RU99121390A - METHOD FOR PRODUCING OXIDO NICKEL ELECTRODE FOR ALKALINE BATTERY - Google Patents
METHOD FOR PRODUCING OXIDO NICKEL ELECTRODE FOR ALKALINE BATTERYInfo
- Publication number
- RU99121390A RU99121390A RU99121390/09A RU99121390A RU99121390A RU 99121390 A RU99121390 A RU 99121390A RU 99121390/09 A RU99121390/09 A RU 99121390/09A RU 99121390 A RU99121390 A RU 99121390A RU 99121390 A RU99121390 A RU 99121390A
- Authority
- RU
- Russia
- Prior art keywords
- alkaline battery
- electrode
- oxido
- producing
- heat treatment
- Prior art date
Links
- 238000004519 manufacturing process Methods 0.000 title claims 2
- GNRSAWUEBMWBQH-UHFFFAOYSA-N oxonickel Chemical compound [Ni]=O GNRSAWUEBMWBQH-UHFFFAOYSA-N 0.000 title 1
- 238000010438 heat treatment Methods 0.000 claims 4
- 238000005470 impregnation Methods 0.000 claims 3
- 238000001035 drying Methods 0.000 claims 2
- PXHVJJICTQNCMI-UHFFFAOYSA-N nickel Chemical compound [Ni] PXHVJJICTQNCMI-UHFFFAOYSA-N 0.000 claims 2
- KBJMLQFLOWQJNF-UHFFFAOYSA-N Nickel(II) nitrate Chemical compound [Ni+2].[O-][N+]([O-])=O.[O-][N+]([O-])=O KBJMLQFLOWQJNF-UHFFFAOYSA-N 0.000 claims 1
- WZOZCAZYAWIWQO-UHFFFAOYSA-N [Ni].[Ni]=O Chemical compound [Ni].[Ni]=O WZOZCAZYAWIWQO-UHFFFAOYSA-N 0.000 claims 1
- 239000003513 alkali Substances 0.000 claims 1
- 239000002585 base Substances 0.000 claims 1
- 229910052759 nickel Inorganic materials 0.000 claims 1
- 238000005406 washing Methods 0.000 claims 1
Claims (1)
где К - потеря массы электрода при термообработке, М0, М1 и М2 - масса электрода соответственно до пропитки, после пропитки и после термообработки.A method of manufacturing a nickel oxide-nickel electrode of an alkaline battery, including impregnation of a porous sintered nickel base in a solution of nickel nitrate, drying, processing in an alkali solution, washing, drying and heat treatment, characterized in that the heat treatment is carried out according to the conditions providing the mass loss of the electrode from 1 to 10%, which is calculated from the expression
where K is the mass loss of the electrode during heat treatment, M 0 , M 1 and M 2 are the mass of the electrode, respectively, before impregnation, after impregnation and after heat treatment.