- Publication number
- RU95111025A RU95111025A RU95111025/02A RU95111025A RU95111025A RU 95111025 A RU95111025 A RU 95111025A RU 95111025/02 A RU95111025/02 A RU 95111025/02A RU 95111025 A RU95111025 A RU 95111025A RU 95111025 A RU95111025 A RU 95111025A
- Authority
- RU
- Russia
- Prior art keywords
- steel
- lining
- ladle
- casting
- metal
- Prior art date
Abstract
Изобретение относится к области черной металлургии, в частности, к способам производства стали. Способ производства стали включает нагрев металла в сталеплавильном агрегате, выпуск в сталеразливочный ковш с высокоглиноземистой футеровкой, доводку металла по химическому составу, разливку стали на МНЛЗ через промежуточный ковш. Новым в способе является то, что для разливки стали на МНЛЗ через промежуточный ковш с холодной футеровкой металл в сталеплавильном агрегате нагревают до температуры 1690-1740С и выпускают в сталеразливочный ковш с высокоглиноземистой футеровкой, а для разливки стали на МНЛЗ через промежуточный ковш с горячей футеровкой металл нагревают до температуры 1660-1690С и выпускают в сталеразливочный ковш с шамотной футеровкой, верхняя часть которой выполнена из периклазохромитовых огнеупоров.
Claims (1)
- Изобретение относится к области черной металлургии, в частности, к способам производства стали. Способ производства стали включает нагрев металла в сталеплавильном агрегате, выпуск в сталеразливочный ковш с высокоглиноземистой футеровкой, доводку металла по химическому составу, разливку стали на МНЛЗ через промежуточный ковш. Новым в способе является то, что для разливки стали на МНЛЗ через промежуточный ковш с холодной футеровкой металл в сталеплавильном агрегате нагревают до температуры 1690-1740oС и выпускают в сталеразливочный ковш с высокоглиноземистой футеровкой, а для разливки стали на МНЛЗ через промежуточный ковш с горячей футеровкой металл нагревают до температуры 1660-1690oС и выпускают в сталеразливочный ковш с шамотной футеровкой, верхняя часть которой выполнена из периклазохромитовых огнеупоров.