TW515753B - Method of injection-molding polyethylene shoe sole having bi-hardness - Google Patents
Method of injection-molding polyethylene shoe sole having bi-hardness Download PDFInfo
- Publication number
- TW515753B TW515753B TW91105549A TW91105549A TW515753B TW 515753 B TW515753 B TW 515753B TW 91105549 A TW91105549 A TW 91105549A TW 91105549 A TW91105549 A TW 91105549A TW 515753 B TW515753 B TW 515753B
- Authority
- TW
- Taiwan
- Prior art keywords
- color
- injection
- shoe
- mold
- dual
- Prior art date
Abstract
Description
丄 J 五、發明說明(1) 本發明係提供-種雙硬度聚乙烯鞋底射出方法;具體 ς挪是指一種運用(1)·雙色射出機射出雙色雙密度鞋邊 舜二:丨(2).置入模具步驟;(3 )·同色同密度材質射出包 =二4,(4 )·開核步驟·’等四個製造步驟,解決以往鞋底 射出不同色鞋邊塊時所產生的溢色問題者。 $,由於現代科技搭配塑膠射出成型技術的水準不斷 汁,所以,塑膠射出成型技術已是目前高技術性工 Μ=重要的技術之一,目前一般所見的鞋類產品更是 枯土膠技術之中的主要產業,但是,由於鞋類塑膠射出 V、生產方式各有不同,故鞋類塑膠射出技術是 幸乂 ^的成果便成為採用者最為重視的問題;因此, mIZ毛出一種具有更佳功效的射出成型技術,早已變成 衣造商取想克服的問題,而上述内容中所呈現的 口〜也是本案發明人研發本案的動機。 一般目W最常見的鞋類聚乙烯塑膠射出成型方法,其 大體上係依據2 (1 )·射出成型鞋邊塊步驟;(2 )·置入模具 步驟;(3 )·不同色、不同密度材質射出步驟;(4 )·開模步 驟;藉由上述四個步驟可以生產出具有較硬質鞋邊塊的鞋 底成品’此種習用鞋類聚乙烯塑膠射出成型方法已在市面 上銷售、使用許久’但是因為下列問題,會造成有待發明 者改進的課題,在此一—分析解說於下: 其一 ’因習用鞋底的鞋邊塊必需採用較硬質的聚乙烯丄 J V. Description of the invention (1) The present invention provides a method for injection of a double-hardness polyethylene sole; specifically, refers to a method of using (1) · two-color injection machine to shoot two-color dual-density shoe soles Shunji: 丨 (2) Steps of inserting the mold; (3) · Same color and same density material injection package = two 4, (4) · core-opening step · 'four manufacturing steps to solve the overflowing color generated when soles shot different color shoe blocks in the past Problem person. $, As the level of modern technology combined with plastic injection molding technology continues to increase, plastic injection molding technology has become one of the most important high-tech industrial technologies at present, and the footwear products generally seen today are even more sublime rubber technology. The main industry in China, however, because footwear plastic injection V and production methods are different, so the shoe plastic injection technology is the result of Xing Yi ^ ^ has become the most important issue for adopters; therefore, mIZ hair has a better The effective injection molding technology has already become a problem that clothing manufacturers want to overcome, and the mouth presented in the above content is also the motivation of the inventor of this case to develop this case. The most common injection molding method for footwear polyethylene plastics in general is generally based on 2 (1) · injection molding of shoe block; (2) · step of inserting molds; (3) · different colors and different densities Material injection step; (4) · moulding step; through the above four steps, a finished shoe sole with a harder shoe block can be produced. 'This custom footwear polyethylene plastic injection molding method has been sold on the market and used for a long time. 'But because of the following problems, it will cause problems that need to be improved by the inventors, here one-analysis and explanation are as follows: First,' because the conventional shoe sole block must use harder polyethylene
515753 五、發明說明(2) 塑膠材料,才可以達成保護鞋底、增加使用壽命的效果, 故一般鞋邊塊的聚乙烯塑膠材料密度與其他鞋底材質不同 ,故當射出成型發泡完成後,二種不同密度的聚乙烯塑膠 材質不易融合^常常會造成聚乙稀塑膠鞋底與鞋邊塊容易 分離脫落的問題,也間接降低了產品的品質與使用壽命者 其二,習用鞋底生產業者通常都會將鞋邊塊採用不同 -顏色的聚乙烯塑膠材料,藉此達成整體設計感與亮眼的外 ‘ 觀,但是,由於鞋邊塊與其他鞋底為前、後分別射出,故 -當其他鞋底材料射出成型發泡後,該鞋邊塊週邊都會混雜馨 形成另一材質的溢出材料(業界通常以「溢色」稱之), 不但影響鞋子成品的整體精緻感,且二種不同顏色聚乙烯 塑膠材質的混亂溢色更是降低產品品質的主因;是故,針 對以上缺陷,在求理想、實用與進步之今日,誠為一極待 努力追求改善之目標。 - 有鑑於斯,本案發明人乃經詳思細索,並積多年從事 各種鞋類塑膠射出成型機構與相關鞋類射出產品之販售、 * 研究與開發之經驗,終而得以開發出一種可以解決以往鞋 φ 底射出不同色鞋邊塊所產生之溢色問題的雙硬度聚乙烯鞋 底射出方法。 本發明之首要目的,在於提供一種可以解決以往鞋底 射出不同色鞋邊塊所產生之溢色問題的雙硬度聚乙烯鞋底515753 V. Description of the invention (2) Only the plastic material can achieve the effect of protecting the sole and increasing the service life. Therefore, the density of the polyethylene plastic material of the general shoe block is different from that of other sole materials. Polyethylene plastic materials of different densities are not easy to blend ^ It often causes the problem of easy separation and fall off of polyethylene soles and shoe soles, which also indirectly reduces the quality and service life of the product. Second, manufacturers of custom shoe soles usually use The shoe soles are made of different-colored polyethylene plastic materials to achieve the overall design sense and dazzling appearance. However, because the shoe soles and other soles are shot separately from the front and rear, so-when other shoe materials are shot After molding and foaming, the periphery of the shoe block will be mixed with Xin to form an overflow material of another material (usually referred to as "overflow" in the industry), which not only affects the overall exquisite feeling of the finished shoe, but also two different colors of polyethylene plastic material The chaotic overflow of colors is the main reason for reducing product quality; therefore, in view of the above defects, we are seeking ideals, practicality and progress. , To be very honest to strive for a goal of improvement. -In view of this, the inventor of this case has carefully considered and accumulated many years of experience in the sales, research and development of various types of footwear plastic injection molding institutions and related footwear injection products. A dual-hardness polyethylene sole injection method that solves the problem of color overflow caused by the injection of shoe blocks of different colors in the past. The primary object of the present invention is to provide a dual-hardness polyethylene sole that can solve the problem of color overflow caused by shoe soles of different colors in the past.
第5頁 515753 五、發明說明(3) 射出方法,本發明主要係運用四個製造步驟之中的(1 ) •雙色射出機射出雙色雙密度鞋邊塊步驟、(3 ) •同色 同密度材質射出包覆步驟,藉由上述二個步驟可以使鞋邊 塊射出結果不受雙硬度聚乙烯塑膠材質影響,確實能夠達 成解決以往溢色問題之目的者。 本發明之次要目的,在於提供一種可以加強材質結合 效果的雙硬度聚乙烯鞋底射出方法,本發明運用具有雙密 度的鞋邊塊與同密度的聚乙烯塑膠材質結合,藉此,可以 達成結合效果更佳的產品者。 首先,請參閱第一圖所示,依據本發明所提供之一種 雙硬度聚乙烯鞋底射出方法,係包括下列之製造步驟為其 特徵者: (1 ) •雙色射出機射出雙色雙密度鞋邊塊步驟:運 用雙色射出機射出具有雙色雙密度的鞋邊塊者; (2 ) •置入模具步驟:將鞋邊塊置入模具内者; (3 ) •同色同密度材質射出包覆步驟:在模具内射 出與該鞋邊塊外層顏色、密度相同的聚乙烯塑膠者; (4 ) •開模步驟:開模取出成品者。 有關本案發明為達成上述目的、技術,所採用之詳細 手段及其他功效,茲列舉一較佳可實施例並配合圖式詳細 說明如後,相信本案發明之目的、特徵及其他優點,當可Page 5 515753 V. Description of the invention (3) Injection method, the present invention mainly uses (1) • two-color injection machine to inject two-color dual-density shoe blocks, (3) • same color and same density material In the injection coating step, the above two steps can make the injection result of the shoe block not affected by the double-hardness polyethylene plastic material, and can indeed achieve the purpose of solving the problem of past color overflow. A secondary object of the present invention is to provide a dual-hardness polyethylene sole injection method that can enhance the material combination effect. The present invention uses a shoe block with double density to combine with a polyethylene plastic material of the same density, thereby achieving a combination Those who perform better. First, please refer to the first figure. According to the present invention, a dual-hardness polyethylene shoe injection method includes the following manufacturing steps as its characteristics: (1) • A two-color injection machine emits a two-color dual-density shoe block. Steps: Use a two-color injection machine to shoot shoe blocks with two colors and two densities; (2) • Place in the mold step: Place shoe blocks in the mold; (3) • Injection coating with the same color and density material: Those who inject a polyethylene plastic with the same color and density as the outer layer of the shoe block in the mold; (4) • Mold opening step: Take out the finished product after opening the mold. Regarding the detailed methods and other effects adopted by the invention of this case to achieve the above-mentioned objects, technologies, a preferred embodiment can be listed and illustrated in detail with the drawings. I believe that the purpose, characteristics and other advantages of this invention will be
第6頁 515753 第 閱 參 請 再 解 瞭 之 體 具 而 入 4)深 /IV 明一 說得 明 t 發之 」由 五 二 四 ^ 請C :塊 :驟邊 行步鞋 進塊出 段邊射 手鞋機 及度出 驟密射 步雙色 作色雙 操雙用 之出運 9射係 下機明 據出發 依射本 係色, 明雙示 發·所 本 圖 , 1-^二 示C第 所 閱 圖 參 IX 1± (1 層 色層 一色 第 一 之第 高且 較 ’ 度} 硬2 有1 具C } 層 ο色 1 二 C第 塊之 邊低 43-*·· 該度 , 項 }與 ο- 色側 二後 第及 用側 運下 ? Λ 觀側 美上 確的 明 隔1 分^~_ 的C 間層 之色 } 一 2第 1在 C覆 層包 色 二 CXI Λ/Γ弟 Τ-Η 與C } 層 將 示 ; 所 者圖 3 二 ο第 1—I 閱 C參 塊請 邊樣 鞋同 的: 度驟 密步 雙具 色模 雙入 有置 具· 個} 一 2 成C 完 具恰 模} 的 ^"I )1~_ ο ( 2 層 C色 穴一 模第 型之; 鞋高者 設較上 預度面 有硬壁 具的 入 ο 置 1 ο )(2 ο 塊C 1邊穴 {鞋模 塊該該 邊且在 鞋,靠 該内貼 三邊浠 第鞋乙 閱該聚 參與的 請出同 :射相 驟内度 步}密 覆ο 、 包 2 色 出C顏 射穴之 質模} 材型2 度鞋1 密的{ 同且(層 色模色 同在二 •,第 } 示 3 所 ο /1\ 圖 1 四C 、塊 膠 塑 3 4 ;穴 者模 \ly ^ ο鞋 3的 (具 底模 鞋該 一啟 成開 泡: 發驟 且步 並模 ,開 底 鞋 的 成 完 泡 發 出 取 内 \)y ο 2 /^X 穴 模 型 鞋。 該者 自品 ,成 \»y \)/ ο ο 2 3 以明 可1隔 侧1—^^分 一 C的 品層間 成色之 ο 第 2 3 之 1 C 高 C 底較層 鞋度色 的硬二 明}第 發ο與 本 τ—- , κ(χ r-H 是塊1 的邊c 提鞋層 一該色 得到一 值見第 楚且 清,Page 6 515753 Please refer to the body equipment that you have already solved. 4) Deep / IV Mingyi made it clear. "From May 2 ^ ^ Please C: block: stepping shoes into the block out of the edge Sagittarius shoe machine and a flash shot with a dense shooting step. Two-color color and dual-use dual-use operation. The 9-shooting system will start according to the color of the shooting system. Read the picture reference IX 1 ± (1 layer color layer first color first highest and more than 'degree} hard 2 has 1 C} layer ο color 1 second C block edge is 43- * ·· this degree, item } And ο- the color side is the second and the next side to carry it down? Λ Look at the side of the C layer that is clearly separated by 1 minute ^ ~ _} 1 2 1st in the C coating color 2 CXI Λ / Γ 弟 Τ-Η and C} layers will be shown; so Figure 3 II ο 1—I read the C reference block, please sample the same shoes: degree of dense steps, double color mode, double-insertion device, one} 2 into C complete with exactly} ^ " I) 1 ~ _ ο (2 layers of C-colored holes in the first mold type; the shoe height is set to have a hard-walled tool above the pre-planned surface ο set 1 ο) (2 ο Block C 1 side hole {Shoe module that side and in the shoe, leaning inside Post the three sides of the second shoes, read the participation of the same, please share the same: shot phase step} close coverage ο, package 2 color out C quality of the model of Cyan shot points} shape 2 degree shoes 1 dense {same and ( Layer color model color is the same as the second one, No. 3 shown ο / 1 \ Figure 1 Four C, block plastic 3 4; hole model \ ly ^ ο shoes 3 (with bottom mold shoes should be opened into a bubble : Step and step and mold, open the bottom of the shoes to finish the inside out \) y ο 2 / ^ X cavity model shoes. The self-made, become \ »y \) / ο ο 2 3 Yi Ming Ke 1 On the other side, 1 ~ ^^ points of a C of the inter-layer color ο 2 3 1 1 C high C bottom harder than the shoes of the second color} the first ο and the τ ---, κ (χ rH is block 1 The edge c of the shoe lift layer should get a value for this color.
的時C } ,1 觀泡底2 以3 美發鞋1所彳 確}該彳,膠 明1與層3塑 分3 }色侧稀 十C 2 二後乙 有膠1—^第及聚。 具塑丨該侧與前 }稀層因下 j眼 ο 乙色C 、2者 1聚二間側1用 C該第}上C使 塊而該1的層在 邊,在3 }色現 鞋線生C 1 二呈 的邊發膠1第果 明}會塑C的效 發1果烯層色色 本1效乙色顏溢 5)故C色聚一同讓 ,層一一/ilL之^^ 、 合日 奶觀色的}在度不 £美一生ο覆密將 、確第產3包同} 五 1—I 一一 C 層 1—I 藉 3 C膠色C , C合塑二層果 膠融烯第色效。 塑相乙的二合者 烯}聚 > 第結果 乙2明ο該的效 聚1發1與佳合 之C本C }更結 }層且塊1有的 ο色,邊3 具佳 3 二 }鞋C會更 C第質該膠間有 底之材於塑之具 鞋}膠同烯者會 該ο塑相乙二品 於^^稀度聚,產 由C乙密該後出 ,塊聚、在接射 面邊A色故黏的 方鞋V顏,合明 一該E的}融發 另與是} 2相本 係 皆 T-Η Η /--'χ , } 者 3 c 2 此 515753 綜上所述,本發明係依據:(l).雙色射出機射出雙色 雙密度鞋邊塊步驟;(2).置入模具步驟;(3).同色同密度 材質射出包覆步驟;(4).開模步驟;藉由上述的四個製造 步驟,可以解決以往鞋底射出不同色鞋邊塊時所產生的溢 色問題,故本發明確實是一種最實用的雙硬度聚乙烯鞋底 射出方法者;所以本發明之『具有產業之可利用性』應已 毋庸置疑,此外,本案發明實施例所揭露之構造,在申請 之前並未曾見於諸刊物,亦未曾被公開使用,不但具有如The time C}, 1 view the foam bottom 2 to 3 hairdressing shoes 1}}}, 胶, gelatin 1 and layer 3 plastic 3} color side dilute ten C 2 second two have rubber 1 — ^ and poly. With plastic 丨 the side and the front} thin layer because of the lower eye ο B color C, 2 of 1 together two sides 1 with C, the first} make C block, and the 1 layer is on the side, the shoes are shown in 3} color Thread C1, two-sided edge gel, 1st fruit} will shape the effect of C1, the color of the alkene layer, the color of the first effect, and the color of the second effect. 5) Therefore, let C color together, let ’s layer one by one / ilL ^^ 、 The color of the milk of the day is not in the United States, a lifetime, a close package, and the first three packages are produced} 5 1-I 1-C layer 1-I borrow 3 C gel color C, C plastic pectin Melting effect. Plastic phase B diene ene} Polymerization> The second result B2. The effect poly 1 hair 1 and Jiahe C C C} More knot} layer and block 1 color, edge 3 with good 3 Two} shoes C will be more quality C. The material with the bottom of the glue room is plastic and the shoes are made of plastic. Those who are glued with ene will be ο plastic phase. Blocky, A-colored and sticky square shoes V Yan on the side of the shooting surface, together Mingyiyi E}} fusion and yes} 2 phases are all T-Η Η /-'χ,} 3 c 2 This 515753 In summary, the present invention is based on: (l) the step of injecting a two-color dual-density shoe block by a two-color injection machine; (2) the step of placing a mold; (3) the step of injecting and covering a material of the same color and density; (4). Mold opening step; through the above-mentioned four manufacturing steps, the problem of color overflow that occurred when soles shot different color shoe blocks in the past can be solved, so the invention is indeed a most practical dual-hardness polyethylene sole injection Therefore, the "availability of the industry" of the present invention should not be doubted. In addition, the structure disclosed in the embodiment of the present invention has not been seen in publications or applied before application. Open use, not only as having
第8頁 515753 五、發明說明(6) 上功效增進之事實,更具有生產快速、節省人工、節省生 產加工時間、降低生產成本及品質較佳等不可輕忽的附加 功效,是故,本發明之『新穎性』以及『進步性』都均已 符合專利法規,爰依法提出發明專利之申請,祈請惠予審 查並早曰賜准專利,實感德便。Page 8 515753 V. Description of the invention (6) The fact that the effect is enhanced has more important effects such as fast production, saving labor, saving production and processing time, reducing production cost and better quality. Therefore, the present invention Both "newness" and "progressiveness" have met the patent regulations, and they have applied for patents for inventions in accordance with the law. I hope that they will be examined and granted patents soon.
第9頁 515753 圖式簡單說明 圖式部份 第一圖 係本發明之步驟圖。 第二圖 係本發明之鞋邊塊立體示意圖。 第三圖 係本發明之鞋底射出完成後之剖視圖 第四圖 係本發明之鞋底射出完成後之上視圖 第五圖 係本發明之成品立體圖。 圖號部份 (1 1 )第一色層 〇 )鞋邊塊 2 )第二色層 2 0 )鞋型模穴 〇)鞋底 3 聚乙烯塑膠Page 9 515753 Brief description of the drawings Schematic part The first drawing is a step diagram of the present invention. The second figure is a schematic perspective view of a shoe block according to the present invention. The third figure is a sectional view of the sole of the present invention after the injection is completed. The fourth figure is the upper view of the sole of the present invention after the injection is completed. The fifth figure is a perspective view of the finished product of the present invention. Drawing number part (1 1) first color layer 〇) shoe block 2) second color layer 20) shoe mold cavity 0) sole 3 polyethylene plastic
第10頁Page 10
Claims (1)