SU498667A1 - Способ изготовлени цинкового электрода химического источника тока - Google Patents
Способ изготовлени цинкового электрода химического источника токаInfo
- Publication number
- SU498667A1 SU498667A1 SU1992313A SU1992313A SU498667A1 SU 498667 A1 SU498667 A1 SU 498667A1 SU 1992313 A SU1992313 A SU 1992313A SU 1992313 A SU1992313 A SU 1992313A SU 498667 A1 SU498667 A1 SU 498667A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- current source
- zinc electrode
- chemical current
- making zinc
- making
- Prior art date
Description
1
Известен способ изготовлени цинкового электрода химического источника тока путем смешивани окиси цинка с цинковой пылью, поливиниловым спиртом и пенообразователем, многократного пропускани смеси через сита, сушки и напрессовки на токоотвод.
Однако изготовленный таким способом элекТ1род имеет низкую механическую прочность в св зи с тем, что используют небольшое давление прессовани при нанесении смеси на токоотвод .
С .целью повышени механической прочности предлагаетс пенообразователь предварительно вводить в поливиниловый спирт в соотношении 1 : 100.
Предложенный способ заключаетс в следуюш ,ем.
Пенообразователь, например, ОП-7 (оксиэтилированный моно- и диалкифенол ввод т в раствор поливинилового спирта в соотношении 1 : 100. Раствор взбалтывают на механической мешалке до образовани пены. Пену смешивают с цинковой пылью и окисью цинка. Смесь подсушивают до влажности 12-15%, после чего пропускают через сито с размером чеек 1 мм, повторно сушат до влажности
2
0,1-0,5%, пропускают через сито с размером чеек 2 мм, затем гранулированную массу напрессовывают на токоотвод.
При сушке смеси из гранул выдел етс заключенный в пене воздух, что способствует образованию высокоразвитой, пористой структуры частиц.
Полученный таким образом порошок обладает меньшей объемной массой. Изготовленные из него электроды имеют высокую прочность , так как соответственно увеличиваетс объем дозы порошка, который, в свою очередь, позвол ет при заданной толщине электрода увеличить давление прессовани .
Предмет изобретени
Способ изготовлени цинкового электрода химического источника тока, путем смешивани окиси цинка с цинковой пылью, поливиниловым спиртом и пенообразователем, многократного пропускани смеси через сита, сушки и напрессовки на токоотвод, отличающийс тем, что, с целью повышени механической прочности, пенообразователь предварительно ввод т в поливиниловый спирт в соотношении 1 : 100.