SU443682A1 - Способ обезвоживани - Google Patents

Способ обезвоживани

Info

Publication number
SU443682A1
SU443682A1 SU1854996A SU1854996A SU443682A1 SU 443682 A1 SU443682 A1 SU 443682A1 SU 1854996 A SU1854996 A SU 1854996A SU 1854996 A SU1854996 A SU 1854996A SU 443682 A1 SU443682 A1 SU 443682A1
Authority
SU
USSR - Soviet Union
Prior art keywords
clay
dehydration method
products
enrichment
particles
Prior art date
Application number
SU1854996A
Other languages
English (en)
Inventor
Леонид Федорович Долина
Витольд Савельевич Каминский
Исаак Григорьевич Резников
Зоя Петровна Перель
Валерий Петрович Молокоедов
Original Assignee
Коммунарский горно-металлургический институт
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Коммунарский горно-металлургический институт filed Critical Коммунарский горно-металлургический институт
Priority to SU1854996A priority Critical patent/SU443682A1/ru
Application granted granted Critical
Publication of SU443682A1 publication Critical patent/SU443682A1/ru

Description

1
Изобретение относитс  к процессам обогащени  полезных ископаемых и может использоватьс , например дл  отделени  глинистых частиц от угольных продуктов на грохотах и центрифугах, в процессах обогащени  глинистых руд (железных, марганцевых, калийных и других), дл  промывки и протирки их в скрубберах, в промывочных башн х, реечных и спиральных классификаторах.
Известны и широко примен ютс  различные реагенты дл  депрессии глин в процессах флотации сильвинитовых и калийных руд, а также в процессах флокул ции углеглинистых суспензий.
Однако существующие способы отделени  глинистых минералов от продуктов обогащени  имеют низкую эффективность, требуют применени  дорогих дефицитных, токсичных и биологически не разлагаемых реагентов, сложны при удалении глинистых осадков, имеют малую производительность и другие недостатки .
Предлагаемый способ отличаетс  тем, что в качестве поверхностно-активного вещества (ПАВ) в обезвоживаемый материал добавл ют водный раствор динатриевой соли моноэфиров сульфо нтарной кислоты и моноэтаноламидов синтетических кислот Сю-Cie.
Это позволит отделить глинистые частицы от продуктов обогащени , например угольного концентрата.
Флокул нт имеет структурную формулу
СООНа RCOIHCH CHzOCOCHi-СН
где R Сю-Ci
и представл ет собой нетоксичную светложелтую пасту, хорошо раствор ющуюс  в воде. Товарна  форма нового реагента «дне А10-16 содержит 47% активного вещества . Новый реагент не вазимодействует с металлической поверхностью и устойчив в слабокислых и щелочных средах и в жесткой воде. Получаетс  из доступных, вырабатываемых промышленностью продуктов - моноалкилоамидов , малеинового ангидрида и сульфита натри . Содержание основного (активного ) вещества может измен тьс  в желаемых пределах от 20 до 50%.
Анионоактивный реагент имеет плотность от 1,05 до 1,10 кг/дм и мол. вес пор дка 470- 490. 34
Предмет изобретени мер угольного концентрата, в качестве ПАВ в
Способ обезвоживани  на грохотах и цент- раствор динатриевой соли моноэфиров сульрифугах с применением ПАВ, отличаю- фо нтарной кислоты и моноэтаноламидов синщ и и с   тем, что, с целью отделени  глини- 5 тетических жирных кислот Сю-Cie. стых частиц от продуктов обогащени , напри4436&2
обезвоживаемый материал добавл ют водный
SU1854996A 1972-12-11 1972-12-11 Способ обезвоживани SU443682A1 (ru)