PL147597B1 - Method of obtaining a developing agent for positive radiosensitive coatings - Google Patents
Method of obtaining a developing agent for positive radiosensitive coatings Download PDFInfo
- Publication number
- PL147597B1 PL147597B1 PL26110786A PL26110786A PL147597B1 PL 147597 B1 PL147597 B1 PL 147597B1 PL 26110786 A PL26110786 A PL 26110786A PL 26110786 A PL26110786 A PL 26110786A PL 147597 B1 PL147597 B1 PL 147597B1
- Authority
- PL
- Poland
- Prior art keywords
- disodium
- sodium metasilicate
- trisodium phosphate
- developing agent
- coatings
- Prior art date
Links
Landscapes
- Paints Or Removers (AREA)
Claims (3)
- Zastrzezenia patentowe 1. * Sposób wytwarzania srodka wywolujecego dla pozytywowych powlok promienio¬ czulych polegajecy na rozpuszczeniu i wymieszaniu metakrzemianu sodu i fosforanu dwusodo¬ wego i/lub trójsodowego w wodzie, a nastepnie oddzieleniu osadu, znamienny tym, ze do wody uprzednio podgrzanej do temperatury 60-100°C, nastepnie schlodzonej do tempera¬ tury 10-40°C i nasyconej gazem obojetnym wprowadza sie katalityczne ilosci czwartorzedowych soli amoniowych i/lub wodorotlenków metali alkalicznych, po czym w otrzymanym roztworze rozpuszcza sie metakrzemian sodu i fosforan dwusodowy i/lub trójsodowy w sumarycznej ilosci do 3% wagowych w przeliczeniu na substancje stale, przy czym proces mieszania oraz oddziela¬ nia osadu prowadzi sie w atmosferze gazu obojetnego*
- 2. * Sposób wedlug zastrz*l, znamienny tym, ze stosunek wagowy meta¬ krzemianu sodu do fosforanu dwusodowego l/lub trójsodowego wynosi od 2s3 do 3t2*
- 3. * Sposób wedlug zastrz.l, znamienny tym, ze czwartorzedowe sole amoniowe i/lub wodorotlenki metali alkalicznych dodaje sie w ilosci 0,0001 - 1% wagowych* Pracownia Poligraficzna UP PRL. Naklad 100 egz. Cena 400 zl PL