Institutul De Chimie Macromoleculara "Petru Poni", Iasi, Ro
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Institutul De Chimie Macromoleculara "Petru Poni", Iasi, RofiledCriticalInstitutul De Chimie Macromoleculara "Petru Poni", Iasi, Ro
Priority to RO1988135068ApriorityCriticalpatent/RO101937A2/en
Publication of RO101937B1publicationCriticalpatent/RO101937B1/en
Publication of RO101937A2publicationCriticalpatent/RO101937A2/en
The adhesive comprises natural rubber 15-25, polyisoprene elastomer of 15-25 Mooney plasticity 0-20, acrylic cooplymers 20-25, acrylovinyl copolymers 0-15, resol-type phenol formaldehyde resins 30-80, colophony 0-5, petroleum resins of 75-115 deg.C softening point 0-5, and zinc oxide 0-2 parts. It also incorporates dioctyl phthalate 0-15, mineral oil 0-4, aminic anti-oxidant 0.5-1 parts, e.g. phenyl naphthylamine, and sufficient cyclohexane to give 10-20 per cent dry matter content. The tape is used in electrical insulation work.
RO1988135068A1988-09-071988-09-07Adhesive composition for pressure sensitive self-adhesive straps