TH14743C3 - Production process of ready-mixed concrete, reinforced concrete, prestressed concrete - Google Patents

Production process of ready-mixed concrete, reinforced concrete, prestressed concrete

Info

Publication number
TH14743C3
TH14743C3 TH1603001343U TH1603001343U TH14743C3 TH 14743 C3 TH14743 C3 TH 14743C3 TH 1603001343 U TH1603001343 U TH 1603001343U TH 1603001343 U TH1603001343 U TH 1603001343U TH 14743 C3 TH14743 C3 TH 14743C3
Authority
TH
Thailand
Prior art keywords
concrete
cement
sand
mixer
per cubic
Prior art date
Application number
TH1603001343U
Other languages
Thai (th)
Other versions
TH14743A3 (en
Inventor
มากุล นายณัฏฐ์
Filing date
Publication date
Application filed filed Critical
Publication of TH14743A3 publication Critical patent/TH14743A3/en
Publication of TH14743C3 publication Critical patent/TH14743C3/en

Abstract

------29/01/2561------(OCR) หน้า 1 ของจำนวน 1 หน้า บทสรุปการประดิษฐ์ กรรมวิธีการผลิตคอนกรีตผสมเสร็จสำหรับงานคอนกรีตเสริมลวดอัดแรงมีวัตถุประสงค์เพื่อนำวัตถุดิบ ของการผลิตคอนกรีตงานคอนกรีตเสริมลวดอัดแรงมาทำการผสมตามขั้นตอนเฉพาะโดยเครื่องผสมที่มี สมรรถนะเฉพาะ โดยเริ่มจากการเตรียมเครื่องผสมคอนกรีตที่ภายในมีความสะอาด ชั่งหินขนาดโตสุด 19.0 มิลลิเมตร และปูนซีเมนต์ใส่ลงในเครื่องผสมคอนกรีต จากนั้นจึงเปิดเครื่องเพื่อผสมให้หินและทรายและ ปูนซีเมนต์คลุกเคล้าเป็นเนื้อเดียวกันในเครื่องผสม เมื่อส่วนผสมคลุกเคล้าเข้ากันดีแล้ว จึงเติมนํ้าที่ใช้ผสม ทั้งหมด เมื่อน้ำที่เติมลงผสมเข้ากันดีแล้วกับทราย หิน และปูนซีเมนต์ จึงเริ่มเติมน้ำยาผสมคอนกรีตปริมาณ 2.30 ลิตรต่อลูกบาศก์เมตร พร้อมเปิดเครื่องผสมคอนกรีตเพื่อให้นํ้ายาที่เติมลงไปเข้ากันได้ดีกับส่วนผสมของ คอนกรีตเป็นเวลา 1 นาที จึงเสร็จสิ้นกระบวนการผสม ------------ แก้ไข 2/6/60 กรรมวิธีการผลิตคอนกรีตผสมเสร็จสำหรับงานคอนกรีตเสริมลวดอัดแรงมีวัตถุประสงค์เพื่อเพื่อนำ วัตถุดิบของการผลิตคอนกรีตเสริมลวดอัดแรงมาทำการผสมตามขั้นตอนเฉพาะโดยเครื่องผสมที่มี สมรรถนะเฉพาะ โดยเริ่มจากการเตรียมเครื่องผสมคอนกรีตที่ภายในมีความสะอาด ชั่งหินขนาดโตสุด 19.0 มิลลิเมตร และปูนซีเมนต์ใส่ลงในเครื่องผสมคอนกรีต จากนั้นจึงเปิดเครื่องเพื่อผสมให้หินและทรายและ ปูนซีเมนต์คลุกเคล้าเป็นเนื้อเดียวกันในเครื่องผสม เมื่อส่วนผสมคลุกเคล้าเข้ากันดีแล้ว จึงเติมน้ำที่ใช้ผสม ทั้งหมด เมื่อน้ำที่เติมลงผสมเข้ากันดีแล้วกับทราย หิน และปูนซีเมนต์ จึงเริ่มเติมน้ำยาผสมคอนกรีตปริมาณ 2.30 ลิตรต่อลูกบาศก์เมตร พร้อมเปิดเครื่องผสมคอนกรีตเพื่อให้น้ำยาที่เติมลงไปเข้ากันได้ดีกับส่วนผสมของ คอนกรีตเป็นเวลา 1 นาที จึงเสร็จสิ้นกระบวนการผสม ....................................................................................................................................................... กรรมวิธีการผลิตคอนกรีตผสมเสร็จสำหรับงานคอนกรีตเสริมลวดอัดแรงมีวัตถุประสงค์เพื่อเพื่อนำ วัตถุดิบของการผลิตงานคอนกรีตงานคอนกรีตเสริมลวดอัดแรงมาทำการผสมตามขั้นตอนเฉพาะโดยเครื่องผสมที่มี สมรรถนะเฉพาะ โดยเริ่มจากการเตรียมเครื่องผสมคอนกรีตที่ภายในมีความสะอาด ชั่งหินขนาดโตสุด 19.0 มิลลิเมตร และปูนซีเมนต์ใส่ลงในเครื่องผสมคอนกรีต จากนั้นจึงเปิดเครื่องเพื่อผสมให้หินและทรายและ ปูนซีเมนต์คลุกเคล้าเป็นเนื้อเดียวกันในเครื่องผสม เมื่อส่วนผสมคลุกเคล้าเข้ากันดีแล้ว จึงเติมน้ำที่ใช้ผสม ทั้งหมด เมื่อน้ำที่เติมลงผสมเข้ากันดีแล้วกับทราย หิน และปูนซีเมนต์ จึงเริ่มเติมน้ำยาผสมคอนกรีตปริมาณ 2.30 ลิตรต่อลูกบาศก์เมตร พร้อมเปิดเครื่องผสมคอนกรีตเพื่อให้น้ำยาที่เติมลงไปเข้ากันได้ดีกับส่วนผสมของ คอนกรีตเป็นเวลา 1 นาที จึงเสร็จสิ้นการบวนการผสม ------ 29/01/2018 ------ (OCR) page 1 of number 1 page invention summary. Production process of ready-mixed concrete for prestressed concrete reinforcement is intended to bring raw materials. Of concrete production, reinforced concrete works, prestressed concrete, to be mixed according to a specific process by a mixer with specific performance starting from the preparation of a concrete mixer with a clean interior The maximum size of stone is 19.0 mm and the cement is placed in the concrete mixer. Then turn on the machine to mix the rocks and sand and Homogeneous mix of cement in a mixer. When the ingredients are well mixed together. Then add all the water used to mix when the added water is mixed well with sand, stone and cement. Therefore began to add a concrete admixture of 2.30 liters per cubic meter Ready to turn on the concrete mixer so that the added solution mixes well with the mixture Concrete for 1 minute to complete the mixing process. ------------ Correction 2/6/60 Precast concrete production process for prestressed concrete. The raw materials for the production of prestressed concrete are mixed according to a specific process by a specific performance mixer starting from the preparation of a concrete mixer with a clean interior. The maximum size of stone is 19.0 mm and the cement is placed in the concrete mixer. Then turn on the machine to mix the rocks and sand and Homogeneous mix of cement in a mixer. When the ingredients are well mixed together. Then add all the water used to mix when the added water is mixed well with sand, stone and cement. Therefore began to add a concrete admixture of 2.30 liters per cubic meter Ready to turn on the concrete mixer so that the added solution is compatible with the mixture Concrete for 1 minute to complete the mixing process. .................................................. .................................................. .................................................. . The production process of ready-mixed concrete for prestressed concrete is intended to bring Raw materials of concrete production, reinforced concrete, prestressed concrete, are mixed according to specific steps by special performance mixers starting from the preparation of concrete mixers that are clean inside. The maximum size of stone is 19.0 mm and the cement is placed in the concrete mixer. Then turn on the machine to mix the rocks and sand and Homogeneous mix of cement in a mixer. When the ingredients are well mixed together. Then add all the water used to mix when the added water is mixed well with sand, stone and cement. Therefore began to add a concrete admixture of 2.30 liters per cubic meter Ready to turn on the concrete mixer so that the added solution is compatible with the mixture Concrete for 1 minute, then the mixing process is complete.

Claims (3)

ข้อถือสิทธฺ์ (ทั้งหมด) ซึ่งจะไม่ปรากฏบนหน้าประกาศโฆษณา :------29/01/2561------(OCR) หน้า 1 ของจำนวน 1 หน้า ข้อถือสิทธิ 1. กรรมวิธีการผลิตคอนกรีตผสมเสร็จชนิดงานคอนกรีตเสริมลวดอัดแรงมีขั้นตอนดังนี้ ก. เตรียมเครื่องผสมคอนกรีตที่ภายในมีความสะอาดและที่ผิวภายในมีความชุ่มน้ำ (ไม่แห้งสนิท) และ มวลรวม (หินและทราย) ที่มีความชื้นอยู่ในสภาวะอิ่มตัวด้วยนํ้าและผิวแห้ง (saturated surface dry) ข. ชั่งหินขนาดโตสุด 19.0 มิลลิเมตร ปริมาณเท่ากับ 1065 กิโลกรัมต่อลูกบาศก์เมตร และปูนซีเมนต์ 450 กิโลกรัมต่อลูกบาศก์เมตร ใส่ลงในเครื่องผสมคอนกรีต จากนั้นจึงเปิดเครื่องด้วยความเร็วรอบ 20 รอบ ต่อนาที เพื่อผสมให้หินและทรายและปูนซีเมนต์คลุกเคล้าเป็นเนื้อเดียวกันในเครื่องผสม เป็นเวลา 1 นาที ค. เมื่อปูนซีเมนต์ ทรายและหิน คลุกเคล้าเข้ากันดีแล้ว จึงเติมน้ำทั้งหมด ทั้งนี้ระหว่างเติมน้ำให้เปิดเครื่อง ผสมคอนกรีตเพื่อให้นํ้าที่เติมลงไปเข้ากันได้ดีกับส่วนผสมของทรายและปูนซีเมนต์เป็นเวลา 25 วินาที ง. เมื่อน้ำที่เติมลงผสมเข้ากันดีแล้วกับทราย หิน และปูนซีเมนต์ จึงเริ่มเติมนํ้ายาผสมคอนกรีต ปริมาณ 2.30 ลิตรต่อลูกบาศก์เมตร พร้อมเป็ดเครื่องผสมคอนกรีตเพื่อให้นํ้ายาที่เติมลงไปเข้ากันได้ดีกับส่วนผสม ของคอนกรีตเป็นเวลา 1 นาที จึงเสร็จสิ้นกระบวนการผสม 2. กรรมวิธีการผลิตคอนกรีตผสมเสร็จชนิดงานคอนกรีตเสริมลวดอัดแรงตามข้อถือสิทธิที่ 1 ที่ซึ่งปูนซีเมนต์ ปอร์ตแลนด์ประเภทที่ 1 มีปริมาณองค์ประกอบเคมีโดยน้ำหนัก ประกอบไปด้วย อะลูมิเนียมออกไซด์ (Al2O3) ร้อยละ 4.35 ซิลิคอนไดออกไซด์ (SiO2) ร้อยละ 20.10 โพแทสเซียมออกไซด์ (K2O) ร้อยละ 0.63 แคลเซียมออกไซด์ (CaO) ร้อยละ 62.32 ไทเทเนียมไดออกไซด์ (TiO2) ร้อยละ 0.23 เหล็กออกไซด์ (Fe2O3) ร้อยละ 3.24 และมีค่าร้อยละการสูญเสียน้ำหนักเนื่องจากการเผาไหม้ร้อยละ 1.71 ในขณะที่มี สมบัติทางกายภาพอันประกอบไปด้วย ขนาดเฉลี่ยเท่ากับ 623.8 ไมโครเมตร พื้นที่ผิวจำเพาะเท่ากับ 472 ตารางเมตรต่อกิโลกรัม ความถ่วงจำเพาะเท่ากับ 3.10 และปริมาณความชื้นร้อยละ 0.12 3. คอนกรีตผสมเสร็จชนิดงานคอนกรีตเสริมลวดอัดแรงตามข้อถือสิทธิที่ 1 หรือ 2 ที่ซึ่งสูตรมีดังต่อไปนี้ ปริมาณปูนซีเมนต์เท่ากับ 450 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณน้ำผสมคอนกรีตเท่ากับ 165 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณทรายเท่ากับ 835 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณหิน เท่ากับ 1065 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณน้ำยาผสมคอนกรีตเท่ากับ 2.30 ลิตรต่อลูกบาศก์เมตร ------------ แก้ไข 2 มิ.ย. 2560 1. กรรมวิธีการผลิตคอนกรีตผสมเสร็จชนิดงานคอนกรีตเสริมลวดอัดแรงมีขั้นตอนดังนี้ ก. เตรียมเครื่องผสมคอนกรีตที่ภายในมีความสะอาดและที่ผิวภายในมีความชุ่มน้ำ (ไม่แห้งสนิท) และ มวลรวม (หินและทราย) ที่มีความชื้นอยู่ในสภาวะอิ่มตัวด้วยน้ำและผิวแห้ง (saturated surface dry) ข. ชั่งหินขนาดโตสุด 19.0 มิลลิเมตร ปริมาณเท่ากับ 165 กิโลกรัมต่อลูกบาศก์เมตร และปูนซีเมนต์ 450 กิโลกรัมต่อลูกบาศก์เมตร ใส่ลงในเครื่องผสมคอนกรีต จากนั้นจึงเปิดเครื่องด้วยความเร็วรอบ 20 รอบ ต่อนาที เพื่อผสมให้หินและทรายและปูนซีเมนต์คลุกเคล้าเป็นเนื้อเดียวกันในเครื่องผสม เป็นเวลา 1 นาที ค. เมื่อปูนซีเมนต์ ทรายและหิน คลุกเคล้าเข้ากันดีแล้ว จึงเติมน้ำทั้งหมด ทั้งนี้ระหว่างเติมน้ำให้เปิดเครื่อง ผสมคอนกรีตเพื่อให้น้ำที่เติมลงไปเข้ากันได้ดีกับส่วนผสมของทรายและปูนซีเมนต์เป็นเวลา 25 วินาที ง. เมื่อน้ำที่เติมลงผสมเข้ากันดีแล้วกับทราย หิน และปูนซีเมนต์ จึงเริ่มเติมน้ำยาผสมคอนกรีต ปริมาณ 2.30 ลิตรต่อลูกบาศก์เมตร พร้อมเปิดเครื่องผสมคอนกรีตเพื่อให้น้ำยาที่เติมลงไปเข้ากันได้ดีกับส่วนผสม ของคอนกรีตเป็นเวลา 1 นาที จึงเสร็จสิ้นกระบวนการผสม 2. กรรมวิธีการผลิตคอนกรีตผสมเสร็จชนิดงานคอนกรีตเสริมลวดอัดแรงมีตามข้อถือสิทธิที่ 1 ที่ซึ่งปูซีเมนต์ ปอร์ตแลนด์ประเภทที่ 1 มีปริมาณองค์ประกอบเคมีโดยน้ำหนัก ประกอบไปด้วย อะลูมิเนียมออกไซด์ (Al2O3) ร้อยละ 4.35 ซิลิคอนไดออกไซด์ (SiO2) ร้อยละ 20.10 โพแทสเซียมออกไซด์ (K2O) ร้อยละ 0.63 แคลเซียมออกไซด์ (CaO) ร้อยละ 62.32 ไทเทเนียมไดออกไซด์ (TiO2) ร้อยละ 0.23 เหล็กออกไซด์ (Fe2O3) ร้อยละ 3.24 และมีค่าร้อยละการสูญเสียน้ำหนักเนื่องจากการเผาไหม้ร้อยละ 1.71 ในขณะที่มี สมบัติทางกายภาพอันประกอบไปด้วย ขนาดเฉลี่ยเท่ากับ 623.8 ไมโครเมตร พื้นที่ผิวจำเพาะเท่ากับ 472 ตารางเมตรต่อกิโลกรัม ความถ่วงจำเพาะเท่ากับ 3.10 และปริมาณความชื้นร้อยละ 0.12 3. สูตรสัดส่วนผสมคอนกรีตชนิดงานคอนกรีตเสริมลวดอัดแรงตามข้อถือสิทธิที่ 1 หรือ 2 ที่ซึ่งสูตรมีดังต่อไปนี้ ปริมาณปูนซีเมนต์เท่ากับ 450 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณน้ำผสมคอนกรีตเท่ากับ 165 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณทรายเท่ากับ 835 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณหิน เท่ากับ 1065 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณน้ำยาผสมคอนกรีตเท่ากับ 2.30 ลิตรต่อลูกบาศก์เมตร .......................................................................................................................................................Disclaimer (all) which will not appear on the advertisement page. : ------ 29/01/2018 ------ (OCR) Page 1 of 1 page Claims 1. Production process of ready-mixed concrete, reinforced concrete, prestressed concrete, has the following steps: Prepare a concrete mixer with a clean interior and a wet interior. (Not completely dry) and aggregates (rock and sand) with moisture in the state saturated with water and dry (saturated surface dry). B. Weigh rock size 19.0 mm. And 450 kg of cement per cubic meter Put into the concrete mixer Then turn on the machine at a speed of 20 rpm to mix the stone and sand and cement homogeneous in the mixer for 1 minute. C. When the cement, sand and stone are mixed well. Therefore add all the water However, while adding water, turn on the machine. Mix the concrete so that the added water mixes well with the sand and cement mixture for 25 seconds. D. When the added water is mixed well with the sand, stone and cement. Therefore began to add a concrete admixture of 2.30 liters per cubic meter Ready to mix concrete mixer to make the added solution mix well with the mixture. Of concrete for 1 minute, then the mixing process is completed. 2. Production process of ready-mixed concrete, reinforced concrete, prestressed concrete according to claim 1, where the cement Portland Type 1 contains the chemical composition by weight, consisting of 4.35% aluminum oxide (Al2O3), 20.10% silicon dioxide (SiO2), 0.63% potassium oxide (K2O), calcium oxide (CaO), 62.32% titanium dioxide. (TiO2) 0.23% iron oxide (Fe2O3) 3.24% and the percentage of weight loss due to combustion of 1.71%, while the physical properties including The average size was 623.8 micrometers, the specific surface area was 472 square meters per kilogram. Specific gravity is 3.10 and moisture content of 0.12% 3. Ready-mixed concrete, reinforced concrete, prestressed concrete according to claim 1 or 2, where the formula is as follows: The amount of cement is 450 kilograms per cubic meter. The amount of water mixed with concrete is 165 kilograms per cubic meter. The amount of sand is 835 kilograms per cubic meter, the rock volume is 1065 kilograms per cubic meter. The volume of concrete admixture is 2.30 liters per cubic meter. ------------ Revised 2 June 2017 1. Production process of ready-mixed concrete, prestressed concrete, the steps are as follows: a. Concrete mixer inside is clean and inside surface is wet. (Not completely dry) and aggregate (rock and sand) with moisture in the state of saturated water and dry surface (saturated surface dry). B. Weighing rock size 19.0 mm, volume equal to 165 kg / m3 And 450 kg of cement per cubic meter Put into the concrete mixer Then turn on the machine at a speed of 20 rpm to mix the stone and sand and cement homogeneous in the mixer for 1 minute. C. When the cement, sand and stone are mixed well. Therefore add all the water However, while adding water, turn on the machine. Mix the concrete so that the added water mixes well with the sand and cement mixture for 25 seconds. D. When the added water is mixed well with the sand, stone and cement. Therefore began to add a concrete admixture of 2.30 liters per cubic meter Ready to turn on the concrete mixer to make the added solution mix well with the mixture Of concrete for 1 minute, then the mixing process is completed. 2. The production process of ready-mixed concrete, reinforced concrete, prestressed concrete, is subject to claim 1 where the cement is laid. Portland Type 1 contains the chemical composition by weight, consisting of 4.35% aluminum oxide (Al2O3), 20.10% silicon dioxide (SiO2), 0.63% potassium oxide (K2O), calcium oxide (CaO), 62.32% titanium dioxide. (TiO2) 0.23% iron oxide (Fe2O3) 3.24% and the percentage of weight loss due to combustion of 1.71%, while the physical properties including The average size was 623.8 micrometers, the specific surface area was 472 square meters per kilogram. The specific gravity is 3.10 and the moisture content of 0.12% 3. The formula for the proportion of concrete mix, reinforced concrete, prestressed concrete, according to claim 1 or 2, where the formula is as follows The amount of cement is 450 kilograms per cubic meter. The amount of water mixed with concrete is 165 kilograms per cubic meter. The amount of sand is 835 kilograms per cubic meter, the rock volume is 1065 kilograms per cubic meter. The volume of concrete admixture is 2.30 liters per cubic meter. .................................................. .................................................. .................................................. . 1. กรรมวิธีการผลิตคอนกรีตผสมเสร็จมีขั้นตอนดังนี้ ก. เตรียมเครื่องผสมคอนกรีตที่ภายในมีความสะอาดและที่ผิวภายในมีความชุ่มน้ำ (ไม่แห้งสนิท) และ มวลรวม (หินและทราย) ที่มีความชื้นอยู่ในสภาวะอิ่มตัวด้วยน้ำและผิวแห้ง (saturated surface dry) ข. ชั่งหินขนาดโตสุด 19.0 มิลลิเมตร ปริมาณเท่ากับ 1065 กิโลกรัมต่อลูกบาศก์เมตร และปูนซีเมนต์ 450 กิโลกรัมต่อลูกบาศก์เมตร ใส่ลงในเครื่องผสมคอนกรีต จากนั้นจึงเปิดเครื่องด้วยความเร็วรอบ 20 รอบ ต่อนาที เพื่อผสมให้หินและทรายและปูนซีเมนต์คลุกเคล้าเป็นเนื้อเดียวกันในเครื่องผสม เป็นเวลา 1 นาที ค. เมื่อปูนซีเมนต์ ทรายและหิน คลุกเคล้าเข้ากันดีแล้ว ให้ทำการชั่งเถ้าลอยในปริมาณ 165 กิโลกรัมต่อ ลูกบาศก์เมตร แล้วจึงเติมทั้งหมด ทั้งนี้ระหว่างเติมน้ำให้เปิดเครื่องผสมคอนกรีตเพื่อให้น้ำที่เติมลงไป เข้ากันได้ดีกับส่วนผสมของทรายและปูนซีเมนต์เป็นเวลา 25 วินาที ง. เมื่อน้ำที่เติมลงผสมเข้ากันดีแล้วกับทราย หิน และปูนซีเมนต์ จึงเริ่มเติมน้ำยาผสมคอนกรีต ปริมาณ 2.30 ลิตรต่อลูกบาศก์เมตร พร้อมเปิดเครื่องผสมคอนกรีตเพื่อให้น้ำยาที่เติมลงไปเข้ากันได้ดีกับส่วนผสม ของคอนกรีตเป็นเวลา 1 นาที จึงเสร็จสิ้นกระบวนการผสม1. The production process of ready-mixed concrete has the following steps: a. Prepare a concrete mixer that is clean inside and that the inside surface is wet. (Not completely dry) and aggregates (rock and sand) with moisture in the state of saturated water and dry surface (saturated surface dry). B. Weigh rock size 19.0 mm. And 450 kg of cement per cubic meter Put into the concrete mixer Then turn on the machine at a speed of 20 rpm to mix the stone and sand and cement homogeneous in the mixer for 1 minute. C. When the cement, sand and stone are mixed well. To weigh the fly ash in the amount of 165 kg per cubic meter and then add all. However, while adding water, turn on the concrete mixer to allow the added water. Goes well with sand and cement mixture for 25 s. D. When the added water is mixed well with sand, stone and cement. Therefore began to add a concrete admixture of 2.30 liters per cubic meter Ready to turn on the concrete mixer to make the added solution mix well with the mixture Of concrete for 1 minute to complete the mixing process. 2. กรรมวิธีการผลิตคอนกรีตผสมเสร็จตามข้อถือสิทธิที่ 1 ที่ซึ่งปูซีเมนต์ปอร์ตแลนด์ประเภทที่ 1 มีปริมาณ องค์ประกอบเคมีโดยน้ำหนัก ประกอบไปด้วย อะลุมิเนียมออกไซด์ (Al2O3) ร้อยละ 4.35 ซิลิคอนได ออกไซด์ (SiO2) ร้อยละ 20.10 โพแทสเซียมออกไซด์ (K2O) ร้อยละ 0.63 แคลเซียมออกไซด์ (CaO) ร้อยละ 62.32 ไทเทเนียมไดออกไซด์ (TiO2) ร้อยละ 0.23 เหล็กออกไซด์ (Fe2O3) ร้อยละ 3.24 และมีค่า ร้อยละการสูญเสียน้ำหนักเนื่องจากการเผาไหม้ร้อยละ 1.71 ในขณะที่มีสมบัติทางกายภาพอันประกอบไป ด้วย ขนาดเฉลี่ยเท่ากับ 623.8 ไมโครเมตร พื้นที่ผิวจำเพาะเท่ากับ 472 ตารางเมตรต่อกิโลกรัม ความถ่วงจำเพาะเท่ากับ 3.10 และปริมารความชื้นร้อยละ 0.122. Production process for ready-mixed concrete according to claim 1, where type 1 Portland cement has chemical composition by weight, consisting of 4.35 percent Al2O3, silicon dioxide (SiO2) percent. 20.10, 0.63% potassium oxide (K2O), 0.63% calcium oxide (CaO), 62.32%, titanium dioxide (TiO2), 0.23%, iron oxide (Fe2O3) 3.24%, and the percentage of weight loss due to combustion 1.71%. On the other hand, its physical properties consist of a mean size of 623.8 μm, a specific surface area of 472 square meters per kilogram. Specific gravity is 3.10 and the moisture content of 0.12%. 3. สูตรสัดส่วนผสมคอนกรีตตามข้อถือสิทธิที่ 1 และ 2 มีดังต่อไปนี้ ปริมาณปูนซีเมนต์เท่ากับ 450 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณน้ำผสมคอนกรีตเท่ากับ 165 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณทรายเท่ากับ 835 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณหิน เท่ากับ 1065 กิโลกรัมต่อลูกบาศก์เมตร ปริมาณน้ำยาผสมคอนกรีตเท่ากับ 2.30 ลิตรต่อลูกบาศก์เมตร3. The concrete mix proportion formula according to claim 1 and 2 are as follows. The amount of cement is 450 kilograms per cubic meter. The amount of water mixed with concrete is 165 kilograms per cubic meter. The amount of sand is 835 kilograms per cubic meter, the rock volume is 1065 kilograms per cubic meter. The volume of concrete admixture is 2.30 liters per cubic meter.
TH1603001343U 2016-08-01 Production process of ready-mixed concrete, reinforced concrete, prestressed concrete TH14743C3 (en)