SU482475A1 - The method of obtaining phenol-furan binder - Google Patents

The method of obtaining phenol-furan binder

Info

Publication number
SU482475A1
SU482475A1 SU2026027A SU2026027A SU482475A1 SU 482475 A1 SU482475 A1 SU 482475A1 SU 2026027 A SU2026027 A SU 2026027A SU 2026027 A SU2026027 A SU 2026027A SU 482475 A1 SU482475 A1 SU 482475A1
Authority
SU
USSR - Soviet Union
Prior art keywords
furan binder
phenol
obtaining phenol
binder
obtaining
Prior art date
Application number
SU2026027A
Other languages
Russian (ru)
Inventor
Юлдаш Маматович Маматов
Владимир Степанович Кожевников
Суфия Абдурахмановна Акбарова
Вера Александровна Соколова
Антонина Андреевна Сорокина
Original Assignee
Предприятие П/Я М-5885
Всесоюзный научно-исследовательский институт литейного машиностроения, литейной технологии и автоматизации литейного производства
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Предприятие П/Я М-5885, Всесоюзный научно-исследовательский институт литейного машиностроения, литейной технологии и автоматизации литейного производства filed Critical Предприятие П/Я М-5885
Priority to SU2026027A priority Critical patent/SU482475A1/en
Application granted granted Critical
Publication of SU482475A1 publication Critical patent/SU482475A1/en

Description

вого спирта 2,0-3,0%, содержание гидроксильных групп 8,0-10,0%.alcohol 2,0-3,0%, the content of hydroxyl groups of 8.0-10.0%.

К 150 г получепного олигомера последовательно При перемешивапии добавл ют 350 г фенолоспирта и продолжают кондепсацию 2 час при 80-85°С и рН 8,0-9,0. Затем обратный холодильник переключают на пр мой и отгон ют воду при 70°С и остаточном давлении 250-300 мм рт. ст. Отгон прекрапдают, когда в зкость смолы достигнет 50-120 сек по вискозиметру ВЗ-4.To 150 g of the obtained oligomer, 350 g of phenol-alcohol are added successively under stirring and the condensation is continued for 2 hours at 80-85 ° C and pH 8.0-9.0. Then the reflux condenser is switched to direct and water is distilled off at 70 ° C and a residual pressure of 250-300 mm Hg. Art. The distillation is stopped when the viscosity of the resin reaches 50-120 seconds using the OT-4 viscometer.

Свойства св зующего, полученного по примеру 1, и стержневых смесей с его использованием приведены в таблице.The properties of the binder obtained in example 1, and core mixtures with its use are shown in the table.

Пример ы 2-4. Методика опытов аналогична npHMenv 1, мен ютс  лишь реагенты и их количества:Example s 2-4. The experimental procedure is similar to npHMenv 1, only the reagents and their amounts are changed:

Пример 2 - 200 г олигамера + 300 г фенолоспирта .Example 2 - 200 g of oligamer + 300 g of phenol-alcohol.

Пример 3-150 г олигомера+300 г фенолоспирта-|-50 г мочевиноформальдегидной смолы.Example 3-150 g of oligomer + 300 g of phenol-alcohol - | -50 g of urea-formaldehyde resin.

Пример 4 - 200 г олигомера+ 200 г фенолоспирта+ЮО г мочевиноформальдегидной смолы.Example 4 - 200 g of oligomer + 200 g of phenol-alcohol + 10 g of urea-formaldehyde resin.

Свойства св -зующих, полученных по -примерам 2-4, и стержневых смесей с их использованием приведены в таблице.Properties sv-zyuschih, obtained in examples 2-4, and core mixtures with their use are shown in the table.

SU2026027A 1974-05-22 1974-05-22 The method of obtaining phenol-furan binder SU482475A1 (en)