the cost, but also consume space. …… There is a lot of trouble here, the inventor of this case has thought about it carefully, and accumulated many years of experience in the production and research and development of hand curtains, and finally has the invention of this invention. That is, the main object of the present invention is to provide a method for processing and processing wooden curtain blades and a finished product thereof, which uses water-based paint as a raw material for riding equipment, which can reduce environmental pollution and reduce the health of workers.彳 Furthermore, a secondary object of the present invention is to provide a method for processing wooden curtain blades and a finished product thereof, which uses far-infrared radiation as a drying treatment after painting, which can shorten the drying time and improve processing efficiency. Another object of the present invention is to provide a method for processing a wooden curtain blade and a finished product thereof, the cost of which is reduced and the entire painting and coating equipment takes up space.

! ψ S ! yt I § !閱 1 5 讀 1 背 Ί 1 ® 1 !之 '1 注 I 意 I 事 I 項 署 再 I !填 ! 寫 裝 本 頁 I 訂 經濟部智慧財產局員工消費合作社印製! ψ S! yt I §! Read 1 5 Read 1 Back 1 1 1! of '1 Note I Note I Matter I Item I and then I! Fill out! Write this page I Order Printed by the Intellectual Property Bureau Employee Consumer Cooperatives of the Ministry of Economic Affairs system

! ϊ “緣以達成上述之目的,本發明所提供之一種木質窗簾I ! 葉片之加工處理方法及其成品,係包含下列步驟:進料:| ψ 板片素材往預定方向傳送;底漆塗裝作業··《 1」 、木貝板片表面塗上—水性底漆,並以遠紅外線照射使# | 20底漆快速乾燥;面漆塗裝作業:以水性面漆塗佈於該具有| 良/黍的木貝板片表面上,同樣以遠紅外線照射而使得該面|丨 漆快速乾燥;下料:將該面漆已形成乾燥之木質板片為⑯I I 集。 ! ϊ 以下,茲列舉本發明之較佳實施例,並配合下列圖示 丨丨 本紙張尺錢财 _ X 297 524921 玄巴劑塗裝作業 A7 五、發明說明() 詳細說明於后,其中: 第一圖為本發明之著色劑塗裝作業流程圖。 第二圖為本發明之底漆塗裝作業流程圖。 第三圖為本發明之面漆塗裝作業流程圖。 5 第四圖為本發明木質窗簾葉片之剖示圖。 4參閱第一至三圖所示,本發明木質窗簾葉片之加工 處理方去,主要係對已完成殺菌、防腐及脫水等程序處理 的H片素材進行表面上漆塗裝作業,其促使製成成品 々έ簾葉片極具^感,以及可防範因日曬受潮與蟲姓等問 題而造成結構破壞。 而在本發明實施财,仙表轉核呈現的木質板 片為塗裝對象,以下兹就本發明用以達成上述目的的加工 步驟敘述: 15 A ·進料: 首先,將該表面非木紋呈現的木質板片素材往預定的 方向傳送。 係將水性的著色劑以噴附的方式而對步驟A的木^ 片素材表面進行第—職附,之後,靜置ι分鐘使妇 劑^歡依㈣木質板片表面上,爾後,以遠紅外驾 m耆色劑的木質板片進行烘乾處理,於此步驟b 的逆紅外線照射溫度控制在㈣〜靴之間4佳,且其 射争間孩2〜4分鐘左右,同時,在遠紅外線照射之後ϊ "In order to achieve the above-mentioned purpose, a wooden curtain I provided by the present invention, and a processing method and a finished product of the blade, include the following steps: feeding: | ψ board material is transferred in a predetermined direction; primer coating Installation operation ··· 1, Coating the surface of wooden panel—water-based primer, and fast-drying # | 20 primer with far-infrared radiation; topcoat coating operation: apply water-based topcoat to the On the surface of the wooden shell sheet of / 黍, the surface is also irradiated with far-infrared rays to make the surface dry quickly; cutting: the wooden board which has been dried by the top coat is set as ⑯I I. ϊ In the following, the preferred embodiments of the present invention are enumerated, with the following illustrations 丨 丨 This paper rule money_ X 297 524921 Xuanba agent coating operation A7 V. Description of the invention () Details are described later, of which: The first figure is a flowchart of the toner coating operation of the present invention. The second figure is a flowchart of the primer coating operation of the present invention. The third figure is a flow chart of the topcoat coating operation of the present invention. 5 The fourth figure is a sectional view of a wooden curtain blade of the present invention. 4 Referring to the first to third figures, the processing methods of the wooden curtain blades of the present invention are mainly the surface painting and coating operations on the H pieces of materials that have completed the sterilization, antiseptic and dehydration procedures, which promotes the production of The finished hand-made curtain blades have a strong sense, and can prevent structural damage caused by sunlight and moisture and insect names. However, in the implementation of the present invention, the wooden board presented by the fairy watch is a coating object. The following describes the processing steps of the present invention to achieve the above purpose: 15 A · Feeding: First, the surface is not wood grained The rendered wood slab material is transferred in a predetermined direction. The water-based coloring agent is spray-attached to the surface of the wooden sheet material in step A. After that, it is left to stand for one minute to make the feminine powder on the surface of the wooden board, and then, in the far infrared The wooden board of the m toner is dried, and in this step b, the temperature of the reverse infrared irradiation is controlled to be 4 between 靴 and the boots, and the shot is about 2 to 4 minutes, and at the same time, the far infrared After irradiation

* i —a §5 is 033 I i SI —5 ϋ —g ! = M3— Ml yi δ— I 3— is yc , * If J ε s I as I SI i I a {、請先閱讀背面之注意事項再填寫本頁) 20 經濟部智慧財產局員工消費合作社印製 -5-* i —a §5 is 033 I i SI —5 ϋ —g! = M3— Ml yi δ— I 3— is yc, * If J ε s I as I SI i I a {, please read the note on the back first Please fill in this page again for details) 20 Printed by the Consumer Cooperatives of the Intellectual Property Bureau of the Ministry of Economic Affairs-5-

經濟部智慧財產局員工消費合作社印製 524921 A7 —~~—~ ..........................丨丨_ w丨」__ 五、發明說明() 辅以熱風屬吹拂以縮短乾燥時間;至此,該木質板片表面 呈現有預設的花紋色彩,如木紋。 c·底漆塗裝作業: 〜將經過步驟B處理後的木質板片同樣以喷附方式而使 5仔-水性的透明底漆覆蓋於該表面具有預設花、纹的木質板 片上,其經過短暫的靜置後,利用遠紅外線對之照射,而 於該步驟C巾的遠紅外線照射溫度則控制纟武〜6代之 間為佳,其照射時間持續約2分鐘,之後再以熱風扇吹拂 使得底漆可快速乾燥; 10 而在遍步驟C中,其木質板片於經過遠紅外線照射之 後更可再系二過土少一循環的表面砂磨、水性底漆喷附、 短暫靜置、再-次的遠紅外線照射(溫度控制在6〇<t〜8〇c>c (間,其照射0争間則在4分鐘為佳)及熱風扇吹拂等處理, 以促使該底漆層紮實且表面平整。 15 D ·面漆塗裝作業: 其同樣以屬水性且乾燥後呈透明的面漆對底漆已乾燥 的木質板片進行喷附,再於靜置卜2分鐘之後,以照射溫 度控制在60°C左右的遠紅外線持續對之照射2分鐘左右, 及以熱風扇吹拂降溫,俾可獲得快速的烘乾效果,又,於 20此步驟D巾,可再施以另一次的遠紅外線照射(其照射溫度 &制在80 C左右’照射時間在2分鐘為佳)與熱風扇吹拂, 以確保面漆完全乾燥並得以保護該底漆層。 E ·下料: 將經過上述各步驟處理後且面漆已形成乾燥的木質板 -6· 本紙張尺度適用 I ! ! ! I ! I I ! ! I 3 # I!着 — ' (請先閱讀背面之注意事項再填寫本頁) 524921 A7 B7 五、發明說明( 經濟部智慧財產局員工消費合作社印製 片為收集,如此可再經過組裝作業後而獲得所需之窗簾。 以上即為本發明木質窗簾葉片之加工處理方法,而其 結構如第四圖所示,其由内朝外依序為一木質板片10、_ 著色層20、一底漆層30與一面漆層40。 5 另,在步驟C中的水性底漆成份控制在85%的丙埽酸 聚合物(Acrylic emulsion Binder) - 0.1 % 的氨水 (Ammonia)、5% 的純水(Deionic Water)、1 〜3% 的硬脂酸鋅 (Znst Stearate)、2〜5% 的丁基二甘醇(Butyl-Glcol)、2〜5% 的分散劑(Dispersant)、0.3% 的消泡劑(Defoamer)、0.3% 的 1〇 防黴劑(Fungicidal Agent)與 0.3% 的增稠劑(Thickener)為 佳;而在步驟D中水性面漆成份則控制在95%的壓克力 PU 共聚物(Copolymer of Acrylic PU)、0.1% 的三乙胺 (Triethylamine)、4% 的純水(Deionic Water)、1% 白勺 丁基二 甘醇(Butyl-Glcol)、0.1% 的濕潤劑(Wetting Agent)、0.1% 15 的防黴劑(Fungicidal Agent)、0.1 〜0.3% 的增稠劑(Thickener) 與0.1〜0.3%的消泡劑(Defoamer)為佳。 取後’將本發明之優點整理如下: 1 ·本發明以遠紅外線照射做為上漆之後的主要乾燥 處理,可縮短乾燥時間,提昇加工效率,其改善傳統上漆 20 乾燥所需設備多而耗佔空間及乾燥時間長等缺失。 2 ·同第1點,該遠紅外線由於波長較長,能量相對 較低,所以使用時較無燙傷之顧慮,具有較佳的安全性, 其無使用紅外線照射易對人體皮膚產生灼傷及傷害眼睛水 晶體等疾病問題。 3 .i yaa ,,asa ss anaa 15 «aas S8 i IKa saa 5a π Is n (請先閱讀背面之注音^事項再填寫本頁) 8 iua ϋ ei 線! -n 886 n fis on HI a—8 n n- 本紙張尺度適用中國國家標準(CNS)A4規格(210 X 297公爱) 524921 A7 五、發明說明() 3 ·本發明以屬水性的漆料作為上漆塗裝原料使用, 於噴漆加工過程中不會有刺鼻的味道產生,且無溶劑污染 壤境之缺失。 4 ·本發明於著色劑塗裝作業中,可依需求而選擇不 5同顏色呈現的水性著色劑,待於爾後的透明底漆與透明面 漆覆蓋後’该選定的顏色得以展現。 另外,必須一提的是,本發明技術若應用於表面為木 紋呈現的木質板片塗裝時,則該著色劑塗裝作業可以省 略,直接以透明的底漆與面漆塗附即可,其使得 10 呈現最原始的木紋。 综上所述,本發明於同類產品中實具有其進步實用 性,且使用上万便,又,本發明於申請前並無相同物品見 於刊物或公開使用’是以,本發明實已具備發明專利要件, 爰依法提出申請。 15 唯,以上所述者,僅為本發明之較佳可行實施例而已, 故舉凡應用本發明說明書及申請專利範圍所為之等效結構 變化,理應包含在本發明之專利範圍内。 » I li ewi ss 8SH 0i is ssa fl! is si n s y ss (請先閱讀背面之注意事項再填寫本頁)Printed by the Consumer Cooperative of the Intellectual Property Bureau of the Ministry of Economic Affairs 524921 A7 — ~~ — ~ ............... 丨 丨 _ w 丨 」__ V. Description of the invention () It is supplemented with hot air to shorten the drying time. At this point, the surface of the wooden board has a preset pattern color, such as wood grain. c. Primer coating operation: ~ Apply 5 pieces of water-based transparent primer to the wooden boards with pre-designed flowers and patterns on the surface of the wooden boards after the treatment in step B by spraying. After a short period of standing, it is irradiated with far-infrared rays. In this step, the far-infrared irradiation temperature of the towel C is preferably controlled between 6th and 6th generation. The irradiation time lasts about 2 minutes, and then the heat fan Blowing allows the primer to dry quickly; 10 In step C, after the far-infrared light is irradiated on the wooden board, the surface can be sanded, the water-based primer is sprayed, and left to stand for a short time. And re-far-infrared irradiation (temperature controlled at 60 ° < t ~ 80 ° c) (the interval is better than 4 minutes when the irradiation is 0 °) and hot fan blowing to promote the primer The layer is solid and the surface is flat. 15 D · Topcoat coating operation: It also sprays the dried wooden board with the primer with a water-based and transparent topcoat that dries after drying. After standing for 2 minutes, Far-infrared rays controlled at about 60 ° C continuously Irradiate for about 2 minutes, and use a hot fan to cool down to obtain a quick drying effect. In addition, at step 20, the D towel can be subjected to another far-infrared irradiation (the irradiation temperature is & made at 80 C). The left and right 'irradiation time is preferably 2 minutes) and blown with a hot fan to ensure that the topcoat is completely dry and protects the primer layer. E · Cutting: After the above steps are processed and the topcoat has formed a dry wooden board -6 · This paper size applies to I!!! I! II!! I 3 # I! 着 — '(Please read the precautions on the back before filling this page) 524921 A7 B7 V. Description of Invention (Intellectual Property Bureau, Ministry of Economic Affairs The printed pieces of the employee consumer cooperative are collected, so that the required curtains can be obtained after the assembly operation. The above is the processing method of the wooden curtain blades of the present invention, and its structure is shown in the fourth figure, which is from the inner side The outer part is a wooden board 10, a colored layer 20, a primer layer 30, and a top coat layer 40. 5 In addition, the water-based primer composition in step C is controlled to 85% of the polymer of propionic acid ( Acrylic emulsion Binder)-0.1% Ammonia 5% pure water (Deionic Water), 1 ~ 3% zinc stearate (Znst Stearate), 2 ~ 5% butyl diethylene glycol (Butyl-Glcol), 2 ~ 5% dispersant , 0.3% of defoamer, 0.3% of 10 fungidal agent and 0.3% of thickener (Thickener) are preferred; and in step D, the water-based topcoat composition is controlled at 95% Copolymer of Acrylic PU, 0.1% Triethylamine, 4% Deionic Water, 1% Butyl-Glcol, 0.1 % Of wetting agent (Wetting Agent), 0.1% of 15 fungidal agent (Fungicidal Agent), 0.1 ~ 0.3% of thickener (Thickener) and 0.1 ~ 0.3% of defoamer (Defoamer) are preferred. After taking it, the advantages of the present invention are summarized as follows: 1. The present invention uses far-infrared radiation as the main drying treatment after painting, which can shorten the drying time and improve the processing efficiency. It improves the traditional painting and requires more equipment and drying. Missing space and long drying time. 2 · As in point 1, the far infrared ray has relatively long wavelength and relatively low energy, so it has no concerns about burns when used, and has better safety. It does not use infrared rays to easily burn human skin and damage eyes. Disease issues such as water crystals. 3 .i yaa ,, asa ss anaa 15 «aas S8 i IKa saa 5a π Is n (Please read the note on the back ^ before filling this page) 8 iua ϋ ei line! -n 886 n fis on HI a—8 n n- The size of this paper applies to Chinese National Standard (CNS) A4 (210 X 297 public love) 524921 A7 V. Description of the invention (3) The invention is based on water-based paint Used as paint coating raw material, there will be no pungent smell during spray painting process, and there is no lack of solvent pollution in the soil. 4 · In the colorant coating operation of the present invention, an aqueous colorant of different colors can be selected according to requirements, and the selected color will be displayed after the subsequent transparent primer and transparent topcoat are covered. In addition, it must be mentioned that if the technology of the present invention is applied to the coating of wooden boards with a wood grain surface, the colorant coating operation can be omitted, and it can be directly coated with a transparent primer and topcoat. , Which makes 10 the most original wood grain. In summary, the present invention has its practicality in similar products, and it can be used for tens of thousands of uses. In addition, the present invention did not have the same article in the publication or public use before the application. For the patent elements, the application was filed in accordance with the law. 15 However, the above are only the preferred and feasible embodiments of the present invention. Therefore, any equivalent structural changes made by applying the description of the present invention and the scope of patent application should be included in the patent scope of the present invention. »I li ewi ss 8SH 0i is ssa fl! Is si n s y ss (Please read the notes on the back before filling this page)

eia 3SV 訂| 線· 經濟部智慧財產局員工消費合作社印製 8-eia 3SV Order | Line · Printed by Employee Consumption Cooperative of Intellectual Property Bureau, Ministry of Economic Affairs 8-

本紙張尺度適用中國國家標準(CNS)A4規格297公Ϊ7This paper size is applicable to Chinese National Standard (CNS) A4 size 297 cmΪ7

524921 A7 B7 五、發明說明() 【圖示簡單說明】 第一圖為本發明之著色劑塗裝作業流程圖。 第二圖為本發明之底漆塗裝作業流程圖。 第三圖為本發明之面漆塗裝作業流程圖。 5 第四圖為本發明木質窗簾葉片之剖示圖。524921 A7 B7 V. Description of the invention () [Simplified illustration of the figure] The first figure is a flow chart of the toner coating operation of the present invention. The second figure is a flowchart of the primer coating operation of the present invention. The third figure is a flow chart of the topcoat coating operation of the present invention. 5 The fourth figure is a sectional view of a wooden curtain blade of the present invention.

(請先閱讀背面之注意事項再填寫本頁)(Please read the notes on the back before filling this page)

a — III. 經濟部智慧財產局員工消費合作社印製 9- -9— fias Is saflfl imam 2β i 【圖號說明】 10 木質板片 20 著色層 10 30 底漆層 40 面漆層 本紙張尺度適用中國國家標準(CNS)A4規格(210 X 297公釐)a — III. Printed by the Consumer Cooperative of the Intellectual Property Bureau of the Ministry of Economic Affairs 9- -9— fias Is saflfl imam 2β i [Illustration of the drawing number] 10 Wooden board 20 Colored layer 10 30 Primer layer 40 Topcoat layer This paper is applicable to the paper scale China National Standard (CNS) A4 specification (210 X 297 mm)

Claims (1)

524921 A8 B8 C8 no524921 A8 B8 C8 no 步驟 種木質窗簾葉片之加工處理方法,係包含下列 15 經濟部智慧財產局員工消費合作社印製 20 工 進料:將一木質板片素材往預定方向傳送; 、底漆塗裝作業:係對該木質板片表面塗上一水性底 漆’並以遠紅外線照射使得底漆快速乾燥; 面漆塗裝作業:以水性面漆塗佈於該具有底漆的木質 板片表面上同樣以返紅外線照射而使得該面漆快速乾燥; 下料·將該面漆已形成乾燥之木質板片為收集。 2 ·依據申請專利範圍第i項所述木質窗簾葉片之加 工處理万法,其更可於底漆塗裝作業之前增設一著色劑塗 裝作業流程,其以水性著色劑對木質板片素材表面進行塗 附’再以遠紅外線對被覆有著色劑的木質板片為乾燥處理。 3·依據申請專利範圍第2項所述木質窗簾葉片之加 工處理方法,其中該著色劑塗裝作業過程中之遠紅外線照 射溫度控制在60。(:〜80。〇:之間,其照射時間在2〜4分鐘。 4 ·依據申請專利範圍第丄項所述木質窗簾葉片之加 工處理方法,其中該底漆塗裝作業之遠紅外線照射溫度控 制在50 C〜60¾之間為佳,其照射時間約2分鐘。 5 ·依據申請專利範圍第4項所述木質窗簾葉片之加 處理方法,其木質板片經遠紅外線照射後,可再經過至 少循環的表面砂磨、水性底漆噴附及遠紅外線照射等強 化處理。 6 ·依據申請專利範圍第5項所述木質窗簾葉片之加 處理方法,其中於強化處理過程中之遠紅外線溫度控制 請 先 閱 讀 背, 之 注' 意 事 項 再 i 裝 訂 工 -10- 524921 A8 B8 C8 D8 1 - 六、申請專利範圍 在60°C〜8〇°C之間,其照射時間則在4分鐘為佳。 7 ·依據申請專利範圍第1項所述木質窗簾葉片之加 工處理方法,其中該面漆塗裝作業之遠紅外線照射溫度# 制在60°C左右,其照射時間在2分鐘為佳。 5 8 ·依據申請專利範圍第7項所述木質窗簾葉片之加 工處理方法’其經运紅外線照射之木質板片可於略作風乾 後,再經過另一次的遠紅外線照射,而該後者之遠紅外線 照射溫度控制在80°C左右,其照射時間在2分鐘為佳。 9·依據申請專利範圍第1項所述木質窗簾葉片之加 10 工處理方法,其中該水性底漆成份包括85%的丙晞酸聚合 物(Acrylic emulsion Binder)、0.1% 的氨水(Ammonia)、5% 的純水(Deionic Water)、1 〜3% 的硬脂酸鋅(Znst Stearate)、 2〜5 %的丁基二甘醇(Butyl-Glcol)、2〜5 %的分散劑 (Dispersant)、0.3% 的消泡劑(Defoamer)、0.3% 的防黴劑 15 (Fungicidal Agent)與 0.3% 的增稠劑(Thickener)。 10 ·依據申請專利範圍第1項所述木質窗簾葉片之加 工處理方法,其中該水性面漆成份包括95%的壓克力PU 共聚物(Copolymer of Acrylic PU)、0.1 % 的三乙胺 (Triethylamine)、4% 的純水(Deionic Water)、1% 的 丁基二 20 甘醇(Butyl-Glcol)、0.1% 的濕潤劑(Wetting Agent)、0.1% 的防黴劑(Fungicidal Agent)、0.1 〜0·3% 的增稠劑(Thickener) 與0.1〜0.3%的消泡劑(Defoamer)。 11 · 一種木質窗簾葉片結構,包含有: 一木質板片,為一長條形的薄板面體; -11- 本紙張尺度適用中國國家標準(CNS ) A4規格(210 X 297公釐) ----------裝II (請先閱讀背面之没意事項再填寫本頁} •訂 線- 經濟部智慧財產局員工消費合作社印製 524921 申請專利範園 上,且 層,讀用水性漆料塗料該 經逆紅外線照射後而乾燥形成之層面· 貝板片 面並 =層,同樣使用水性漆;塗附於該底漆層表 氬逐紅外線照射而乾燥形成之層面。 依據申明專利範圍第1 1項所述之木質窗簾葉片、择 構,其更包括有-著色層,其同樣以水性漆料塗附且經遠 紅外線照射後而乾燥形成之層面,該著色層介於該木質板 片表面與該底漆層之間。 裝 訂 線· 經濟部智慧財產局員工消費合作社印製 準 標 家 國 國 中 用 適 尺 I張 ,紙 本 A4 V)/ S N 2- 釐 一公 97 2The step of processing the wooden curtain blades includes the following 15 printed by the Intellectual Property Bureau employee consumer cooperative of the Ministry of Economic Affairs and printed by 20 workers: feeding a wooden board material in a predetermined direction; and primer coating operation: The surface of the wooden board is coated with a water-based primer and irradiated with far infrared rays to make the primer dry quickly; Topcoat coating operation: coating the surface of the wooden board with the primer with a water-based topcoat and also irradiated with back infrared rays. Allows the topcoat to dry quickly; cutting down · The topcoat has been collected to form a dry wooden panel. 2. According to the processing method of wooden curtain blades described in item i of the scope of the patent application, it can further add a colorant coating operation process before the primer coating operation, which uses water-based colorants to the surface of the wooden board material After coating, the wooden boards coated with the colorant are dried by far-infrared rays. 3. According to the processing method of wooden curtain blades described in item 2 of the scope of the patent application, wherein the far-infrared radiation temperature during the colorant coating operation is controlled to 60. (: ~ 80.〇: In between, the irradiation time is 2 ~ 4 minutes. 4 · According to the processing method of wooden curtain blades described in item 丄 of the application patent scope, wherein the far infrared irradiation temperature of the primer coating operation It is better to control between 50 C ~ 60¾, and the irradiation time is about 2 minutes. 5 · According to the method of adding treatment to the wooden curtain blades described in item 4 of the patent application scope, after the wooden panel is exposed to far infrared rays, it can be passed through again. At least cyclic surface sanding, water-based primer spraying, and far-infrared irradiation, etc. 6 · Addition of the treatment method of wooden curtain blades according to item 5 of the scope of patent application, in which the far-infrared temperature is controlled during the strengthening process Please read the back first, and note the “Notes” and then i. Bookbinding -10- 524921 A8 B8 C8 D8 1-VI. The scope of patent application is between 60 ° C ~ 80 ° C, and the irradiation time is preferably 4 minutes. 7. According to the processing method of wooden curtain blades described in item 1 of the scope of patent application, the far infrared irradiation temperature # of the topcoat coating operation is controlled at about 60 ° C, and the irradiation time is 2 A clock is better. 5 8 · According to the processing method of wooden curtain blades described in item 7 of the scope of the patent application, the wood panel irradiated with infrared rays can be slightly air-dried and then subjected to another far-infrared irradiation, and The far-infrared irradiation temperature of the latter is controlled at about 80 ° C, and the irradiation time is preferably 2 minutes. 9. According to the processing method of adding 10 steps of the wooden curtain leaf described in the first patent application scope, wherein the water-based primer composition Includes 85% Acrylic emulsion Binder, 0.1% Ammonia, 5% Deionic Water, 1 ~ 3% Znst Stearate, 2 ~ 5 % Butyl-Glcol, 2 ~ 5% Dispersant, 0.3% Defoamer, 0.3% Fungicidal Agent and 0.3% increase Thickener (10) According to the processing method of wooden curtain blades according to item 1 of the scope of patent application, wherein the composition of the water-based topcoat includes 95% of Copolymer of Acrylic PU, 0.1% Triethylamine, 4% pure water ( Deionic Water), 1% Butyl-Glcol, 0.1% Wetting Agent, 0.1% Fungidal Agent, 0.1 ~ 0.3% thickener (Thickener) and 0.1 ~ 0.3% Defoamer. 11 · A wooden curtain leaf structure, comprising: a wooden plate, a long thin sheet surface; -11- This paper size applies to China National Standard (CNS) A4 (210 X 297 mm)- -------- Install II (please read the unintentional matter on the back before filling in this page) • Threading-Printed by the Consumer Cooperatives of the Intellectual Property Bureau of the Ministry of Economic Affairs 524921 on the patent application park, and it is for reading Water-based paint coating This layer is formed by drying after reverse infrared irradiation. The shell is one-sided, and the same layer is used. Water-based paint is also used; the layer formed on the surface of the primer layer is dried by infrared irradiation and irradiated. According to the scope of the declared patent The wooden curtain blade and optional structure described in item 11 further include a coloring layer, which is also a layer formed by coating with a water-based paint and drying after being irradiated with far infrared rays, and the coloring layer is interposed between the wooden board Between the surface of the sheet and the primer layer. Gutter · Printed by the Consumer Cooperatives of the Intellectual Property Bureau of the Ministry of Economic Affairs, a standard-size paper for domestic and international use, A4 paper on paper) / SN 2- centimeter 97 2
TW91114780A 2002-07-04 2002-07-04 A processing method of wooden curtain slats and the products thereof TW524921B (en)