SU423767A1 - METHOD FOR HANDLING WATER OF THE CONSTRUCTION MIXTURE FILLING - Google Patents
METHOD FOR HANDLING WATER OF THE CONSTRUCTION MIXTURE FILLINGInfo
- Publication number
- SU423767A1 SU423767A1 SU1619028A SU1619028A SU423767A1 SU 423767 A1 SU423767 A1 SU 423767A1 SU 1619028 A SU1619028 A SU 1619028A SU 1619028 A SU1619028 A SU 1619028A SU 423767 A1 SU423767 A1 SU 423767A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- handling water
- mixture filling
- construction mixture
- strength
- water
- Prior art date
Description
1one
Изобретение онтоситс к промышленности строительных материалов и может быть применено нри производстве изделий из бетона и железобетона.The invention of ontosis to the building materials industry and can be applied in the manufacture of concrete products and reinforced concrete.
Известен способ обработки воды затворени строительной смеси, нанример, нри нроизводстве бетонных изделий путем воздействи на нее магнитным -полем. Недостаток известного способа заключаетс в нестабильности прочлостных характеристик бетонов и раство,р01В.A known method for treating the mixing water of a building mixture, for example, is the production of concrete products by exposing it to a magnetic field. The disadvantage of this method is the instability of the translatting characteristics of concrete and mortar, p01B.
Целью насто щего изобретени вл етс повышение и стабилизаци прочности изделий .The purpose of the present invention is to increase and stabilize the strength of the products.
Достигаетс цель тем, что на воду затворени воздействуют вращаюш.имс 1магнитным полем .с напр женностью 100-2000 а/см при промышленной частоте электрического тока и скорости Протекани воды 0,,5 м/сек.The goal is achieved by the fact that the mixing water is affected by a rotating magnet 1 magnetic field with a strength of 100-2000 A / cm at an industrial frequency of electric current and a Water Flow rate of 0, 5 m / s.
Суш,ность способа заключаетс в том, что через враш;ающеес магнитное (Поле, создаваемое трехфазным электрическим током в трехфазной обмотке, перпендикул рно магнитным силовым лини м но трубопроводу нз неферромагнитного материала пропускают воду. При промышленной частоте электрического тока и скорости протекани воды 0,5- 2,5 м/сек на-пр женность магнитного нол составл ет 100-2000 а/см.The dryness of the method lies in the fact that the magnetic field (the field created by the three-phase electric current in the three-phase winding is perpendicular to the magnetic power line through the non-ferromagnetic material pipeline) is passed through the vras; 5-2.5 m / s. The magnetic zero field strength is 100-2000 A / cm.
Способ обеспечивает стабильное повышение прочности бетона и раствора не менее, чем на 15-20%, благодар чему достигаетс экономи цемента примерно на 10%.The method provides a stable increase in the strength of concrete and mortar by no less than 15-20%, due to which cement savings of about 10% are achieved.
Предмет изобретени Subject invention
Способ обработки воды затворени строительной смеси, например, при производствеThe method of processing mixing water mix, for example, in the manufacture
бетонных изделий, заключающийс в воздействии на нее магнитным полем, отличающийс тем, что, с целью повышени и стабилизации прочности изделий, па воду затворени воздействуют . вращающимс магнитным полем с напр женностью 100-2000 а/см нри промышленной частоте электрического тока и скорости протекани воды 0,5-2,5 м/сек.concrete products, consisting in exposure to a magnetic field, characterized in that, in order to increase and stabilize the strength of the products, the gate water is affected. rotating magnetic field with a intensity of 100-2000 A / cm at the industrial frequency of electric current and water flow rate of 0.5-2.5 m / s.