SU1603822A1 - METHOD OF CHEMICAL-THERMAL TREATMENT OF METAL PRODUCTS - Google Patents

METHOD OF CHEMICAL-THERMAL TREATMENT OF METAL PRODUCTS

Info

Publication number
SU1603822A1
SU1603822A1 SU4641339/02A SU4641339A SU1603822A1 SU 1603822 A1 SU1603822 A1 SU 1603822A1 SU 4641339/02 A SU4641339/02 A SU 4641339/02A SU 4641339 A SU4641339 A SU 4641339A SU 1603822 A1 SU1603822 A1 SU 1603822A1
Authority
SU
USSR - Soviet Union
Prior art keywords
metal products
alloying
chemical
composition
thermal treatment
Prior art date
Application number
SU4641339/02A
Other languages
Russian (ru)
Inventor
В.И. Люленков
В.С. Чалков
А.С. Шинкаренко
Original Assignee
Сибирский металлургический институт им. Серго Орджоникидзе
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Сибирский металлургический институт им. Серго Орджоникидзе filed Critical Сибирский металлургический институт им. Серго Орджоникидзе
Priority to SU4641339/02A priority Critical patent/SU1603822A1/en
Application granted granted Critical
Publication of SU1603822A1 publication Critical patent/SU1603822A1/en

Abstract

Способ химико-термической обработки металлических изделий, включающий контакт легирующего состава с обрабатываемым изделием при нагреве, отличающийся тем, что, с целью интенсификации процесса насыщения, сокращения энергетических затрат, повышения износостойкости, контакт легирующего состава с обрабатываемой поверхностью осуществляют в локальной зоне, при этом легирующий состав вносят в зону обработки по касательной к поверхности изделия со скоростью от 90 до 150 м/с под давлением 0,12-40 МПа и при перемещении зоны обработки по поверхности изделия со скоростью от 1 до 200 м/с.The method of chemical heat treatment of metal products, including the contact of the alloying composition with the processed product during heating, characterized in that, in order to intensify the saturation process, reduce energy costs, improve wear resistance, the alloying composition contacts the treated surface in the local zone, while the alloying the composition is introduced into the treatment area tangentially to the surface of the product at a speed of from 90 to 150 m / s under a pressure of 0.12-40 MPa and when moving the treatment area over the surface products with speeds from 1 to 200 m / s.

SU4641339/02A 1989-01-25 1989-01-25 METHOD OF CHEMICAL-THERMAL TREATMENT OF METAL PRODUCTS SU1603822A1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
SU4641339/02A SU1603822A1 (en) 1989-01-25 1989-01-25 METHOD OF CHEMICAL-THERMAL TREATMENT OF METAL PRODUCTS

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
SU4641339/02A SU1603822A1 (en) 1989-01-25 1989-01-25 METHOD OF CHEMICAL-THERMAL TREATMENT OF METAL PRODUCTS

Publications (1)

Publication Number Publication Date
SU1603822A1 true SU1603822A1 (en) 2011-05-10

Family

ID=60520058

Family Applications (1)

Application Number Title Priority Date Filing Date
SU4641339/02A SU1603822A1 (en) 1989-01-25 1989-01-25 METHOD OF CHEMICAL-THERMAL TREATMENT OF METAL PRODUCTS

Country Status (1)

Country Link
SU (1) SU1603822A1 (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
RU2466002C1 (en) * 2011-06-01 2012-11-10 Государственное образовательное учреждение высшего профессионального образования "Сибирский государственный индустриальный университет" Method of making wear resistant flat surface of friction pairs

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
RU2466002C1 (en) * 2011-06-01 2012-11-10 Государственное образовательное учреждение высшего профессионального образования "Сибирский государственный индустриальный университет" Method of making wear resistant flat surface of friction pairs

Similar Documents

Publication Publication Date Title
FR2396250A1 (en) NEW PROCESS FOR THE TREATMENT OF THERMOSENSITIVE MATERIALS
GB1365180A (en) Surface hardening
SU1603822A1 (en) METHOD OF CHEMICAL-THERMAL TREATMENT OF METAL PRODUCTS
ZA835377B (en) Quenching bath and quenching method for metals
Li Vanadizing and Post-Treating of Screw Die
Kalita Mullite-- Corundum Articles for Post-Tapping Treatment and Continuous Steel Casting
Bauer Low-Cost Heat Treatment of Tools and Components in a Vacuum
Kulikov Hardening of Steels and Irons by Surface Passivation and Heat Treatment[[Previously Titled: Hardening of Steels and Cast Irons by Passivation of Their Surface and Heat Treatment.]]
Gosset et al. Quenching Bath and Quenching Method for Metals
Wilhelmsson Special Stainless Steels for the Process Industry. II
Kulikov Hardening of Steels and Irons by Surface Passivation and Heat Treatment
Chang et al. The Heat Treatment of M 42 High-Speed Steel
Hua Athermal Thermochemical Treatment
Laverroux Forming of Stainless Steels by Wire Drawing
Wang et al. Study on Improving the Thermo-Fatigue Resistance of HM 3 Steel
JPS56156712A (en) Cooling method of metallic band in continuous heat treatment line
Neiderman High Pressure Gas Quenching of Tool Steels in Vacuum.(Abstract Only)
von Hagen et al. Method for Hardening a Hollow Article
ES2142440T3 (en) METHOD FOR TREATING THE IRONING SURFACE OF THE BASE OF AN IRON.
Geiger Amelioration of the Surface Quality of NF-Metal Products and Fine Metallurgical Articles
Bystricky et al. Brittleness of Nitrided Parts and Its Causes
Chen et al. Investigation on the technique of delay quenching after forging
Natarajan et al. Some Aspects of Hot Dip Galvanising of Tubes--Experience at Tata Steel
Ma et al. Analysis for the Corrosion of Workpieces Treated by Salt Bath
Puozzo et al. Method for Preparing Large Cast Iron Dies, Particularly for Vehicle Sheet Metal Pressing, and the Apparatus for Its Implementation