SU445697A1 - Method of refining low-silicon ferrosilicon - Google Patents

Method of refining low-silicon ferrosilicon

Info

Publication number
SU445697A1
SU445697A1 SU1878385A SU1878385A SU445697A1 SU 445697 A1 SU445697 A1 SU 445697A1 SU 1878385 A SU1878385 A SU 1878385A SU 1878385 A SU1878385 A SU 1878385A SU 445697 A1 SU445697 A1 SU 445697A1
Authority
SU
USSR - Soviet Union
Prior art keywords
ferrosilicon
chlorides
sang
graphite
carbonates
Prior art date
Application number
SU1878385A
Other languages
Russian (ru)
Inventor
Юрий Павлович Канаев
Герман Васильевич Серов
Вячеслав Иванович Ольков
Жорж Ефимович Слепцов
Борис Петрович Бурылев
Original Assignee
ФОНД энепЕртов
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ФОНД энепЕртов filed Critical ФОНД энепЕртов
Priority to SU1878385A priority Critical patent/SU445697A1/en
Application granted granted Critical
Publication of SU445697A1 publication Critical patent/SU445697A1/en

Description

1one

Изобретение относитс  к области черной металлургии и касаетс  повышени  качества ферросилици .The invention relates to the field of ferrous metallurgy and concerns the improvement of the quality of ferrosilicon.

Низкокремнистые сорта ферросилици , особенно 18%- и 25%-цый, содержат повышенное технологически неизбежное содержание углерода, достигаюшее 0,8-1,5%- В процессе остывани  и кристаллизации в мульдах конвейерной разливочной машины при температуре 1300-1400°С часть углерода выдел етс  в виде графитной спели и заполн ет раковины и полости слитка. Использование такого ферросилици  дл  легировани  чугунов приводит к ухудшению качества отливок.Low silicon grades of ferrosilicon, especially 18% and 25%, contain an elevated technologically unavoidable carbon content, reaching 0.8-1.5%. During the cooling and crystallization process in the molds of the conveyor casting machine at a temperature of 1300-1400 ° C, some of the carbon released in the form of graphite sang and fills the shells and cavities of the ingot. The use of such ferrosilicon to alloy cast irons leads to a deterioration in the quality of castings.

Известны способы рафинировани  низкопроцентного ферросилици  от графитной спели , основанные на его выделении в процессе охлаждени  сплава, например, путем перелива из ковша в ковш или длительной выдержки перед разливкой.Methods are known for refining low-grade ferrosilicon from graphite sang, based on its isolation during the process of cooling the alloy, for example, by overflowing from a ladle into a ladle or long exposure before casting.

Недостатками таких способов  вл ютс  удлинение цикла разливки и увеличение потерь ферросилици  со скрапом.The disadvantages of such methods are lengthening the casting cycle and increasing the loss of ferrosilicon with scrap.

Целью изобретени   вл етс  ускорение удалени  круцнопластинчатой графитной спели. The aim of the invention is to accelerate the removal of a cruciform graphite sang.

Поставленна  цель достигаетс  обработкой жидкого ферросилици  при температуре 1300-1400°С перед кристаллизацией в мульдах разливочной машины хлоридами или карбонатами «атри , кали  или магни  в количестве 3-5 кг на I т сплава. Наиболее просто процесс рафинировани  может быть осу цествлен введением указанных хлоридов, например , в виде поваренной соли NaCl или соды Ыа2СОз в раствор, которым орошаетс  рабоча  поверхность мульд, с целью образовани  противопригарного сло . При контактировании последнего с л идким ферросилицием происходит интенсивное разложение и испарение карбонатов и хлоридов натри , кали  или магни , ускор юш,ее удаление из расплава выделившейс  крупнопластинчатой графитной спели; оставшийс  углерод в виде мелкодисперсных включений и карбидов не ухудшает качества чугунного лить .This goal is achieved by treating liquid ferrosilicon at a temperature of 1300-1400 ° C before crystallization in the molds of the filling machine with chlorides or carbonates of atri, potassium or magnesium in an amount of 3-5 kg per ton of alloy. Most simply, the refining process can be carried out by introducing these chlorides, for example, in the form of sodium chloride NaCl or Na 2 SO 3 soda into the solution, which is irrigated with the working surface of the mold, in order to form a nonstick layer. When the latter is contacted with liquid ferrosilicon, intensive decomposition and evaporation of carbonates and chlorides of sodium, potassium or magnesium occurs, accelerating, removing it from the melt of precipitated large-plate graphite sang; the remaining carbon in the form of fine particles and carbides does not impair the quality of the cast iron.

Предмет изобретени Subject invention

Claims (2)

1.Снособ рафинировани  низкокремнистого ферросилици , включаюший выделение графитной спели из сплава при его остывании и кристаллизации, о т л и ч а ю ш, и и с   тем, что, с целью ускорени  удалени  крупнопластннчатой графитной спели, жидкий ферросилиций непосредственно перед кристаллизацией обрабатывают хлоридами или карбонатами натри  или кали , или магни  в .мульдах разливочной машины.1. The method of refining low-silicon ferrosilicon, including the separation of graphite sang from the alloy during its cooling and crystallization, is about tl and h and w, and with the aim of accelerating the removal of large-grafted graphite sang, liquid ferrosilicon is treated with chlorides directly before crystallization with chlorides or carbonates of sodium or potassium, or magnesium in the pulp casting machine. 2.Способ по п. 1, отличающийс  тем, что хлориды или карбонаты натри  или кали , или магни  нанос т на рабочую поверхность мульд вместе с раствором противопригарного состава.2. A method according to claim 1, characterized in that the chlorides or carbonates of sodium or potassium or magnesium are applied onto the working surface of the mold together with the solution of the non-stick composition.
SU1878385A 1973-02-02 1973-02-02 Method of refining low-silicon ferrosilicon SU445697A1 (en)