SU367145A1 - METHOD OF DEVELOPING LEATHER - Google Patents

METHOD OF DEVELOPING LEATHER

Info

Publication number
SU367145A1
SU367145A1 SU1433870A SU1433870A SU367145A1 SU 367145 A1 SU367145 A1 SU 367145A1 SU 1433870 A SU1433870 A SU 1433870A SU 1433870 A SU1433870 A SU 1433870A SU 367145 A1 SU367145 A1 SU 367145A1
Authority
SU
USSR - Soviet Union
Prior art keywords
solution
desalting
chromic
leather
softening
Prior art date
Application number
SU1433870A
Other languages
Russian (ru)
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to SU1433870A priority Critical patent/SU367145A1/en
Application granted granted Critical
Publication of SU367145A1 publication Critical patent/SU367145A1/en

Description

1one

Известный способ выработки кож хромового или хромрастительного дублени  предусматривает об зательную промывку обеззоленного и м гчеиного голь  с последующим проведением процессов пикелевани  и дублени  на свежеприготовленной ванне. Это приводит к з 1ачительному расходу воды и удлин ет техиологпческий процесс.The known method of producing leather of chromic or chrome-plant tanning involves the obligatory washing of desalted and milky ashes, followed by the processes of pickling and tanning in a freshly prepared bath. This leads to a significant consumption of water and lengthens the technological process.

Предлагаемый способ сокращает производстве1Н1ый цикл, так как позвол ет провести процессы обеззоливани , м гчени  и хромового дублени  в одной ванне. Это достигаетс  за счет того, что в обеззоливающий раствор ввод т вещества, обладающие комплексноактивными по отнощению к хрому свойствами и образующие растворимые соединени  кальци .The proposed method reduces the production of the 1H1 cycle, as it allows for the processes of desalting, softening and chrome tanning in one bath. This is achieved due to the fact that substances having complex active properties with respect to chromium and forming soluble calcium compounds are introduced into the desalting solution.

В качестве таких веп1,еств могут быть использованы ароматические сульфокислоты или их соли, например, продукт нейтрализации конденсированной нафталинсульфокислоты (синтан Н. К.).Aromatic sulfonic acids or their salts, for example, the product of neutralization of condensed naphthalenesulfonic acid (N. K. syntan), can be used as such products.

Дл  осуществлени  нредлагаемого способа голье обеззоливают, причем в обеззоливающий раствор ввод т синтан НК, м гчат в этой же ванне, после подкислени  раствора до необходимого значени  рН дуб т хромовым экстрактом. Введение сиптана НК позвол ет совместить хромовый дубитель, содержащий основной сернокислый хром со слабощелочной обеззоливающе-м гчительной жидкостью. In order to carry out the proposed process, the cinder is ash-free, and in this solution, the syntan NK is introduced into the desalting solution, grinded in the same bath, after acidifying the solution to the required pH value, a double layer of chromium extract. The introduction of syptane NK allows one to combine the chromic tanning agent containing basic chromic sulphate with a weakly alkaline bleach-free thickening liquid.

22

11 р Н М е р. Зеленое голье промывают проточной водой, в последнюю промывную воду при ж.к.1 в барабан заливают раствор сульфата аммони . Обработку ведут до достижени  сквозного обеззоливани  при пробе реза на фенолфталеин, после чего в эту ванну задают анпюниое ПАВ - 0,1%, синтан НК-2- 2,5% и м гчнтель. Расход м гчител  и длительность м гчени  соответствлют нормам типовых :иетодик. После м гчепп  корректируют рП раствора до 3,8-4,2 путем добавлени  разбавленной серной кислоты. Затем в барабан заливают хромовый экстракт основностью 40-42% из расчета 60-70% от общего расхода дубнтел . Обработка продолжаетс  до достижени  сквозного прокраса (2-4 час}, после чего добавл ют остаток хромового экстракта . Дубление продолжают до удовлетворительной пробы на «кип.11 p N MER. The green hide is rinsed with running water, and the ammonium sulfate solution is poured into the drum at the last wash water at the rail tower 1. The treatment is carried out until a through desalting is achieved during the cutting test for phenolphthalein, after which an add-on surfactant is set in this bath - 0.1%, Sintan NK-2 - 2.5% and softener. The consumption of the softener and the duration of the softening correspond to the standards of the standard: method. After softening, adjust the RP of the solution to 3.8-4.2 by adding dilute sulfuric acid. Then chromic extract with basicity of 40-42% is poured into the drum at the rate of 60-70% of the total consumption of dubtel. Processing continues until a through dyeing is obtained (2-4 hours}, after which the remainder of the chromic extract is added.

Предмет изобретени Subject invention

Способ выработки кож, заключающийс  в обеззоливании, м гчении, хромовом дублении, отличаюишйс  тем, что, с целью сокращени  производственного цикла, в обеззоливающий раствор ввод т вещества, обладающие комплексно-акти1виыми по отношениюiKхрому свойствами и образующие растворимые соединени  кальци , например, ароматические сульфокислоты или их соли.The method of producing leather, which consists in desalting, softening, chrome tanning, is distinguished by the fact that, in order to shorten the production cycle, substances containing complex active with respect to khrom properties and forming soluble calcium compounds, for example, aromatic sulfonic acids or their salts.

SU1433870A 1970-05-04 1970-05-04 METHOD OF DEVELOPING LEATHER SU367145A1 (en)