RU2183743C2 - Method of heap leaching of metals under conditions - Google Patents
Method of heap leaching of metals under conditions Download PDFInfo
- Publication number
- RU2183743C2 RU2183743C2 RU2000117258/03A RU2000117258A RU2183743C2 RU 2183743 C2 RU2183743 C2 RU 2183743C2 RU 2000117258/03 A RU2000117258/03 A RU 2000117258/03A RU 2000117258 A RU2000117258 A RU 2000117258A RU 2183743 C2 RU2183743 C2 RU 2183743C2
- Authority
- RU
- Russia
- Prior art keywords
- stack
- leaching
- hollow
- rocks
- leaching process
- Prior art date
Abstract
Description
Изобретение относится к горному делу и может быть использовано для кучного выщелачивания металлов в условиях многолетней мерзлоты. The invention relates to mining and can be used for heap leaching of metals in permafrost.
Известен способ кучного выщелачивания металлов при отрицательной температуре окружающей среды, включающий формирование антифильтрационного основания и выщелачиваемого штабеля и подачу в штабель растворов реагентов [1]. A known method of heap leaching of metals at a negative ambient temperature, including the formation of an antifiltration base and a leachable stack and feeding reagent solutions into the stack [1].
Недостатками этого способа являются:
- сложность возведения антифильтрационного основания;
- ограниченность использования заявленных реагентов.The disadvantages of this method are:
- the complexity of the construction of anti-filtration base;
- limited use of the claimed reagents.
Известен способ кучного выщелачивания в условиях многолетней мерзлоты, включающий подачу в штабель раствора реагентов [2]. Недостатком известного способа является сложность его исполнения. A known method of heap leaching in permafrost conditions, including the supply of a stack of reagent solution [2]. The disadvantage of this method is the complexity of its execution.
Предлагаемый способ включает формирование антифильтрационного основания, укладку на нем штабеля из выщелачиваемых пород и подачу в штабель реагeнтoв, при этом согласно изобретению в теплое время года с участка, предназначенного для размещения штабеля, удаляют оттаявший грунт до мерзлоты, размещают его за пределами этого участка, устанавливают в месте с минимальной отметкой оборудование для откачки продуктивного раствора, а выщелачивание начинают после возведения штабеля над углублением еще до наступления холодного времени года, причем откачку продуктивного раствора ведут до максимального промерзания штабеля или завершения процесса выщелачивания. The proposed method includes the formation of an antifiltration base, laying on it a stack of leachable rocks and supplying reagents to the stack, while according to the invention, in the warm season, the thawed soil is removed to the frozen ground, placed outside the area, installed in the place with the minimum mark, equipment for pumping the productive solution, and leaching begins after the erection of the stack over the well before the onset of the cold season, m pumping of the productive solution is carried out until the maximum freezing of the stack or the completion of the leaching process.
Способ поясняется чертежом, где показан в разрезе штабель во время выщелачивания металлов. The method is illustrated in the drawing, which shows in section the stack during the leaching of metals.
Условные обозначения, принятые на чертеже: 1 - участок, выбранный для кучного выщелачивания; 2 - оттаявший грунт; 3 - чашеобразная выемка; 4 - граница сезонного протаивания; 5 - многолетняя мерзлота; 6 - оборудование для откачки раствора; 7 - штабель; 8 - граница замерзших пород штабеля. Symbols adopted in the drawing: 1 - section selected for heap leaching; 2 - thawed soil; 3 - cup-shaped recess; 4 - seasonal thawing boundary; 5 - permafrost; 6 - equipment for pumping the solution; 7 - a stack; 8 - the boundary of the frozen rocks of the stack.
Способ осуществляют следующим образом. The method is as follows.
На участке 1, выбранном для кучного выщелачивания, в теплое время года оттаявший грунт 2 извлекают и размещают за пределами участка 1, обваловывая будущий штабель выщелачиваемых пород. По мере оттайки эту операцию повторяют до тех пор, пока чашеобразная выемка 3 не разместится ниже границы сезонного протаивания 4 в зоне многолетней мерзлоты 5. При этом выемке 3 придают чашеобразную форму. В месте с минимальной отметкой размещают оборудование 6 для откачки продуктивного раствора в процессе выщелачивания. Затем чашеобразную выемку 3 заполняют выщелачиваемыми породами и формируют из них штабель 7. Процесс выщелачивания металлов начинают до наступления холодного времени года подачей в штабель растворов реагентов. Продуктивные растворы откачивают при помощи оборудования 6, которое в течение всего процесса выщелачивания находится в талой зоне с положительными или даже отрицательными температурами. При наступлении отрицательных температур штабель 7 начинает замерзать с поверхности, а граница замерзших пород штабеля 7 - фронт промерзания - перемещаться все ниже, оттесняя примеси в растворе и повышая его концентрацию и создавая напорное давление в поровом растворе внутри штабеля 7. Это усиливает интенсивность процесса выщелачивания и способствует более полному извлечению продуктивных растворов. После окончания выщелачивания металлов и откачки всего продуктивного раствора оборудование 6 извлекают из штабеля 7. Впоследствии все породы штабеля 7 и грунт, находящийся под ним, промерзают. Остатки растворов реагентов и продуктивных растворов в нижней части штабеля 7 и даже не замерзшие локализуются в углублении, далее не распространяются и не наносят вреда окружающей среде. In section 1, selected for heap leaching, in the warm season, thawed soil 2 is removed and placed outside of section 1, bunding a future stack of leached rocks. As the defrost is performed, this operation is repeated until the cup-shaped recess 3 is located below the seasonal thawing border 4 in the permafrost zone 5. In this case, the recess 3 is given a cup-shaped shape. In place with a minimum mark place equipment 6 for pumping productive solution in the leaching process. Then the cup-shaped recess 3 is filled with leachable rocks and a stack 7 is formed from them. The metal leaching process is started before the cold season begins by feeding reagent solutions to the stack. Productive solutions are pumped out using equipment 6, which during the entire leaching process is in the melt zone with positive or even negative temperatures. When negative temperatures occur, the pile 7 begins to freeze from the surface, and the boundary of the frozen rocks of the pile 7 — the freezing front — moves ever lower, displacing impurities in the solution and increasing its concentration and creating pressure in the pore solution inside the pile 7. This increases the intensity of the leaching process and contributes to a more complete extraction of productive solutions. After the leaching of metals and pumping out of the entire productive solution, the equipment 6 is removed from the stack 7. Subsequently, all the rocks of the stack 7 and the soil beneath it are frozen. The remains of the reagent solutions and productive solutions in the lower part of the stack 7 and not even frozen are localized in the recess, then they do not spread and do not harm the environment.
Преимуществами способа являются:
- продление процесса выщелачивания на зимнее время;
- простота способа;
- экологическая чистота выщелачивания.The advantages of the method are:
- extension of the leaching process for winter time;
- simplicity of the method;
- ecological purity of leaching.
Источники информации
1. Патент РФ 2091573, Е 21 В 43/28, 1997 г.Sources of information
1. RF patent 2091573, E 21 B 43/28, 1997
2. Патент РФ 2150581, Е 21 С 41/00, 2000 г. 2. RF patent 2150581, E 21 C 41/00, 2000
Claims (1)