RU2467985C1 - Шпаклевка - Google Patents

Шпаклевка Download PDF

Info

Publication number
RU2467985C1
RU2467985C1 RU2011139978/03A RU2011139978A RU2467985C1 RU 2467985 C1 RU2467985 C1 RU 2467985C1 RU 2011139978/03 A RU2011139978/03 A RU 2011139978/03A RU 2011139978 A RU2011139978 A RU 2011139978A RU 2467985 C1 RU2467985 C1 RU 2467985C1
Authority
RU
Russia
Prior art keywords
putty
water
portland cement
quartz sand
specific surface
Prior art date
Application number
RU2011139978/03A
Other languages
English (en)
Inventor
Юлия Алексеевна Щепочкина
Original Assignee
Юлия Алексеевна Щепочкина
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Юлия Алексеевна Щепочкина filed Critical Юлия Алексеевна Щепочкина
Priority to RU2011139978/03A priority Critical patent/RU2467985C1/ru
Application granted granted Critical
Publication of RU2467985C1 publication Critical patent/RU2467985C1/ru

Abstract

Изобретение касается составов шпаклевок для выравнивания поверхностей бетонных изделий. Шпаклевка содержит, мас.%: портландцемент 28,0-32,0, вода 20,0-22,0, гидросиликаты кальция 0,1-0,15, молотый до удельной поверхности 4500-5000 см2/г кварцевый песок 45,4-51,3, нейтрализованная воздухововлекающая смола СНВ 0,1-0,15, суперпластификатор С-3 0,3-0,5. Технический результат - повышение прочности сцепления с поверхностью бетона. 1 табл.

Description

Изобретение касается составов шпаклевок для выравнивания поверхностей бетонных изделий.
Известна шпаклевка, содержащая, мас.%: цемент (портландцемент) 38,0-45,0; глина 26,5-32,5; вода 23,0-29,0; костный клей 2,65-2,95; гидросиликаты кальция 0,19-0,22 [1].
Задача изобретения состоит в повышении прочности сцепления шпаклевки с поверхностью бетона.
Технический результат достигается тем; что шпаклевка, содержащая портландцемент, воду, гидросиликаты кальция, дополнительно содержит молотый до удельной поверхности 4500-5000 см2/г кварцевый песок, нейтрализованную воздухововлекающую смолу СНВ и суперпластификатор С-3 при следующем соотношении компонентов, мас.%: портландцемент 28,0-32,0; вода 20,0-22,0; гидросиликаты кальция 0,1-0,15; указанный молотый кварцевый песок 45,4-51,3; нейтрализованную воздухововлекающую смолу СНВ 0,1-0,15; суперпластификатор С-3 0,3-0,5.
В таблице приведены составы шпаклевки.
Таблица
Компоненты Состав, мас.%:
1 2 3
Портландцемент 28,0 30,0 32,0
Вода 20,0 21,0 22,0
Гидросиликаты кальция 0,1 0,125 0,15
Молотый кварцевый песок
- до удельной поверхности 4500 см2 51,3 - 45,4
- до удельной поверхности 5000 см2 - 48,35 -
Нейтрализованная воздухововлекающая смола СНВ 0,1 0,125 0,15
Суперпластификатор С-3 0,5 0,4 0,3
Прочность сцепления с поверхностью бетона, МПа не менее 2,5 не менее 2,5 не менее 2,5
Компоненты дозируют в требуемых количествах. Портландцемент (марки 400) и молотый кварцевый песок (удельная поверхность 4500-5000 см2/г) смешивают, добавляют воду, гидросиликаты кальция (удельная поверхность 4500-5000 см2/г), нейтрализованную воздухововлекающую смолу СНВ, суперпластификатор С-3 (получаемый на базе продуктов конденсации нафталинсульфокислоты и формальдегида) и еще раз тщательно смешивают. Полученной шпаклевкой заполняют раковины и неровности поверхности бетонных изделий.
Источник информации
1. Шпаклевка. // Строительные материалы, оборудование и технологии XXI века. - 2007. - №11. - С.26-27.

Claims (1)

  1. Шпаклевка, содержащая портландцемент, воду, гидросиликаты кальция, отличающаяся тем, что дополнительно содержит молотый до удельной поверхности 4500-5000 см2/г кварцевый песок, нейтрализованную воздухововлекающую смолу СНВ и суперпластификатор С-3 при следующем соотношении компонентов, мас.%:
    портландцемент 28,0-32,0 вода 20,0-22,0 гидросиликаты кальция 0,1-0,15 молотый кварцевый песок 45,4-51,3 нейтрализованная воздухововлекающая смола СНВ 0,1-0,15 суперпластификатор С-3 0,3-0,5
RU2011139978/03A 2011-09-30 2011-09-30 Шпаклевка RU2467985C1 (ru)