SU37795A1 - Method for removing bristles from pigskin - Google Patents

Method for removing bristles from pigskin

Info

Publication number
SU37795A1
SU37795A1 SU128625A SU128625A SU37795A1 SU 37795 A1 SU37795 A1 SU 37795A1 SU 128625 A SU128625 A SU 128625A SU 128625 A SU128625 A SU 128625A SU 37795 A1 SU37795 A1 SU 37795A1
Authority
SU
USSR - Soviet Union
Prior art keywords
bristles
pigskin
bath
removing bristles
alkaline
Prior art date
Application number
SU128625A
Other languages
Russian (ru)
Inventor
Д.А. Зеликов
А.Б. Межерицкий
Original Assignee
Д.А. Зеликов
А.Б. Межерицкий
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Д.А. Зеликов, А.Б. Межерицкий filed Critical Д.А. Зеликов
Priority to SU128625A priority Critical patent/SU37795A1/en
Application granted granted Critical
Publication of SU37795A1 publication Critical patent/SU37795A1/en

Description

Новый способ удалени  щетины из свиных шку.) основан на ослаблении св зи луковиц щетины перед выдергиванием их механическим путем, с применением, в цел х ослаблени  св зи луковиц со шкурой, обработки щкур сначала растворами щелочей, а затем щелочным раствором поджелудочной железы с сульфатом аммони .A new method of removing bristles from pigskin .

Практически новый способ выполн ют следующим образом. Подобранна  по плотности парти  свиных щкур подвергаетс  12-часовой отмоке в баркасе с последующим мездрением на мездрильной машине и строжкой косой с завернутым жалом. Подготовленной таким образом партии свиных шкур дают щелочную ванну в баркасе при посто нйом вращении в течение 8 часов. Температура этой ванны 25-26°; ,5-10.In practice, the new method is performed as follows. A density-matched batch of pigskin is exposed to a 12-hour soak in a long-haul, followed by disdain on the felting machine and gouging with a rolled-up sting. A batch of pigskins prepared in this way gives an alkaline bath in the long-run with constant rotation for 8 hours. The temperature of this bath is 25-26 °; 5-10.

Цель этой обработки - приподн ть ткань кожи и обезжирить как самую кожу, так и щетину. Одновременно образовавшимс  мылом производитс  мытье щетины от гр зи. Расход кальцинированной соды составл ет 2% от веса мокросоленого сырь .The purpose of this treatment is to lift the skin tissue and degrease both the skin and the bristles. At the same time the resulting soap is used to wash the bristles from dirt. The consumption of soda ash is 2% by weight of the wet-salted raw material.

После щелочной ванны, не выгружа  кожи из баркаса, спускают щелочную жидкость (эта хсидкость содержит значительное количестьо омыленгюго жира, который может быть извлечен).After an alkaline bath, without discharging the skin from the bark, they release the alkaline liquid (this fluid contains a significant amount of omilengo fat that can be extracted).

В баркас наливают чистую в.,ду температурой 30-32° и пускают баркас вIn the barge pour clean in., Do the temperature of 30-32 ° and let the bark in

ход. На ХОД} R баркас дают Р/о кальцинированной соды. Отде ьно размешивают в воде /а/о концентрвта и на ходу добавл ют его в баркас. РН 8,5-9. Концентрат состоит из поджелудочной железы, древесных опилок и сернокислого аммони .move On HOD} R barkas give R / o soda ash. Separately, stir in water (a / o concentrate) and add it to the launch as it goes. PH 8.5-9. The concentrate consists of the pancreas, sawdust and ammonium sulphate.

Втора  ванна должна только слегка нарушить эпителиальную ткань (эпидермис ) так, чтобы щетина дергалась сравнительно легко. После второй ванны шкуры тщательно промывают и подают на станки дл  дергани , одерганные поступают в золку на четаеро суток с переборкой . Дальше опе 1ации протекают по нормальной методике.The second bath should only slightly break the epithelial tissue (epidermis) so that the bristles jerk relatively easily. After the second bath, the skins are thoroughly washed and fed to the dergani machines, the tapered ones enter the gold for four days with a bulkhead. Further operations proceed according to the normal procedure.

Щетина получаетс  высщего качества, не требует обезжировки и мойки и можег идти непосредственно в работу на щетинные фабрики.The bristles are of superior quality, do not require degreasing and washing and can go directly to work at the bristle factories.

Содержание жира в щетине после означенной переработки 0,29%.The fat content in the bristles after the above processing of 0.29%.

Предмет изобретени .The subject matter of the invention.

Способ удалени  щетины из свиных шкур, отличающийс  тем, что сначала, в цел х ослаблени  щетины, щкуры обрабатывают раствором щелочи при температуре выше 20° в течение около 5-10 часов , а затем щелочным раствором поджелудоиюй железы с сульфатом аммони , после; как вых (-пераций ослабле; ную щетину удал ют.A method of removing bristles from pigskins, characterized in that first, in order to weaken the bristles, the skins are treated with an alkali solution at a temperature above 20 ° for about 5-10 hours, and then with an alkaline pancreas solution with ammonium sulphate, after; as outlets (weaker operations; loose bristles removed.

SU128625A 1933-05-13 1933-05-13 Method for removing bristles from pigskin SU37795A1 (en)