SU440A1 - The method of ore dressing - Google Patents

The method of ore dressing

Info

Publication number
SU440A1
SU440A1 SU67577A SU67577A SU440A1 SU 440 A1 SU440 A1 SU 440A1 SU 67577 A SU67577 A SU 67577A SU 67577 A SU67577 A SU 67577A SU 440 A1 SU440 A1 SU 440A1
Authority
SU
USSR - Soviet Union
Prior art keywords
ore
ore dressing
sulfuric acid
copper
per ton
Prior art date
Application number
SU67577A
Other languages
Russian (ru)
Inventor
Неттер Э.Г.
Original Assignee
Неттер Э.Г.
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Неттер Э.Г. filed Critical Неттер Э.Г.
Priority to SU67577A priority Critical patent/SU440A1/en
Application granted granted Critical
Publication of SU440A1 publication Critical patent/SU440A1/en

Description

Предложение касаетс  способа концентрации руд по методу всплывани  с образованием пены. Существует целый р д углеводородов, в особенности непредельных, которые при обработке серною кислотою образуют соединени , весьма подход щие дл  применени  в качестве вспенивающих агентов при концентрации руд по методу всплывани  с образованием пены, при чем с некоторыми рудами эти реактивы образуют более чистый концентрат или более устойчивую пену. Такие продукты получаютс  при обработке серной кислотой углеводородов, как-то: нефти, керосина , газовой смолы и т. под., и в особенности при обработке их дистилл тов . Типичным примером таких продуктов  вл етс  известный кислый шлам; по опытам автора, такой щлам, получаемый при обработке серной кислотой керосина, добытого из Калифорнийской нефти, будучи применен в качестве вспенивающего реактива, дает чрезвычайно благопри тные результаты . Нижеследующий пример по сн ет применение предлагаемого способа. Обработке подвергались „хвосты с промывательных концентрационных столов, служивших дл  обогащени  медной руды, при чем эти хвосты содержали, по анализу , 2,26% меди. К кашке, содержащей этот материал в пропорции 24,0% твердого вещества, было прибавлено тывалась в соответствующем аппарате, при чем она подвергалась взбалтыванию дл  образовани  пены, котора  была отделена. Концентраты показали содержание 10,1% меди, а остатки содержали 0,2% меди. ченные действием серной кислоты на углеводороды, во многих случа х оказываютс  более эффективными в качестве вспенивающих реактивов, если они просто т некоторое врем  или если они 2,3 фунта кислого шлама на тонну руды, 2,3 „ древесного креозота на тонну руды, 0,21 „ печного масла на тонну руды, 12,7 „ серной кислоты на тонну Нагрета  до 97° Фар. кашка обрабаПо мнению автора, вещества, полуThe proposal relates to a method of concentrating ores according to the method of floating up with the formation of foam. There are a number of hydrocarbons, especially unsaturated ones, which, when treated with sulfuric acid, form compounds that are very suitable for use as blowing agents for ore concentration using the froth formation method with foam formation, and with some ores these reagents form a more pure concentrate or more stable foam. Such products are obtained by treating sulfuric acid with hydrocarbons, such as oil, kerosene, gas tar, etc., and especially when processing their distillates. A typical example of such products is the well-known acidic slurry; According to the author's experiments, such schlich, obtained by treating kerosene with sulfuric acid, extracted from California oil, being used as a foaming reagent, gives extremely favorable results. The following example illustrates the application of the proposed method. The tailings from the washing concentration tables, which served to enrich the copper ore, were treated, and these tailings contained, according to analysis, 2.26% copper. To a gruel containing this material in a proportion of 24.0% solids was added in an appropriate apparatus, and it was shaken to form a foam that was separated. Concentrates showed a content of 10.1% copper, and residues contained 0.2% copper. The effects of sulfuric acid on hydrocarbons are, in many cases, more effective as foaming reagents if they are simply for a while or 2.3 pounds of acid sludge per ton of ore, 2.3 "wood creosote per ton of ore, 0, 21 ”oven oil per ton of ore, 12.7” sulfuric acid per ton Heated to 97 ° Far. According to the author, substance, sex

SU67577A 1915-09-16 1915-09-16 The method of ore dressing SU440A1 (en)