TW201625067A - Cold light effect producing method - Google Patents

Cold light effect producing method Download PDF

Info

Publication number
TW201625067A
TW201625067A TW103144731A TW103144731A TW201625067A TW 201625067 A TW201625067 A TW 201625067A TW 103144731 A TW103144731 A TW 103144731A TW 103144731 A TW103144731 A TW 103144731A TW 201625067 A TW201625067 A TW 201625067A
Authority
TW
Taiwan
Prior art keywords
layer
conductive
conductive sheet
luminescent
sheet
Prior art date
Application number
TW103144731A
Other languages
Chinese (zh)
Other versions
TWI530228B (en
Inventor
Wen-Shan Hong
Original Assignee
Wen-Shan Hong
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wen-Shan Hong filed Critical Wen-Shan Hong
Priority to TW103144731A priority Critical patent/TWI530228B/en
Application granted granted Critical
Publication of TWI530228B publication Critical patent/TWI530228B/en
Publication of TW201625067A publication Critical patent/TW201625067A/en

Abstract

The present invention relates to a cold light effect producing method, particularly to an improvement method provided when the cold light effect on an uneven surface cannot be decorated by printing, which includes steps 1~8; wherein step 1 to step 5 are spraying a pattern layer on a non-conductive substrate, adhering a first conductive sheet on the edge of the pattern layer, spraying at least one time a first conductive paint layer on the pattern layer and the first conductive sheet, spraying at least one time a light emitting paint layer on the first conductive paint layer. and adhering a second conductive sheet on the edge of the light emitting paint layer; and step 6 to step 8 are spraying at least one time a second conductive paint layer on the light emitting paint layer and the second conductive sheet, spraying at least one time a transparent paint layer on the second conductive paint layer, and using a controller to electrically connect the first conductive sheet and the second conductive sheet. Thus, the method may also exhibit a pattern with cold light effect on an uneven surface.

Description

冷光效果製造方法Cold light effect manufacturing method

  本發明係屬於一種冷光效果,特別是一種如何在不平整表面呈現冷光效果的製造方法。The present invention belongs to a luminescent effect, and more particularly to a manufacturing method of how to exhibit a luminescent effect on an uneven surface.

  隨著科技的進步以及年輕人或不同組群的喜好,每個組群皆會有某些特別喜歡的嗜好或圖像,以至於這些不同組群的人們會將特別喜歡的嗜好或圖像加入在某些物品上,不僅增加個人的觀感喜愛程度,亦可提升每個消費組群的購買意願。例如:有些年輕人會在機車外殼加入時下流行的卡通人物或是加入一些酷炫的圖像而吸引異性;或者是有些人會在汽車外殼加入一些圖像而增加觀感或風趣。
  習知技術利用貼紙將該些圖像貼附於某些物品上,如第1圖所示,在車頭前的一平面板1上貼設一貼紙10,以增加車體的觀賞度。但該貼紙10方式在趣味性及特殊性上皆不足夠,對此,提高車體的觀感度是有限的,對於追求時下流行的人們是不滿足的。因此,為了能提高趣味性及特殊性,習知技術以印刷方式使圖像呈現冷光效果,然,目前印刷方式並無法適用於非平面的位置,進而浪費實體上的空間利用性。為了使實體上的所有位置皆可以具有冷光效果的裝飾,故,在不平整表面裝飾圖像的方法亦有加以改良之必要。
With the advancement of technology and the preferences of young people or different groups, each group will have some favorite hobbies or images, so that people from these different groups will add special favorite hobbies or images. In some items, not only increase the personal perception of love, but also increase the willingness to buy each consumer group. For example, some young people will join the popular cartoon characters in the locomotive shell or add some cool images to attract the opposite sex; or some people will add some images in the car shell to increase the look or interest.
Conventional techniques use stickers to attach the images to certain items. As shown in FIG. 1, a sticker 10 is attached to a flat panel 1 in front of the front of the vehicle to increase the visibility of the vehicle body. However, the sticker 10 method is not sufficient in terms of fun and particularity. Therefore, the improvement of the perception of the car body is limited, and it is unsatisfactory for people who are popular in the present. Therefore, in order to enhance the interest and particularity, the conventional technology makes the image appear cold-light effect by printing. However, the current printing method cannot be applied to a non-planar position, thereby wasting physical availability on the solid. In order to make the decoration of all the positions on the solid body have a cold light effect, the method of decorating the image on the uneven surface is also necessary to be improved.

  本發明主要目的在於提出一種可在不平整表面產生冷光效果的冷光效果製造方法。
  根據前述目的,本發明提出一種冷光效果製造方法,尤指適用於不平整表面的裝飾,其包含有以下步驟:
  步驟一:噴塗圖像層在非導電底材上;
  步驟二:黏貼一第一導電片在該圖像層之邊緣上;
  步驟三:噴塗至少一次第一導電漆層在該圖像層及該第一導電片上,該第一導電漆層與該第一導電片電性連接;
  步驟四:噴塗至少一次發光漆層在該第一導電漆層上;
  步驟五:黏貼一第二導電片在該發光漆層之邊緣上;
  步驟六:噴塗至少一次第二導電漆層在該發光漆層及該第二導電片上,該第二導電漆層與該第二導電片電性連接;
  步驟七:噴塗至少一次透明漆層在該第二導電漆層上;以及
  步驟八:利用控制器電性連接該第一導電片及該第二導電片。
  進一步地,其中步驟六及步驟七之間,更包含有一步驟:在該第二導電漆層及該透明漆層之間噴塗至少一次水性透明塗料層。
  進一步地,該水性透明塗料層替換為透明導電塗料層。
  進一步地,在步驟六中的該第二導電漆層替換為透明導電塗料層,在步驟七中的該透明漆層替換為二液型金油層。
  進一步地,該非導電底材為導電底材時,該步驟三省略。
  再者,本發明提出另一種冷光效果製造方法,尤指適用於不平整表面的裝飾,其主要以線條表現圖形,包含有以下步驟:
  步驟A:描畫線條圖層在非導電底材上;
  步驟B:黏貼一第一導電片在該線條圖層之線條上;
  步驟C:描畫至少一次第一導電漆層在該線條圖層及該第一導電片上,該第一導電漆層與該第一導電片電性連接;
  步驟D:描畫至少一次發光漆層在該第一導電漆層上;
  步驟E:黏貼一第二導電片在該發光漆層之邊緣上;
  步驟F:黏貼銅片層在該發光漆層及該第二導電片上,該銅片層與該第二導電片電性連接;
  步驟G:描畫至少一次透明漆層在該銅片層、該發光漆層及該第二導電片上;以及
  步驟H:利用控制器電性連接該第一導電片及該第二導電片。
  進一步地,其中步驟F及步驟G之間,更包含有一步驟:在該銅片層及該透明漆層之間描畫至少一次水性透明塗料層。
  進一步地,該水性透明塗料層替換為透明導電塗料層。
  進一步地,在步驟G中的該透明漆層替換為二液型金油層。
  進一步地,該非導電底材為導電底材時,該步驟C省略。
  本發明之特點在於:
 1.本發明藉由該些步驟使該圖像層或該線條圖層可在不平整表面上呈現冷光效果。
 2.本發明藉由噴塗該圖像層在該導電底材或該非導電底材上,可依實際需求而選擇圖像所搭配的底材及其步驟。
 3.本發明藉由描畫該線條圖層在該導電底材及該非導電底材上,可依實際需求而選擇線條圖所搭配的底材及其步驟。
 4.本發明可藉由增設該水性透明塗料層以增加導電率。
 5.本發明的該透明漆層能作為保護或絕緣,以避免對人體造成觸電危害。
The main object of the present invention is to provide a method for manufacturing a luminescent effect which can produce a luminescent effect on an uneven surface.
In accordance with the foregoing objects, the present invention provides a method of fabricating a luminescent effect, particularly a decoration suitable for an uneven surface, comprising the steps of:
Step 1: spraying the image layer on the non-conductive substrate;
Step 2: pasting a first conductive sheet on an edge of the image layer;
Step 3: spraying the first conductive paint layer on the image layer and the first conductive sheet at least once, the first conductive paint layer is electrically connected to the first conductive sheet;
Step 4: spraying at least one luminescent paint layer on the first conductive lacquer layer;
Step 5: pasting a second conductive sheet on the edge of the luminescent paint layer;
Step 6: spraying at least one second conductive lacquer layer on the luminescent paint layer and the second conductive sheet, the second conductive lacquer layer being electrically connected to the second conductive sheet;
Step 7: spraying at least one transparent lacquer layer on the second conductive lacquer layer; and step 8: electrically connecting the first conductive sheet and the second conductive sheet by a controller.
Further, between step 6 and step 7, there is further included a step of spraying at least one aqueous clear coating layer between the second conductive paint layer and the transparent paint layer.
Further, the aqueous clear coating layer is replaced with a transparent conductive coating layer.
Further, the second conductive lacquer layer in step 6 is replaced by a transparent conductive paint layer, and the transparent lacquer layer in step VII is replaced by a two-component gold oil layer.
Further, when the non-conductive substrate is a conductive substrate, the third step is omitted.
Furthermore, the present invention proposes another method for manufacturing a luminescent effect, in particular for a decoration of an uneven surface, which mainly represents a figure in a line, comprising the following steps:
Step A: drawing a line layer on a non-conductive substrate;
Step B: pasting a first conductive sheet on the line of the line layer;
Step C: drawing at least one first conductive paint layer on the line layer and the first conductive sheet, the first conductive paint layer being electrically connected to the first conductive sheet;
Step D: drawing at least one luminescent paint layer on the first conductive lacquer layer;
Step E: pasting a second conductive sheet on the edge of the luminescent paint layer;
Step F: bonding a copper sheet layer on the luminescent paint layer and the second conductive sheet, the copper sheet layer being electrically connected to the second conductive sheet;
Step G: drawing at least one transparent lacquer layer on the copper sheet layer, the luminescent paint layer and the second conductive sheet; and step H: electrically connecting the first conductive sheet and the second conductive sheet by a controller.
Further, between step F and step G, there is further included a step of drawing at least one aqueous clear coating layer between the copper sheet layer and the transparent lacquer layer.
Further, the aqueous clear coating layer is replaced with a transparent conductive coating layer.
Further, the clear lacquer layer in step G is replaced with a two-component gold oil layer.
Further, when the non-conductive substrate is a conductive substrate, the step C is omitted.
The invention is characterized by:
1. The present invention enables the image layer or the line layer to exhibit a luminescent effect on an uneven surface by the steps.
2. In the present invention, by spraying the image layer on the conductive substrate or the non-conductive substrate, the substrate to which the image is matched and the steps thereof can be selected according to actual needs.
3. The present invention can select the substrate to which the line drawing is matched and the steps thereof by drawing the line layer on the conductive substrate and the non-conductive substrate.
4. The present invention can increase conductivity by adding the aqueous clear coating layer.
5. The transparent lacquer layer of the present invention can be used as a protection or insulation to avoid electric shock hazard to the human body.

﹝習知﹞
1‧‧‧平面板
10‧‧‧貼紙
﹝本發明﹞
2‧‧‧圖像層
3‧‧‧非導電底材
30‧‧‧第一導電片
31‧‧‧第一導電漆層
32‧‧‧發光漆層
33‧‧‧第二導電片
34‧‧‧第二導電漆層
35‧‧‧透明塗料層
35‧‧‧透明漆層
4‧‧‧控制器
5‧‧‧線條圖層
6‧‧‧銅片層
[study]
1‧‧‧flat board
10‧‧‧Sticker [present invention]
2‧‧‧Image layer
3‧‧‧ Non-conductive substrate
30‧‧‧First conductive sheet
31‧‧‧First conductive paint layer
32‧‧‧Lighting paint layer
33‧‧‧Second conductive sheet
34‧‧‧Second conductive paint layer
35‧‧‧Transparent paint layer
35‧‧‧Transparent paint layer
4‧‧‧ Controller
5‧‧‧Line layer
6‧‧‧copper layer

第1圖:為習知圖像裝飾的立體圖。
第2圖:為本發明第一實施例的步驟流程圖。
第3圖:為第2圖運用在實體上的立體圖。
第4-1圖:為第3圖的部分放大立體圖。
第4-2圖:為第4-1圖於A-A位置剖視圖。
第5圖:為本發明第二實施例的步驟流程圖。
第6-1圖:為第5圖運用在實體上的立體圖。
第6-2圖:為第6-1圖的局部放大平面圖。
第7-1圖:為第6-1圖的部分立體圖。
第7-2圖:為第7-1圖於B-B位置剖視圖。
Figure 1: A perspective view of a conventional image decoration.
Figure 2 is a flow chart showing the steps of the first embodiment of the present invention.
Figure 3: A perspective view of the entity applied to Figure 2.
Fig. 4-1 is a partially enlarged perspective view of Fig. 3.
Figure 4-2: A cross-sectional view taken at line AA in Figure 4-1.
Figure 5 is a flow chart showing the steps of the second embodiment of the present invention.
Figure 6-1: A perspective view of the physical image used in Figure 5.
Fig. 6-2 is a partially enlarged plan view of Fig. 6-1.
Figure 7-1: A partial perspective view of Figure 6-1.
Figure 7-2: is a sectional view of the 7-1 position at the BB position.

  以下配合所附的圖示,詳加說明本發明的結構如何組合、使用,應當更容易瞭解本發明的目的、技術內容、特點及其所達成的功效,在詳細描述本發明之前,要注意的是,在以下的說明內容中,相同元件的不同態樣的實施,是以相同的符號表示。
  請參閱第2圖至第4-2圖所示,本發明提出一種尤指適用於不平整表面的冷光效果製造方法,其包含有以下步驟:
  步驟一:噴塗圖像層2在非導電底材3上;
  步驟二:黏貼一第一導電片30在該圖像層2之邊緣上;
  步驟三:噴塗至少一次第一導電漆層31在該圖像層2及該第一導電片30上,該第一導電漆層31與該第一導電片30電性連接,其中該第一導電漆層31在噴塗之前,會將該第一導電漆層31稀釋至適當黏度並均勻噴塗在該圖像層2上及該第一導電片30黏貼在該圖像層2的一端,待該第一導電漆層31乾燥後進行下一步驟;
  步驟四:噴塗至少一次發光漆層32在該第一導電漆層31上,將該發光漆層32均勻噴塗在該第一導電漆層31上,待該發光漆層32乾燥後進行下一步驟;
  步驟五:黏貼一第二導電片33在該發光漆層32之邊緣上,該第二導電片33與該第一導電片30錯開設置,以避免該第一導電片30與該第二導電片33接觸而造成線路短路,進而引起火花等意外事故;
  步驟六:噴塗至少一次第二導電漆層34在該發光漆層32及該第二導電片33上,該第二導電漆層34與該第二導電片33電性連接,其中該第二導電漆層34在噴塗之前,會將該第二導電漆層34稀釋至適當黏度並根據圖形將該第二導電漆層34均勻噴塗在該發光漆層32及該第二導電片33黏貼在該發光漆層32的一端,待該第二導電漆層34乾燥後進行下一步驟;
  步驟七:噴塗至少一次透明漆層36在該第二導電漆層34上,將該透明漆層36均勻噴塗在該第二導電漆層34上,以作為保護層或絕緣層,避免人碰觸而觸電,待該透明漆層36乾燥後進行下一步驟;
  步驟八:利用控制器4電性連接該第一導電片30及該第二導電片33,以該控制器4電性連接該第一導電片30及該第二導電片33,使該圖像層2呈現冷光效果而提高觀賞度。此外,該控制器4的輸出電力係配合於圖像大小,當該圖像層2之圖示面積越大時,則該控制器4的輸出電力需求就越大。
  進一步地,為了增加該第二導電漆層34的導電率,在步驟六及步驟七之間,更包含有一步驟:在該第二導電漆層34及該透明漆層36之間噴塗至少一次水性透明塗料層35。此外,為了使業者可依消費者或實際狀況選擇適合的材料,本發明更可將該水性透明塗料層35替換為透明導電塗料層,或是在步驟六中的該第二導電漆層34可替換為透明導電塗料層,又或者是在步驟七中的該透明漆層36替換為二液型金油層,以滿足不同消費者的需求。
  此外,在本發明該圖像層2如何在該非導電底材3上呈現冷光效果的方法步驟中,可進一步地將該非導電底材3設為導電底材,由於該導電底材本身具有導電特性,在噴塗順序上便不需要額外再噴塗該第一導電漆層31,對此,可將該步驟三的動作省略掉,利用其他步驟讓該圖像層2在該導電底材上亦能呈現冷光效果。
  再者,本發明提出另一種適用於不平整表面的冷光效果製造方法,其主要以線條表現圖形,請搭配第5圖至第7-2圖所示,其包含有以下步驟:
  步驟A:描畫線條圖層5在該非導電底材3上;
  步驟B:黏貼該第一導電片30在該線條圖層5之線條上;
  步驟C:描畫至少一次第一導電漆層31在該線條圖層5及該第一導電片30上,該第一導電漆層31與該第一導電片30電性連接,其中該第一導電漆層31在噴塗之前,會將該第一導電漆層31稀釋至適當黏度並均勻噴塗在該線條圖層5上及該第一導電片30黏貼在該線條圖層5的一端,待該第一導電漆層31乾燥後進行下一步驟;
  步驟D:描畫至少一次發光漆層32在該第一導電漆層31上,將該發光漆層32均勻噴塗在該第一導電漆層31上,待該發光漆層32乾燥後進行下一步驟;
  步驟E:黏貼該第二導電片33在該發光漆層32之邊緣上,該第二導電片33與該第一導電片30錯開設置,以避免該第一導電片30與該第二導電片33接觸而造成線路短路,進而引起火花等意外事故;
  步驟F:黏貼銅片層6在該發光漆層32及該第二導電片33上,該銅片層6與該第二導電片33電性連接;在本案實施例中,在該線條圖層5之所有線條皆有該銅片層6之線條分佈且將該銅片層6之線條黏貼成如第6-2圖所示之形式,為了不讓該銅片層6之線條佈滿於該線條圖層5之線條上而造成該線條圖層5之圖示的冷光效果無法呈現,在本發明之該銅片層6之線條的寬度設為小於該線條圖層5之線條寬度,且於較佳的實施例中,當該銅片層6之線條的寬度越小於該線條圖層5之線條寬度,該線條圖層5所能呈現的冷光效果範圍就越大;
  步驟G:描畫至少一次透明漆層36在該銅片層6、該發光漆層32及該第二導電片33,該透明漆層36作為保護層或絕緣層,避免人碰觸而觸電,待透明漆層36乾燥後進行下一步驟;
  步驟H:利用該控制器4電性連接該第一導電片30及該第二導電片33,以該控制器4電性連接該第一導電片30及該第二導電片33,使該線條圖層5呈現冷光效果而提高觀賞度。此外,該控制器4的輸出電力係配合於該線條圖層5之圖示大小,當該線條圖層5之圖示面積大時,則該控制器4的輸出電力需求就越大。
  同樣地,為了增加該第二導電漆層34的導電率,在步驟F及步驟G之間,更包含有一步驟:在該銅片層5及該透明漆層36之間描畫至少一次水性透明塗料層35。且,為了使業者可依消費者或實際狀況選擇適合的材料,本發明更可將該水性透明塗料層35替換為透明導電塗料層,或者是在步驟H中的該透明漆層36替換為二液型金油層,以滿足消費者的需求。相同地,在本發明該線條圖層5如何在該非導電底材3上呈現冷光效果的方法步驟中,可將該非導電底材3設為導電底材,由於該導電底材本身具有導電特性,在噴塗順序上便不需要額外再噴塗該第一導電漆層31,對此,可將該步驟C的動作省略掉,利用其他步驟讓該線條圖層5在該導電底材上亦能呈現冷光效果。
  此外,於本發明以線條表現圖形的另一種冷光效果製造方法中,在同一底材上可分別描畫出複數個如第6-1圖所示的圓圈及符號8的個別圖形,並以上述步驟A至步驟H的程序讓每一該圖形個別呈現冷光效果,亦可進一步地利用如微處理器的複數控制器分別控制每一該圖形的冷光效果,讓每一該圖形的冷光效果同時呈現或個別呈現,甚至是控制每一該圖形呈現冷光效果的時間,使每一該圖形的冷光效果可依設定時間來呈現。而在其他可能的實施例中,其該些圖形相互電性連接而可僅以一控制器或一微處理器來控制每一該圖形的冷光效果呈現,但不僅以該些實施態樣為限。
  綜上所述,本發明藉由該些步驟使該圖像層2或該線條圖層5呈現冷光效果。且透過底材為該導電底材或該非導電底材3,業者可依實際需求而選擇該圖像層2或該線條圖層5及所搭配的底材與步驟。本發明藉由該透明漆層36作為保護或絕緣,以避免對人體造成觸電危害。此外,本發明可藉由增設該水性透明塗料層35來增加該第二導電漆層34的導電率。
  惟前述者僅為本發明的較佳實施例,其目的在使熟習該項技藝者能夠瞭解本發明的內容而據以實施,並非用來限定本發明實施的範圍;故舉凡依本發明申請範圍所述的形狀、構造及特徵所為的均等變化或修飾,均應包括在本發明的申請專利範圍內。
In the following, in conjunction with the accompanying drawings, how to combine and use the structure of the present invention, it should be easier to understand the object, technical content, features and effects achieved by the present invention, which should be noted before describing the present invention in detail. In the following description, the implementation of different aspects of the same elements is denoted by the same reference numerals.
Referring to Figures 2 to 4-2, the present invention provides a method for manufacturing a luminescent effect, particularly for an uneven surface, comprising the following steps:
Step 1: spraying the image layer 2 on the non-conductive substrate 3;
Step 2: pasting a first conductive sheet 30 on the edge of the image layer 2;
Step 3: spraying the first conductive lacquer layer 31 on the image layer 2 and the first conductive sheet 30 at least once, the first conductive lacquer layer 31 is electrically connected to the first conductive sheet 30, wherein the first conductive layer Before the lacquer layer 31 is sprayed, the first conductive lacquer layer 31 is diluted to an appropriate viscosity and uniformly sprayed on the image layer 2 and the first conductive sheet 30 is adhered to one end of the image layer 2, After the conductive paint layer 31 is dried, the next step is performed;
Step 4: spraying at least one luminescent lacquer layer 32 on the first conductive lacquer layer 31, uniformly spraying the luminescent lacquer layer 32 on the first conductive lacquer layer 31, and after the luminescent lacquer layer 32 is dried, proceeding to the next step. ;
Step 5: pasting a second conductive sheet 33 on the edge of the luminescent paint layer 32, the second conductive sheet 33 is offset from the first conductive sheet 30 to avoid the first conductive sheet 30 and the second conductive sheet 33 contact causes a short circuit, which in turn causes accidents such as sparks;
Step 6: spraying the second conductive lacquer layer 34 on the luminescent paint layer 32 and the second conductive sheet 33 at least once, the second conductive lacquer layer 34 is electrically connected to the second conductive sheet 33, wherein the second conductive layer Before the spraying, the second conductive paint layer 34 is diluted to a proper viscosity, and the second conductive paint layer 34 is uniformly sprayed on the luminescent paint layer 32 and the second conductive sheet 33 is adhered to the illuminating according to the pattern. One end of the lacquer layer 32, after the second conductive lacquer layer 34 is dried, the next step is performed;
Step 7: spraying at least one transparent lacquer layer 36 on the second conductive lacquer layer 34, uniformly spraying the transparent lacquer layer 36 on the second conductive lacquer layer 34 as a protective layer or an insulating layer to prevent human touch And the electric shock, after the transparent lacquer layer 36 is dried, the next step is performed;
Step 8: The first conductive sheet 30 and the second conductive sheet 33 are electrically connected to the controller 4, and the first conductive sheet 30 and the second conductive sheet 33 are electrically connected to the controller 4 to make the image. Layer 2 exhibits a luminescent effect to enhance viewing. In addition, the output power of the controller 4 is matched to the image size, and the larger the illustrated area of the image layer 2, the greater the output power demand of the controller 4.
Further, in order to increase the conductivity of the second conductive lacquer layer 34, between step 6 and step 7, there is further included a step of spraying at least one water between the second conductive lacquer layer 34 and the transparent lacquer layer 36. Clear coating layer 35. In addition, in order to enable the operator to select a suitable material according to the consumer or the actual situation, the present invention can further replace the aqueous clear coating layer 35 with a transparent conductive coating layer, or the second conductive paint layer 34 in step 6 can be It is replaced by a transparent conductive paint layer, or the transparent paint layer 36 in step 7 is replaced by a two-component gold oil layer to meet the needs of different consumers.
In addition, in the method step of how the image layer 2 of the present invention exhibits a luminescent effect on the non-conductive substrate 3, the non-conductive substrate 3 can be further configured as a conductive substrate, since the conductive substrate itself has conductive properties. In the spraying sequence, the first conductive paint layer 31 is not required to be additionally sprayed. For this, the action of the third step can be omitted, and the image layer 2 can be presented on the conductive substrate by other steps. Cold light effect.
Furthermore, the present invention proposes another method for manufacturing a luminescent effect suitable for an uneven surface, which is mainly characterized by lines, as shown in Figures 5 to 7-2, which includes the following steps:
Step A: drawing a line layer 5 on the non-conductive substrate 3;
Step B: pasting the first conductive sheet 30 on the line of the line layer 5;
Step C: drawing the first conductive paint layer 31 on the line layer 5 and the first conductive sheet 30 at least once, the first conductive paint layer 31 is electrically connected to the first conductive sheet 30, wherein the first conductive paint Before the spraying, the first conductive paint layer 31 is diluted to a proper viscosity and uniformly sprayed on the line layer 5 and the first conductive sheet 30 is adhered to one end of the line layer 5, and the first conductive paint is to be applied. After layer 31 is dried, the next step is performed;
Step D: drawing at least one luminescent lacquer layer 32 on the first conductive lacquer layer 31, uniformly spraying the luminescent lacquer layer 32 on the first conductive lacquer layer 31, and after the luminescent lacquer layer 32 is dried, proceeding to the next step. ;
Step E: pasting the second conductive sheet 33 on the edge of the luminescent paint layer 32, the second conductive sheet 33 is offset from the first conductive sheet 30 to avoid the first conductive sheet 30 and the second conductive sheet 33 contact causes a short circuit, which in turn causes accidents such as sparks;
Step F: bonding the copper sheet layer 6 on the luminescent paint layer 32 and the second conductive sheet 33, the copper sheet layer 6 is electrically connected to the second conductive sheet 33; in the embodiment, in the line layer 5 All the lines have the line distribution of the copper layer 6 and the line of the copper layer 6 is adhered to the form as shown in Fig. 6-2, in order to prevent the line of the copper layer 6 from being filled with the line. The cold light effect of the line layer 5 is not shown in the line of the layer 5, and the width of the line of the copper sheet layer 6 in the present invention is set to be smaller than the line width of the line layer 5, and is preferably implemented. In the example, when the width of the line of the copper sheet layer 6 is smaller than the line width of the line layer 5, the range of the luminescent effect that the line layer 5 can exhibit is larger;
Step G: drawing at least one transparent lacquer layer 36 on the copper sheet layer 6, the luminescent lacquer layer 32 and the second conductive sheet 33, the transparent lacquer layer 36 serving as a protective layer or an insulating layer to prevent human touch and electric shock, After the transparent lacquer layer 36 is dried, the next step is performed;
Step H: The first conductive sheet 30 and the second conductive sheet 33 are electrically connected to the controller 4, and the first conductive sheet 30 and the second conductive sheet 33 are electrically connected to the controller 4 to make the line Layer 5 exhibits a cool light effect to enhance viewing. In addition, the output power of the controller 4 is matched to the illustrated size of the line layer 5. When the graphical area of the line layer 5 is large, the output power demand of the controller 4 is larger.
Similarly, in order to increase the conductivity of the second conductive lacquer layer 34, between step F and step G, there is further included a step of drawing at least one water-based clear coating between the copper sheet layer 5 and the transparent lacquer layer 36. Layer 35. Moreover, in order to enable the operator to select a suitable material according to the consumer or the actual situation, the present invention may further replace the aqueous clear coating layer 35 with a transparent conductive coating layer, or replace the transparent lacquer layer 36 in step H with two. Liquid gold oil layer to meet the needs of consumers. Similarly, in the method step of how the line layer 5 of the present invention exhibits a luminescent effect on the non-conductive substrate 3, the non-conductive substrate 3 can be used as a conductive substrate, since the conductive substrate itself has conductive properties, The first conductive paint layer 31 is not required to be sprayed in the spraying sequence. For this reason, the action of the step C can be omitted, and the line layer 5 can also exhibit a cold light effect on the conductive substrate by other steps.
In addition, in another method for manufacturing a cold light effect in which the line is represented by a line in the present invention, a plurality of individual patterns such as a circle and a symbol 8 shown in FIG. 6-1 can be separately drawn on the same substrate, and the above steps are performed. The program from A to step H causes each of the graphics to be individually presented with a luminosity effect, and the multiplex light controller such as a microprocessor can be further used to separately control the luminescence effect of each of the graphics, so that the luminescence effect of each of the graphics is simultaneously presented or Individually presenting, even controlling the time each of the graphics exhibits a luminescent effect, so that the luminescence effect of each of the graphics can be presented at a set time. In other possible embodiments, the graphics are electrically connected to each other, and the luminescence effect of each of the graphics may be controlled by only one controller or a microprocessor, but not limited to the implementation manners. .
In summary, the present invention causes the image layer 2 or the line layer 5 to exhibit a luminescent effect by these steps. And through the substrate is the conductive substrate or the non-conductive substrate 3, the user can select the image layer 2 or the line layer 5 and the matched substrate and steps according to actual needs. The transparent paint layer 36 is protected or insulated by the present invention to avoid electric shock hazard to the human body. In addition, the present invention can increase the conductivity of the second conductive lacquer layer 34 by adding the aqueous clear coating layer 35.
The foregoing is only a preferred embodiment of the present invention, which is intended to be understood by those skilled in the art and is not intended to limit the scope of the present invention. Equivalent variations or modifications of the shapes, configurations and features are intended to be included within the scope of the present invention.


國內寄存資訊【請依寄存機構、日期、號碼順序註記】
國外寄存資訊【請依寄存國家、機構、日期、號碼順序註記】

Domestic registration information [please note according to the registration authority, date, number order]
Foreign deposit information [please note according to the country, organization, date, number order]

2‧‧‧圖像層 2‧‧‧Image layer

3‧‧‧非導電底材 3‧‧‧ Non-conductive substrate

30‧‧‧第一導電片 30‧‧‧First conductive sheet

31‧‧‧第一導電漆層 31‧‧‧First conductive paint layer

32‧‧‧發光漆層 32‧‧‧Lighting paint layer

33‧‧‧第二導電片 33‧‧‧Second conductive sheet

34‧‧‧第二導電漆層 34‧‧‧Second conductive paint layer

35‧‧‧透明塗料層 35‧‧‧Transparent paint layer

36‧‧‧透明漆層 36‧‧‧Transparent paint layer

4‧‧‧控制器 4‧‧‧ Controller

Claims (10)

【第1項】[Item 1] 一種冷光效果製造方法,尤指適用於不平整表面的裝飾,包含有以下步驟:
  步驟一:噴塗圖像層在非導電底材上;
  步驟二:黏貼一第一導電片在該圖像層之邊緣上;
  步驟三:噴塗至少一次第一導電漆層在該圖像層及該第一導電片上,該第一導電漆層與該第一導電片電性連接;
  步驟四:噴塗至少一次發光漆層在該第一導電漆層上;
  步驟五:黏貼一第二導電片在該發光漆層之邊緣上;
  步驟六:噴塗至少一次第二導電漆層在該發光漆層及該第二導電片上,該第二導電漆層與該第二導電片電性連接;
  步驟七:噴塗至少一次透明漆層在該第二導電漆層上;以及
  步驟八:利用控制器電性連接該第一導電片及該第二導電片。
A method for manufacturing a luminescent effect, especially for a decorative surface, comprising the following steps:
Step 1: spraying the image layer on the non-conductive substrate;
Step 2: pasting a first conductive sheet on an edge of the image layer;
Step 3: spraying the first conductive paint layer on the image layer and the first conductive sheet at least once, the first conductive paint layer is electrically connected to the first conductive sheet;
Step 4: spraying at least one luminescent paint layer on the first conductive lacquer layer;
Step 5: pasting a second conductive sheet on the edge of the luminescent paint layer;
Step 6: spraying at least one second conductive lacquer layer on the luminescent paint layer and the second conductive sheet, the second conductive lacquer layer being electrically connected to the second conductive sheet;
Step 7: spraying at least one transparent lacquer layer on the second conductive lacquer layer; and step 8: electrically connecting the first conductive sheet and the second conductive sheet by a controller.
【第2項】[Item 2] 如申請專利範圍第1項所述之冷光效果製造方法,其中步驟六及步驟七之間,更包含有一步驟:在該第二導電漆層及該透明漆層之間噴塗至少一次水性透明塗料層。The luminescence effect manufacturing method of claim 1, wherein the step 6 and the step VII further comprise a step of spraying at least one water-based transparent coating layer between the second conductive lacquer layer and the transparent lacquer layer. . 【第3項】[Item 3] 如申請專利範圍第2項所述之冷光效果製造方法,其中,該水性透明塗料層替換為透明導電塗料層。The luminescent effect manufacturing method according to claim 2, wherein the aqueous clear coating layer is replaced with a transparent conductive coating layer. 【第4項】[Item 4] 如申請專利範圍第1項所述之冷光效果製造方法,其中,在步驟六中的第二導電漆層替換為透明導電塗料層,在步驟七中的透明漆層替換為二液型金油層。The luminescent effect manufacturing method according to claim 1, wherein the second conductive lacquer layer in the step 6 is replaced with a transparent conductive paint layer, and the transparent lacquer layer in the step VII is replaced with a two-component gold oil layer. 【第5項】[Item 5] 如申請專利範圍第1項至第4項其中一項所述之冷光效果製造方法,其中,非導電底材為導電底材時,該步驟三省略。The method of manufacturing a luminescent effect according to any one of the items 1 to 4, wherein the step 3 is omitted when the non-conductive substrate is a conductive substrate. 【第6項】[Item 6] 一種冷光效果製造方法,尤指適用於不平整表面的裝飾,其主要以線條表現圖形,包含有以下步驟:
  步驟A:描畫線條圖層在非導電底材上;
  步驟B:黏貼一第一導電片在該線條圖層之線條上;
  步驟C:描畫至少一次第一導電漆層在該線條圖層及該第一導電片上,該第一導電漆層與該第一導電片電性連接;
  步驟D:描畫至少一次發光漆層在該第一導電漆層上;
  步驟E:黏貼一第二導電片在該發光漆層之邊緣上;
  步驟F:黏貼銅片層在該發光漆層及該第二導電片上,該銅片層與該第二導電片電性連接;
  步驟G:描畫至少一次透明漆層在該銅片層、該發光漆層及該第二導電片上;以及
  步驟H:利用控制器電性連接該第一導電片及該第二導電片。
A method for manufacturing a luminescent effect, in particular for a decoration of an uneven surface, which mainly represents a figure in a line, comprising the following steps:
Step A: drawing a line layer on a non-conductive substrate;
Step B: pasting a first conductive sheet on the line of the line layer;
Step C: drawing at least one first conductive paint layer on the line layer and the first conductive sheet, the first conductive paint layer being electrically connected to the first conductive sheet;
Step D: drawing at least one luminescent paint layer on the first conductive lacquer layer;
Step E: pasting a second conductive sheet on the edge of the luminescent paint layer;
Step F: bonding a copper sheet layer on the luminescent paint layer and the second conductive sheet, the copper sheet layer being electrically connected to the second conductive sheet;
Step G: drawing at least one transparent lacquer layer on the copper sheet layer, the luminescent paint layer and the second conductive sheet; and step H: electrically connecting the first conductive sheet and the second conductive sheet by a controller.
【第7項】[Item 7] 如申請專利範圍第6項所述之冷光效果製造方法,其中步驟F及步驟G之間,更包含有一步驟:在該銅片層及該透明漆層之間描畫至少一次水性透明塗料層。The luminescent effect manufacturing method of claim 6, wherein the step F and the step G further comprise a step of: drawing at least one aqueous clear coating layer between the copper sheet layer and the transparent lacquer layer. 【第8項】[Item 8] 如申請專利範圍第7項所述之冷光效果製造方法,其中,該水性透明塗料層替換為透明導電塗料層。The luminescent effect manufacturing method of claim 7, wherein the aqueous clear coating layer is replaced with a transparent conductive coating layer. 【第9項】[Item 9] 如申請專利範圍第6項所述之冷光效果製造方法,其中,在步驟G中的透明漆層替換為二液型金油層。The luminescent effect manufacturing method according to claim 6, wherein the transparent lacquer layer in the step G is replaced with a two-component gold oil layer. 【第10項】[Item 10] 如申請專利範圍第6項至第9項其中一項所述之冷光效果製造方法,其中,非導電底材為導電底材時,該步驟C省略。The method of manufacturing a luminescent effect according to any one of the items 6 to 9, wherein the step C is omitted when the non-conductive substrate is a conductive substrate.
TW103144731A 2014-12-22 2014-12-22 Cold light effect manufacturing method TWI530228B (en)