SU888798A1 - Method for making accelerating tube - Google Patents

Method for making accelerating tube Download PDF

Info

Publication number
SU888798A1
SU888798A1 SU802958600A SU2958600A SU888798A1 SU 888798 A1 SU888798 A1 SU 888798A1 SU 802958600 A SU802958600 A SU 802958600A SU 2958600 A SU2958600 A SU 2958600A SU 888798 A1 SU888798 A1 SU 888798A1
Authority
SU
USSR - Soviet Union
Prior art keywords
accelerating tube
titanium electrodes
ceramic cylinders
making
aluminosilicate
Prior art date
Application number
SU802958600A
Other languages
Russian (ru)
Inventor
А.Т. Ермолаев
И.Ф. Малышев
В.М. Уродков
С.Г. Цепакин
Р.С. Чечиков
Original Assignee
Предприятие П/Я А-7904
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Предприятие П/Я А-7904 filed Critical Предприятие П/Я А-7904
Priority to SU802958600A priority Critical patent/SU888798A1/en
Application granted granted Critical
Publication of SU888798A1 publication Critical patent/SU888798A1/en

Abstract

СПОСОБ ИЗГОТОВЛЕНИЯ УСКОРИТЕЛЬНОЙ ТРУБКИ путем диффузионной сварки алюмосиликатных или алюмооксидных керамических цилиндров и титановых электродов при их нагреве 3 вакууме 1,33-10 -1,33 ю; Па и сжимающем давлении 1,97-3,92-10 Па отличающийс  т.ем, что, с целью повышени  механической прочности, между керамическими цилиндрами и титановыми электродами ввод т прокладку из алюмини  толщиной METHOD OF MAKING A QUICKNESS TUBE by diffusion welding of aluminosilicate or alumina ceramic cylinders and titanium electrodes when heated by a 3 vacuum 1.33-10 -1.33 o; Pa and a compressive pressure of 1.97-3.92-10 Pa. In other words, in order to increase mechanical strength, an aluminum gasket is inserted between ceramic cylinders and titanium electrodes.

Description

Фиг. 1FIG. one

Claims (1)

СПОСОБ ИЗГОТОВЛЕНИЯ УСКОРИТЕЛЬНОЙ ТРУБКИ путем диффузионной сварки алюмосиликатных или алюмооксидных керамических цилиндров и титановых электродов при их нагреве в вакууме 1 ,33 -10'4-1,33 · 10(2 Па и сжимающем давлении 1,97-3,92·107Па отличающийся т.ем, что, с целью повышения механической прочности, между керамическими цилиндрами и титановыми электродами вводят прокладку из алюминия толщиной (0,03-0,2) ’ Ю'^М, а сварку осуществляют при БбО-ЬЗО^С.METHOD FOR PRODUCING AN ACCELERATING TUBE by diffusion welding of aluminosilicate or alumina ceramic cylinders and titanium electrodes when they are heated in a vacuum of 1, 33 -10 ' 4 -1.33 · 10 ( 2 Pa and a compressive pressure of 1.97-3.92 · 10 7 Pa characterized in that, in order to increase the mechanical strength, a gasket of aluminum with a thickness of (0.03-0.2) Ю 'М M is introduced between the ceramic cylinders and titanium electrodes, and welding is carried out with BbO-L3O ^ C. ро 00 00 соro 00 00 s ЬоB
SU802958600A 1980-07-11 1980-07-11 Method for making accelerating tube SU888798A1 (en)