TW200724199A - Golf club body and superficial painting method thereof - Google Patents
Golf club body and superficial painting method thereofInfo
- Publication number
- TW200724199A TW200724199A TW094147490A TW94147490A TW200724199A TW 200724199 A TW200724199 A TW 200724199A TW 094147490 A TW094147490 A TW 094147490A TW 94147490 A TW94147490 A TW 94147490A TW 200724199 A TW200724199 A TW 200724199A
- Authority
- TW
- Taiwan
- Prior art keywords
- film
- fundamental
- metal
- club body
- paint film
- Prior art date
Abstract
Provided is a golf club body and a superficial painting method thereof. The club body includes a non-metal plain club, a set of fundamental paint film, a metal ceramic film and a protection film. The fundamental paint film set has a priming paint film coating on the plain club. The metal ceramic film is related to utilize a vacuum magnetron sputtering method to deposit a metal ceramic material composed of a metal material and a carbon-containing gas on the surface of the fundamental paint film set. The protection film is related to coat transparent protection paint on the surface of the metal ceramic film. By directly carrying out the sputtering on the fundamental paint film set, the manufacturing process can be simplified as well as the time can be shortened, which can also save the manufacturing cost. Furthermore, by adjusting the ratio of the metal material and carbon, the club body can display more various kinds of colors provided to be selected whereby the desire of purchasing can be heightened.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
TW94147490A TWI264320B (en) | 2005-12-30 | 2005-12-30 | Golf club body and superficial painting method thereof |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
TW94147490A TWI264320B (en) | 2005-12-30 | 2005-12-30 | Golf club body and superficial painting method thereof |
Publications (2)
Publication Number | Publication Date |
---|---|
TWI264320B TWI264320B (en) | 2006-10-21 |
TW200724199A true TW200724199A (en) | 2007-07-01 |
Family
ID=37969293
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
TW94147490A TWI264320B (en) | 2005-12-30 | 2005-12-30 | Golf club body and superficial painting method thereof |
Country Status (1)
Country | Link |
---|---|
TW (1) | TWI264320B (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
TWI740756B (en) * | 2020-12-25 | 2021-09-21 | 明安國際企業股份有限公司 | Multi-color coating process of golf club head |
-
2005
- 2005-12-30 TW TW94147490A patent/TWI264320B/en not_active IP Right Cessation
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
TWI740756B (en) * | 2020-12-25 | 2021-09-21 | 明安國際企業股份有限公司 | Multi-color coating process of golf club head |
Also Published As
Publication number | Publication date |
---|---|
TWI264320B (en) | 2006-10-21 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US20120275130A1 (en) | Electronic device housing and method of manufacturing thereof | |
EP1789461A4 (en) | Direct to metal polyurethane coating compositions | |
JP2010094992A (en) | Housing and method for producing the same | |
TWI348486B (en) | High-solid antifouling paint composition, antifouling coating film, base material with coating film, antifouling base material, method for forming coating film on surface of base material, antifouling method for base material, and high-solid multi-packag | |
JP2010094989A (en) | Housing and method for manufacturing the same | |
MXPA05003631A (en) | High tg coatings. | |
TWI300446B (en) | ||
EP2033717A3 (en) | Decorated resin molded article and method for producing the same | |
SG171631A1 (en) | A method for the manufacture of a coating | |
TW201328490A (en) | Housing and method for making the same | |
PL366047A1 (en) | Process for coating metallic substrate surfaces | |
MY157931A (en) | Coating for decorative metals with improved mar and scratch resistance and methods of application | |
JP2014156116A (en) | Housing and method for manufacturing the same | |
CN202856811U (en) | Mobile phone film-plated shell | |
TW200728763A (en) | Optical thin film and manufacturing method thereof | |
TWI264320B (en) | Golf club body and superficial painting method thereof | |
TW201311090A (en) | Housing and method for making the same | |
CN206457942U (en) | A kind of stainless checkered plate PE diaphragms | |
WO2006019803A3 (en) | Electro-coat adhesion layer with a siloxane top coat | |
TWI535498B (en) | Housing and method for making the same | |
KR20110017828A (en) | Method for coating non-conductive film | |
TW200724706A (en) | A light metal with colorful surface coating and the manufacture method of the same | |
CN107460448A (en) | A kind of modified coatings of matrix surface and preparation method thereof | |
TW201326438A (en) | Coated article and method for making the same | |
TW200724198A (en) | Golf club shaft and coating method of the same |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
MM4A | Annulment or lapse of patent due to non-payment of fees |