PL102499B1 - A VOLATILE FLUX FOR BRAZING METALS BY GASEOUS BLOWPIPES ALSO A METHOD OF PRODUCING VOLATILE FLUX FOR BRAZING METALS BY GASEOUS BLOWPIPES - Google Patents

A VOLATILE FLUX FOR BRAZING METALS BY GASEOUS BLOWPIPES ALSO A METHOD OF PRODUCING VOLATILE FLUX FOR BRAZING METALS BY GASEOUS BLOWPIPES Download PDF

Info

Publication number
PL102499B1
PL102499B1 PL18942276A PL18942276A PL102499B1 PL 102499 B1 PL102499 B1 PL 102499B1 PL 18942276 A PL18942276 A PL 18942276A PL 18942276 A PL18942276 A PL 18942276A PL 102499 B1 PL102499 B1 PL 102499B1
Authority
PL
Poland
Prior art keywords
flux
blowpipes
gaseous
brazing metals
volatile flux
Prior art date
Application number
PL18942276A
Other languages
Polish (pl)
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to PL18942276A priority Critical patent/PL102499B1/en
Publication of PL102499B1 publication Critical patent/PL102499B1/en

Description

Przedmiotem wynalazku jest topnik w postaci plynnej oraz sposób jego wytwarzania do twardego lutowania palnikami gazowymi. Topnik dozowany jest do srefy lu¬ towania za pomoca gazu palnego, zasilajacego palnik gazowy.The subject of the invention is a liquid flux and a method of producing it for brazing gas burners. The flux is dosed to the sphere of the barrel burner feeding with fuel gas gas.

Ujemna ceche stosowanych dotychczas topników do twardego lutowania stanowi charakterystyczna szklista powloka zuzla potopnikowego, trwale przylegajacego do lutowiny i jej poboczy. Zuzel potopnikowy z reguly nie rozpuszcza sie w wodzie i jest bardzo trudny do usuniecia "tak na drodze mechanicznej jak i chemicznej, a w wiekszosci przypadków musi byc usuwany ze wzgledu na zadana antykorozyjnosc i estetyke wyrobu, nakladanie powlok galwanicznych, lakierniczych itp. W konsekwencji wyste¬ puje koniecznosc stosowania niezwykle pracochlonnego Tecznego odbijania lub szlifowania zuzla, przy czym usu¬ niecie go z trudno dostepnych miejsc jest czesto w ogóle niemozliwe.The negative characteristics of the fluxes used so far do brazing is a characteristic glassy the coating of the post-flux tube, permanently adhering to solder and its edges. As a rule, Zuzel Potopnikowy does not dissolves in water and is very difficult to remove "both mechanically and chemically, and mostly cases must be deleted because of the requested anticorrosion and product aesthetics, application of coatings electroplating, varnishing etc. As a consequence, there were there is a necessity to use an extremely labor-intensive one Effectively reflect or grind the scrap, and remove it It is often removed from hard-to-reach places at all impossible.

Celem wynalazku jest opracowanie topnika, który nie pozostawialby zuzla na polutowanych polaczeniach i elimi¬ nowalby tym samym trudnosci z jego usuwaniem.The object of the invention is to provide a flux that does not it would leave badges on soldered connections and elimi it would have no problem with removing it.

Cel ten osiagnieto opierajac sklad chemiczny topnika na alkoholowym roztworze boranu trójmetylowego z dodat¬ kami stabilizatora oraz aktywizatora, których wprowadzenie do topnika wymaga odpowiedniej technologii laczenia surowców.This goal was achieved by basing the chemical composition of the flux on an alcoholic solution of trimethyl borate with the addition of kami stabilizer and activator, which introduction to the flux requires an appropriate joining technology raw materials.

Topnik zawiera wagowo: boran trójmetylowy 30 do 70%, •alkohol metylowy 25 do 64%, glikol etylenowy 5 do 8%, -wode do 0,90% oraz fluorek kwasny z grupy potasowców 4o0,07%.The flux contains by weight: trimethyl borate 30 to 70%, • methyl alcohol 25 to 64%, ethylene glycol 5 to 8%, - water up to 0.90% and acid fluoride from the group of potash 4o0.07%.

Przykladowy sklad topnika w przeliczeniu na surowce wyjsciowe moze byc nastepujacy: boran trójmetylowy — 620 ml alkohol metylowy — 310 ml glikol etylenowy — 62 ml woda — 8 ml fluorek kwasny z grupy potasowców — 0,6 g Zaleznie od potrzeb mozna uzyskac szeroka zmiane wlasnosci lutowniczych topnika, a w szczególnosci jego aktywnosc poprzez dobór odpowiedniego fluorku kwasnego z grupy potasowców oraz zmiane zawartosci boranu trój¬ metylowego.An example of the composition of the flux in terms of raw materials the output may be as follows: trimethyl borate - 620 ml methyl alcohol - 310 ml ethylene glycol - 62 ml water - 8 ml acid fluoride from the group Potashites - 0.6 g Depending on your needs, you can get a wide change the soldering properties of the flux, especially its activity by selecting the appropriate acid fluoride from the group of potassium and changes in the content of tris borate methyl.

Topnik otrzymuje sie mieszajac dokladnie rozdrobniony i rozpuszczony w wodzie fluorek kwasny z alkoholem metylowym i nastepnie dodajac boran trójmetylowy oraz glikol etylenowy. Topnik ma postac plynna i wyróznia sie okreslona lotnoscia w temperaturach otoczenia w wyniku czego jego dozowanie w strefe lutowania odbywa sie bez bezposredniego udzialu lutowacza.The flux is obtained by mixing finely ground and acid fluoride dissolved in water with alcohol and then by adding trimethyl borate and ethylene glycol. The flux is in a liquid and distinctive form become determined aerobic at ambient temperatures as a result what its dosing in the soldering zone is done without direct involvement of the solder.

W procesie lutowania, nastepuje rozklad topnika na zwia¬ zki aktywne oczyszczajace laczone metale i spoiwo nie two¬ rzac przy tym zuzlowych pozostalosci. Uzyskane polaczenia lutowane cechuje wysoka jakosc oraz metaliczna czystosc hitowin i przyleglych powierzchni elementów, bedacych podczas lutowania pod dzialaniem plomienia gazowego zawierajacego topnik.In the brazing process, the flux is decomposed into a solid active detoxifying combined metals and non-forming binder throwing away the deadly remains. Connections obtained solder is characterized by high quality and metallic purity hitowin and adjacent surfaces of the elements being when soldering under the action of a gas flame containing flux.

W rezultacie zlacza lutowane lotnym topnikiem spelniaja 102 499102 499 .3 4 warunki techniczne nakladania pokryc lakierowanych lub H20 do 0,90% i fluorek kwasny z grupy potasowców da galwanicznych. 0,07%.As a result, the joints soldered with volatile flux do not work properly 102 499 102 499 .3 4 technical conditions for applying varnished coatings or H20 up to 0.90% and acid fluoride from the group of potashites galvanic. 0.07%.

Claims (1)

Zastrzezeniapatentowe ^ o *u *_ • * -i_ i ^ j ^ j ^ 2. Sposób wytwarzania topnika lotnego do twardegoPatent claims ^ o * u * _ • * -i_ i ^ j ^ j ^ 2. Method for producing volatile to hard flux 1. Topnik lotny do twardego lutowania metali palnikami 5 lutowania metali palnikami gazowymi, znamienny tym, gazowymi, znamienny tym, ze w przeliczeniu na surowce ze fluorek kwasny z grupy potasowców po dokladnym wyjsciowe zawiera wagowo: boran trójmetylowy B(OCH3)3 rozdrobnieniu i rozpuszczeniu w wodzie miesza sie z alko- — 30 do 70%, alkohol metylowy CH3OH — 25 do 64%5 holem metylowym, a nastepnie dodaje sie boran trójmetylo- glikol etylenowy HO • CH2 • CH3 • OH — 5 do 8%, woda wy oraz glikol etylenowy. LZG Z-d 3 zarm 21I2-TO, nakl. los + » egz. Cena 45 zl1. Volatile flux for brazing metals with burners for brazing metals with gas burners, characterized in that, based on the raw materials of acid fluoride from the potassium group, it contains exactly by weight: trimethyl borate B (OCH3) 3 by grinding and dissolving in water it is mixed with alcohol - 30 to 70%, methyl alcohol CH3OH - 25 to 64% 5 methyl alcohol, and then trimethyl borate ethylene glycol is added HO • CH2 • CH3 • OH - 5 to 8%, water and ethylene glycol. LZG Z-d 3 zarm 21I2-TO, nakl. ticket + »copies Price PLN 45
PL18942276A 1976-05-07 1976-05-07 A VOLATILE FLUX FOR BRAZING METALS BY GASEOUS BLOWPIPES ALSO A METHOD OF PRODUCING VOLATILE FLUX FOR BRAZING METALS BY GASEOUS BLOWPIPES PL102499B1 (en)