SU1240450A1 - Способ обогащени руд - Google Patents

Способ обогащени руд Download PDF

Info

Publication number
SU1240450A1
SU1240450A1 SU843808445A SU3808445A SU1240450A1 SU 1240450 A1 SU1240450 A1 SU 1240450A1 SU 843808445 A SU843808445 A SU 843808445A SU 3808445 A SU3808445 A SU 3808445A SU 1240450 A1 SU1240450 A1 SU 1240450A1
Authority
SU
USSR - Soviet Union
Prior art keywords
separation
class
dolomite
magnetic separation
heavy
Prior art date
Application number
SU843808445A
Other languages
English (en)
Inventor
Вадим Борисович Кусков
Елена Николаевна Дмитрук
Original Assignee
Ленинградский Ордена Ленина,Ордена Октябрьской Революции И Ордена Трудового Красного Знамени Горный Институт Им.Г.В.Плеханова
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Ленинградский Ордена Ленина,Ордена Октябрьской Революции И Ордена Трудового Красного Знамени Горный Институт Им.Г.В.Плеханова filed Critical Ленинградский Ордена Ленина,Ордена Октябрьской Революции И Ордена Трудового Красного Знамени Горный Институт Им.Г.В.Плеханова
Priority to SU843808445A priority Critical patent/SU1240450A1/ru
Application granted granted Critical
Publication of SU1240450A1 publication Critical patent/SU1240450A1/ru

Description

Изобретение относитс  к обогаще- нию полезных ископаемых и может быть использовано при обогащении руд, содержащих компоненты, различающиес  по плотности и по пористости.
Целью изобретени   вл етс  сниже - ние стоимости обогащени  руд, содержащих флюорит и доломит, с одновременным повышением извлечени  полезного ксЛшонента.
Способ осуществл ют следующим образом .
Материал раздел ют на классы крупнее и мельче 1,5-2 мм, обрабатывают крупный класс керосином в количестве 500-1500 г/т пористого компонента (доломита) и обогащают в т желой жидкости . Мелкий класс обрабатывают рас вором хлорного железа в количестве 1000-2000 г/т пористого компонента в контактном чане и всю получившуюс  суспензию направл ют на магнитную сепарацию в сильном поле.
Пример. Обогащению, подвергались хвосты ручной рудоразборки одРедактор Н. Горват Заказ 3426/4
Составитель Е.Киселева Техред О.Гортвай
Тираж 514 ВНИИПИ Государственного комитета СССР
по делам изобретений и открытий 113035, Москва, Ж-35, Раушска  наб., д. 4/5 .
Производственно-полиграфическое предпри тие, г. Ужгород, ул. Проектна , 4
ного из флюоритовык месторождений, содержащие 57,44% флюорита и 40,49% доломита. Руда рассеивалась на классы крупнее и мельче 1,5 мм, обрабатывалась указанными реагентаьда и. подвергалась магнитной и т желосредней сепарации в т желой жидкости М-45.
При обогащении руд, содержащих пористые компоненты, в т желой жидкости , больщое количество жидкости тер етс  за счет проникновени  в поры . При обработке материала керосином он обволакивает пористые частицы и закупоривает поры. Это преп тствует проникновению жидкости в поры, ,что дает возможность сэкономить большое количество т желой жидкости.
20
При обработке мелкого класса раствором хлорного железа последнее проникает в поры и делает пористые частицы магнитными, что дает возможность раздел ть материал путем магнитной 25 сепарации..
Корректор И.Эрдейи Подписное

Claims (1)

  1. СПОСОБ ОБОГАЩЕНИЯ РУД, включающий классификацию с последующими тяжелосредным разделением Одного класса и магнитной сепарацией другого класса, отличающийся тем, что, с целью снижения стоимости обогащения руд, содержащих флюорит и доломит, с одновременным повышением- качества концентрата и извлечения полезных компонентов, перед тяжело·» средним разделением руду обрабатывают керосином, а перед магнитной сепарацией - раствором хлорного железа.
    с 9
SU843808445A 1984-10-31 1984-10-31 Способ обогащени руд SU1240450A1 (ru)