SU907636A1 - Method of explosion-protection of kinescopes - Google Patents

Method of explosion-protection of kinescopes Download PDF

Info

Publication number
SU907636A1
SU907636A1 SU802988730A SU2988730A SU907636A1 SU 907636 A1 SU907636 A1 SU 907636A1 SU 802988730 A SU802988730 A SU 802988730A SU 2988730 A SU2988730 A SU 2988730A SU 907636 A1 SU907636 A1 SU 907636A1
Authority
SU
USSR - Soviet Union
Prior art keywords
rings
kinescope
critical zone
force
critical
Prior art date
Application number
SU802988730A
Other languages
Russian (ru)
Inventor
Эвальд Адамович Предикер
Валерий Кузьмич Тюпин
Original Assignee
Предприятие П/Я Г-4294
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Предприятие П/Я Г-4294 filed Critical Предприятие П/Я Г-4294
Priority to SU802988730A priority Critical patent/SU907636A1/en
Application granted granted Critical
Publication of SU907636A1 publication Critical patent/SU907636A1/en

Description

(5) способ ВЗРЫВОЗАИ ТЫ КИНЕСКОПОВ(5) EXPLOSION KINESCOPE method

II

Изобретение относитс  к производству кинескопов, в частности к слособам взрывозащиты кинескопов.The invention relates to the production of picture tubes, in particular to the explosion protection methods of picture tubes.

Известен способ взрывозащиты кинескопов обкаткой стальной лентой |1 J.The known method of explosion protection kinescopes run-in steel tape | 1 J.

Однако это опасно дл  целостности кинескопа.However, it is dangerous to the integrity of the kinescope.

Известен также способ взрывозащиты , заключающийс  в том, что на стык между колбой и экраном накладываетс  металлический бандаж, на концы которого прикладываетс  внешнее ст гивающее усилие дл  обжати  критической зоны кинескопа, затем на концы бандажа накладываетс  отрезок ленты, который привариваетс  к последним точечной сваркой 2.An explosion protection method is also known in that a metal band is applied to the joint between the flask and the screen, the ends of which are externally applied to compress the critical area of the kinescope, then a piece of tape is applied to the ends of the bandage, which is welded to the last spot welding 2.

Недостатком известного способа  вл етс  необходимость приложени  большого ст гивающего усили  до 9000 И на концы бандажа, а также необходимость производить сварку бандажа непосредственно на самом кинескопе.The disadvantage of this method is the necessity of applying a large shaking force up to 9000 on the ends of the band, as well as the need to weld the band directly on the tube itself.

Цель изобретени  - уменьшение прилагаемых внешних усилий дл  получени  необходимого обжати  критической зоны кинескопа.The purpose of the invention is to reduce the applied external efforts to obtain the necessary reduction of the critical zone of the kinescope.

Поставленна  цель достигаетс  тем, что согласно способу взрывозащиты кинескопов , включающему наложение металлического бандажа на критическую зону кинескопа, и обжатием критической зоны, в качестве бандажа исполь10 зуют два металлических кольца, отформованных по периметру критической зоны кинескопа, между которыми вставл ют распорки, внешнее усилие дл  обжати  критической зоны приклады15 вают к упом нутым кольцам в направлении , перпендикул рном их плоскости, в промежутках между распорками.The goal is achieved by the fact that, according to the method of explosion protection of kinescopes, including the imposition of a metal band on the critical zone of the kinescope, and the crimping of the critical zone, two metal rings formed around the perimeter of the critical zone of the kinescope, between which the spacers are inserted, are used as a bandage the compression of the critical zone is applied to the said rings in the direction perpendicular to their plane, in the intervals between the struts.

На чертеже изображен кинескоп с использованием предлагаемого способа The drawing shows a kinescope using the proposed method

20 взрывозащиты.20 explosion protection.

Claims (2)

Металлические кольца 1 надевают на критическую зону 2 кинескопа 3 с рассто нием между ними - В - 1 4 мм. Затем между кольцами 1 на боковых участках критической зоны 2 на рассто кии L 100 - 150 мм друг от. друга вставл ют распорки k. Посреди не между двум  соседними распорками к кольцам 1 прикладывают внешнее усилие F в направлении, перпендикул рном плоскости колец. На места пр ложени  внешнего усили  накладывают металлическую полоску 5 шириной 5 - 10 мм и толщиной 0,2 - 0,3 мм и закрепл ют, например, точечной сваркой б или другим известным способом . Крепежные уголки 7 вставл ют до нат жени  колец 1 между стеклом оболочки кинескопа 3 и кольцами, либо приваривают к кольцам до надевани  их на кинескрп. Рассто ние ме ду распорками k и их количество выбираетс , исход  из желаемой величи ны внешнего усили  F, необходимой величины силы обжати  критической зоны кинескопа и плотности первоначального прилегани  колец к критической зоне кинескопа. При этом небольшим внешним усилием ст гивани  F достигаетс  значительное усилие обжати  критической зоны кинескопа, равное ( - 20) F. Пример. На критическую зо ну оболочки кинескопа 61ЛКЗБ 1адева ют отформованные кольца из стальной проволоки диаметром 3 мм, концы которой сварены встык. Рассто ние меж кольцами 13 мм. На длинные стороны критической зоны кинескопа устанавливают по три распорки, на короткие по две. Рассто ние между соседними распорками 1QO мм. Максимальное вне нее усилие ст гивани  колец составл ет 600 И. При этом, в случае каса ни  колец при их ст гивании усилие обжати  критической зоны составл ет 10-0 ) 9230 И . Така  вели ( 2-600чина усили  обжати  критической зоны обеспечивает взрывобезопасность кинескопа. 4 Использование предлагаемого способа взрывозащиты позвол ет в 14 20 раз уменьшить величину прилагаемого внешнего усили , необходимого дл  обжати  критической зоны, без ухудшени  взрывобезопасности кинескопа и исключает необходимость сварки бандажа непосредственно на кинескопе . Предлагаемый способ взрывозащиты позвол ет значительно упростить станки дл  намотки бандажа, так как отпадает необходимость в специальном устройстве намотки бандажной ленУы с определенным усилием. При этом производительность труда повышаетс  в 1, - 1 ,8 раза, снижаетс  рйсход материала дл  бандажа. Ожидаемый экономический эффект от использовани  предлагаемого способа составл ет 300 - 400 тыс.руб. в год. Формула изобретени  Способ взрывозащиты кинескопов, включающий наложение металлического бандажа на критическую зону кинескопа , обжатие критической зонь, о т ли чающий с   тем, что, с целью уменьшени  прилагаемых внешних усилий дл  получени  необходимого обжати  критической зоны, в качестве бандажа используют два металлических кольца, отформованных по периметру критической зоны кинескопа, между которыми вставл ют распорки, внешнее усилие дл  обжати  критической зоны прикладывают к упом нутым кольцам в направлении, перпендикул рном к их плоскости, в промежутках между распорками. Источники информации, прин тые во внимание при экспертизе 1.Патент ГДР № 61577, кл. 21 g 13/28, 1967. The metal rings 1 are put on the critical zone 2 of the kinescope 3 with a distance between them - B - 1 4 mm. Then between the rings 1 on the side sections of the critical zone 2 for distances L 100 - 150 mm from each other. friend insert struts k. In the middle, not between two adjacent struts, an external force F is applied to the rings 1 in a direction perpendicular to the plane of the rings. A metal strip 5 5-10 mm wide and 0.2-0.3 mm thick is applied to the places of external force application and secured, for example, by spot welding with b or by another known method. The fixing angles 7 are inserted before tensioning the rings 1 between the glass tube of the kinescope 3 and the rings, or welded to the rings before putting them on the kineskrp. The distance between the struts k and their number is chosen based on the desired external force F, the required amount of force of compression of the critical zone of the kinescope and the density of the initial fit of the rings to the critical zone of the kinescope. In this case, with a small external shaking force F, a considerable force is achieved to compress the critical zone of the kinescope, equal to (- 20) F. Example. Molded rings of steel wire with a diameter of 3 mm, the ends of which are butt-welded, are deposited at the critical zone of the shell of the 61LKZB 1 kinescope. The distance between the rings is 13 mm. Three long spacers are installed on the long sides of the critical zone of the kinescope, for two short ones. The distance between adjacent spacers is 1QO mm. The maximum shrinking force of the rings outside of it is 600 I. At the same time, in the case of tangency of the rings during their tightening, the compressing force of the critical zone is 10-0) 9230 I. This was done (2-600 points of compression of the critical zone ensures the explosion safety of the kinescope. 4 Using the proposed method of explosion protection reduces the external force required to reduce the critical zone 14 to 20 times without reducing the explosion safety of the kinescope and eliminates the need to weld the band directly on the tube. The proposed method of explosion protection makes it possible to significantly simplify the machines for winding the bandage, since there is no need for a special winding device. with a certain effort. At the same time, labor productivity increases by 1, - 1, 8 times, the cost of the material for the bandage decreases. The expected economic effect from using the proposed method is 300-400 thousand rubles per year. including the imposition of a metal band on the critical zone of the kinescope, compression of the critical zone, so that, in order to reduce the applied external efforts to obtain the necessary reduction of the critical zone, as a bandage Two metal rings molded around the perimeter of the critical zone of the kinescope are used, between which spacers are inserted, an external force for compressing the critical area is applied to the said rings in the direction perpendicular to their plane, between the spacers. Sources of information taken into account in the examination 1. GDR patent number 61577, cl. 21 g 13/28, 1967. 2.Патент Японии N 22826, кл. Н 01 J 29/36, 1971 прототип .2. Japanese Patent N 22826, cl. H 01 J 29/36, 1971 prototype.
SU802988730A 1980-10-03 1980-10-03 Method of explosion-protection of kinescopes SU907636A1 (en)