SU318315A1 - Method of protecting steel from atmospheric corrosion - Google Patents

Method of protecting steel from atmospheric corrosion

Info

Publication number
SU318315A1
SU318315A1 SU7001401869A SU1401869A SU318315A1 SU 318315 A1 SU318315 A1 SU 318315A1 SU 7001401869 A SU7001401869 A SU 7001401869A SU 1401869 A SU1401869 A SU 1401869A SU 318315 A1 SU318315 A1 SU 318315A1
Authority
SU
USSR - Soviet Union
Prior art keywords
atmospheric corrosion
protecting steel
solution
steel
corrosion
Prior art date
Application number
SU7001401869A
Other languages
Russian (ru)
Inventor
Н.А. Саверина
Ю.С. Дольская
Л.В. Малов
Г.Я. Кондратьева
Original Assignee
Институт Органической Химии Им. Н.Д.Зелинского
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Институт Органической Химии Им. Н.Д.Зелинского filed Critical Институт Органической Химии Им. Н.Д.Зелинского
Priority to SU7001401869A priority Critical patent/SU318315A1/en
Application granted granted Critical
Publication of SU318315A1 publication Critical patent/SU318315A1/en

Description

Известен способ защиты стали от атмосферной коррозии с помощью ингибитора аминного типа,.например дициклогексиламина.There is a method of protecting steel against atmospheric corrosion with an amine-type inhibitor, for example, dicyclohexylamine.

Цель изобретени  - одновременна  защита стали от коррозии в кислой среде и в растворе хлористого натри .The purpose of the invention is the simultaneous protection of steel against corrosion in an acidic medium and in a solution of sodium chloride.

Дл  достижени  этой цели в качестве ингибитора примен ют алифатические имины общей формулы RCH NR где R и R- алкил.To achieve this goal, aliphatic imins of the general formula RCH NR are used as the inhibitor, where R and R are alkyl.

В качестве ингибиторов атмосферной коррозии стали мо1Ч г быт1) применены К-бутилидепаллнламин () и N-.этилиденбутиламии (И). В качестве ингибиторов коррозии стали в растворах хлористо о натри  и сол ной кислоты эффективны Ы-бутилндеиаллиламии, N-этилиден бутила ми и и К-//з« -бу1ил иденизобутепила .м и II (I I).As an inhibitor of atmospheric corrosion of steel m1ch g byt1), K-butylideplamine () and N-ethylidenebutylamine (I) were used. As inhibitors of corrosion of steel in solutions of sodium chloride and hydrochloric acid, N-ethylbenyl and allylamine, N-ethylidene butyl and and K are effective // z3-bu1il anddenisobuteyl and m (II) I.

Данные исиытаииП, в которых в качестве металла используетс  Ст. 3, приведены в таблице .IsytaiP data, in which Art. 3 are shown in the table.

В атмосферных услови х выщеуказанные имииы полностью защищают сталь от коррозии . Образцы после 3-5 мес цев испытаний сохран ют блест щую, непораженную поверхность .In atmospheric conditions, the above mentioned chemicals completely protect steel from corrosion. Samples after 3-5 months of testing retain a shiny, unaffected surface.

В растворе хлористого натри  имины уменьщают скорость коррозии стали в 2-4 раза,In a solution of sodium chloride, imines reduce the corrosion rate of steel by 2–4 times,

Использземый иминImine used

1()|„-111)111 раствор НС1 с дооавкоЛ 0,5% имппа1 () | „-111) 111 HC1 solution with additional 0.5% imp

10ten

3%-Hbiii раствор NaCI с добанко: 1% имIIна3% -Hbiii solution NaCI with dobanko: 1% imIIna

Claims (1)

при этом заг-цитный эффект достигает 65- 85%. За 168 ч испытани  контрольные образцы покрываютс  рыхлым слоем ржавчины. Поверхность образцов, наход щихс  в растворе с добавкамн иминов, остаетс  блест щей. 3 Формула изобретени  Способ защиты стали от атмосферной коррозии с помощью ингибитора аминного типа, отличающийс  тем, что, с целью одновре- 5 4 менной защиты в кислой среде и в растворе хлористого натри , в качестве ингибитора примен ют алифатические имины общей формулы RCH NR где R и R - алкил. at the same time, the caption effect reaches 65-85%. Over 168 hours of testing, control samples are covered with a loose layer of rust. The surface of the samples in solution with added imines remains shiny. 3 The claims of the method of protecting steel against atmospheric corrosion with an amine-type inhibitor, characterized in that, for the purpose of simultaneous protection in an acidic medium and in sodium chloride solution, aliphatic imines of the general formula RCH NR where R and R is alkyl.
SU7001401869A 1970-01-28 1970-01-28 Method of protecting steel from atmospheric corrosion SU318315A1 (en)