SU90731A1 - Method of pouring cement into the absorption zone during drilling - Google Patents

Method of pouring cement into the absorption zone during drilling

Info

Publication number
SU90731A1
SU90731A1 SU418097A SU418097A SU90731A1 SU 90731 A1 SU90731 A1 SU 90731A1 SU 418097 A SU418097 A SU 418097A SU 418097 A SU418097 A SU 418097A SU 90731 A1 SU90731 A1 SU 90731A1
Authority
SU
USSR - Soviet Union
Prior art keywords
cement
absorption zone
during drilling
zone during
pouring cement
Prior art date
Application number
SU418097A
Other languages
Russian (ru)
Inventor
А.А. Колтаков
Original Assignee
А.А. Колтаков
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by А.А. Колтаков filed Critical А.А. Колтаков
Priority to SU418097A priority Critical patent/SU90731A1/en
Application granted granted Critical
Publication of SU90731A1 publication Critical patent/SU90731A1/en

Description

Дл  борьбы с уходод промывочио ЖИДКОСТИ В зону поглощени, при турбинно-роторном бурении скважин, нрнмен ютс  paзлив rыe быстросхватывающиес  смеси высокой в зкости. Эти смеси заполн ют зону поглощени  и преграждают уход промывочной жидкости. Чтобы избежать ухода быстрозахватывающейс  смеси и возможности удержат , се, В начале зоны поглои1сни  предлагаетс  исиользовать  вление вакуума дл  заме.п, продвижени  столба цементного раствора В зону пог.тощени .To combat flushing fluid, turbo-rotary drilling of wells is absorbed into the absorption zone by mixing high-viscosity mixtures. These mixtures fill the absorption zone and stop the washing liquid from escaping. In order to avoid the withdrawal of the quick-setting mixture and the possibility of retaining it, ce, At the beginning of the zone of absorption, it is proposed to use the phenomenon of vacuum to replace the advance of the column of cement slurry Into the area of the accumulated sludge.

Способ состоит В следующем. Перед началом бурени  в устье шахтового направлени  бетонируетс  на 5-6 м обсадна  труба диамет К )м 16-18 заканчиваюгиа с  вверху муфтой.The method consists in the following. Before starting drilling, the casing pipe of diameter K) m 16-18 with a coupling at the top is concreted for 5-6 m at the mouth of the mine direction.

При по вленш поглощени  во вре-м  бурени  скважины уровень промывочной жидкости упадет. Производитс  подсчет необходимого количества цементного раствора дл  заполнени  зоны поглощени .When absorption occurs during drilling, the level of flushing fluid will drop. The required amount of cement slurry is calculated to fill the absorption zone.

Через заливочную головку, установленную на муфте обсадной трубы , закачиваетс  необходимое количество п,емент1 ого раствора с 40-50°о консистениией цемента.Through the filling head installed on the casing coupling, the required amount of n, cement solution is pumped from 40-50 ° about the consistencies of the cement.

Заливочна  головка, краны и места соединений должны быть проверены на герметичность.The filler head, taps and connections must be leak tested.

После п юкачки цемента, закрываютс  краны как на головке, так и па за. ивочном агрегате.After pumping the cement, the taps are closed both on the head and the pas. spring assembly.

Закаченный в скважину цемент будет удерживатье  под заливочпой ГОЛОВКОЙ за счет образовавщегос  вакуума, который образуетс  пои передв11жении в скважине цементного столба.The cement pumped into the well will be held under the filling head due to the resulting vacuum, which is formed by penetration into the cement column in the well.

Предмет и з о б i5 е т е и :И  Subject and d i i e et e: i

Способ заливки цемента в зону поглощени  при бурении скважин, . о т л и ч а ю ш, и и с   гем, что, :с целью замедлени  продвижени  столбаMethod of pouring cement into the absorption zone during drilling,. About tl and h and y w, and with hem, that,: in order to slow down the progress of the column

цемента ВвЗрну ухода, непосредственно после прокачки цемента и нагнетани  его в зону ухода в KOfiH4ecT)3e по расчету, имеющиес  на заливочной толрвке и насосах :задвижки и краны перекрывают с тем, чтобы дальнейшее .-продвижел-Чие цементного столба создало вакуум под заливочной головкой, замедл ющий продвижение цемента .до его схватыCement VZRNU care, immediately after pumping cement and pumping it into the care zone in KOfiH4ecT) 3e by calculation, available on the primer and pumps: valves and taps overlap so that further. slowing the progress of the cement. to his arms

SU418097A 1950-05-15 1950-05-15 Method of pouring cement into the absorption zone during drilling SU90731A1 (en)