Известно, что при пенистом обогащении, к суспензи м тонко измельченной руды примешивают незначительное количество нредохранительпого коллоидного реагента, как-то: крахмала, альбумина, кле , декстрина или сапонина.It is known that in a frothy enrichment, an insignificant amount of preservative colloidal reagent, such as starch, albumin, glue, dextrin or saponin, is added to the suspensions of finely ground ore.
Предлагаетс использовать коллоидный раствор крахмала в качестве разрушител пены при обезвоживании серных концентратов. При этом крахмал выполн ет роль селективного депрессора или каогул нта.It is proposed to use a colloidal starch solution as a foam breaker when dehydrating sulfur concentrates. At the same time, starch acts as a selective depressor or caogulta.
Способ применени крахмала в качестве разрушител иены при флотации руд самородной серы заключаетс в следующемКоллоидный раствор крахмала с концентрацией 1-2% добавл ют в серный флотационный концентрат в количестве 0,15-0,2 кг на TOHHV иЪеремешивают в течение 5 минут.The method of using starch as a destroyer of yen in the flotation of native sulfur ores is as follows. A colloidal solution of starch with a concentration of 1-2% is added to sulfur flotation concentrate in an amount of 0.15-0.2 kg per TOHHV and stirred for 5 minutes.
В результате разрушени пены почти в 10 раз снижаютс потери твердого остатка со сливом сгустител , и при этом по вл етс возможность использовани этого слива в качестве оборотной воды, что приводит к уменьшению затрат на воду. Кроме того, повышаетс удельна производительность сгустител и насосов, перекачивающих концентратную пульпу.As a result of the destruction of the foam, the loss of solid residue with a thickener discharge decreases by almost 10 times, and it becomes possible to use this drain as recycled water, which reduces the cost of water. In addition, the specific productivity of the thickener and pumps pumping concentrate pulp is increased.
Предмет изобретени Subject invention
Способ разрушени пены серных концентратов с помощью реагентов , отличающийс тем, что, с целью разрушени пены серных концентратов , в качестве реагента примен ют крахмал.A method of breaking up sulfur concentrate concentrates using reagents, characterized in that starch is used as a reactant to destroy the foam concentrates of sulfur.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
SU654938A SU134218A1 (en) | 1960-02-16 | 1960-02-16 | Method of breaking sulfur concentrates foam using reagents |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
SU654938A SU134218A1 (en) | 1960-02-16 | 1960-02-16 | Method of breaking sulfur concentrates foam using reagents |
Publications (1)
Publication Number | Publication Date |
---|---|
SU134218A1 true SU134218A1 (en) | 1960-11-30 |
Family
ID=48405193
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
SU654938A SU134218A1 (en) | 1960-02-16 | 1960-02-16 | Method of breaking sulfur concentrates foam using reagents |
Country Status (1)
Country | Link |
---|---|
SU (1) | SU134218A1 (en) |
-
1960
- 1960-02-16 SU SU654938A patent/SU134218A1/en active
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB996220A (en) | Improvements in and relating to ores | |
ES445703A1 (en) | Recovery of lead, zinc and iron sulfide | |
PE20030700A1 (en) | OXIDATION UNDER PRESSURE AND HIGH TEMPERATURE OF MINERALS AND MINERAL CONCENTRATES CONTAINING SILVER, USING CONTROLLED PRECIPITATION OF SULPHATE SPECIES | |
SU134218A1 (en) | Method of breaking sulfur concentrates foam using reagents | |
US2364777A (en) | Concentration of oxidized iron ores | |
GB1041439A (en) | Improvements in or relating to the froth flotation of phosphates from phosphate ores | |
Lovell | Industrial flotation reagents | |
US2000350A (en) | Froth flotation process for oxide ores | |
DE1404877C2 (en) | Liquid feeder | |
SU125773A1 (en) | The method of flotation of ores | |
US2570119A (en) | Recovery of carnotite from its ores | |
SU140002A1 (en) | Method of flotation concentration of polymetallic ores | |
SU77571A1 (en) | The method of selective flotation of sulfide ores | |
GB2012621A (en) | Concentration of coal by froth flotation | |
SU63909A1 (en) | Method of flotation beneficiation of copper-molybdenum ore | |
PE20001220A1 (en) | IMPROVED REACTOR | |
MUKAI et al. | Effect of Sulfurous Acid on the Floatability of Sulfide Minerals | |
SU476026A1 (en) | The method of flotation of fluorite ores | |
SU694220A1 (en) | Frothing agent for flotation of sulphide antimony ores | |
CY251A (en) | Process for the froth flotation of sulphide ores | |
SU118472A1 (en) | The method of obtaining pyrite concentrates from the tailings of copper and zinc flotation | |
SU135841A1 (en) | The method of flotation of pyrochlore ores | |
GB798768A (en) | Process of concentrating niobium minerals by froth flotation | |
SU668709A1 (en) | Collector for flotation recovery of clay slime from potassium-containing ores | |
SU123481A1 (en) | The method of flotation of ores |