SU1138189A1 - Method of flotation clayish-carbonate slime from potassium ores - Google Patents

Method of flotation clayish-carbonate slime from potassium ores Download PDF

Info

Publication number
SU1138189A1
SU1138189A1 SU833621266A SU3621266A SU1138189A1 SU 1138189 A1 SU1138189 A1 SU 1138189A1 SU 833621266 A SU833621266 A SU 833621266A SU 3621266 A SU3621266 A SU 3621266A SU 1138189 A1 SU1138189 A1 SU 1138189A1
Authority
SU
USSR - Soviet Union
Prior art keywords
collector
radical
carbon atoms
flotation
alkyl sulfates
Prior art date
Application number
SU833621266A
Other languages
Russian (ru)
Inventor
Евгений Иванович Щербина
Евгения Ивановна Грушова
Витольд Яковлевич Юшков
Виктор Владимирович Бочаров
Галина Владимировна Жевжик
Афанасий Егорович Фролов
Татьяна Степановна Шаститко
Галина Дмитриевна Кудинова
Александр Николаевич Моргунов
Анатолий Ефимович Поляков
Original Assignee
Белорусский Ордена Трудового Красного Знамени Технологический Институт Им.С.М.Кирова
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Белорусский Ордена Трудового Красного Знамени Технологический Институт Им.С.М.Кирова filed Critical Белорусский Ордена Трудового Красного Знамени Технологический Институт Им.С.М.Кирова
Priority to SU833621266A priority Critical patent/SU1138189A1/en
Application granted granted Critical
Publication of SU1138189A1 publication Critical patent/SU1138189A1/en

Abstract

СПОСОБ ФЛОТАЦИИ ГЛИНИСТОКАРБОНАТНЫХ ШЛАМОВ ИЗ КАЛИЙНЫХ. РУД, включающий последовательную обработку пульпы собирателей на основе оксиэтилированного спирта и флокул нтом - водным раствором полиакриламида , отличающийс  тем, что, с целью повьшени  селективности путем снижени  потерь хлористого кали  в шламовом продукте, собиратель дополнительно содержит триэтаноламиновую соль синтетических жирных кислот с числом атомов углерода в радикале 7-9 и алкилсульфаты с числом атомов углерода в радикале 10-18 при соотношении компонентов, мас.%: (Л Триэтаноламинова  соль синтетических жирных кислот с числом атомов углерода в радикале 7-9 60-80 Алкилсульфаты с числом атомов углерода в радикале 10-18 15-30 со Оксиэтилированный 00 спирт5-10 00 соMETHOD OF FLOTATION OF CLINIC AND CARBONATE SLUDGE FROM POTASSIUM. ORE, including the sequential processing of collector pulp based on ethoxylated alcohol and flocculant - aqueous solution of polyacrylamide, characterized in that, in order to increase selectivity by reducing potassium chloride losses in the slurry product, the collector additionally contains a triethanolamine salt of synthetic fatty acids with carbon atoms radicals 7-9 and alkyl sulfates with the number of carbon atoms in radical 10-18 with a ratio of components, wt.%: (L Triethanolamine salt of synthetic fatty acid t with the number of carbon atoms in the radical 7-9 60-80 Alkyl sulfates with the number of carbon atoms in the radical 10-18 15-30 with ethoxylated 00 alcohol 5-10 00 with

Description

.1 Изобретение относитс  к области обогащени  полезных ископаемых флотационным методом и может быть использовано на предпри ти х, перерабатывающих калийсодержащие руды, Известно применение в качестве собирател  ij глинисто-карбонатных шламов из калийсодержащих руд эмуль сии, содержащей жировой гудрон, под мыльный щелок, неионогенный змульга тор (преимущественно оксиэтилированные алкилфенолы, кислоты, спирты или диэтаноламиды) при следующем соотношении компонентов, мае.%: Жиррвой гудрон 2-10 Неионогенный эмульгатор1-5 Подмыльиый щелок 20-50 ВодаОстальное Однако использование известного собирател  не позвол ет достаточно полно и селективно выдел ть глинисто-карбонатные шламы из руд. Известен процесс выделени  пшамов из руд с использованием в качестве .собирател  коллоида на базе кр мала или целлюлозы 2J . Однако указанные реагенты  вл ют с  дефицитными и дорогосто щими и не обеспечивают высокой эффективнос ти шламовой флотации. Известен процесс флотации глинис то-карбонатных шламов из руд с прим нением водного раствора полиакрилам да (промьшлснный процесс) з. Однако применение данного реаген та ие обеспечивает высокой селектив ности процесса. Кроме того, высоки потери хлористого кали  со шламовым продуктом. Наиболее близким по технической сущности и достигаемому результату к предлагаемому  вл етс  способ фло тации глинисто-карбонатных шламов из калийных руд, включающий последовательную обработку пульпы собира телем на основе оксиэтилированного спирта и флокул нтом - водным раствором полиакриламида. Структурна  формула собирател  на основе оксиэтилированного спирта (синтанол ДС . RO(CH2CHjO)H, где R - алкильньй остаток; II - число оксиэтилированных групп. Дл  ДС-10.число атомов С в алг кильном остатке 10-18, число оксиэтилированных групп 10 4 . 91 Однако известный собиратель ьз обеспечивает высокой селективности процесса. Кроме того, высоки потери хлористого ка.аи  со шламовым продуктом . Цель изобретени  - повьшение селективно,сти путем снижени  потерь хлористого кали  в шламовом продукте . Поставленна  цель достигаетс  тем, что согласно способу флотации глинисто-карбонатных шламов из калийных руд, включающему последовательную обработку пульпы собирателем на основе оксиэтилированного спирта и флокул нтом - водным раствором полиакриламида, собиратель дополнительно содержит триэтаноламиновую соль синтетических жирных кислот с числом атомов углерода в радикале 7-9 и алкилсульфаты с числом атомов углерода в радикале I0jl8 при соотношении компонентов , мас.%: Триэтаноламинова  соль синтетических жирных кислот с чис- лом атомов углерода в радикале 7-9 60-80 Алкилсульфаты с числом атомов углерода в радикале 10-18 15-30 Оксиэтилированный спирт5-10 Триэтаноламинова  соль синтетических жирных кислот с числом атомов углерода в радикале 7-9 - жидкость или паста светло-коричневого цвета, хорошо растворима в воде. Известно ее применение в производстве моющих средств. Алкилсульфаты формулы О S О, Na, где n 0-18j- паста от белого до светло-коричневого цвета, хорошо растворима в воде, нетоксична. Известно применение алкилсульфатов в производстве бытовых и технических моющих средств. Оксиэтилированньм спирт формулы (C,)H, где п 10-13 . жидкость или паста от белого до желтого цвета, хорошо растворима в воде , Известно применение оксиэтилиро ванного спирта в качестве эмульгатора , стабилизатора пены. Собиратель дл  флотации шламов, содержащий триэтаноламиновую соль синтетических жирных кислот с числом атомов углерода в радикале 7-9,. 3 алкилсульфаты с числом атомов угле рода в радикале 10-18 и оксиэтилированный спирт, получают путем сме шени  его компонентов при 40-50 С. Применение указанной смеси в качестве собирател  глинисто-карбонатных шламов из калийсодержащих руд неизвестно. Способ осуществл ют следующим о разом. Измельченную руду измельчают до крупности -0,8+0 мм, оттирают 20 мин при , затем разбавл  ют пульпу до ,5 и обрабатываю последовательно собирателем и флокул нтом и флотируют хлористьй калий . Предлагаемый собиратель испытан в лабораторных услови х при флотации глинисто-карбонатных шламов из калийсодержащей руды Старобинского месторождени . Пример 1. Калийсодержащую РУДУ в составе которой присутству ет 25,6 мас.% хлористого кали  и 3,48 мас.% нерастворимого остатка (и.о. крупностью -0,8-0), оттирают 20 мин при . Затем пульпу разбавл ют до ,5 и обрабатывают последовательно вначале собирателем а затем флокул нтом, например 1%-ны водным раствором полиакриламида. Собиратель, например 1%-ный раствор смеси, включает, мас.%; триэтанолам нова  соль синтетических жирных кис лот 80; алкилсульфаты 15; оксиэтили рованный спирт 5. Расход собирател  60 г на 1 т перерабатываемой руды. Расход полиакриламида (ПАА) 20 г на 1 т перерабатываемой руды. Врем  ко тактировани  с собирателем 60 с, с ПАА 30 с. Флотацию осуществл ют в течение с. Пример 2, Щпамовую флотаци осуществл ют аналогично примеру 1. Собиратель содержит, мас.%: триэтан аминова  соль синтетических жирных кислот 70; алкилсульфаты 20; оксиэтилированный срирт 10. Расход собирател  100 г на 1 т руды, т.е. 0,01% от количества перерабатываемой руды. Пример 3, Шламовую флотацию осуществл ют аналогично примеру 1. Собиратель содержит, мас.%: триэтаноламинова  соль синтетических жирных кислот 60; алкилсульфаты 30; оксиэтилированный спирт 10. Рас ход собирател  150 г на 1 т руды, 894 т.е. 0,015 нас..7, от количества флотируемой калийсодержащей руды. Пример 4. Шламовую флотацию осуществл ют аналогично примеру . Собиратель содержит, мас.%: триэтаноламинова  соль синтетических жирных кислот 75; алкилсульфаты 18, оксиэтилированный спирт 7. Расход собирател  180 г на 1т руды, т.е. 0,018 мас.% от количества перерабатываемой руды. Примеры 5 и 6 аналогичны i-4. Пример 7 (известный собиратель ) . Шламовую флотацию осуществл ют аналогично примеру 1. Собиратель - синтанол ДС-10. Расход собирател  125 г на I т руды, т.е. 0,0125 мас.% от количества перерабатьшаемой руды. В таблице представлены показатели , характеризующие эффективность предлагаемого (принтеры 1-6) и известного (пример 7) собирателей дл  флотации щламов. Согласно данным таблицы применение предлагаемого собирател  в сравнении с известным.позвол ет повысить содержание,нерастворимого остатка в ашамовом продукте с 61,5 до 64,5%, а степень извлечени  с 50,0 до 52,1%. При этом содержание хлористого кали  в щламовом продукте и извлечение (т.е. потери хлористого кали ) уменьщаютс  с 7,89 (прототип ) до 5,43-6,11%, т.е. VB 1,4 раза, и с 0,87 до 0,59-0,66%, т.е. Б v-1,3-1,5 раза, соответственно. Селективность щламовой флотации, рассчитанна  согласно (.1) при использовании предлагаемого собирател  0,986-0,988, а известного - ниже 0,983. Использование составов собирател , ВЫКОДЯ1ЦИХ за предлагаемые пределы , нецелесообразно. Так, например , если собиратель содержит, мас..%: триэтаноламинова  соль синтетических жирных кислот 85, алкилсульфаты 12, оксиэтилированный спирт 3, и его расход 50 г на.1т руды (пример 5), то содержание н.о. в шламовом продукте 58,5%, т.е. ниже, чем в известном способе. При расходе собирател  200 г на 1 т руды и при содержании в нем, мас.%: триэтаноламинова  соль синтетических жирных кислот 50, алкилсульфаты 35, оксиэтилированный спирт 15 (пример 6), содержание хлористого кали  в шламовом продук-те 9,8%..1 The invention relates to the field of enrichment of minerals by the flotation method and can be used in plants that process potassium-containing ores. It is known to use clay-carbonate sludge from potassium-containing ores of emulsion containing fatty tar, soap lye, non-ionic pulp, as collector ij torus (predominantly ethoxylated alkylphenols, acids, alcohols or diethanolamides) in the following ratio of components, may.%: fatty tar 2-10 non-ionic emulsifier1-5 lymphocyan liquor 20-50 Water Remaining However, the use of a known collector does not allow sufficiently complete and selective extraction of clay-carbonate sludge from ores. The process of isolating psham from ores using a crloid-based colloid or cellulose 2J is known. However, these reagents are scarce and expensive and do not provide high efficiency slurry flotation. The process of flotation of clay-to-carbonate sludges from ores is known, with the use of an aqueous solution of polyacrylates and the industrial process. However, the use of this reagent ensures high selectivity of the process. In addition, the loss of potassium chloride with a slurry product is high. The closest in technical essence and the achieved result to the proposed is the method of flotation of clay-carbonate sludge from potash ores, including the sequential processing of the pulp with a collection based on ethoxylated alcohol and flocculant - aqueous solution of polyacrylamide. The structural formula of the collector based on ethoxylated alcohol (synthanol DS. RO (CH2CHjO) H, where R is an alkyl residue; II is the number of ethoxylated groups. For DS-10. The number of C atoms in the alkyl residue is 10-18, the number of ethoxylated groups is 10 4 91 However, a well-known collector provides a high selectivity of the process. In addition, the loss of potassium chloride with the slurry product is high. The purpose of the invention is to selectively reduce the loss of potassium chloride in the slurry product. clayey-carbonate slimes from potash ores, including sequential pulping by a collector based on ethoxylated alcohol and flocculant - an aqueous solution of polyacrylamide; the collector additionally contains triethanolamine salt of synthetic fatty acids with carbon atoms in radical 7-9 and alkyl sulfates with carbon atoms in radical I0jl8 with a ratio of components, wt.%: The triethanolamine salt of synthetic fatty acids with the number of carbon atoms in the radical 7-9 60-80 Alkyl sulfates with the number a volumes of carbon in radical 10-18 15-30 Polyoxyethylene alcohol 5-10 The triethanolamine salt of synthetic fatty acids with the number of carbon atoms in radical 7-9 is a light brown liquid or paste, well soluble in water. Its application in the production of detergents is known. Alkyl sulfates of the formula O S O, Na, where n 0-18j is a white to light brown paste, soluble in water, non-toxic. It is known the use of alkyl sulfates in the production of household and technical detergents. Oxyethylated alcohol of the formula (C,) H, where n 10-13. White to yellow liquid or paste, well soluble in water. It is known to use ethoxylate alcohol as an emulsifier, foam stabilizer. A collector for flotation of sludges containing a triethanolamine salt of synthetic fatty acids with the number of carbon atoms in radical 7-9. 3 alkyl sulfates with the number of carbon atoms in the radical 10-18 and ethoxylated alcohol are obtained by mixing its components at 40-50 C. The use of this mixture as a collector of clay-carbonate sludge from potassium ores is unknown. The method is carried out as follows. The crushed ore is crushed to a particle size of -0.8 + 0 mm, scrubbed for 20 minutes at, then the pulp is diluted to 5, and processed sequentially with a collector and flocculated and the potassium chloride is floated. The proposed collector was tested under laboratory conditions during the flotation of clay-carbonate sludges from the potassium-containing ore of the Starobin deposit. Example 1. Potassium-containing ore, which contains 25.6% by weight of potassium chloride and 3.48% by weight of the insoluble residue (i.e. -0.8-0), is scrubbed for 20 minutes at. The pulp is then diluted to 5, and treated successively at first with a collector and then with flocculant, for example with a 1% aqueous solution of polyacrylamide. The collector, for example, a 1% solution of the mixture, includes, wt.%; triethanolam new salt of synthetic fatty acids 80; alkyl sulfates 15; ethoxylated alcohol 5. Collector consumption 60 g per 1 ton of ore processed. Polyacrylamide (PAA) consumption 20 g per 1 ton of processed ore. Time to clocking with the collector 60 s, with PAA 30 s. Flotation is carried out for s. Example 2 Chimpam flotation was carried out analogously to example 1. The collector contains, in wt%: triethane, an amine salt of synthetic fatty acids 70; alkyl sulfates 20; ethoxylated solvent 10. The collector's consumption of 100 g per 1 ton of ore, i.e. 0.01% of the amount of ore processed. Example 3 Slurry flotation was carried out analogously to example 1. The collector contains, in wt%: the triethanolamine salt of synthetic fatty acids 60; alkyl sulfates 30; ethoxylated alcohol 10. Collector consumption 150 g per 1 ton of ore, 894 ie 0,015 nas.7, on the amount of potassium-containing ore being floated. Example 4. Slurry flotation was carried out analogously to an example. The collector contains, wt%: the triethanolamine salt of synthetic fatty acids 75; alkyl sulfates 18, ethoxylated alcohol 7. The collector's consumption of 180 g per 1 ton of ore, i.e. 0,018 wt.% From the amount of processed ore. Examples 5 and 6 are similar to i-4. Example 7 (famous collector). Slurry flotation was carried out analogously to example 1. The collector was DS-10 syntanol. The consumption of the collector is 125 g per ton of ore, i.e. 0,0125 wt.% From the amount of processed ore. The table presents the indicators characterizing the effectiveness of the proposed (printers 1-6) and well-known (example 7) collectors for the flotation of scales. According to the table, the use of the proposed collector in comparison with the known one allows to increase the content of the insoluble residue in the asham product from 61.5% to 64.5%, and the recovery rate from 50.0% to 52.1%. At the same time, the content of potassium chloride in the slime product and the recovery (i.e., loss of potassium chloride) decreases from 7.89 (prototype) to 5.43–6.11%, i.e. VB 1.4 times, and from 0.87 to 0.59-0.66%, i.e. B v-1.3-1.5 times, respectively. The selectivity of the slime flotation, calculated according to (.1) when using the proposed collector 0.986-0.988, and the known - below 0.983. The use of collector compositions, WITHOUTS beyond the proposed limits, is impractical. For example, if the collector contains, by wt ..%: the triethanolamine salt of synthetic fatty acids 85, alkyl sulfates 12, ethoxylated alcohol 3, and its consumption is 50 g per.1 tons of ore (example 5), then the content of n. in the slurry product 58.5%, i.e. lower than in the known method. When the collector consumed 200 g per 1 ton of ore and its content, wt%: the triethanolamine salt of synthetic fatty acids 50, alkyl sulfates 35, ethoxylated alcohol 15 (example 6), the content of potassium chloride in the slurry product 9.8%.

При использовании, предлагаемого реагента-депрессора снижаетс  расходWhen used, the proposed depressant reagent decreases consumption

дефицитного реагента-депрессора сильвиновой флотации - натриевой соли карбоксиметилцеллюлозы на 157 г/т РУДЫ.deficient sylvinic flotation depressant reagent - sodium carboxymethylcellulose per 157 g / ton of ore.

Claims (1)

СПОСОБ ФЛОТАЦИИ ГЛИНИСТОКАРБОНАТНЫХ ШЛАМОВ ИЗ КАЛИЙНЫХ. РУД, включающий последовательную обработ* ку пульпы собирателем на основе оксиэтилированного спирта и флокулянтом - водным раствором полиакриламида, отличающийся тем, что, с целью повышения селективности путем снижения потерь хлористого калия в шламовом продукте, собиратель дополнительно содержит триэта ноламиновую соль синтетических жирных кислот с числом атомов углерода в радикале 7-9 и алкилсульфаты с числом атомов углерода в радикале 10-18 при соотношении компонентов, мас.%:METHOD OF FLOTATION OF CLAY CARBONATE Sludge. ORE, including sequential treatment of pulp * with a collector based on ethoxylated alcohol and a flocculant - an aqueous solution of polyacrylamide, characterized in that, in order to increase selectivity by reducing the loss of potassium chloride in the sludge product, the collector additionally contains triethyl nolamine salt of synthetic fatty acids with the number of atoms carbon in the radical 7-9 and alkyl sulfates with the number of carbon atoms in the radical 10-18 with a ratio of components, wt.%: Триэтаноламиновая соль синтетических жирных кислот с числом атомов углерода в радикале 7-9 60-80Triethanolamine salt of synthetic fatty acids with the number of carbon atoms in the radical 7-9 60-80 Алкилсульфаты с числом атомов углерода в радикале 10-18 15-30Alkyl sulfates with the number of carbon atoms in the radical 10-18 15-30 Оксиэтилированный спирт 5-10Ethoxylated alcohol 5-10 KSTRrrr'TiSKSTRrrr'TiS
SU833621266A 1983-07-08 1983-07-08 Method of flotation clayish-carbonate slime from potassium ores SU1138189A1 (en)