SU742409A1 - Method of finishing construction articles - Google Patents

Method of finishing construction articles Download PDF

Info

Publication number
SU742409A1
SU742409A1 SU772487455A SU2487455A SU742409A1 SU 742409 A1 SU742409 A1 SU 742409A1 SU 772487455 A SU772487455 A SU 772487455A SU 2487455 A SU2487455 A SU 2487455A SU 742409 A1 SU742409 A1 SU 742409A1
Authority
SU
USSR - Soviet Union
Prior art keywords
finishing
solution
product
hardening
wax
Prior art date
Application number
SU772487455A
Other languages
Russian (ru)
Inventor
Борис Анатольевич Шаршунов
Григорий Ефимович Бугаенко
Николай Григорьевич Ярмоленко
Original Assignee
Научно-Исследовательский Институт Строительных Конструкций Госстроя Ссср
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Научно-Исследовательский Институт Строительных Конструкций Госстроя Ссср filed Critical Научно-Исследовательский Институт Строительных Конструкций Госстроя Ссср
Priority to SU772487455A priority Critical patent/SU742409A1/en
Application granted granted Critical
Publication of SU742409A1 publication Critical patent/SU742409A1/en

Description

1one

Изобретение относитс  к производству строительных изделий и конструкций.The invention relates to the manufacture of building products and structures.

Известен способ изготовлени : декоративных строительных изделий, включшощий нанесение на дно и стенки формы антиадгезионной смазки, укладку эпоксидной смолы , положение строительного элемента с последующей вибрацией в течение 1030 с. l .A known method of manufacturing: decorative building products, including applying anti-adhesive lubricant to the bottom and walls of the mold, laying epoxy resin, positioning the construction element with subsequent vibration for 1030 s. l.

Наиболее близким из известных к пред-,« латаемому по технической (ущности   достигаемому результату  вл етс  способ отделки строительных изделий, вкпючаюпшй нанесение гипсового отделочного растворе йа гладкую форму и укладку на него иап©-,5 ЛИЯ с последующим твердением раслворThe closest of the known to the pre-, “technical” (the main result is the method of finishing building products, including the application of a plaster finishing solution and a smooth form and laying on it ip © -, 5 LIA, followed by hardening

Целью изобретени   вл етс  гаэвышениб . качества отделки и повышение производительности труда.The aim of the invention is gaevyshenib. quality finishes and increased productivity.

Это достигаетс  тем, что в способе 0 отделки строительных изделий, включающем нанесение гипсового отделочного раствора на гладкую форму и укладку на не го издели  с последующим твердениемThis is achieved by the fact that in method 0 of finishing building products, including applying a plaster finishing solution on a smooth form and laying on a non-product, followed by hardening

раствс а, форму предварительно смазывюот всюковой мастикой, а после тверцени  р створом форму с изделием нагревают до 5О-9О С и выдерживают до пропитки от цепочного раствора слоем воска.After dissolving, the form is pre-lubricated with an all-purpose mastic, and after being twisted with a mortar, the form with the product is heated to 5О-9О С and kept up to the impregnation from the chain solution with a layer of wax.

Способ осуществл ют в следуюшвй последов аггельности. На полированное дно формы HffiiocHT восковую мастику епоем 0,2-1 мм, после затвердевани  которой в эту ж©-форму укладывают птсовый отделочный раствор, а затем изделие ооарвЕасают с отделочным раствором и вьшер жйвают до полного его схввгывав а с нэаел {ем , после 4его форму с надел ем н0rjpeeaioT до 50-90°С и выдерживают до полвого расплавлени  и вп тьюан   мастики отделочньш раствором.The method is carried out as follows. At the polished bottom of the HffiiocHT form, wax mastic is applied by Epoi 0.2-1 mm, after which it hardens, the PCT finishing solution is placed into this V # form, and then the product is coated with the finishing solution and extracted until it is fully grasped. 4 form it with the nrjpeeaioT imparting up to 50-90 ° С and can be kept until it has been melted and mixed with mastic finishing solution.

Пример, Попированнов дно и стенки формы смйзывают вос совой слоем 0,5 мм, отверждают последнюю, 1нанос т гипсовый отделочный раствор   укладывают бетонный элемент. После за  гипсового отделочного раствс ра форму с изделием нагревают до 374240 и выдерживают до полного впитьюани  мвст ки шпсовым раствором. Иэдв и , изготовленные по предлагавмому способу, имеют гладкую полированн ю повертность. Формула изобретени  Оюсоб отделки строительных изделий, екгасцающвй ненесение гипсового отделоч о-Ш го раствора на гладкую форму и укладку на него издели  с последукадим таердением . рас -вора, отлича.ющийс  тем, 94 чтб, с цепью повышени  качества отдепки и повышени  производительности труда, форму прэдв з тельно смазывают восковой мастикой, а после твердени  раствора с иэдвпшм нагревают до 5О-90 С и вьиерживают до n ontenai отдело«пюго раствора сшоем восжа. Источшйи информации, прин тые во внимшве при экспертизе 1, Авторское евидетельсгвЬ СССР N 399484, клГс О4 В 27/О4, 1071. 2.. Авторское .свидетельство СССР № 43326,кл. С 04 В 27/О4, 1935.For example, Popirovanov bottom and walls of the mold are waxed with a layer of 0.5 mm, they cure the last, 1 plastering plaster finishing mortar and the concrete element is laid. After the gypsum finishing solution, the form with the product is heated to 374240 and held until it is completely absorbed with the solution. The edging and, made according to the proposed method, have a smooth polished twist. Claims of the invention of the finishing of building products, the exclusion of the plaster finishing of the mortar on a smooth form and the laying of the product on it with a subsequent incision. dissolving, 94 in order, with a chain of improvement in the quality of separation and increase in labor productivity, the form is preliminarily smeared with wax mastic, and after hardening the solution with extrusion is heated to 5 ° -90 ° C and held down to n ontenai; solution with voszh. Sources of information, received attentively at examination 1, Author's Research Council of the USSR N 399484, class O4 В 27 / О4, 1071. 2 .. Author's certificate of the USSR № 43326, cl. C 04 B 27 / O4, 1935.

Claims (1)

Отособ отделки строительных изделий» вкпкчающий ненесение гипсового отделочно-10 го раствора на гладкую форму и укладку на него изделия с последующим твердением .раствора, отлич&ющийся тем,Finishing of construction products finishing ”including the application of a plaster finishing 10th mortar onto a smooth form and laying the product on it, followed by hardening of the solution, characterized in that 742409 * что, с целью повышения качества отделки и повышения производительности труда, форму предварительно смазывают восковой мастикой, а после твердения раствора форму с изделием нагревают до 50-90*С и вьиержявают до пропитки отделочного раствора' споем воска.742409 * that, in order to improve the quality of finishing and increase labor productivity, the mold is pre-lubricated with wax mastic, and after hardening the solution, the mold with the product is heated to 50-90 * C and vyjerilat until the finish solution is soaked with a wax.
SU772487455A 1977-05-19 1977-05-19 Method of finishing construction articles SU742409A1 (en)