SU126736A1 - Combined mine hammer mill - Google Patents

Combined mine hammer mill

Info

Publication number
SU126736A1
SU126736A1 SU632748A SU632748A SU126736A1 SU 126736 A1 SU126736 A1 SU 126736A1 SU 632748 A SU632748 A SU 632748A SU 632748 A SU632748 A SU 632748A SU 126736 A1 SU126736 A1 SU 126736A1
Authority
SU
USSR - Soviet Union
Prior art keywords
mill
particles
hammer mill
combined
combined mine
Prior art date
Application number
SU632748A
Other languages
Russian (ru)
Inventor
С.К. Соболев
Original Assignee
С.К. Соболев
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by С.К. Соболев filed Critical С.К. Соболев
Priority to SU632748A priority Critical patent/SU126736A1/en
Application granted granted Critical
Publication of SU126736A1 publication Critical patent/SU126736A1/en

Description

Д.1  тонкого изме.1ьчеи11  минерального сырь  примен ют комбинированные шахтные молотковые А елы1нцы. Недостаток известных подобных мельниц состоит в том, что они не обеспечивают возможности измельчени  в зких материалов и их классификации в шахте мельницы.Dia. 1 of a thin dimension. 1 11 of the mineral raw material is used in combined mine hammer hammers. A disadvantage of such known mills is that they do not provide the possibility of grinding viscous materials and their classification in the mine of the mill.

В предлагаемой мельнице шахта снабжена разделительной перегородкой , за которой установлен наклонный грохот с воронкой дл  вывода из мельницы подрешетного продукта, прошедшего через перегородку под действием воздушного потока, и предохранени  от выбрасывани  из ельницы недостаточно измельченных частиц.In the proposed mill, the shaft is provided with a dividing partition, behind which an inclined screen with a funnel is installed to remove the undersize product from the mill that has passed through the partition under the action of the air flow and to prevent insufficiently crushed particles from being ejected from the mill.

На чертеже изображена предлагаема  мельница в двух проекци х.The drawing shows the proposed mill in two projections.

Материал, предназначенный дл  измельчени , подаетс  питателем / из бункера 2 в молотковую мельницу 3 где измельчаетс  и центробежной силой, возникшей при вращении ротора, выбрасываетс  в полость 4 комбинпрованной шахты-сепаратора. Чем крупнее частицы, выбрасываемые в шахту, тем больший запас кинетической эпергип она имеет. Нри движении частиц вверх эта энерги  затрачиваетс  на преодоление сопротивлени  воздушной среды, которое зависит от массы частиц. В результате мелкие частицы расходуют свою кинетическую энергию быстрее , чем крупные, и падают обратпо па молотки. В иолость 5 шахты попадают , главным образом, наиболее крупные частицы, отбрасываемые от верхней части шахты и те наиболее мелкие частицы, скорость витани  которых меньше скорости воздушного потока, движущегос  вверх в по .тости 4 шахты. На пути движени  смеси крупных и мелких частиц в полости о установлено наклонное сито 6 с крупными  чейками. Частицы с размером большим, чем  чейки сита б, скатываютс  на молотки, а мелка  фракци  поступает в коллектор 7 и ссыпаетс  в дл  изме,1ьченпого материалаThe material to be crushed is supplied by the feeder / from the hopper 2 to the hammer mill 3 where it is crushed and the centrifugal force generated by the rotation of the rotor is thrown into the cavity 4 of the combined separator shaft. The larger the particles emitted into the mine, the more kinetic epergip it has. As the particles move upward, this energy is expended to overcome the resistance of the air medium, which depends on the mass of the particles. As a result, small particles spend their kinetic energy faster than large ones, and the hammers reverse. Most of the largest particles, dropped from the upper part of the mine, and those smallest particles, whose soar speed is less than the speed of the air flow moving upwards in part 4 of the mine, get into the iolost 5 of the shaft. On the way of the mixture of large and small particles in the cavity o, an inclined sieve 6 with large cells was installed. Particles larger than the sieves of the b screen are rolled into hammers, and the fine fraction is fed to the collector 7 and poured into for measuring the desired material

Размер- чеек сита намного превышает диаметр отвеиваемых частиц вследствие чего ие происходит его замазывани . Высота перегородки 8 должна быть такой, чтобы через нее могли быть переброшены лишь-частицы с размером, большим, чем  чейки сита.The mesh size of the sieve is much larger than the diameter of the particles to be scaled, as a result of which it is not smeared. The height of the partition 8 must be such that only particles with a size larger than the sieve cells can be transferred through it.

П р е д м е т и з о б р е т е и и  PRIOR DIRECTORSHIP and

Комбинированна  шахтна  молоткова  мельница дл  тонкого из мельчеии  минерального сырь , отличаюша с  тем, что, с целью обеспечени  возможности измельчени  в зких материалов и их кчассификации в шахте мельницы, шахта снабжена разделительной перегородкой , за которой установлен наклонный грохот с воронкой дл  вывода т мельницы подрешетного продукта, выносимого потоком воздуха через перегородку, а также предохранени  от выбрасывани  из мельницы нодостаточно измельченных частииA combined hammermill shaft for finely mined minerals is different in that, in order to allow grinding of viscous materials and their crushing in the mill shaft, the shaft is equipped with a dividing partition, behind which an inclined screen with a funnel is installed to output a mill pit of the undersize product carried by the air flow through the septum, as well as protection from ejection of the crushed parts from the mill

SU632748A 1959-07-03 1959-07-03 Combined mine hammer mill SU126736A1 (en)