Prior art keywords
amount
functional additive
relation
weight
concretes
Prior art date
Application number
PL423586A
Other languages
English (en)
Other versions
PL238983B1 (pl
Inventor
Jacek Kosno
Bożena Twardochleb
Beata Tarczyńska
Halina MITKA
Michał Babiak
Original Assignee
Inst Ciezkiej Syntezy Organicznej Blachownia
Politechnika Poznanska
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Inst Ciezkiej Syntezy Organicznej Blachownia, Politechnika Poznanska filed Critical Inst Ciezkiej Syntezy Organicznej Blachownia
Priority to PL423586A priority Critical patent/PL238983B1/pl
Publication of PL423586A1 publication Critical patent/PL423586A1/pl
Publication of PL238983B1 publication Critical patent/PL238983B1/pl

Links

Landscapes

  • Curing Cements, Concrete, And Artificial Stone (AREA)

Abstract

Przedmiotem zgłoszenia jest sposób hydrofobizacji betonów, który polega na tym, że miesza się składniki betonu, dodaje się pył krzemionkowy w ilości 0,1 - 50,0% w stosunku do ilości cementu oraz dodatek funkcyjny w ilości 0,1 - 40,0% w stosunku do ilości cementu, zawierający glikolan diamidoaminy w ilości 0,1 - 100% w stosunku do sumy masy dodatku funkcyjnego, hydroksypiwalan diamidoaminy w ilości 0,1 - 100% w stosunku do sumy masy dodatku funkcyjnego i mleczan diamidoaminy w ilości 0,1 - 99,9% w stosunku do masy dodatku funkcyjnego, przy czym pył krzemionkowy, oraz dodatek funkcyjny wprowadza się albo razem ze wszystkimi składnikami betonu albo do zaczynu cementowego.
PL423586A 2017-11-27 2017-11-27 Sposób hydrofobizacji betonów PL238983B1 (pl)

Priority Applications (1)

Application Number Priority Date Filing Date Title
PL423586A PL238983B1 (pl) 2017-11-27 2017-11-27 Sposób hydrofobizacji betonów

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
PL423586A PL238983B1 (pl) 2017-11-27 2017-11-27 Sposób hydrofobizacji betonów

Publications (2)

Publication Number Publication Date
PL423586A1 true PL423586A1 (pl) 2019-06-03
PL238983B1 PL238983B1 (pl) 2021-10-25

Family

ID=66649267

Family Applications (1)

Application Number Title Priority Date Filing Date
PL423586A PL238983B1 (pl) 2017-11-27 2017-11-27 Sposób hydrofobizacji betonów

Country Status (1)

Country Link
PL (1) PL238983B1 (pl)

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
PL202379B1 (pl) * 2002-12-23 2009-06-30 Inst Szk & Lstrok A Ceramiki M Sposób wytwarzania szczelnego betonu
CN103979883A (zh) * 2014-04-23 2014-08-13 中国海洋石油总公司 一种海洋油气管道修补用环氧砂浆及其制备方法

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
PL202379B1 (pl) * 2002-12-23 2009-06-30 Inst Szk & Lstrok A Ceramiki M Sposób wytwarzania szczelnego betonu
CN103979883A (zh) * 2014-04-23 2014-08-13 中国海洋石油总公司 一种海洋油气管道修补用环氧砂浆及其制备方法

Also Published As

Publication number Publication date
PL238983B1 (pl) 2021-10-25

Similar Documents

Publication Publication Date Title
MY182724A (en) Concrete materials with modified rheology, methods of making, and uses thereof
SG11201806649RA (en) Rapid-hardening mortar composition
GB2532158A (en) Novel cement composition for lost circulation application
MY176491A (en) Additive for improving homogeneity of epoxy resin and cement composites
MX2016005630A (es) Composiciones de parche cementicio y metodos.
JP2017502907A5 (pl)
PL423586A1 (pl) Sposób hydrofobizacji betonów
PL423591A1 (pl) Sposób hydrofobizacji betonów
PL423588A1 (pl) Sposób hydrofobizacji betonów
PL423589A1 (pl) Sposób hydrofobizacji betonów
PL423594A1 (pl) Sposób hydrofobizacji betonów
WO2016005610A8 (en) Compositions and methods for well cementing
WO2019068084A3 (en) Struvite-k/syngenite building compositions comprising silicate materials and building articles such as wallboards made therefrom
NZ759197A (en) Additive formulation for reduction or prevention of microbially induced corrosion in concrete or cementitious material
BR112021021240A2 (pt) Métodos para cimentar um poço de petróleo
PL423585A1 (pl) Beton hydrofobizowany
PL423587A1 (pl) Beton hydrofobizowany
PL423593A1 (pl) Beton hydrofobizowany
PL423590A1 (pl) Beton hydrofobizowany
PL423592A1 (pl) Beton hydrofobizowany
MX2018007873A (es) Panel cementoso de peso ligero que posee alta durabilidad.
FR2986523B1 (fr) Nouvelle chape a base de sulfate de calcium
PL409671A1 (pl) Autoklawizowany beton komórkowy oraz zastosowanie haloizytu jako dodatku do autoklawizowanego betonu komórkowego
RU2496737C1 (ru) Масса для производства фосфогипсовых плит (варианты)
PL425913A1 (pl) Sposób wytwarzania hydrofobizowanego pyłu perlitowego, zastosowanie hydrofobizowanego pyłu perlitowego