TH8343B - "Welding repair methods and composite welding equipment for metal parts" - Google Patents
"Welding repair methods and composite welding equipment for metal parts"Info
- Publication number
- TH8343B TH8343B TH9501002242A TH9501002242A TH8343B TH 8343 B TH8343 B TH 8343B TH 9501002242 A TH9501002242 A TH 9501002242A TH 9501002242 A TH9501002242 A TH 9501002242A TH 8343 B TH8343 B TH 8343B
- Authority
- TH
- Thailand
- Prior art keywords
- welding
- electrode
- mixed
- metal
- arc
- Prior art date
Abstract
ส่วนที่เป็นโลหะ เช่น แม่พิมพ์โลหะ เป็นต้น สามารถที่จะถูกซ่อมอย่างมั่นคงโดยเครื่องเชื่อม และเครื่องหลอมเหลวด้วยไฟอาร์ค ปริมาณที่เหมาะสมของผงเชื่อมที่ละเอียดหรือวัสดุเชื่อมชนิดแผ่น บางถูกจัดไว้บนส่วนของส่วนที่เป็นโลหะที่จะถูกซ่อม ขั้วไฟฟ้าอันดับแรกของเครื่องเชื่อมจะถูกกด เข้ากับส่วนของผงเชื่อมหรือวัสดุเชื่อม กระแสพัลส์สูง 300-1500 แอมแปร์ จะถูกจ่ายไปยังขั้วไฟฟ้า อันดับแรกนั้นเป็นเวลาสั้นๆ 1/1000-4/1000 วินาที เพื่อทำเป็นวัสดุที่ถูกเชื่อมที่มีรูปร่างเป็นจุดจะหลอม เหลวบนส่วนที่เป็นโลหะ ที่ซึ่งส่วนที่หลอมเหลวจะถูกทำขึ้นเพื่อต่อหรือกันอย่างเนื่องกับโลหะ ที่ถูกเชื่อมจำนวนมากจะหลอมเหลว ดังนั้น การเชื่อมผสมด้วยส่วนที่หลอมเหลว แนวของส่วนที่หลอม เหลวหรือชั้นของส่วนที่หลอมเหลวจะถูกสร้างขึ้นและส่วนที่ถูกเชื่อมจะมีความหนาที่ต้องการในบริเวณ ที่ต้องการของส่วนที่จะถูกซ่อม ส่วนที่ถูกเชื่อมผสมของส่วนที่เป็นโลหะที่จะถูกซ่อมนี้จะถูกห่อหุ้มใน บรรยากาศแก๊สที่ไม่ไวต่อปฏิกิริยา ขั้วไฟฟ้าอันดับแรกของเครื่องหลอมเหลวด้วยไฟอาร์ค จะถูกวาง ตำแหน่งที่ที่อยู่ติดกับส่วนที่ถูกเชื่อมผสมและเครื่องหลอมเหลวด้วยไฟอาร์คนี้จะจ่ายไฟอาร์คไปยังล่วน ที่ผสมเป็นเวลาสั้นๆเพือที่จะหลอมเหลวโลหะที่ถูกเชื่อมอีกครั้งหนึ่ง ส่วนที่ถูกเชื่อมผสมที่มากเกินไป จะถูกเอาออกภายหลังจากที่ส่วนที่ถูกเชื่อมผสมแข็งตัวและการซ่อมจะถูกทำให้สิ้นสุดโดยการขัดมัน Metal parts such as metal molds, etc. can be fixed firmly by the welding machine. And the arc melting device The right amount of fine welding powder or plate type welding material. Some are arranged on the metal part to be repaired. The first electrode of the welding machine is pressed. To the part of the welding powder or welding material A high pulse current of 300-1500 amperes is supplied to the electrode. First of all, it is a short time. 1 / 1000-4 / 1000 s to form a point-shaped welded material will melt. Liquid on metal parts Where the molten part is made in order to connect or continue with the metal Many of the welds are molten, so the molten weld mixes with the Orientation of the melted part A liquid or layer of the molten part is created and the welded part has the required thickness in the area. Required of the part to be repaired The mixed part of the metal to be repaired is encased in Inert gas atmosphere The first electrode of the arc melting machine is positioned adjacent to the mixed welding part, and the arc melting machine supplies the arc power. It is mixed for a short time to melt the welded metal again. The part being welded too much It is removed after the weld is solidified and the repair is finished by polishing.
Claims (5)