TH132081A - Low-cost, low-carbon, low-sulfur, and low-nitrogen steel is produced using conventional steelmaking equipment. - Google Patents
Low-cost, low-carbon, low-sulfur, and low-nitrogen steel is produced using conventional steelmaking equipment.Info
- Publication number
- TH132081A TH132081A TH1201006540A TH1201006540A TH132081A TH 132081 A TH132081 A TH 132081A TH 1201006540 A TH1201006540 A TH 1201006540A TH 1201006540 A TH1201006540 A TH 1201006540A TH 132081 A TH132081 A TH 132081A
- Authority
- TH
- Thailand
- Prior art keywords
- molten steel
- low
- vtd
- steel
- less
- Prior art date
Abstract
DC60(17/12/55) วิธีการผลิตเหล็กกล้าคาร์บอนต่ำน้อยกว่า0.035%โดยน้ำหนักที่รวมด้วยขั้นตอนของ การจัดเตรียมการให้ความร้อนองค์ประกอบเหล็กกล้าหลอมเหลวในเตาทำเหล็กกล้าจนถึงอุณหภูมิ ถ่ายเหล็กกล้าหลอมเหลวตามต้องการสำหรับการขจัดกำมะถันที่VTD,การถ่ายองค์ประกอบ เหล็กกล้าหลอมเหลวที่มีระดับออกซิเจนระหว่างประมาณ600และ1120ppmเข้าไปที่กะพ้อม,การ จัดให้มีสารประกอบสร้างขี้ตะกรันกับกะพ้อมเพื่อสร้างขี้ตะกรันคลุมทับเหนือองค์ประกอบเหล็กกล้า หลอมเหลวในกะพ้อม,การเคลื่อนย้ายเหล็กกล้าหลอมเหลวไปที่VTD,การขจัดคาร์บอนใน องค์ประกอบเหล็กกล้าหลอมเหลวที่VTDโดยการดูดอากาศออกจนมีสุญญากาศที่ระดับน้อยกว่า650 มิลลิบาร์และหลังการขจัดคาร์บอนแล้วมีการเคลื่อนย้ายเหล็กกล้าหลอมเหลวไปที่LMFและมีการดี ออกซิเดชันองค์ประกอบเหล็กกล้าหลอมเหลวและหลังดีออกซิเดชันจะส่งย้อนกลับไปที่VTDเพื่อ ขจัดกำมะถันและไล่ก๊าซในองค์ประกอบเหล็กกล้าหลอมเหลวและการหล่อขึ้นรูปองค์ประกอบ เหล็กกล้าหลอมเหลวเพื่อสร้างเป็นเหล็กกล้าคาร์บอนต่ำน้อยกว่า0.035%โดยน้ำหนัก DC60(17/12/55) Method for producing low carbon steel less than 0.035% by weight including the steps of Arrangement for heating molten steel elements in a steelmaking furnace to temperature Transfer molten steel as needed for desulfurization at VTD, element transfer. Molten steel with an oxygen level between approximately 600 and 1120ppm enters the sump, Provide a slag generating compound to the cassette to create a slag covering over the steel element. Melting in the vat, moving the molten steel to the VTD, removing carbon in Molten steel composition at VTD by exhausting air to a vacuum of less than 650 millibar and after decarbonization the molten steel is moved to LMF and is oxidation of the molten steel elements and after de-oxidation returns to the VTD to Desulfurizes and degasses molten steel elements and element castings. Molten steel to form low carbon steel of less than 0.035% by weight.
Claims (1)