SU415313A1 - - Google Patents
Info
- Publication number
- SU415313A1 SU415313A1 SU1803673A SU1803673A SU415313A1 SU 415313 A1 SU415313 A1 SU 415313A1 SU 1803673 A SU1803673 A SU 1803673A SU 1803673 A SU1803673 A SU 1803673A SU 415313 A1 SU415313 A1 SU 415313A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- metal
- slag
- content
- dephosphorization
- silicon
- Prior art date
Links
Landscapes
- Refinement Of Pig-Iron, Manufacture Of Cast Iron, And Steel Manufacture Other Than In Revolving Furnaces (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
SU1803673A SU415313A1 (ko) | 1972-06-30 | 1972-06-30 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
SU1803673A SU415313A1 (ko) | 1972-06-30 | 1972-06-30 |
Publications (1)
Publication Number | Publication Date |
---|---|
SU415313A1 true SU415313A1 (ko) | 1974-02-15 |
Family
ID=20519879
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
SU1803673A SU415313A1 (ko) | 1972-06-30 | 1972-06-30 |
Country Status (1)
Country | Link |
---|---|
SU (1) | SU415313A1 (ko) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
RU2761852C1 (ru) * | 2018-12-03 | 2021-12-13 | Наньян Ханье Спешал Стил Ко., Лтд | Способ выпуска шлака в процессе производства стали со сверхнизким содержанием фосфора и способ производства стали со сверхнизким содержанием фосфора |
-
1972
- 1972-06-30 SU SU1803673A patent/SU415313A1/ru active
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
RU2761852C1 (ru) * | 2018-12-03 | 2021-12-13 | Наньян Ханье Спешал Стил Ко., Лтд | Способ выпуска шлака в процессе производства стали со сверхнизким содержанием фосфора и способ производства стали со сверхнизким содержанием фосфора |
US11718885B2 (en) | 2018-12-03 | 2023-08-08 | Nanyang Hanye Special Steel Co., Ltd | Slag discharging method in process of producing ultra-low phosphorus steel and method for producing ultra-low phosphorus steel |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS63481B2 (ko) | ||
SU415313A1 (ko) | ||
GB1041269A (en) | Method for adding additives to molten steel while tapping | |
US4022613A (en) | Metallurgical material and process for treating iron or steel therewith | |
US1818556A (en) | Method for the purification of iron and steel | |
SU476328A1 (ru) | Сплав дл раскислени стали | |
SU367156A1 (ko) | ||
SU417489A1 (ko) | ||
SU439528A1 (ru) | Смесь дл легировани стали и сплавов | |
SU485170A1 (ru) | Чугун | |
JPS5934768B2 (ja) | 金属あるいは合金溶湯の精錬方法 | |
SU410105A1 (ko) | ||
SU1666568A1 (ru) | Модификатор | |
SU427083A1 (ru) | Смесь для раскисления стали | |
SU499325A1 (ru) | Способ раскислени подшипниковых сталей | |
SU449976A1 (ru) | Сплав дл раскислени и легировани стали | |
SU939568A1 (ru) | Порошкообразна дефосфорирующа смесь | |
SU631539A1 (ru) | Способ производства азотсодержащей стали | |
SU581151A1 (ru) | Способ выплавки вольфрамсодержащей стали и сплавов | |
SU398621A1 (ru) | ВПТБФОНД S:iOOEPT03О. С. Бобкова, Г. Б. Ширер, Л. Ф. Косой, В. А. Черн ков, А. Г. Шалимов и С. Г. Воиновим. И. П. Бардинаi | |
SU398634A1 (ru) | Способ обработки стали в ковше жидким синтетическим шлаком | |
SU460301A1 (ru) | Шихта дл получени синтетического шлака | |
RU2131931C1 (ru) | Способ микролегирования углеродистой стали | |
SU432203A1 (ru) | Шлак для рафинирования металлов | |
Henry et al. | Different types of calcium treatment as a contribution to the development of the continuous casting process |