PL74885B2 - - Google Patents

Download PDF

Info

Publication number
PL74885B2
PL74885B2 PL15338672A PL15338672A PL74885B2 PL 74885 B2 PL74885 B2 PL 74885B2 PL 15338672 A PL15338672 A PL 15338672A PL 15338672 A PL15338672 A PL 15338672A PL 74885 B2 PL74885 B2 PL 74885B2
Authority
PL
Poland
Prior art keywords
parts
phase
monomeric
blowing agent
introducing
Prior art date
Application number
PL15338672A
Other languages
English (en)
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to PL15338672A priority Critical patent/PL74885B2/pl
Publication of PL74885B2 publication Critical patent/PL74885B2/pl

Description

Sposób wedlug wynalazku jest przedstawiony w przykladach wykonania.Przyklad I. Do 250 czesci wody o tempe¬ raturze 80°C wprowadza sie 2 czesci zelatyny i po calkowitym rozpuszczaniu dodaje sie 50 czesci glikolu etylenowego i 100 czesci siarczanu sodo¬ wego. Po obnizeniu temperatury do 70°C dodaje sie faze monomeryczna, która sporzadza sie z 36 czesci swiezo destylowanego kwasu metakrylowe- 15 25 30 40 go i 6 czesci dwuwinylobenzenu oraz 1 czesci nadtlenku benzoilu i 32 czesci n-heptanu. Proces kopolimeryzacji prowadzi sie w temperaturze 70°C przy szybkosci obrotów mieszadla 250 obrotów/min.Po 30 minutach nastepuje zelowanie, a po 540 mi¬ nutach konczy sie kopolimeryzacje. Kationit od¬ sacza sie od fazy wodnej, która zwraca sie do nastepnej syntezy. Uzyskany produkt wymywa sie wrzaca woda, a nastepnie woda z kwasem w ce¬ lu usuniecia stabilizatora i innych dodatków sto¬ sowanych przy kopolimeryzacji, a nastepnie suszy sie w suszarce prózniowej w temperaturze 70°C przez 12 godzin.Przyklad II. Do 500 czesci wody w tempe¬ raturze 70°C wprowadza sie 5 czesci fosforanu wapnia i 300 czesci chlorku wapniowego. Po roz¬ puszczaniu soli dodaje sie monomery sporzadzone z 72 czesci swiezo destylowanego kwasu metakry¬ lowego i 12 czesci dwuwinylobenzenu, oraz 2 czes¬ ci nadtlenku benzoilu i 4 czesci oleju parafino¬ wego. Czas polimeryzacji w temperaturze 75°C wynosi 2 godziny, w 80°C równiez 2 godziny, a w 85°C 3 godziny. Dalej postepuje sie jak w przykladzie I. PL PL

Claims (1)

1. Zastrzezenie patentowe Sposób wytwarzania porowatego kationitu kar- boksylowego z kwasu metakrylowego lub akrylo¬ wego i dwuwinylobenzenu metoda polimeryzacji suspensyjnej, polegajacy na wprowadzeniu srodka porotwórczego do fazy monomerycznej i stosowa¬ niu stabilizatorów zawiesiny oraz na wprowadza¬ niu soli nieorganicznych do fazy wodnej celem wysolenia monomerów, znamienny tym, ze jako srodek porotwórczy wprowadza sie weglowodory alifatyczne od heptanu do nonadekanu lub mie¬ szaniny weglowodorów jak nafta, olej parafinowy, w ilosci 5% do 80% objetosciowych, najkorzyst¬ niej od 20% do 40% w stosunku do fazy mono¬ merycznej. CZYTELNIA Urzedu Patentowego Polskiej Bzeczyio^; e| Ly.wj W.D.Kart. C/1502/74, 115+15, A4 Cena 10 zl PL PL
PL15338672A 1972-02-09 1972-02-09 PL74885B2 (pl)