RU2009131881A - METHOD FOR WELDING THREE-PHASE ARC - Google Patents

METHOD FOR WELDING THREE-PHASE ARC Download PDF

Info

Publication number
RU2009131881A
RU2009131881A RU2009131881/02A RU2009131881A RU2009131881A RU 2009131881 A RU2009131881 A RU 2009131881A RU 2009131881/02 A RU2009131881/02 A RU 2009131881/02A RU 2009131881 A RU2009131881 A RU 2009131881A RU 2009131881 A RU2009131881 A RU 2009131881A
Authority
RU
Russia
Prior art keywords
phase
arc
welding
metal
weld pool
Prior art date
Application number
RU2009131881/02A
Other languages
Russian (ru)
Other versions
RU2418661C1 (en
Inventor
Валерий Валентинович Ельцов (RU)
Валерий Валентинович Ельцов
Александр Сергеевич Зеленков (RU)
Александр Сергеевич Зеленков
Олег Анатольевич Дитенков (RU)
Олег Анатольевич Дитенков
Павел Сергеевич Харитонов (RU)
Павел Сергеевич Харитонов
Original Assignee
Общество с ограниченной ответственностью "СВАРКОМ ТФ" (RU)
Общество с ограниченной ответственностью "СВАРКОМ ТФ"
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Общество с ограниченной ответственностью "СВАРКОМ ТФ" (RU), Общество с ограниченной ответственностью "СВАРКОМ ТФ" filed Critical Общество с ограниченной ответственностью "СВАРКОМ ТФ" (RU)
Priority to RU2009131881/02A priority Critical patent/RU2418661C1/en
Publication of RU2009131881A publication Critical patent/RU2009131881A/en
Application granted granted Critical
Publication of RU2418661C1 publication Critical patent/RU2418661C1/en

Abstract

Способ сварки трехфазной дугой, включающий плавление металла дугой, горящей между двумя неплавящимися электродами и изделием, с подачей в образовавшуюся сварочную ванну присадочной проволоки, подключенной к средней фазе источника питания трехфазной дуги, отличающийся тем, что в момент окончания процесса сварки в зону сварки вносится подключенный к фазе изделия вольфрамовый катетер на расстояние от оси горелки 8-10 мм, что обеспечивает уменьшение объема расплавленного металла и нейтрализацию воздействия силовой составляющей трехфазной дуги на металл сварочной ванны, что обеспечивает уменьшение геометрических размеров усадочной раковины, за счет чего повышается качество сварного соединения. A method of welding with a three-phase arc, including melting the metal by an arc burning between two non-consumable electrodes and a workpiece, with filler wire supplied to the resulting weld pool connected to the middle phase of a three-phase arc power source, characterized in that a connected wire is introduced into the welding zone at the end of the welding process to the product phase, a tungsten catheter at a distance from the axis of the burner is 8-10 mm, which ensures a decrease in the volume of molten metal and the neutralization of the impact of the three-phase power component arc on the metal of the weld pool, which reduces the geometric dimensions of the shrink shell, thereby improving the quality of the welded joint.

Claims (1)

Способ сварки трехфазной дугой, включающий плавление металла дугой, горящей между двумя неплавящимися электродами и изделием, с подачей в образовавшуюся сварочную ванну присадочной проволоки, подключенной к средней фазе источника питания трехфазной дуги, отличающийся тем, что в момент окончания процесса сварки в зону сварки вносится подключенный к фазе изделия вольфрамовый катетер на расстояние от оси горелки 8-10 мм, что обеспечивает уменьшение объема расплавленного металла и нейтрализацию воздействия силовой составляющей трехфазной дуги на металл сварочной ванны, что обеспечивает уменьшение геометрических размеров усадочной раковины, за счет чего повышается качество сварного соединения. A method of welding with a three-phase arc, including melting the metal by an arc burning between two non-consumable electrodes and a workpiece, with filler wire supplied to the resulting weld pool connected to the middle phase of a three-phase arc power source, characterized in that a connected wire is introduced into the welding zone at the end of the welding process to the product phase, a tungsten catheter at a distance from the axis of the burner is 8-10 mm, which ensures a decrease in the volume of molten metal and the neutralization of the impact of the three-phase power component arc on the metal of the weld pool, which reduces the geometric dimensions of the shrink shell, thereby improving the quality of the welded joint.
RU2009131881/02A 2009-08-25 2009-08-25 Method of welding by three-phase arc RU2418661C1 (en)