RU2005104314A - METHOD FOR DRYING WOOD, PREVIOUSLY OF BAR OR LOGS (OPTIONS) - Google Patents

METHOD FOR DRYING WOOD, PREVIOUSLY OF BAR OR LOGS (OPTIONS) Download PDF

Info

Publication number
RU2005104314A
RU2005104314A RU2005104314/06A RU2005104314A RU2005104314A RU 2005104314 A RU2005104314 A RU 2005104314A RU 2005104314/06 A RU2005104314/06 A RU 2005104314/06A RU 2005104314 A RU2005104314 A RU 2005104314A RU 2005104314 A RU2005104314 A RU 2005104314A
Authority
RU
Russia
Prior art keywords
logs
timber
slots
drying
slot
Prior art date
Application number
RU2005104314/06A
Other languages
Russian (ru)
Other versions
RU2298139C2 (en
Inventor
Тагир Фарухович Каримов (RU)
Тагир Фарухович Каримов
Original Assignee
Тагир Фарухович Каримов (RU)
Тагир Фарухович Каримов
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Тагир Фарухович Каримов (RU), Тагир Фарухович Каримов filed Critical Тагир Фарухович Каримов (RU)
Priority to RU2005104314/06A priority Critical patent/RU2298139C2/en
Publication of RU2005104314A publication Critical patent/RU2005104314A/en
Application granted granted Critical
Publication of RU2298139C2 publication Critical patent/RU2298139C2/en

Links

Landscapes

  • Drying Of Solid Materials (AREA)
  • Chemical And Physical Treatments For Wood And The Like (AREA)

Claims (21)

1. Способ сушки древесины, преимущественно бруса или бревен, включающий нагрев изнутри бруса или бревна, отличающийся тем, что вдоль продольной оси бруса или бревна выполняют прорезь, в которой размещают источник тепла в виде электропроводящего нагревательного элемента, после чего прорезь заполняют влагонепроницаемым теплоизоляционным термостойким упругим материалом.1. The method of drying wood, mainly beams or logs, including heating from the inside of the beams or logs, characterized in that along the longitudinal axis of the beams or logs, a slot is made in which a heat source is placed in the form of an electrically conductive heating element, after which the slot is filled with a moisture-proof heat-insulating heat-resistant elastic material. 1. Способ по п.1, отличающийся тем, что прорезь выполняют глубиной до геометрического центра поперечного сечения бруса или бревна или близко к нему.1. The method according to claim 1, characterized in that the slot is performed in depth to or close to the geometric center of the cross section of the beam or log. 2. Способ по п.1, отличающийся тем, что со стороны, противоположной стороне с прорезью, выполняют продольные пазы для компенсации температурного расширения и снятия напряжений при сушке.2. The method according to claim 1, characterized in that from the side opposite to the slotted side, longitudinal grooves are made to compensate for thermal expansion and stress relief during drying. 3. Способ по п.1, отличающийся тем, что сушку ведут при температуре электропроводящего нагревательного элемента 90-150°С в течение всего времени сушки при температуре окружающего воздуха 30-50°С, относительной влажности 60-70% и скорости обдува 1-3 м/с до достижения остаточной влажности древесины не более 20%.3. The method according to claim 1, characterized in that the drying is carried out at a temperature of an electrically conductive heating element of 90-150 ° C during the entire drying time at an ambient temperature of 30-50 ° C, a relative humidity of 60-70% and a speed of blowing 1- 3 m / s until a residual moisture content of wood of not more than 20% is reached. 4. Способ по п.1, отличающийся тем, что в процессе сушки периодически проводят термовлагообработку бруса или бревен продолжительностью в 1 ч при температуре окружающего воздуха 90-95°С и относительной влажности 95-100%.4. The method according to claim 1, characterized in that during the drying process, thermal moisture treatment of the timber or logs is carried out periodically for 1 hour at an ambient temperature of 90-95 ° C and a relative humidity of 95-100%. 5. Способ сушки древесины преимущественно бруса или бревен, включающий нагрев изнутри бруса или бревен, отличающийся тем, что с одной стороны бруса или бревна вдоль продольной оси и симметрично относительно нее выполняют, по меньшей мере, по одной прорези, в каждой из которых размещают источник тепла в виде электропроводящего нагревательного элемента, после чего прорези заполняют влагонепроницаемым теплоизоляционным термостойким упругим материалом.5. The method of drying wood predominantly timber or logs, including heating from the inside of the timber or logs, characterized in that on one side of the timber or logs along the longitudinal axis and symmetrically relative to it, at least one slot is made, in each of which a source is placed heat in the form of an electrically conductive heating element, after which the slots are filled with a moisture-proof heat-insulating heat-resistant elastic material. 6. Способ по п.6, отличающийся тем, что для бруса прорези выполняют со следующими соотношениями а=L/2-L/5, Н/4<b≤Н/2 и с=2-3 мм, где L - ширина бруса, Н - высота бруса, а - расстояние между прорезями, b - глубина прорези, с - ширина прорези.6. The method according to claim 6, characterized in that for the slit beam is performed with the following ratios a = L / 2-L / 5, N / 4 <b≤N / 2 and c = 2-3 mm, where L is the width timber, N - the height of the timber, a - the distance between the slots, b - the depth of the slot, c - the width of the slot. 7. Способ по п.6, отличающийся тем, что для бревна прорези выполняют со следующими соотношениями а=D/2-D/5, D/4<b≤D/2 и с=2-15 мм, где D - диаметр бревна, а - расстояние между прорезями, b - глубина прорези, с - ширина прорези.7. The method according to claim 6, characterized in that for the logs of the slot is performed with the following ratios a = D / 2-D / 5, D / 4 <b≤D / 2 and c = 2-15 mm, where D is the diameter logs, a is the distance between the slots, b is the depth of the slot, c is the width of the slot. 8. Способ по п.6, отличающийся тем, что со стороны, противоположной стороне бруса или бревна с прорезями, выполняют продольные пазы для компенсации температурного расширения и снятия напряжений при сушке.8. The method according to claim 6, characterized in that from the side opposite to the side of the timber or logs with slots, perform longitudinal grooves to compensate for thermal expansion and stress relief during drying. 9. Способ по п.6, отличающийся тем, что сушку ведут при температуре электропроводящего нагревательного элемента 90-150°С, в течение всего времени сушки при температуре окружающего воздуха 30-50°С, относительной влажности 60-70% и при скорости обдува 1-3 м/с до достижения остаточной влажности древесины не более 20%.9. The method according to claim 6, characterized in that the drying is carried out at a temperature of the electrically conductive heating element 90-150 ° C, during the entire drying time at an ambient temperature of 30-50 ° C, relative humidity of 60-70% and at a speed of blowing 1-3 m / s to achieve a residual moisture content of wood no more than 20%. 10. Способ по п.7, отличающийся тем, что в процессе сушки периодически проводят термовлагообработку бревен или бруса продолжительностью в 1 ч при температуре окружающего воздуха 90-95°С и относительной влажности 95-100%.10. The method according to claim 7, characterized in that during the drying process, thermal moisture treatment of logs or timber is carried out periodically for 1 hour at an ambient temperature of 90-95 ° C and a relative humidity of 95-100%. 11. Способ сушки древесины преимущественно бруса или бревен, включающий нагрев изнутри бруса или бревен, отличающийся тем, что с одной стороны бруса или бревна вдоль продольной оси и симметрично относительно нее выполняют, по меньшей мере, по одной прорези, и, по меньшей мере, одну прорезь между ними с противоположной стороны бруса или бревна, в каждой из которых размещают источник тепла в виде электропроводящего нагревательного элемента, после чего прорезь заполняют влагонепроницаемым теплоизоляционным термостойким упругим материалом.11. The method of drying wood predominantly timber or logs, comprising heating from the inside of the timber or logs, characterized in that on one side of the timber or logs along the longitudinal axis and symmetrically relative to it, at least one slot, and at least one slot between them on the opposite side of the timber or log, in each of which a heat source in the form of an electrically conductive heating element is placed, after which the slot is filled with a moisture-proof heat-insulating heat-resistant elastic material. 12. Способ по п.12, отличающийся тем, что глубина каждой прорезей не достигает плоскости, перпендикулярной прорезям и проходящей через продольную ось бруса или бревна.12. The method according to p. 12, characterized in that the depth of each of the slots does not reach a plane perpendicular to the slots and passing through the longitudinal axis of the beam or log. 13. Способ по п.12, отличающийся тем, что для бруса прорези выполняют со следующими соотношениями а=L/2-L/5, b<Н/2, b*<b, с=2-15 мм, где L - ширина бруса, Н - высота бруса, а - расстояние между прорезями, b - глубина прорезей с одной стороны бруса, b* - глубина прорези со стороны, противоположной стороне с прорезями с глубиной b, с - ширина прорезей b и b*.13. The method according to p. 12, characterized in that for the slit beam is performed with the following ratios a = L / 2-L / 5, b <H / 2, b * <b, c = 2-15 mm, where L - beam width, N is the height of the beam, and a is the distance between the slots, b is the depth of the slots on one side of the beam, b * is the depth of the slots from the side opposite to the slots with depth b, c is the width of the slots b and b *. 14. Способ по п.12, отличающийся тем, что для бревна прорези выполняют со следующими соотношениями а=D/2-D/5, b<D/2, b*<b, с=2-15 мм, где D - диаметр бревна, а - расстояние между прорезями, b - глубина прорези с одной стороны бруса, b* - глубина прорези со стороны, противоположной стороне с прорезями с глубиной b, с - ширина прорезей b и b*.14. The method according to p. 12, characterized in that for the logs of the slot is performed with the following ratios a = D / 2-D / 5, b <D / 2, b * <b, c = 2-15 mm, where D - the diameter of the log, a is the distance between the slots, b is the depth of the slit on one side of the beam, b * is the depth of the slit from the side opposite to the slots with depth b, c is the width of the slots b and b *. 15. Способ по п.12, отличающийся тем, что сушку ведут при температуре электропроводящего нагревательного элемента 90-150°С в течение всего времени сушки при температуре окружающего воздуха 30-50°С, относительной влажности 60-70% и скорости обдува 1-3 м/с до достижения остаточной влажности древесины не более 20%.15. The method according to p. 12, characterized in that the drying is carried out at a temperature of an electrically conductive heating element of 90-150 ° C during the entire drying time at an ambient temperature of 30-50 ° C, a relative humidity of 60-70% and a speed of blowing 1- 3 m / s until a residual moisture content of wood of not more than 20% is reached. 16. Способ по п.12, отличающийся тем, что в процессе сушки периодически проводят термовлагообработку бревен или бруса продолжительностью в 1 ч при температуре окружающего воздуха 90-95°С и относительной влажности 95-100%.16. The method according to p. 12, characterized in that in the drying process periodically carry out thermal moisture treatment of logs or timber for 1 hour at an ambient temperature of 90-95 ° C and a relative humidity of 95-100%. 17. Способ сушки древесины преимущественно бруса или бревен, включающий нагрев изнутри бруса или бревна, отличающийся тем, что вдоль продольной оси бруса или бревна с одной стороны и симметрично с противоположной стороны выполняют прорези, в каждой из которых размещают источник тепла в виде электропроводящего нагревательного элемента, после чего прорези заполняют влагонепроницаемым теплоизоляционным термостойким упругим материалом.17. The method of drying wood predominantly timber or logs, including heating from the inside of the timber or logs, characterized in that along the longitudinal axis of the timber or logs on one side and symmetrically on the opposite side, cuts are made, in each of which a heat source is placed in the form of an electrically conductive heating element after which the slots are filled with a moisture-proof heat-insulating heat-resistant elastic material. 18. Способ по п.18, отличающийся тем, что глубина прорезей меньше половины высоты бруса или половины диаметра бревна, а расстояние между внутренними торцами прорезей не менее 4 см.18. The method according to p. 18, characterized in that the depth of the slots is less than half the height of the beam or half the diameter of the log, and the distance between the inner ends of the slots is not less than 4 cm 19. Способ по п.18, отличающийся тем, что с обеих сторон бруса или бревна с прорезями выполняют продольные пазы для компенсации температурного расширения и снятия напряжений при сушке.19. The method according to p. 18, characterized in that on both sides of the timber or logs with slots perform longitudinal grooves to compensate for thermal expansion and stress relief during drying. 20. Способ по п.18, отличающийся тем, что сушку ведут при температуре электропроводящего нагревательного элемента 90-150°С в течение всего времени сушки при температуре окружающего воздуха 30-50°С, относительной влажности 60-70% и скорости обдува 1-3 м/с до достижения остаточной влажности древесины не более 20%.20. The method according to p. 18, characterized in that the drying is carried out at a temperature of an electrically conductive heating element of 90-150 ° C during the entire drying time at an ambient temperature of 30-50 ° C, relative humidity of 60-70% and a speed of blowing 1- 3 m / s until a residual moisture content of wood of not more than 20% is reached. 21. Способ по п.18, отличающийся тем, что в процессе сушки периодически проводят термовлагообработку бруса или бревен продолжительностью в 1 ч при температуре окружающего воздуха 90-95°С и относительной влажности 95-100%.21. The method according to p. 18, characterized in that during the drying process, thermal moisture treatment of timber or logs is carried out periodically for 1 hour at an ambient temperature of 90-95 ° C and a relative humidity of 95-100%.
RU2005104314/06A 2005-02-11 2005-02-11 Timber drying method, mainly beams or logs (variants) RU2298139C2 (en)