TH90133B - High-strength steel plates with excellent formability, thermal grinding capabilities, and methods for manufacturing them. - Google Patents

High-strength steel plates with excellent formability, thermal grinding capabilities, and methods for manufacturing them.

Info

Publication number
TH90133B
TH90133B TH601006181A TH0601006181A TH90133B TH 90133 B TH90133 B TH 90133B TH 601006181 A TH601006181 A TH 601006181A TH 0601006181 A TH0601006181 A TH 0601006181A TH 90133 B TH90133 B TH 90133B
Authority
TH
Thailand
Prior art keywords
less
strength steel
steel plates
hot
tensile
Prior art date
Application number
TH601006181A
Other languages
Thai (th)
Other versions
TH88184B (en
TH137163A (en
TH90133A (en
Inventor
วิลเลียม สแตเนียร์ นายปีเตอร์
ฟูนากาว่า นายโยชิมาซ่า
Original Assignee
เจเอฟอี สตีล คอร์ปอเรชั่น
อีเนียน ซิลิการส์ ลิมิเต็ด
Filing date
Publication date
Publication of TH90133A publication Critical patent/TH90133A/en
Application filed by เจเอฟอี สตีล คอร์ปอเรชั่น, อีเนียน ซิลิการส์ ลิมิเต็ด filed Critical เจเอฟอี สตีล คอร์ปอเรชั่น
Publication of TH137163A publication Critical patent/TH137163A/en
Publication of TH88184B publication Critical patent/TH88184B/en
Publication of TH90133B publication Critical patent/TH90133B/en

Abstract

------13/02/2562------(OCR) หน้า 1 ของจำนวน 1 หน้า บทสรุปการประดิษฐ์ เพื่อจัดให้มีแผ่นเหล็กกล้าความแข็งแรงสูงที่ดีเยี่ยมในความสามารถในการขึ้นรูปปั๊มอุ่น (warmstamp formability) และวิธีการสำหรับผลิตสิ่งเดียวกันนั้น เหล็กกล้าที่มีส่วนประกอบที่มี, ในแง่ของ %โดยมวล, คาร์บอน : 0.01% ถึง 0.2%, ซิลิคอน : 0.5% หรือตํ่ากว่า, แมงกานีส: 2% หรือตํ่ากว่า, ฟอลฟอรัส: 0.03% หรือตํ่ากว่า, กำมะกัน : 0.01% หรือตํ่ากว่า, อัลลูมินัม : 0.07% หรือตํ่ากว่า, และไนโตรเจน : 0.01% หรือตํ่ากว่า และยังมีอีกหนึ่งหรือสองธาตุหรือมากกว่าที่เลือกจากไททาเนียม, นิโอเบียม, วานาเดียม, โมลิบดินัม , ทังสเตน, และโบรอน ถูกนำไปอย่างต่อเนื่องกันสู่ขบวนการรีดร้อนที่ประกอบด้วย การเผากึงช่วงอุณหภูมิเฟสเดี่ยวออสเตนไนต์, ทำการรีดร้อนที่อุณหภูมิยุติการรีดนั้นสำเร็จที่ 860 ํC หรือสูงกว่า, และจากนั้น ขดที่อุณหภูมิที่ 400 ํC หรือสูงกว่าและตํ่ากว่า 600 ํC และสู่กระบวนการการปฏิบัติการความร้อนที่ประกอบด้วย การทำการปฏิบัติการความร้อนในช่วงอุณหภูมิที่ 650 กึง 750 ํ C ดังนั้น, แผ่นเหล็กกล้าที่ดีเยี่ยมในความสามารถในการขึ้นรูปปั๊มอุ่นที่มีคุณสมบัติแรงดึง ที่ซึ่งการยืดตัวเฉพาะที่มากกว่าการยืดตัวที่เป็นเอกภาพ ที่อุณหภูมิทดสอบที่ 400 ํ C หรือสูงกว่า และคุณสมบัติแรงดึงที่ซึ่งการยืดตัวที่เป็นเอกภาพเป็น 40% หรือมากกว่าในแง่ของอัตราส่วนต่อการยืดตัวรวม ที่อุณหภูมิทดสอบที่ตํ่ากว่า 400 ํ C และยังมีเนื้อสารแม่, ซึ่งเป็นเฟสเดี่ยวเฟอร์ไรต์อย่างมาก และโครสร้างที่ซึ่งคาร์ไบด์ อัลลอยด์ที่มีขนาดที่ตํ่ากว่า 10 nmถูกกระจาย และถูกทำให้ตกตะกอนในเนื้อสารแม่ในสภาพที่มีการไม่เลือกตัวแปร (no variantselection) ------------ หน้า 1 ของจำนวน 1 หน้า บทสรุปการประดิษฐ์ เพื่อจัดให้มีแผ่นหล็กกล้าความแข็งแรงสูงที่ดีเยี่ยมในความสามารถในการขึ้นรูปปั๊มอุ่น (warm stamp formability) และวิธีการสำหรับผลิตสิ่งเดียวกันนั้น เหล็กกล้าที่มีส่วนประกอบที่มี, ในแง่ ของ % โดยมวล,คาร์บอน : 0.01%ถึง0.2%, ซิลิคอน :0.5% หรือตํ่ากว่า,แมงกานีส: 2% หรือ ตํ่ากว่า,ฟอสฟอรัส: 0.03%หรือตํ่ากว่า,กำมะกัน:0.01% หรือตํ่ากว่า,อัลลูมินัม :0.07%หรือตํ่า กว่า, และไนโตรเจน : 0.01 % หรอตํ่ากว่า และยังมีอีกหนึ่งหรอสองธาตุหรือมากกว่าที่เลือกจาก ไททาเนียม, นิโอเปียม, วานาเดียม, โมลิบดีนัม, ทังสเตน, และโบรอน ถูกนำไปอย่างต่อเนื่องกัน ส่ขบวนการรดร้อนที่ประกอบด้วย การเผาถึงช่วงอุณหภูมิเฟสเดี่ยวออสเตนไนต์, ทำการรดร้อนที่ อุณหภูมิยุติการรดขั้นสำเร็จที่ 860 องศาc หรือสูงกว่า, และจากนั้น ขดที่อุณหภูมิที่ 400 องศาc หรือสูงกว่า และตํ่ากว่า 600 องศา c และส่กระบวนการการปฏิบัติการความร้อนที่ประกอบด้วย การทำการปฏิบัติการ ความร้อนในช่วงอุณหภูมิที่ 650 ถึง 750 องศา c ดังนั้น, แผ่นเหล็กกล้าที่ดีเยี่ยมในความสามารถในการ ขึ้นรูปปั๊มอุ่นที่มีคุณสมบัติแรงดึง ที่ชึ่งการยืดดัวเฉพาะที่มากกว่าการยืดดัวที่เป็นเอกภาพ ที่อุณหภูมิ ทดสอบที่ 400 องศา c หรอสูงก,ว่า และคุณสมบัติแรงดึงที่ซึ่งการยืดตัวที่เป็นเอกภาพเป็น 40%หรือมากกว่า ในแง่ของอัตราส่วนต่อการยืดตัวรวม ที่อุณหภูมิทดสอบที่ตํ่ากว่า 400 องศา c และยังมีเนื้อสารแม่, ซึ่งเป็น เฟสเดี่ยวเฟอร์ไรต์อย่างมาก และโครงสร้างที่ซึ่งคาร์ไบด์อัลลอยด์ที่มีขนาดที่ตํ่ากว่า 10 nm ถูก กระจาย และถูกทำให้ตกตะกอนในเนื้อสารแม่ในสภาพที่มีการไม่เลือกตัวแปร (no variant selection)------13/02/2562------(OCR) Page 1 of 1. Abstract of Invention: To provide a high-strength steel sheet with excellent warmstamp formability and a method for producing the same, steel with the following composition, in terms of % by mass: Carbon: 0.01% to 0.2%, Silicon: 0.5% or less, Manganese: 2% or less, Phosphorus: 0.03% or less, Sulfur: 0.01% or less, Aluminum: 0.07% or less, and Nitrogen: 0.01% or less, and one or two or more additional elements selected from titanium, niobium, vanadium, molybdenum, tungsten, and boron, was continuously subjected to a hot rolling process consisting of: The austenite single-phase sintering was performed, followed by hot rolling to a termination temperature of 860°C or higher, and then coiling at temperatures of 400°C or higher and lower than 600°C, and subsequent heat treatment consisting of heat treatment in the temperature range of 650 to 750°C. Thus, the resulting steel plate exhibits excellent warm-stamping formability with tensile properties where specific elongation exceeds uniform elongation at test temperatures of 400°C or higher, and tensile properties where uniform elongation is 40% or more in terms of ratio to total elongation at test temperatures below 400°C. Furthermore, the matrix is predominantly ferritic single-phase, and the structure in which carbides and alloys with particle sizes less than 10 nm are dispersed and precipitated in the matrix under no variant selection conditions. ------------ Page 1 of 1 page. Invention Summary. To provide high-strength steel plates with excellent warm stamp formability and a method for producing the same, steel with the following composition, in terms of % by mass: carbon: 0.01% to 0.2%, silicon: 0.5% or less, manganese: 2% or less, phosphorus: 0.03% or less, sulfur: 0.01% or less, aluminum: 0.07% or less, and nitrogen: 0.01% or less, and one or two or more selected elements from titanium, niopium, vanadium, molybdenum, tungsten, and boron, is continuously subjected to a hot-pressing process consisting of calcination to the single-phase austenite stage, followed by hot-pressing at... The curing temperature is terminated at 860°C or higher, and then coiled at 400°C or higher and below 600°C, followed by a heat treatment process consisting of heat treatments in the temperature range of 650 to 750°C. Therefore, the steel plate exhibits excellent heat-stamping capabilities with tensile properties where the specific elongation exceeds the uniform elongation at a test temperature of 400°C or higher, and tensile properties where the uniform elongation is 40% or more in terms of the ratio to total elongation at a test temperature below 400°C. Furthermore, the matrix is a highly ferritic single-phase structure in which alloy carbides smaller than 10 nm are dispersed and precipitated in the matrix under no variant selection conditions.

Claims (6)

------27/02/2562------(OCR) หน้า 1 ของจำนวน 2 หน้าข้อถือสิทธิ 1. แผ่นเหล็กกล้าความแข็งแรงสูงซึ่งมีกำลังดึงที่ 590 MPa หรือมากกว่าและดีเยี่ยมในความสามารถในการขึ้นรูปปั๊มอุ่น แผ่นเหล็กกล้าความแข็งแรงสูงประกอบด้วย ส่วนประกอบที่มี, ในแง่ของ % โดยมวล,คาร์บอน : 0.01% ถึง 0.2%, ซิลิคอน :0.5% หรือต่ำกว่า, แมงกานีส : 2% หรือตํ่ากว่า,ฟอสฟอรัส : 0.03% หรือตํ่ากว่า, กำมะถัน : 0.01% หรือตํ่ากว่า, อัลลูมินัม : 0.07% หรือตํ่ากว่า,และไนโตรเจน : 0.01% หรือตํ่ากว่า และยังมีอีกธาตุหนึ่งหรือสองธาตุที่เลือกจากไททาเนียม : 0.005ถึง 0.3%, และ นิโอเบียม : 0.005 ถึง 0.6% , หนึ่งหรือสองธาตุหรือมากกว่าที่เลือกจากวานาเดียม : 0.005 ถึง 1.0%, โมลิบดินัม: 0.005 ถึง 0.5%, ทั้งสเตน :0.01 ถึง 1.0%, และโบรอน .0. 0005 ถึง 0.0040% และที่เหลือเป็นเหล็กกับสิ่งเจือปนที่ไม่อาจหลีกเลี่ยงได้ คุณสมบัติแรงดึงที่ซึ่งแรงเครียดจากการระบุของโหลดสูงสุดถึงรอยแตก มากกว่าแรงเครียดก่อนการระบุของโหลดสูงสุดจากการเริ่มต้นของการทดสอบแรงดึงที่ได้มา ในการทดสอบแรงดึงที่ถูกทำขึ้นที่อุณหภูมิทดสอบที่ 400? C หรือสูงกว่า และแรงเครียดก่อนการระบุของโหลดสูงสุดจากการเริ่มต้นของการทดสอบแรงดึงเป็น 40% หรือมากกว่า ในแง่ของอัตราส่วนต่อการยืดตัวรวม จากการเริ่มต้นของการทดสอบแรงดึงถึงรอยแตกที่ได้ในการทดสอบแรงดึง ที่ถูกทำขึ้นที่อุณหภูมิทดสอบที่ตํ่ากว่า400? C เนื้อสารแม่ (matrix), ซึ่งเป็นเฟสเดี่ยวเฟอร์ไรต์อย่างมาก ที่ซึ่งอัตราส่วนพื้นที่ของเฟสเฟอร์ไรต์เป็น 95% หรือมากกว่า ; และ โครงสร้างที่ซึ่งคาร์ไบด์ อัลลอยด์ที่มีขนาดที่ตํ่ากว่า 10 mm ถูกกระจายและถูกทำให้ตกตะกอนในเนื้อสารแม่ในสภาพที่ไม่มีการเลือกที่แตกต่างกันไปในรูปแบบ (no variant selection) 2. แผ่นเหล็กกล้าความแข็งแรงสูงตามข้อถือสิทธิข้อ 1 ..ที่ซึ่งแผ่นเหล็กกล้าความแข็งแรงสูงมีขั้นฉาบผิวบนผิวหน้าหน้า 2 ของจำนวน 2 หน้า3. แผ่นเหล็กกล้าความแข็งแรงลงตามข้อถือสิทธิข้อ 2., ทีซึ่งนั้นฉาบผิวเป็นนั้นกัลวาไนขัหไ'อขันอบเหนียวชุบสิงกะสิ (galvannealed layer)4. วิธีการตำหรับผสิตแผ่นเหล็กกล้าความแข็งแรงสูงซึ่งมีกำลังดีงที่ 590 MPa หรอมากกว่า,มีเนึ๋อสารแม่และโครงลร้างตามข้อถือสิทธิข้อ 1. 1 และรเยี่ยมในความลามารถไนการขึ๋นเปป็มอุ่น,, วิธีการประกอบด้วย :ทำต่อเนื่องกันไปขบวนการรดร้อนที่ประกอบด้วย การเผาเหล็กกล้าที่มีองค์ประกอบที่มี,ในแง่ของ0/0โดยมวล,คาร์บอน : 0.01%ถืง0.2%, ขิสิคอน :0.5% หรอตํ่ากว่า,แมงกานีล: 2%หรอตํ่ากว่า,ฟอลฟอรัส: 0.03%หรอตํ่ากว่า,กำมะกัน:0.01% หรอตํ่ากว่า,อ้ลลูมิน้ม :0.07%หรอตํ่ากว่า,และไนโตรเจน ะ0.01% หรอตํ่ากว่า และยังมีหนื่งหรอลองธาตุที่เลือกจากไททาเนียม. 0.005 ถืง 0.3%, และนีโอเนียม : 0.005 ถืง 0.6% 1 หนื่งหรอลองธาตุห'ร่อมากกว่า ที่เลือกจากวานาเดียม :0.005 ถึง1.0%,โมลืบดินม: 0.005ถึง0.5%, ทังสเตน:0.01 ถึง 1.0%, และโบรอน 0. 0005 ถึง 0.0040% และที่เหลือเป็นเหล็กและสิงเจอปนที่ไม่อาจหลีกเลี่ยงได้ ถึงช่วงอุณหภูมิเฟลเดี่ยวออลเตนในต์, การนำแผ่นเหล็กกล้าไปร่ดร้อนที่อุณหภูมินั้นสำเร็จที่ 860? C หรอสูงกว่า, และจากนั้น ขดแผ่นเหล็กกล้าที่อุณหภูมิที่ 400? C หรอสูงกว่า และตํ่าก'ว่า 600? C เพื่อ สร้างแผ่นรดร้อน ; และขบวนการปฏิบ้ตการความร้อนที่ประกอบด้วย การเอาละเกิดผิวหน้าของแผ่นรดร้อนออก,’และการนำแผ่นรดร้อนไปสู่การปฎิปติการความร้อนในช่วงอุณหภูมิที่ 650 ถึง 750? C5. วิธีการตำหรับผลิตแผ่นเหล็กกล้าความแข็งแรงสูงตามข้อถือสิทธิที่ 4., ยังประกอบด้วยการทำการปฏิปติการฉาบผิวกับแผ่นรดร้อน ที่ถูกนำไปสู่กระบวนการปฎปติการความร้อน 6. วิธีการตำหรับผลืตแผ่นเหล็กกล้าความแข็งแรงสูงตามข้อถือสิทธิข้อ 4., ที่ประกอบด้วยการทำการปฎิปติการกัลวาไนขัหรอการทำการปฏิปติการอบอ่อนชุบลังกะสิ (galvannealingtreatment) ต่อไป ที่ต่อจากขบวนการปฏิปติการความร้อน ------------ ------13/02/2562------(OCR) หน้า 1 ของจำนวน 2 หน้าข้อถือสิทธิ 1. แผ่นเหล็กกล้าความแข็งแรงสูงที่มีความสามารถในการขึ้นรูปบดอุ่น แผ่นเหล็กกล้าความแข็งแรงสูงที่มีความแข็งแรงสูงที่กำลังดึงที่ 590 MPa หรือมากกว่าและคุณสมบัติแรงดึงที่ซึ่งแรงเครียดจากการชี้บอกของโหลดสูงสูดถึงรอยแตก มากกว่าแรงเครียด ก่อนหน้าการชี้บอกของโหลดสูงสุดจากการเริ่มต้นของการทดสอบแรงดึงที่ได้ ในการทดสอบแรงดึงทีถูกทำขึ้นที่อุณหภูมิทดสอบที่ 400 ํC หรือสูงกว่า และแรงเครียดก่อนหน้าการชี้บอกของโหลดสูงสุดจากการเริ่มต้นของการทดสอบแรงดึงเป็น 40% หรือมากกว่า ในแง่ของอัตราส่วนต่อการยืดตัวรวมจากการเริ่มต้นของการทดสอบแรงดึงถึงรอยแตกที่ได้ในการทดสอบแรงดึง ที่ถูกทำขึ้นที่อุณหภูมิทดสอบที่ตํ่ากว่า400 ํC, และ แผ่นเหล็กกล้าความแข็งแรงสูงประกอบด้วย : เนื้อสารแม่ (matrix), ซึ่งเป็นเฟสเดี่ยวเฟอร์ไรต์อย่างมาก ที่ซึ่งอัตราส่วนเนื้อที่ของเฟสเฟอร์ไรต์เป็น 95% หรือมากกว่า ; และ โครงสร้างที่ซึ่งคาร์ไบด์ อัลลอยด์ที่ขนาดที่ตํ่ากว่า 10 nm ถูกกระจาย และถูกทำให้ตกตะกอนในเนื้อสารแม่ในสภาพที่มีการไม่เลือก (no variant selection) 2. แผ่นเหล็กกล้าความแข็งแรงสูงตามข้อถือสิทธิข้อ 1. ประกอบด้วยส่วนประกอบที่มิ, ’ในแง่ของ%โดยมวล,คาร์บอน: 0.01%ถืง0.2%, ซึสิคอน :0.5% หรอตํ่ากว่า,แมงกานีล: 2%ห่รอตํ่าก1ว่า, ฟอสฟอรัส : 0.03% หรอตํ่ากว่า, กำมะลัน : 0.01% ห'รอตํ่ากว่า, อัลดูมินัม : 0.07%หรอตำกว่า, และไนโตรเจน : 0.01% หรอตํ่ากว่า และยังมิอีกหนึ่งหร้อสองธาตุหรอมากกว่าที่เลือกจากไททาเนียม:0.005 ถืง0.3%, นีโอเบียม :0.005 ถืง0.6%,วานาเดียม :0.005 ถืง1.0%, โมลิบดีนัม: 0.005ถืง0.5%, ท้งสเตน :0.01 ถืง 1.0%, และโบรอน :0.0005 ถืง 0.0040%และที่เหลือเป็นเหล็กกับสิงเจือปนที่ไม่อาจหลีกเลี่ยงได้ 3. .แผ่นเหล็กกล้าความแข็งแรงสูงตามข้อถือสิทธิข้อ1.หรอ 2.,ที่ซึ่งแผ่นเหล็กกล้าความแข็งแรงสูงมิชั้น'ฉาบผิวบนผิวหน้าหน้า 2 ของจำนวน 2 หน้า4. แผ่นเหล็กกล้าความแข็งแรงสูงตามข้อถือสิทธิข้อ 3, ที่ขึ่งข้นฉาบผิวเป็นขื่นกัลวาไนข้หรอข้นอบเหนยวๆ]บสิงกะสิ (galvannealed layer)5. วิธีการสำหรับผลิตแผ่นเหล็กกล้าความแข็งแรงสูงขื่งมีกำสิงดึงที่ 590 MPa หรอมากกว่าและดีเยียมในความลามารกในการขื่นรูปบดอุ่น, วิธิการประกอบด้วย : หำอย่างต่อเนืองก้นไปขบวนการรดร้อนที่ประกอบด้วย การเผาเหล็กล้าที่มีสิวนประกอบทีม,ไนแง'ของ0/0โดยมวล,คาร์บอน : 0.01%ถืง0.2%, ซิลิคอน :0.5% ห่รือตํ่ากว่า,แมงกานีส:2% หํร์อตำกว่า, ฟอสฟอรัส : 0.03% หรอตำกว่า, กำมะถัน : 0.01% ?ห‘รอตํ่ากว่า, อัลลูมินิ'ม :0.07% หรอตำกว่า, และไนโตรเจน : 0.01% หรอตํ่ากว่า และยังมีอีกหนึ่งหรอสองธาตุหรอมากกว่าที่เลือกจากไททาเนียม ; 0.005 ถึง 0.3%, นิโอเนียม : 0.005 ถึง 0.6% 1 วานาเดียม : 0.005 ถึง 1.0%,โมลิบดินม: 0.005ถึง0.5%, ทังสเตน:0.01 ถึง 1.0%, และโบรอน :0.0005 ถึง0.0040% และทีเหลือเป็นเหล็กกับลิงเจือปนที่ไม่อาจหลีกเลี่ยงได้ถึงช่วงอุณหภูมิเฟสเดี่ยวออลเตน-ไนต์, การนำแผ่นเหล็กกล้าไ!]รดร้อนที่อุณหภูมิขื่นสำเร็จที่ 860? C หรอสูงกว่า, และจากนั้น ขดแผ่นเหล็กกล้าทีอุณหภูมิที 400? C หํรัอสูงกว่า และตำกว่า 600? C เพื่อสร้างแผ่นเหล็กกล้ารดร้อน ; และกระบวนการปฎิปติการความร้อนทีประกอบด้วย การเอาละเกิดผิวหน้าของแผ่นรดร้อน ออก, และการนำแผ่นรดร้อนไปสู่การปฏิป้ติการความร้อนในช่วงอุณหภูมิที่ 650 ถึง 750? C6. วธการสำหรับผลิตแผ่นเหล็กกล้าความแข็งแรงสูงตามข้อถือสิทธิที่ 5. ยังประกอบด้วยการหำการปฎิปติการฉาบผิวกับแผ่น'รัดร้อน ที่ถูกนำไปสู่กระบวนการปฏิปติการความร้อน7. วิธีการสำหรับผลิตแผ่นเหล็กกล้าความแข็งแรงสูงตามข้อถือสิทธิข้อ 5. ที่ประกอบด้วยการหำ การปฎิป้ติการกัลวาไนข้ หรอการปฎิปติการอบอ่อนชุบสิงกะสิ (galvannealing treatment) ต่อไปต่อจากกระบวนการปฎิปติการความร้อน ------------ หน้า 1 ของจำนวน 2 หน้า ข้อถือสิทธิ------February 27, 2019------(OCR) Page 1 of 2 pages of Claims 1. High-strength steel plates with a tensile strength of 590 MPa or more and excellent warm stamping formability. The high-strength steel plates consist of: The composition, in terms of percentage by mass, is as follows: Carbon: 0.01% to 0.2%, Silicon: 0.5% or less, Manganese: 2% or less, Phosphorus: 0.03% or less, Sulfur: 0.01% or less, Aluminum: 0.07% or less, and Nitrogen: 0.01% or less. There are also one or two other elements selected from Titanium: 0.005 to 0.3%, and Niobium: 0.005 to 0.6%; one or two or more elements selected from Vanadium: 0.005 to 1.0%, Molybdenum: 0.005 to 0.5%, Tungsten: 0.01 to 1.0%, and Boron: 0.0005 to 0.0040%. The remainder is iron and unavoidable impurities. Tensile properties where the specified stress of the maximum load at crack is greater than the pre-specified stress of the maximum load at the start of the tensile test obtained in tensile tests performed at a test temperature of 400°C or higher, and the pre-specified stress of the maximum load at the start of the tensile test is 40% or more in terms of the ratio of total elongation from the start of the tensile test to crack obtained in tensile tests performed at a test temperature lower than 400°C; the matrix, which is predominantly a single ferrite phase where the area ratio of the ferrite phase is 95% or more; and structures in which carbides... 1. Alloys with particle sizes less than 10 mm are distributed and precipitated in the base matrix in a non-variable selection condition. 2. High-strength steel plates according to claim 1.1, in which the high-strength steel plates have a coating on 2 of 2 faces. 3. Lower-strength steel plates according to claim 2., in which the coating is a galvannealed, annealed layer. 4. Method for producing high-strength steel plates with a tensile strength of 590 MPa or more, with a base matrix and structure according to claim 1.1 and excellent heat resistance, the method consists of: a series of hot processes consisting of: The sintering of steel with the following composition, in terms of 0/0 by mass: Carbon: 0.01% to 0.2%, Silicon: 0.5% or less, Manganese: 2% or less, Phosphorus: 0.03% or less, Sulfur: 0.01% or less, Aluminum: 0.07% or less, and Nitrogen: 0.01% or less. Additionally, one or more selected trace elements are present: Titanium: 0.005 to 0.3%, and Neonium: 0.005 to 0.6%. The selected components are vanadium: 0.005 to 1.0%, molybdenum: 0.005 to 0.5%, tungsten: 0.01 to 1.0%, and boron: 0.0005 to 0.0040%, with the remainder being iron and unavoidable impurities. Up to the single-felt altenite temperature range, the steel plate is heated to a temperature of 860°C or higher, and then coiled at temperatures of 400°C or higher and lower than 600°C to form hot plates; and the heat treatment process consists of surface removal of the hot plate, and heat treatment of the hot plate in the temperature range of 650 to 750°C5. The method for producing high-strength steel plates according to claim 4 also includes surface treatment of the hot plate. 6. Method for producing high-strength steel plates according to claim 4., which includes galvanizing or galvanizing treatment following the heat treatment process. ------------ ------13/02/2019------(OCR) Page 1 of 2 pages of claim 1. High-strength steel plates with warm-formable formability. High-strength steel plates with a tensile strength of 590 MPa or more and tensile properties in which the pre-indicator load stress at the point of fracture is greater than the pre-indicator load stress at the start of the tensile test obtained in a tensile test performed at a test temperature of 400 °C or higher, and the pre-indicator load stress at the start of the tensile test is 40% or more in terms of the ratio of total elongation from the start of the tensile test to the point of fracture obtained in the tensile test. Manufactured at test temperatures below 400°C, the high-strength steel plate consists of: a matrix, which is a highly ferrite single-phase material where the ferrite phase area ratio is 95% or more; and a structure containing carbides. 1. Alloys with particle sizes less than 10 nm are distributed and precipitated in the parent material under no variant selection conditions. 2. High-strength steel plates according to claim 1. contain the following components in terms of percentage by mass: Carbon: 0.01% to 0.2%, Sisicon: 0.5% or less, Manganese: 2% or less, Phosphorus: 0.03% or less, Sulfate: 0.01% or less, Aluminum: 0.07% or less, and Nitrogen: 0.01% or less, and one or two or more selectable elements: Titanium: 0.005 to 0.3%, Niobium: 0.005 to 0.6%, Vanadium: 0.005. 1.0%, Molybdenum: 0.005 to 0.5%, Tungsten: 0.01 to 1.0%, and Boron: 0.0005 to 0.0040%, and the remainder being iron and unavoidable impurities. 3. High-strength steel plates according to claim 1 or 2, in which the high-strength steel plates are not coated on 2 of 2 faces. 4. High-strength steel plates according to claim 3, which are coated with a galvanized or annealed layer. 5. Method for producing high-strength steel plates with a tensile strength of 590 MPa or greater and excellent resistance to heat treatment, the method consists of: a continuous hot treatment process consisting of: The sintering of iron with a composition of 0/0 by mass, carbon: 0.01% to 0.2%, silicon: 0.5% or less, manganese: 2% or less, phosphorus: 0.03% or less, sulfur: 0.01% or less, aluminum: 0.07% or less, and nitrogen: 0.01% or less, and one or two or more elements of your choice including titanium: 0.005 to 0.3%, niobium: 0.005 to 0.6%, vanadium: 0.005 to 1.0%, molybdenum: 0.005 to 0.5%, tungsten: 0.01 to 1.0%, and boron: 0.0005. Up to 0.0040% and the remainder are iron and unavoidable impurities up to the single-phase alttenite temperature range, hot-rolling the steel plate to a finished temperature of 860°C or higher, and then coiling the steel plate at temperatures of 400°C or higher and lower than 600°C to form hot-rolled steel plates; and the heat treatment process consisting of removing the surface coating of the hot-rolled plate, and subjecting the hot-rolled plate to a heat treatment in the temperature range of 650 to 750°C6. The method for producing high-strength steel plates according to claim 5. also consists of a surface coating treatment on the hot-rolled plate that has been subjected to a heat treatment process7. The method for producing high-strength steel plates according to claim 5. consists of a galvanizing treatment. Or the galvannealing treatment process, which follows the heat treatment process ------------ Page 1 of 2 pages. Claims 1. แผ่นเหล็กกล้าความแข็งแรงสูงซึงมีกำลังดึงที่ 590 MPa หรือมากกว่า และดีเยี่ยมใน ความสามารถในการขึ้นรูปปั๊มอุ่น แผ่นเหล็กกล้าความแข็งแรงสูงประกอบด้วย : ส่วนประกอบที่มี,ในแง่ของ %โดยมวล, คาร์บอน : 0.01 ถึง 0.2% , ซิลิคอน : 0.5% หรือตํ่ากว่า, แมงกานีส : 2% หรือตํ่ากว่า, ฟอสฟอรัส : 0.03% หรือ ตํ่ากว่า,กำมะถัน:0.01% หรือตํ่ากว่า,อัลลูมินัม : 0.07% หรือตํ่ากว่า,และไนโตรเจน: 0.01% หรือ ตํ่ากว่า และยังมีธาตุหนึ่งหรอสองธาตุที่เลือกจาก ไททาเนียม : 0.005 ถึง 0.3% และ นิโอเปียม : 0.005 ถึง 0.6%, หนึ่งหรือสองธาตุหรอมากกว่าที่เลือกจาก วานาเดียม : 0.005 ถึง 1.0%, โมลิบดินัม 0.005 ถึง 0.5%, ทังสแตน : 0.01 ถึง 1.0%, และโบรอน : 0.0005 ถึง 0.0040% และที่เหลือเป็นเหล็ก กับสิ่งเจือปนที่ไม่อาจหลีกเลี่ยงได้ คุณสมบัติแรงดึงที่ซึ่งแรงเครียดจากการระบุของโหลดสูงสุดถึงรอยแตก มากกว่าแรงเครียดก่อน การระบุของโหลดสูงสุดจากการเริ่มต้นของการทดสอบแรงดึงที่ได้มา ในการทสดลอบแรงดึงที่ถูกทำขึ้นที่ อุณหภูมิทดสอบที่ 400 องศา c หรือสูงว่า และแรงเครียดก่อนการระบุของโหลดสูงสุดจากการเริ่มต้นของการ ทดสอบแรงดึงเป็น40% หรือมากกว่าในแง่ของอัตราส่วนต่อการยืดตัวรวม จากการเริ่มต้นของการ ทดสอบความแรงดึงถึงรอยแตกที่ได้มาในการทดสอบแรงดึง ที่ถูกทำขึ้นที่อุณหภูมิทดสอบที่ตํ่ากว่า 400 องศา c เนื้อสารแม่ (matrix), ซึ่งเป็นเฟสเดี่ยวเฟอร์ไรต์อย่างมาก ที่ซึ่งอัตราส่วนพื้นที่ของเฟสเฟอร์ไรต์ เป็น 95% หรือมากกว่า; และ โครงสร้างที่ซึ่งคาร์ไบด์อัลลอยด์ที่มีขนาดที่ตํ่ากว่า 10 ททา ถูกกระจายและถูกทำให้ตกตะกอน ในเนื้อสารแม่ในสภาพที่ไม่มีการเลือกที่แตกต่างถันไปในรูปแบบ (no variant selection)1. High-strength steel plates with a tensile strength of 590 MPa or more, and excellent warm stamping forming capabilities. High-strength steel plates are composed of: the following elements, in terms of percentage by mass: Carbon: 0.01 to 0.2%, Silicon: 0.5% or less, Manganese: 2% or less, Phosphorus: 0.03% or less, Sulfur: 0.01% or less, Aluminum: 0.07% or less, and Nitrogen: 0.01% or less. Additionally, one or two selected elements may be present: Titanium: 0.005 to 0.3% and Niopium: 0.005 to 0.6%; one or two or more selected elements: Vanadium: 0.005 to 1.0%, Molybdenum: 0.005 to 0.5%, Tungsten: 0.01 to 1.0%, and Boron: 0.0005%. Up to 0.0040%, with the remainder being iron and unavoidable impurities. Tensile properties where the specified stress at the point of crack is greater than the pre-specified stress at the start of the tensile test obtained in tensile tests performed at a test temperature of 400°C or higher, and the pre-specified stress at the start of the tensile test is 40% or more in terms of the ratio of total elongation from the start of the tensile test to crack obtained in tensile tests performed at a test temperature below 400°C. The matrix, which is predominantly ferrite single-phase where the ferrite phase area ratio is 95% or greater; and structures where carbide alloys with a size of less than 10 are distributed and precipitated in the matrix under a no variant selection condition. 2. แผ่นเหล็กกล้าความแข็งแรงสูงตามข้อถือสิทธิข้อ 1, ที่ซึ่งแผ่นเหล็กกล้าความแข็งแรงสูงมี ชั้นฉาบผิวบนผิวหน้า หน้า 2 ของจำนวน 2 หน้า2. High-strength steel plate pursuant to claim 1, where the high-strength steel plate has a coating layer on face 2 of 2 faces. 3. แผ่นเหล็กกล้าความแข็งแรงสูงตามข้อถือสิทธิข้อ 2, ที่ซึ่งชั้นฉาบผิวเป็ชั้นกัลวาไนซ์หรือชั้น อบเหนียวชุบสังกะสี (galvannealed layer)3. High-strength steel plates as per claim 2, where the coating is a galvanized or galvannealed layer. 4. วิธีการสำหรับผลิตแผ่นเหล็กกล้าความแข็งแรงสูงซึ่งมีกำลังดึงที่ 590 MPa หรือมากกว่า, มีเนื้อสารแม่และโครงสร้างตามข้อถือสิทธิข้อ 1, และดีเยี่ยมในความสามารถในการขึ้นรูปปั๊มอุ่น, วิธีการประกอบด้วย: ทำต่อเนื่องกันไปขบวนการรีดร้อนที่ประกอบด้วย การเผาเหล็กกล้าที่มีองค์ประกอบที่มี, ในแง่ของ % โดยมวล, คาร์บอน : 0.01 ถึง 0.2% , ซิลิคอน : 0.5% หรือตํ่ากว่า, แมงกานีส : 2% หรือ ตํ่ากว่า, ฟอสฟอรัส : 0.03% หรือตํ่ากว่า, กำมะถัน: 0.01% หรอตํ่ากว่า, อัลลูมินัม : 0.07% หรือตํ่ากว่า, และ ไนโตรเจน : 0.01% หรือตํ่ากว่า และยังมีหนึ่งหรือสองธาตุที่เลือกจาก ไททาเนียม : 0.005 ถึง 0.3% และ นิโอเปียม : 0.005 ถึง 0.6%, หนึ่งหรือสองธาตุหรือมากกว่า ที่เลือกจากวานาเดียม : 0.005 ถึง1.0%, โมลิบดีนัม 0.005 ถึง 0.5%, ทังสเตน : 0.01 ถึง 1.0%, และโบรอน : 0.0005 ถึง 0.0040% และ ที่เหลือเป็นเหล็กและสิ่งเจือปนที่ไม่อาจหลีกเลี่ยงได้ ถึงช่วงอุณหภูมิเฟสเดี่ยวออสเตนไนต์, การนำแผ่น เหล็กกล้าไบรีดร้อนที่อุณหภูมิขั้นสำเร็จที่ 860?c หรือสูงกว่า, และจากนั้น ขดแผ่นเหล็กกล้าที่อุณหภูมิที่ 400 องศา c หรือสูงกว่า และตํ่ากว่า 600 องศา c เพื่อสร้างแผ่นรีดร้อน; และ ขบวนการปฏิบัติการความร้อนที่ประกอบด้วย การเอาสะเก็ดผิวหน้าของแผ่นรีดร้อนออก, และ การนำแผ่นรีดร้อนไปสู่การปฏิบัติการความร้อนในช่วงอุณหภูมิที่ 650 ถึง 750?c4. Method for producing high-strength steel plates with a tensile strength of 590 MPa or more, with a matrix and structure conforming to Patent 1, and excellent warm-stamping formability, the method consists of: a continuous hot rolling process consisting of sintering the steel with the following composition, in terms of % by mass: Carbon: 0.01 to 0.2%, Silicon: 0.5% or less, Manganese: 2% or less, Phosphorus: 0.03% or less, Sulfur: 0.01% or less, Aluminum: 0.07% or less, and Nitrogen: 0.01% or less, and one or two selected elements from Titanium: 0.005 to 0.3% and Niopium: 0.005 to 0.6%, one or two or more elements. The composition of the steel is selected from vanadium: 0.005 to 1.0%, molybdenum: 0.005 to 0.5%, tungsten: 0.01 to 1.0%, and boron: 0.0005 to 0.0040%, with the remainder being iron and unavoidable impurities. The process involves a single-phase austenite phase, hot-rolling the steel sheet to a finishing temperature of 860°C or higher, and then coiling the steel sheet at temperatures of 400°C or higher and below 600°C to form hot-rolled plates; and a heat treatment process consisting of removing the surface slag from the hot-rolled plate, and subjecting the hot-rolled plate to a heat treatment temperature range of 650 to 750°C. 5. วิธีการสำหรับผลิตแผ่นเหล็กกล้าความแข็งแรงสูงตามข้อถือสิทธิข้อ 4, ยังประกอบด้วยการ ทำการปฏิบัติการฉาบผิวกับแผ่นรีดร้อน ที่ถูกนำไปสู่ขบวนการปฏิบัติการความร้อน5. The method for producing high-strength steel plates under claim 4 also includes surface treatment of hot-rolled sheets that have been subjected to heat treatment processes. 6. วิธีการผลิตแผ่นเหล็กกล้าความแข็งแรงสูงตามข้อถือสิทธิข้อ 4, ที่ประกอบด้วยการทำการ ปฏิบัติการกัลวาไนซ์หรือการทำการปฏิบัติการอบอ่อนซุบสังกะสี (galvannealing treatment) ต่อไป ที่ต่อจากขบวนการปฏิบัติการความร้อน6. The method of manufacturing high-strength steel plates according to claim 4, which includes a galvanizing or zinc-coating treatment following the heat treatment process.
TH601006181A 2011-04-08 High-strength steel plates with excellent formability, thermal grinding capabilities, and methods for manufacturing them. TH90133B (en)