SU39902A1 - Method for producing acid putty - Google Patents

Method for producing acid putty

Info

Publication number
SU39902A1
SU39902A1 SU146559A SU146559A SU39902A1 SU 39902 A1 SU39902 A1 SU 39902A1 SU 146559 A SU146559 A SU 146559A SU 146559 A SU146559 A SU 146559A SU 39902 A1 SU39902 A1 SU 39902A1
Authority
SU
USSR - Soviet Union
Prior art keywords
putty
acid
producing acid
resistant
cement
Prior art date
Application number
SU146559A
Other languages
Russian (ru)
Inventor
Н.П. Белых
Original Assignee
Н.П. Белых
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Н.П. Белых filed Critical Н.П. Белых
Priority to SU146559A priority Critical patent/SU39902A1/en
Application granted granted Critical
Publication of SU39902A1 publication Critical patent/SU39902A1/en

Description

Предметом насто щего изобретени   вл етс  способ получени  кислогоупорных замазок и цементов дл  использевани  их при постройке различной химической аппаратуры. Предлагаемый способ состоит в еледующем . Беретс  га или друга  есте1 фракци , прошедшей чере И.,, Просе нный материал беретс  в вышеуказанном процентном отношении от каждой фракции, хорошо перемешиваетс , после чего к нему добавл ют глет в качестве ускорител  (98,9% РЬО) в количестве от 1% до 8% по отношению к вз тому наполнителю, причем дл  получени  кислотоупорного цемента расход глета будет составл ть 1-У/с,, а дл  получени  быстросхватывающей замазки: 3-8%. Смесь горной породы с ускорителем (глетом) тщательно перемешиваетс  и замешиваетс  с жидким стеклом крепостью 38° Боме (моду/ ь -g.Q2j8 - 3,0). Расход жидкого стекла составл ет 30-34% по отношению к весу вз того наполнител . Масса хорошо перемешиваетс , и полученное | ственна  горна  порода, отличающа с  устойчивостью по отношению к тем ; или другим кислотам; после проверки на кислотостойность, материал измель; 1 чаетс  и просеиваетс  через сита. Ситовой анализ должен соответствоi вать помолу цемента: Сито. 144 5/. з „ . 900 , „ - 10, ,, .4400 , „ -45, „ .10000 „ . - 40, тесто используетс  дл  строительных работ обычным образом. Полученна  по предлагаемому способу замазка имеет целый р д преимуществ по сравнению с известными кислотостойкими замазками и цементами, в которые в качестве ускорител  входит кремнефтористый натрий (NajSiP j). Замазки и цементы, содержащие глет в качестве ускорител , имеют повышенные механические свойства и увеличенную кислотоустойчивость. Кроме того, они обладают повышенной степенью приставани  к цементу, к керамике и хорошо склеивают плавленные горные ; породы. Благодар  этим высоким качествам j j вышеуказанные замазки и цемент моj гут заменить употребл емые до сих порThe object of the present invention is a method for producing acid-resistant putty and cements for use in the construction of various chemical equipment. The proposed method consists in the following. The beret or another este1 fraction, passed through I. .. The sifted material is taken in the above percentage ratio from each fraction, is well mixed, after which glt is added as an accelerator (98.9% PHO) in an amount from 1% up to 8% in relation to the recovered filler, and to obtain acid-resistant cement, the consumption of the slab will be 1-U / s, and to obtain a quick-setting putty: 3-8%. The mixture of rock and accelerator (lithic) is thoroughly mixed and kneaded with liquid glass of 38 ° Bome strength (mode / s-g.Q2j8 - 3.0). The consumption of liquid glass is 30-34% with respect to the weight of the filler taken. The mass is well mixed, and the resulting | mountainous rock, characterized by resistance to those; or other acids; after checking for acid resistance, the material is ground; 1 is sieved and sieved through sieves. Sieve analysis should match the grinding of cement: Sieve. 144 5 /. h „. 900, "- 10 ,, ,, .4400," -45, ".10000". - 40, dough is used for construction work in the usual way. The putty obtained by the proposed method has a number of advantages in comparison with the known acid-resistant putties and cements, which include sodium fluorofluoride (NajSiP j) as an accelerator. Putties and cements containing glat as an accelerator have enhanced mechanical properties and increased acid resistance. In addition, they have a high degree of adherence to cement, ceramics, and well glued fused mountain; breeds. Thanks to these high qualities j j, the above putties and cement can be replaced by those used until now.

импортные замазки и цемент и, кроме того, представл етс  возможным широко использовать плавленные горные породы из естественных кислотоупоров. Указанные кислотостойкие замазки и цемент могут найти себе широкое применение в различных отрасл х народного хоз йства при постройке химической аппаратуры, в качестве аппаратов , котлов, труб, башен, чанов, сцеж и, кроме того, дл  защиты стен зданий, фундаментов, каналов от паров кислотimported putty and cement and, in addition, it is possible to make extensive use of fused rocks from natural acid-resistant materials. These acid-resistant putty and cement can be widely used in various sectors of the national economy in the construction of chemical equipment, as apparatuses, boilers, pipes, towers, vats, drainage, and, in addition, to protect the walls of buildings, foundations, channels from vapors acids

и дл  использовани  плавленных горных пород в качестве футеровочного материала.and for using fused rocks as a lining material.

Предмет изобретени .The subject matter of the invention.

Ciioco6 получени  кислотоупорной замазки , отличающийс  тем, что естественную кислотоупорную горную породу измельчают, просеивают, прибавл ют глет в качестве ускорител  и замешивают с жидким стеклом.Ciioco6 acid-resistant putty, characterized in that the natural acid-resistant rock is crushed, sieved, added as an accelerator glut and mixed with liquid glass.

SU146559A 1934-04-27 1934-04-27 Method for producing acid putty SU39902A1 (en)