SU182890A1 - DEFORMABLE WELDABLE ALLOY BASED ON TITANIUM - Google Patents

DEFORMABLE WELDABLE ALLOY BASED ON TITANIUM

Info

Publication number
SU182890A1
SU182890A1 SU899231A SU899231A SU182890A1 SU 182890 A1 SU182890 A1 SU 182890A1 SU 899231 A SU899231 A SU 899231A SU 899231 A SU899231 A SU 899231A SU 182890 A1 SU182890 A1 SU 182890A1
Authority
SU
USSR - Soviet Union
Prior art keywords
titanium
deformable
alloy based
weldable alloy
alloy
Prior art date
Application number
SU899231A
Other languages
Russian (ru)
Original Assignee
С. Г. Глазунов, В. Н. Моисеев, А. М. Чиненое
ПЛТЕИШ , С. МГС цоэ
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by С. Г. Глазунов, В. Н. Моисеев, А. М. Чиненое, ПЛТЕИШ , С. МГС цоэ filed Critical С. Г. Глазунов, В. Н. Моисеев, А. М. Чиненое
Priority to SU899231A priority Critical patent/SU182890A1/en
Application granted granted Critical
Publication of SU182890A1 publication Critical patent/SU182890A1/en

Description

Известны деформируемые сплавы на основе титапа, содержащие молибден и алюминий. Например, термически-упрочн емый деформируемый силав содержит 6,5-7,5% молибдена, 2,5-3,5% алюмини , 10-11,5% хрома и остальное титан. Этот сплав обладает значительной жаропрочностью (до 500° С) при выдержке 30 мин.Known wrought alloys based on titapa containing molybdenum and aluminum. For example, a heat-hardening wrought sila contains 6.5-7.5% molybdenum, 2.5-3.5% aluminum, 10-11.5% chromium, and the rest titanium. This alloy has significant heat resistance (up to 500 ° C) at a shutter speed of 30 minutes.

Дл  повышени  жаропрочности предлагаетс  сплав па основе титана, содержащий 25- 30% молибдена, 2-5% ниоби  и 0,1-3% алюмини . Описываемый сплав имеет высокие характеристики кратковременной прочности при температуре до 1000° С, хорошо свариваетс , легко деформируетс  в гор чем и холодном состо ни х. Например, предел прочности плоского образца толщиной 0,6 мм за врем  от 20 до 300 сек прн 1000° С равен 10,3 кг/мм, сварпой шов но прочности и пластичности равноценен основному металлу, способен прокатыватьс  в тонкую ленту и фольгу с деформацией 50-70% между отжигами.To increase the heat resistance, titanium-based alloy is proposed, containing 25-30% molybdenum, 2-5% niobium and 0.1-3% aluminum. The described alloy has high characteristics of short-term strength at temperatures up to 1000 ° C, welds well, easily deformed in hot and cold conditions. For example, the tensile strength of a flat specimen with a thickness of 0.6 mm for a time from 20 to 300 sec. Of 1000 ° C is equal to 10.3 kg / mm, the weld and strength and ductility are equivalent to the base metal, capable of rolling into a thin tape and foil with a deformation of 50 -70% between anneals.

Сплав в отожженном состо нии нри комнатной температуре имеет предел прочности (в листах толщиной 0,6-1,2 льи) 92-97 кг1мм-, (в прутках диаметром 12 мм) 81-86 KBIMM, предел текучести соответственно 91-96 кг1ммп ВО-85 /сг/льиз и относительное удлинение и 19-24%.The alloy in the annealed condition at room temperature has a tensile strength (in sheets with a thickness of 0.6-1.2 li) 92-97 kg1mm-, (in rods with a diameter of 12mm) 81-86 KBIMM, yield strength, respectively 91-96 kg1mm VO -85 / sg / liiz and relative lengthening and 19-24%.

Предмет и з о б р е т е м и  Subject and reference

Деформируемый свариваемый сплав на осliOBe титана, содержащий молибден и алюмием , Deformable weldable alloy on osliOBe titanium containing molybdenum and aluminum,

что, с целью повышеимеет следующий хнон %,)that, in order to increase the following khon%,)

25-3025-30

0,1-3 2-5 остальное0.1-3 2-5 the rest

SU899231A 1964-05-09 1964-05-09 DEFORMABLE WELDABLE ALLOY BASED ON TITANIUM SU182890A1 (en)