RU93026057A - Способ "залечивания" поверхностных трещин - Google Patents

Способ "залечивания" поверхностных трещин

Info

Publication number
RU93026057A
RU93026057A RU93026057/08A RU93026057A RU93026057A RU 93026057 A RU93026057 A RU 93026057A RU 93026057/08 A RU93026057/08 A RU 93026057/08A RU 93026057 A RU93026057 A RU 93026057A RU 93026057 A RU93026057 A RU 93026057A
Authority
RU
Russia
Prior art keywords
cracks
healing
source
depth
high energy
Prior art date
Application number
RU93026057/08A
Other languages
English (en)
Other versions
RU2056253C1 (ru
Inventor
Д.М. Гуреев
С.В. Ямщиков
Original Assignee
Д.М. Гуреев
С.В. Ямщиков
Filing date
Publication date
Application filed by Д.М. Гуреев, С.В. Ямщиков filed Critical Д.М. Гуреев
Priority to RU93026057A priority Critical patent/RU2056253C1/ru
Priority claimed from RU93026057A external-priority patent/RU2056253C1/ru
Publication of RU93026057A publication Critical patent/RU93026057A/ru
Application granted granted Critical
Publication of RU2056253C1 publication Critical patent/RU2056253C1/ru

Links

Claims (1)

  1. Способ "залечивания" поверхностных трещин относится к обработке изделий из металлов и сплавов с помощью концентрированных источников энергии. Изобретение способствует "залечиванию" (полному заплавлению) трещин с глубиной, не превышающей глубину проплавления поверхностного слоя изделия, источником с высокой плотностью энергии, например лазерно - дуговым. Для этого способ "залечивания" поверхностных трещин включает в себя оплавление трещины источником с высокой плотностью энергии с предварительным подогревом изделия до температур, обеспечивающих формирование в окрестности вершины трещины напряжений с максимальной интенсивностью, меньшей критической величины вязкости разрушения Кrc.
RU93026057A 1993-05-07 1993-05-07 Способ восстановления деталей с поверхностными трещинами RU2056253C1 (ru)