TH469C3 - Compressed fuel coated with solid alcohol - Google Patents
Compressed fuel coated with solid alcoholInfo
- Publication number
- TH469C3 TH469C3 TH103000100U TH0103000100U TH469C3 TH 469 C3 TH469 C3 TH 469C3 TH 103000100 U TH103000100 U TH 103000100U TH 0103000100 U TH0103000100 U TH 0103000100U TH 469 C3 TH469 C3 TH 469C3
- Authority
- TH
- Thailand
- Prior art keywords
- shell
- coated
- solid
- palm
- solid alcohol
- Prior art date
Abstract
เชื้อเพลิงอัดที่เคลือบด้วยแอลกอฮอล์แข็ง ที่ประกอบด้วย ก. สารสผมที่ประกอบด้วย ถ่านไม้ กะลามะพร้าว และ /หรือ กะลาปาล์ม : ตัวประสาน ในสัดส่วน โดยน้ำหนัก 30 : 70 : 1 ถึง 40 : 60 : 5 ข. ผิวเคลือบที่เป็นแอลกอฮอล์ แข็ง ที่ได้จากกรรมวิธี ที่มีขั้นตอนต่อไปนี้ ก. บดถ่านไม้ กะละมะพร้าว และ/หรือ กะลาปาล์ม อย่างแยกกัน และร่อนแต่ละ ชนิด อย่างแยกกันดัวยตะแกรงร่อน ขนาด ไม่สูงกว่า 4 แมช ข. ผสมผงที่ร่อนแล้วจากข้อ ก. กับตัวประสาน ในสัดส่วนโดยน้ำหนัก ถ่านไม้ : กะลามะพร้าว และ/หรือ กะลาปาล์ม : ตัวประสาน = 30 : 70 : 1 ถึง 40 : 60 . 5 ค. อัดสารผสมที่ได้จากข้อ ข. ให้เป็นก้อนโดยให้มีความหนาแน่น 700-1,200 กก./ลบ.ม. ง. อบเชื้อเพลิงอัดก้อนที่ได้ในข้อ ค. ให้แห้ง จ. เคลือบเชื้อเพลิงอัดก้อนที่แข็งแล้วโดยการนำเชื้อเพลิงอัดก้อนที่แห้งแล้วจากข้อ ง. มาจุ่มหรือ ชุบ หรือ เคลือบ หรือ อัด แบบใดแบบหนึ่ง หรือ สองแบบร่วมกัน ด้วยแอลกอฮอล์แป้งที่มีส่วนผสมตามมาตรฐานผลิตภัณฑ์อุตสาหกรรม มอก. 950 - 2533 เป็นเวลา 1 - 10 นาที ก็จะได้ผลิตภัณฑ์สุดท้ายตามต้องการ: Compressed fuel coated with solid alcohol Containing: A. Hairs consisting of charcoal, coconut shells and / or palm shells: binders in the proportions of 30: 70: 1 to 40: 60: 5 b. Solid alcohol coatings obtained from the process. The steps are as follows: a. Grind the wood charcoal, coconut shell and / or palm shell separately and sift each type separately with a sieve of no higher than 4 matches. B. Mix the sifted powder from Section A with binder in proportion by weight of wood charcoal: coconut shell and / or palm shell: binder = 30: 70: 1 to 40: 60.5 c. Mix the mixture obtained from item B into cubes by To have a density of 700-1,200 kg / m3, dry the briquette fuel obtained in Item C. E. Coat the solid briquette fuel by bringing the dry briquette fuel from the Article C. Dip or plated or coated or pressed in one or two combinations together. With starch alcohol containing TIS 950 - 2533 industrial standard for 1 - 10 minutes, the final product will be obtained as needed:
Claims (2)