RU97106520A - MIXTURE FOR Smelting Ferrosilicon in a Blast Furnace - Google Patents

MIXTURE FOR Smelting Ferrosilicon in a Blast Furnace

Info

Publication number
RU97106520A
RU97106520A RU97106520/02A RU97106520A RU97106520A RU 97106520 A RU97106520 A RU 97106520A RU 97106520/02 A RU97106520/02 A RU 97106520/02A RU 97106520 A RU97106520 A RU 97106520A RU 97106520 A RU97106520 A RU 97106520A
Authority
RU
Russia
Prior art keywords
blast furnace
mixture
ferrosilicon
smelting
smelting ferrosilicon
Prior art date
Application number
RU97106520/02A
Other languages
Russian (ru)
Other versions
RU2112072C1 (en
Inventor
Е.Ф. Лингарт
И.Ш. Туктамышев
Г.П. Зуев
Ю.К. Калинин
Original Assignee
Е.Ф. Лингарт
И.Ш. Туктамышев
Г.П. Зуев
Ю.К. Калинин
Filing date
Publication date
Application filed by Е.Ф. Лингарт, И.Ш. Туктамышев, Г.П. Зуев, Ю.К. Калинин filed Critical Е.Ф. Лингарт
Priority to RU97106520A priority Critical patent/RU2112072C1/en
Priority claimed from RU97106520A external-priority patent/RU2112072C1/en
Application granted granted Critical
Publication of RU2112072C1 publication Critical patent/RU2112072C1/en
Publication of RU97106520A publication Critical patent/RU97106520A/en

Links

Claims (1)

Шихта для выплавки ферросилиция в доменной печи, включающая кокс, флюсы, железорудные материалы и шунгит с соотношением C : SiO2 = 0,25 oC 0,6, отличающаяся тем, что, с целью высокоэффективной выплавки углеродистого ферросилиция в доменной печи, она содержит шунгит в количестве 16 oC 50%, кокс, флюсы и железорудные материалы - остальное.The mixture for smelting ferrosilicon in a blast furnace, including coke, fluxes, iron ore materials and shungite with a ratio of C: SiO 2 = 0.25 o C 0.6, characterized in that, with the aim of highly efficient smelting of carbon ferrosilicon in a blast furnace, it contains shungite in an amount of 16 o C 50%, coke, fluxes and iron ore materials - the rest.
RU97106520A 1997-04-17 1997-04-17 Charge for smelting of ferrosilicon in blast furnace RU2112072C1 (en)