RU2011138897A - METHOD FOR FRICTION WELDING - Google Patents

METHOD FOR FRICTION WELDING Download PDF

Info

Publication number
RU2011138897A
RU2011138897A RU2011138897/02A RU2011138897A RU2011138897A RU 2011138897 A RU2011138897 A RU 2011138897A RU 2011138897/02 A RU2011138897/02 A RU 2011138897/02A RU 2011138897 A RU2011138897 A RU 2011138897A RU 2011138897 A RU2011138897 A RU 2011138897A
Authority
RU
Russia
Prior art keywords
heating
pressure
initial
main
workpiece
Prior art date
Application number
RU2011138897/02A
Other languages
Russian (ru)
Other versions
RU2483849C2 (en
Inventor
Александр Владимирович Егоров
Владимир Ильич Егоров
Виталий Иванович Коминов
Александр Николаевич Мезенцев
Вячеслав Константинович Одинцов
Виктор Владимирович Поляков
Абрам Абрамович Рогальский
Лев Геннадьевич Степанов
Евгений Николаевич Стойко
Original Assignee
Александр Владимирович Егоров
Владимир Ильич Егоров
Виталий Иванович Коминов
Александр Николаевич Мезенцев
Вячеслав Константинович Одинцов
Виктор Владимирович Поляков
Абрам Абрамович Рогальский
Лев Геннадьевич Степанов
Евгений Николаевич Стойко
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Александр Владимирович Егоров, Владимир Ильич Егоров, Виталий Иванович Коминов, Александр Николаевич Мезенцев, Вячеслав Константинович Одинцов, Виктор Владимирович Поляков, Абрам Абрамович Рогальский, Лев Геннадьевич Степанов, Евгений Николаевич Стойко filed Critical Александр Владимирович Егоров
Priority to RU2011138897/02A priority Critical patent/RU2483849C2/en
Publication of RU2011138897A publication Critical patent/RU2011138897A/en
Application granted granted Critical
Publication of RU2483849C2 publication Critical patent/RU2483849C2/en

Abstract

Способ сварки трением, при котором одну из свариваемых заготовок приводят во вращение и прикладывают к ним давление нагрева разное по величине на этой стадии, а затем давление проковки, отличающийся тем, что стадию нагрева разбивают на три периода начальный, основной и окончательный, причем при начальном нагреве удаляют оксидные пленки и загрязнения со стыкуемых поверхностей и заканчивают период начального нагрева снижением давления до величины давления основного нагрева, которое составляет 25…50% от давления начального нагрева и выполняют основной нагрев до температуры сварки в стыке, после чего в период окончательного нагрева отключают привод вращения заготовки и увеличивают давление основного нагрева до давления проковки, при этом длительность нарастания давления меньше или равна длительности прекращения вращения заготовки.A method of friction welding, in which one of the parts to be welded is brought into rotation and a heating pressure of different magnitude is applied to them at this stage, and then the forging pressure, characterized in that the heating stage is divided into three periods, initial, main and final, and at the initial heating remove oxide films and contaminants from abutting surfaces and end the initial heating period by reducing the pressure to a pressure value of the main heating, which is 25 ... 50% of the initial heating pressure and the main heating is heated up to the welding temperature at the butt, after which during the final heating the drive for turning the workpiece is turned off and the pressure of the main heating is increased to the forging pressure, while the duration of the pressure rise is less than or equal to the duration of the cessation of rotation of the workpiece.

Claims (1)

Способ сварки трением, при котором одну из свариваемых заготовок приводят во вращение и прикладывают к ним давление нагрева разное по величине на этой стадии, а затем давление проковки, отличающийся тем, что стадию нагрева разбивают на три периода начальный, основной и окончательный, причем при начальном нагреве удаляют оксидные пленки и загрязнения со стыкуемых поверхностей и заканчивают период начального нагрева снижением давления до величины давления основного нагрева, которое составляет 25…50% от давления начального нагрева и выполняют основной нагрев до температуры сварки в стыке, после чего в период окончательного нагрева отключают привод вращения заготовки и увеличивают давление основного нагрева до давления проковки, при этом длительность нарастания давления меньше или равна длительности прекращения вращения заготовки. A method of friction welding, in which one of the parts to be welded is brought into rotation and a heating pressure of different magnitude is applied to them at this stage, and then the forging pressure, characterized in that the heating stage is divided into three periods, initial, main and final, and at the initial heating remove oxide films and contaminants from abutting surfaces and end the initial heating period by reducing the pressure to a pressure value of the main heating, which is 25 ... 50% of the initial heating pressure and the main heating is heated up to the welding temperature at the butt, after which during the final heating the drive for turning the workpiece is turned off and the pressure of the main heating is increased to the forging pressure, while the duration of the pressure rise is less than or equal to the duration of the cessation of rotation of the workpiece.
RU2011138897/02A 2011-09-22 2011-09-22 Method of friction welding RU2483849C2 (en)