RU2013109080A - METHOD FOR CORRECTION OF METAL STRUCTURAL DEFECTS - Google Patents

METHOD FOR CORRECTION OF METAL STRUCTURAL DEFECTS Download PDF

Info

Publication number
RU2013109080A
RU2013109080A RU2013109080/02A RU2013109080A RU2013109080A RU 2013109080 A RU2013109080 A RU 2013109080A RU 2013109080/02 A RU2013109080/02 A RU 2013109080/02A RU 2013109080 A RU2013109080 A RU 2013109080A RU 2013109080 A RU2013109080 A RU 2013109080A
Authority
RU
Russia
Prior art keywords
insert
base metal
cutting
metal
local heating
Prior art date
Application number
RU2013109080/02A
Other languages
Russian (ru)
Other versions
RU2532577C2 (en
Inventor
Анатолий Иванович Ананьев
Юрий Анатольевич Кузнецов
Александр Александрович Курков
Михаил Васильевич Шибалов
Original Assignee
Федеральное государственное унитарное предприятие "Научно-производственное объединение им. С.А. Лавочкина"
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Федеральное государственное унитарное предприятие "Научно-производственное объединение им. С.А. Лавочкина" filed Critical Федеральное государственное унитарное предприятие "Научно-производственное объединение им. С.А. Лавочкина"
Priority to RU2013109080/02A priority Critical patent/RU2532577C2/en
Publication of RU2013109080A publication Critical patent/RU2013109080A/en
Application granted granted Critical
Publication of RU2532577C2 publication Critical patent/RU2532577C2/en

Abstract

1. Способ исправления дефектов металлоконструкций, включающий механическую разделку дефектного места, установку в нее вставки из сплава, близкого по химическому составу с основным металлом, локальный нагрев и заполнение разделки расплавленным металлом вставки, отличающийся тем, что вставку, соответствующую по форме и размерам разделке, плотно вставляют в указанную разделку, а затем осуществляют локальный нагрев методом контактной точечной сварки с перекрытием литым ядром границы между поверхностями вставки и основного металла, причем образующая контактной поверхности между вставкой и основным металлом совпадает с направлением сварочного тока.2. Способ по п.1, отличающийся тем, что увеличивают площадь сплавления вставки и основного металла, используя технологические накладки в процессе контактной точечной сварки.1. A method for correcting defects in metal structures, including mechanical cutting of a defective place, installation of an insert of an alloy of a similar chemical composition to the base metal, local heating and filling of the cutting with molten metal of the insert, characterized in that the insert is suitable in shape and size for cutting, tightly inserted into the specified grooves, and then carry out local heating by the method of contact spot welding with overlapping cast core the boundary between the surfaces of the insert and the base metal, and forming the contact surface between the insert and the base metal coincides with the direction of the welding current. 2. The method according to claim 1, characterized in that the fusion area of the insert and the base metal is increased using technological overlays in the process of contact spot welding.

Claims (2)

1. Способ исправления дефектов металлоконструкций, включающий механическую разделку дефектного места, установку в нее вставки из сплава, близкого по химическому составу с основным металлом, локальный нагрев и заполнение разделки расплавленным металлом вставки, отличающийся тем, что вставку, соответствующую по форме и размерам разделке, плотно вставляют в указанную разделку, а затем осуществляют локальный нагрев методом контактной точечной сварки с перекрытием литым ядром границы между поверхностями вставки и основного металла, причем образующая контактной поверхности между вставкой и основным металлом совпадает с направлением сварочного тока.1. A method for correcting defects in metal structures, including mechanical cutting of a defective place, installation of an insert of an alloy of a similar chemical composition to the base metal, local heating and filling of the cutting with molten metal of the insert, characterized in that the insert is suitable in shape and size for cutting, tightly inserted into the specified grooves, and then carry out local heating by the method of contact spot welding with overlapping cast core the boundary between the surfaces of the insert and the base metal, and forming the contact surface between the insert and the base metal coincides with the direction of the welding current. 2. Способ по п.1, отличающийся тем, что увеличивают площадь сплавления вставки и основного металла, используя технологические накладки в процессе контактной точечной сварки. 2. The method according to claim 1, characterized in that the fusion area of the insert and the base metal is increased using technological overlays in the process of contact spot welding.
RU2013109080/02A 2013-03-01 2013-03-01 Elimination of metal structure damages RU2532577C2 (en)